Search NASA⌕ Search

SEARCH · Search NASA

Results for “ionic conductivity”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,315 records · Page 73

Thermodynamic controls on the synthesis, structure and reactivity of materials for energy (Final Report)

The major objectives have been: a) to advance and use unique calorimetric capabilities to determine the energetics of oxide and other materials having possible energy applications, with an emphasis on new materials for batteries, fuel cells and solar energy conversion, b) to understand, in terms of both macroscopic energetics and microscopic structure and bonding, the interplay of defect chemistry, oxidation-reduction, and size effects at the bulk and nanoscale in determining materials properties. This project emphasizes mixed ionic-electronic conduction materials containing transition metals of variable valence, especially perovskites and lithium containing phases, with M = Mn, Fe, Co, Ni. The thermochemistry of new families of complex halide, chalcogenide, nitride and hybrid (organic-inorganic) perovskite materials were explored. The major and unique technique employed is high temperature oxide melt solution calorimetry, with careful attention given to materials synthesis and characterization. The thermochemical studies will be coupled with structural studies, especially to characterize order-disorder phenomena by in situ high temperature diffraction techniques.

14 SOLAR ENERGY↗

Machine Learning Thermodynamics And Kinetics of Defects For Accelerated Materials Discovery

Atomistic defects play a pivotal role in functional and structural materials’ performance across a myriad of technology applications. Quantitative prediction of the thermodynamics and kinetics of defect formation and migration, respectively, typically requires accurate but expensive first-principles approaches, such as density functional theory (DFT). Their computational expense limits the throughput needed to perform high-throughput materials discovery/screening exercises or to perform materials modeling tasks relying on extensive sampling techniques. Therefore, in this Sandia National Laboratories Laboratory Directed Research and Development (LDRD) project (Project #229366), we developed a variety of machine learning techniques, trained on density functional theory calculations, to accelerate the discovery and modeling of materials in which vacancy and interstitial defects primarily dictate material performance. These include applications such as metal oxides for water-splitting or mixed ionic-electronic conduction, metal hydrides for hydrogen storage, and transition metal dichalcogenides for electronics, and the approaches developed herein can further be applied to many other domains that similarly depend on materials’ thermodynamic and kinetic defect properties for their desired functionality.

36 MATERIALS SCIENCE↗

The Electrochemical Properties of Sr(Ti,Fe)O 3-δ for Anodes in Solid Oxide Fuel Cells

Reduction-stable mixed ionic and electronic conductors such as Sr(Ti,Fe)O 3-δ (STF) are promising materials for application in anodes of solid oxide fuel cells. The defect chemistry of STF and its properties as solid oxide fuel cell (SOFC) cathode have been studied thoroughly, while mechanistic investigations of its electrochemical properties as SOFC anode material are still scarce. In this study, thin film model electrodes of STF with 30% and 70% Fe content were investigated in H 2 +H 2 O atmosphere by electrochemical impedance spectroscopy. Lithographically patterned thin film Pt current collectors were applied on top or beneath the STF thin films to compensate for the low electronic conductivity under reducing conditions. Oxygen exchange resistances, electronic and ionic conductivities and chemical capacitances were quantified and discussed in a defect chemical model. Increasing Fe content increases the electro-catalytic activity of the STF surface as well as the electronic and ionic conductivity. Current collectors on top also increase the electrochemical activity due to a highly active Pt-atmosphere-STF triple phase boundary. Furthermore, the electrochemical activity depends decisively on the H 2 :H 2 O mixing ratio and the polarization. Lastly, Fe 0 nanoparticles may evolve on the surface in hydrogen rich atmospheres and increase the hydrogen adsorption rate.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Materials and Approaches for Mitigation of SOFC Cathode Degradation in SOFC Power Systems

