Search NASA⌕ Search

SEARCH · Search NASA

Results for “Carbides”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,333 records · Page 74

Melt infiltration of silicon carbide compacts. I - Study of infiltration dynamics

Countergravity, pressure-assisted infiltration with a 2014 Al alloy of suitably tamped porous compacts of platelet shaped single crystals of alpha (hexagonal) silicon carbide was used to measure particulate wettability and infiltration kinetics under dynamic conditions relevant to pressure casting of composites. A threshold pressure P(th) for ingression of the infiltrant was identified based on the experimental penetration length versus pressure profiles for a range of experimental variables which included infiltration pressure, infiltration time, SiC size and SiC surface chemistry. The results showed that P(th) decreased whereas the penetration length increased with increasing SiC size and infiltration time. Cu-coated SiC led to lower P(th) and larger penetration lengths compared to uncoated SiC under identical conditions. These observations have been discussed in the light of theoretical models of infiltration and the kinetics of wetting.

Asthana, Rajiv↗

CVD of silicon carbide on structural fibers - Microstructure and composition

Structural fibers are currently being considered as reinforcements for intermetallic and ceramic materials. Some of these fibers, however, are easily degraded in a high temperature oxidative environment. Therefore, coatings are needed to protect the fibers from environmental attack. Silicon carbide (SiC) was chemically vapor deposited (CVD) on Textron's SCS6 fibers. Fiber temperatures ranging from 1350 to 1500 C were studied. Silane (SiH4) and propane (C2H8) were used for the source gases and different concentrations of these source gases were studied. Deposition rates were determined for each group of fibers at different temperatures. Less variation in deposition rates were observed for the dilute source gas experiments than the concentrated source gas experiments. A careful analysis was performed on the stoichiometry of the CVD SiC coating using electron microprobe. Microstructures for the different conditions were compared. At 1350 C, the microstructures were similar; however, at higher temperatures, the microstructure for the more concentrated source gas group were porous and columnar in comparison to the cross sections taken from the same area for the dilute source gas group.

Veitch, Lisa C.↗

Progress in silicon carbide semiconductor technology

Silicon carbide semiconductor technology has been advancing rapidly over the last several years. Advances have been made in boule growth, thin film growth, and device fabrication. This paper wi11 review reasons for the renewed interest in SiC, and will review recent developments in both crystal growth and device fabrication.

Powell, J. A.↗

Theoretical considerations for Reaction-Formed Silicon Carbide (RFSC) formation by molten silicon infiltration into slurry-derived preforms

For reaction-formed silicon carbide (RFSC) ceramics produced by silicon melt infiltration of porous carbon preforms, equations are developed to relate the amount of residual silicon to the initial carbon density. Also, for a slurry derived preform containing both carbon and silicon powder, equations are derived which relate the amount of residual silicon in the RFSC to the relative density of the carbon in the preform and to the amount of silicon powder added to the slurry. For a porous carbon preform that does not have enough porosity to prevent choking-off of the silicon infiltration, these results show that complete silicon infiltration can occur by adding silicon powder to the slurry mixture used to produce these preforms.

Behrendt, D. R.↗

Deposition of tantalum carbide coatings on graphite by laser interactions

Graphite surfaces can be hardened and protected from erosion by hydrogen at high temperatures by refractory metal carbide coatings, which are usually prepared by chemical vapor deposition (CVD) or chemical vapor reaction (CVR) methods. These techniques rely on heating the substrate to a temperature where a volatile metal halide decomposes and reacts with either a hydrocarbon gas or with carbon from the substrate. For CVR techniques, deposition temperatures must be in excess of 2000 C in order to achieve favorable deposition kinetics. In an effort to lower the bulk substrate deposition temperature, the use of laser interactions with both the substrate and the metal halide deposition gas has been employed. Initial testing involved the use of a CO2 laser to heat the surface of a graphite substrate and a KrF excimer laser to accomplish a photodecomposition of TaCl5 gas near the substrate. The results of preliminary experiments using these techniques are described.

Veligdan, James↗

Interstellar grains in primitive meteorites - Diamond, silicon carbide, and graphite

Primitive meteorites contain a few parts per million (ppm) of pristine interstellar grains that provide information on nuclear and chemical processes in stars. Their interstellar origin is proven by highly anomalous isotopic ratios, varying more than 1000-fold for elements such as C and N. Most grains isolated thus far are stable only under highly reducing conditions (C/O greater than 1), and apparently are 'stardust' formed in stellar atmospheres. Microdiamonds, of median size about 10 A, are most abundant (about 400-1800 ppm) but least understood. They contain anomalous noble gases including Xe-HL, which shows the signature of the r- and p-processes. Silicon carbide, of grain size 0.2-10 microns and abundance about 6 ppm, shows the signature of the s-process and apparently comes mainly from red giant carbon (AGB) stars of 1-3 solar masses. Some grains appear to be not less than 10 exp 9 a older than the solar system. Graphite spherules of grain size 0.8-7 microns and abundance less than 2 ppm contain highly anomalous C and noble gases, as well as large amounts of fossil Mg-26 from the decay of extinct Al-26. They seem to come from at least three sources, probably AGB stars, novae, and Wolf-Rayet stars.

Anders, Edward↗

Electrical characterization of 6H crystalline silicon carbide

Crystalline silicon carbide (SiC) substrates and epilayers, undoped as well as n- and p-doped, have been electrically characterized by performing Hall effect and resistivity measurements (van der Pauw) over the temperature range of approximately 85 K to 650 K (200 K to 500 K for p-type sample). By fitting the measured temperature dependent carrier concentration data to the single activation energy theoretical model: (1) the activation energy for the nitrogen donor ranged from 0.078 eV to 0.101 eV for a doping concentration range of 10(exp 17) cm(exp -3) to 10(exp 18) cm(exp -3) and (2) the activation energy for the aluminum acceptor was 0.252 eV for a doping concentration of 4.6 x 10(exp 18) cm(exp -3). By fitting the measured temperature dependent carrier concentration data to the double activation energy level theoretical model for the nitrogen donor: (1) the activation energy for the hexagonal site was 0.056 eV and 0.093 eV corresponding to doping concentrations of 3.33 x 10 (exp 17