Perovskites such as doped lanthanum manganite and cobaltite have been used successfully as a cathode material in SOFC power systems operating between 700-1000°C. The electrodes, however, remain prone to degradation in presence of Cr containing gas atmosphere under systems operating conditions. Cathode in SOFCs is considered as one of the largest contributors of electrochemical performance degradations, leading to significant increase in ohmic and non-ohmic losses as well as interfacial compound formation. These degradations are mostly irreversible due to permanent changes to chemical and morphological alterations in the electrodes, resulting in the blockage of triple phase boundary (TPB) sites and decrease in oxygen reduction reactions (ORR). Fundamental mechanistic understanding has been developed to elucidate the reaction pathways of electrode poisoning in electronically conducting electrodes (LSM) as well as mixed ionic and electronically conducting electrodes (LSCF). The overall goal of this program has been identification and development of cost effective solutions to mitigate electrode degradations under “real world” systems operating conditions. The overall technological innovations and impact from this work are: The research provides an understanding of the degradation mechanism and cost-effective approaches for implementation in SOFC systems; Develop mitigation processes utilizing low cost getters using conventional synthesis and fabrication route; Develop tailored high surface area powders and coatings for high Cr capture capacity under systems operating conditions; >Developed computational models to understand mechanistic behavior; Experimentally measure rate of Cr evaporation from chromia and alumina forming alloys under SOFC operating conditions; Developed conditions to minimize Cr evaporation from balance-of-plant alloys; This innovation will support the development of getter platform to capture both intrinsic and extrinsic impurities present in air; and, Applications under wide operating temperature range (500-900°C) as well for wide high-temperature electrochemical systems (SOFC, SOEC, and OTM). The work has been successfully developed, validated experimentally and implemented. Successful technology transfer of this knowledge with industrial partners has been accomplished and the getters have been independently tested and validated under their systems operating conditions. The innovation will also find application in related high temperature electrochemical systems such as OTM and SOEC for the prevention of Cr assisted performance degradation. The proposed approach for Cr capture can also be applied to oxy-combustion and other advanced combustion techniques for the reduction of Cr vapor in the exhaust gas stream. This fundamental knowledge gained also has led to the path forward for developing advanced getters for capturing more than one contaminant in air.

01 COAL, LIGNITE, AND PEAT↗

Monitoring of Ionic Silver Biocide with Capacitively-Coupled Contactless Conductivity Detection (C4D)

Monitoring of biocide dosing in spacecraft potable water systems is desirable to ensure dosing system operation and resultant microbial control. Electrolytic conductivity is linearly related to the concentration ionic silver (Ag+, the baseline biocide for future NASA missions) chemically dosed into highly purified water, and could serve as a proxy measurement. Traditional conductivity cells rely on immersed metal or graphite electrodes, which may potentially be subject to significant current-induced or auto-galvanic deposition of Ag+. Furthermore, oxide fouling may potentially induce measurement errors. Capacitively-coupled contactless conductivity detection (C4D) is a promising alternative. C4D uses electrodes placed outside an inert, non-conductive flow path, potentially mitigating such problems. We identified and purchased a commercial C4D system with claimed performance (conductivity range: 20 nS/cm to 4 µS/cm) appropriate for this application. We characterized the instrument’s performance with conductivity standards and Ag+ solutions. We began investigations considering practical and long-term detector operation, including potential current-induced deposition of conductive deposits at the tubing wall. In addition, we designed a side-stream flow system to provide liquid flow through the narrow tubing (1/16” outer diameter) required by the detector and characterized the performance of the combined C4D detector/flow system. Finally, we completed theoretical modeling of expected conductivity change with multiple dosing techniques and water chemistries.

Lance Dean Delzeit↗

Impact of Ionic Liquid on Lithium Ion Battery with a Solid Poly(Ionic Liquid) Pentablock Terpolymer as Electrolyte and Separator

In this work, a ternary blend solid polymer electrolyte (SPE) consisting of a poly(ionic liquid) (PIL) multiblock polymer, lithium salt, and ionic liquid (IL) was investigated with the goal of understanding the influence of IL concentration on ion transport mechanisms and electrochemical stability. The physical, transport, mechanical, morphological, and electrochemical properties of the ternary blend SPE were systematically investigated as a function of IL concentration (r = [IL]/[PIL] mole ratio between 0.1 and 0.7). The results indicate that with increasing IL concentration, the continuous conductive domain increases along with the polymer chain segmental mobility, as well as facilitate ionic conductivity, while the mechanical modulus exhibits a percolation threshold (from 52.17 MPa to 0.55 MPa at r = 0.2 to 0.3). Surprisingly, at higher IL concentrations, there is a reduction in the lithium cation mobility (i.e., 9.3 × 10-12 m2 s-1 versus 3.8 × 10-12 m2 s-1 for r = 0.2 versus r = 0.5, respectively) as evidenced by pulsed-field gradient nuclear magnetic resonance (PFG-NMR), which coincides with an increased overpotential (i.e., 50 mV versus 150 mV for r = 0.2 versus r = 0.5, respectively) evidenced by lithium metal stripping and plating. This work provides valuable insights into the impact of IL on lithium ion conducting PIL block polymers, which may enable the design of new SPEs with both high ionic conductivity and improved stability for the future lithium ion batteries.

Chen, Tzu-Ling↗

Emergence of Rapid Oxygen Surface Exchange Kinetics during in Situ Crystallization of Mixed Conducting Thin Film Oxides

The oxygen surface exchange kinetics of mixed ionic and electronic conducting oxides (MIECs) play a vital role in the efficiency of intermediate-to-high-temperature electrochemical devices. While there is increasing interest in low-temperature preparation of MIEC thin films, the impact of the resultant varied degrees of crystallinity on the surface exchange kinetics has not been widely investigated. Herein, we probe the effect of crystallization on oxygen surface exchange kinetics in situ, by applying an optical transmission relaxation (OTR) approach during annealing of amorphous films. OTR enables contact-free, in situ, and continuous quantification of the oxygen surface exchange coefficient ( k chem ); we previously applied it to Pr x Ce 1– x O 2-δ and SrTi 1– x Fe x O 3-δ thin films. In this work, the OTR approach was successfully extended to other mixed conducting thin film compositions for the first time (i.e., perovskite SrTi 0.65 Co 0.35 O 3-δ and Ruddlesden–Popper Sr 2 Ti 0.65 Fe 0.35 O 4±δ ), as well as to Pr 0.1 Ce 0.9 O 2-δ , enabling quantification of the k chem of their native surfaces and comparison of the behavior of films with different final crystal structures. All thin films were prepared by pulsed laser deposition at 25 or 700–800 °C and subject to subsequent thermal treatments with simultaneous OTR monitoring of k chem . The surface roughness, grain size, and crystallinity were evaluated by scanning probe microscopy, X-ray diffraction, scanning electron microscopy, and transmission electron microscopy. Fluorite Pr 0.1 Ce 0.9 O 2-δ films grown at 25 °C did not exhibit an increase in k chem after annealing, as they were already crystalline as grown at 25 °C. For all other compositions, OTR enabled in situ observation of both the crystallization process and the emergence of rapid surface exchange kinetics immediately upon crystallization. Perovskite SrTi 0.65 Co 0.35 O 3-δ and Ruddlesden–Popper Sr 2 Ti 0.65 Fe 0.35 O 4±δ thin films grown at 25 °C exhibited at least 1–2 orders of magnitude enhanced k chem after annealing compared with highly crystalline thin films grown at 800 °C, indicating the benefits of in situ crystallization.

36 MATERIALS SCIENCE↗

Degradation of Anion Exchange Membranes by Cation Elimination: Impact on Water Uptake, Nanostructure, and Ionic Mobility

Anion exchange membranes (AEMs) are an attractive platform for fuel cell and electrolysis technologies since they enable the use of cheaper, nonplatinum group metal electrodes and components. However, the widespread adoption of AEM-based devices is limited by chemical degradation of the AEM in the highly alkaline medium of operation. Experimental studies report three major pathways of degradation, including substitution (S N 2), elimination (E2), and backbone cleavage. The decline in membrane performance is likely due to a cumulative effect of several pathways, which has proven to be difficult to disentangle through experiments. Here we use coarse-grained molecular simulations to isolate the impact of E2 degradation, where cationic sites are replaced by an alkene group, on AEM water uptake, nanoscale morphology, structure of the ion-conducting channels, water mobility, and ionic conductivity. Our studies focus on the well-studied model AEM polyphenylene oxide with tetraalkylammonium cationic sites (PPO-TMA). We find that about half of the hydrophobic groups resulting from the degradation retract into the hydrophobic domains of the membrane. The reduction in ion exchange capacity (IEC) and the hydrophobicity of the alkene groups decrease both the equilibrium water uptake (%WU) and the number of water molecules per cation (λ) of the membrane. Interestingly, the evolution of λ with the IEC seems to follow that of undegraded PPO-TMA membranes. Additionally, we ascribe this to the similarity between the structure of the degraded monomer and the neutral one in the polymer. We conclude that most of the performance losses originate in the lower hydration of the degraded membrane.

36 MATERIALS SCIENCE↗

A Comparative Study of Imidazolium-Based Ionic Liquid-Single-Walled Carbon Nanotube Composites with Enhanced Conductivity Properties for Supercapacitor Applications

Mixtures of ionic liquids (ILs) containing single-walled carbon nanotubes (SWCNTs) were prepared and characterized to obtain electrolytes with optimized transport properties for use in energy storage devices such as supercapacitors. Imidazolium ILs bearing cations with side chains of different functionality coupled with bis(trifluoromethylsulfonyl)amide (NTf 2- ) or bis(fluorosulfonyl)-amide (FSA-) anions, were used in mixtures containing up to 5 wt% SWCNTs. At and above 2 wt% nanotube loading, the mixtures exhibited higher conductivities than the pure ILs, in spite of the extremely high viscosities. Loadings of 5 wt% produced very high conductivities, and studies of the temperature dependence indicated a change in the charge transport mechanism between 2 and 5 wt% loading. At 5 wt% loading, the highest conductivities (up to 540 mS/cm at 25 °C) were obtained for the ILs containing the NTf 2- anion. Overall, these results can significantly contribute to the development of improved energy storage devices.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thermally sensitive ionic redox transistor

A thermally sensitive ionic redox transistor comprises a solid channel, a solid reservoir layer, and a solid electrolyte layer disposed between the channel and the reservoir layer. A conductance of the channel is varied by changing the concentration of ions such as oxygen vacancies in the channel layer. Ionic conductivity of the gate, electrolyte, and channel layers increase with increasing temperature. Ion or vacancy transport between the channel and the reservoir layer across the electrolyte layer occurs in response to applying a voltage between the channel and the reservoir layer when the device is heated to an elevated temperature. When the device is cooled below the elevated temperature, the ions are trapped in one or more of the layers because the materials lose their ionic conductivity. A state of the redox transistor can be read by measuring the conductance of the channel.

97 MATHEMATICS AND COMPUTING↗

Thermodynamics, local structure, and transport of protons in triple-conducing oxide, BaCo 0.4 Fe 0.4 Zr 0.1 Y 0.1 O 3-δ (BCFZY4411)

Triple-conducting oxides (TCOs) are an emerging class of mixed ionic and electronically conducting materials that show great promise for oxygen reduction/oxygen evolution (ORR/OER) electrocatalysis—primarily in high-temperature ceramic electrochemical cells— but also in aqueous alkaline environments. Their high activity is attributed, at least in part, to their ability to incorporate and transport three mobile charge carriers: protons, oxygen vacancies, and electron-holes Despite their promise, fundamental studies of TCOs are challenging, as transport dynamics from three charge carriers cannot be fully disentangled via traditional electrical measurement techniques. Characterizing proton dynamics in TCOs is particularly difficult as protons are generally the minority carrier, and their conduction response is typically obscured by the oxygen vacancies and electron holes. Here, we demonstrate successful isolation of the proton behavior in an archetypal TCO, BaCo 0.4 Fe 0.4 Zr 0.1 Y 0.1 O 3-δ (BCFZY4411), using a combination of non-electrical techniques. We determine proton uptake and oxygen non-stoichiometry (δ) using thermogravimetric analysis (TGA). X-ray absorption near edge structure (XANES) and neutron diffraction (ND) are used to validate the oxidation state of Co and the δ values obtained through TGA. We apply 1H solid-state magic-angle-spinning (MAS) nuclear magnetic resonance (NMR) to provide insights into local structure, dynamics, and proton kinetics. Finally, the proton transport properties are further quantified using tracer isotope exchange with time-of-flight secondary ion mass spectrometry (ToF-SIMS). Despite the very low proton concentrations in BCFZY4411 (<0.2% under most conditions), our analysis suggests that the oxygen Manuscript File Click here to view linked References 2 reduction and evolution reactions are nevertheless limited by the oxygen ion kinetics (e.g., oxygen surface exchange) rather than the proton kinetics at the reduced operating temperatures (<500 °C) that are targeted for electrochemical cell applications. These findings provide a comprehensive understanding of proton behavior in BCFZY4411 and pave the way for advancing the fundamental study of TCOs.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Percolated Ionic Aggregate Morphologies and Decoupled Ion Transport in Precise Sulfonated Polymers Synthesized by Ring-Opening Metathesis Polymerization

Here, we describe a set of precise single-ion conducting polymers that form self-assembled percolated ionic aggregates in glassy polymer matrices and have decoupled transport of metal cations. These precise single-ion conductors (SICs), synthesized by a scalable ring-opening metathesis polymerization, consist of a polyethylene backbone with a sulfonated phenyl group pendant on every fifth carbon and are fully neutralized by a counterion X + (Li + , Na + , or Cs + ). Experimental X-ray scattering measurements and fully atomistic molecular dynamics (MD) simulations are in good agreement. The MD simulations show that the ionic groups nanophase separate from the polymer backbone to form percolating ionic aggregates. Using graph theory, we find that within the Li + - and Na + -neutralized polymers the percolated aggregates exhibit planar and ribbon-like configurations at intermediate length scales, while the percolated aggregates within the Cs + -neutralized polymers are more isotropic. Electrical impedance spectroscopy measurements show that the ionic conductivities exhibit Arrhenius behavior, with conductivities of 10 –7 to 10 –6 S/cm at 180 °C. In the MD simulations, the cations move between sulfonate groups in the percolated aggregates, larger ions travel further, and overall cations travel further than the polymer backbones, indicating a decoupled ion-transport mechanism. Thus, the percolated ionic aggregates in these polymers can serve as pathways to facilitate decoupled ion motion through a glassy polymer matrix.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Defect Chemistry and Hydrogen Transport in La/Sr-Based Oxyhydrides

Oxyhydrides in the series La 2 – y Sr y LiH 1 + y O 3 – y are attractive materials for solid-state hydride electrolytes. However, their chemical stability is poor, and thus far only La 2 LiHO 3 (y = 0) has been demonstrated in a working fuel cell. Using a first-principles approach to study defect chemistry and stability, we find that La 2 LiHO 3 can be stabilized over a range of H-rich, O-poor chemical conditions, while Sr 2 LiH 3 O has low stability. Here, defects are critical for ionic transport and for stability, particularly in Sr 2 LiH 3 O, in which anion antisites and H vacancies readily form. In fact, we show that the ground-state structure of Sr 2 LiH 3 O is inherently disordered. La 2 LiHO 3 has low conductivity, which we connect to the high formation energy of defects such as VO and OH that are necessary for hydride conduction. When Sr 2 LiH 3 O is grown under carefully selected conditions, V H + defects can be made prevalent; these defects give rise to much higher ionic conductivity than can be obtained in La 2 LiHO 3 . In general, we show that the choice of synthesis conditions is vital when seeking to optimize the stability and ionic conductivity of these oxyhydrides, thereby tailoring them for use in solid-state hydrogen fuel cells.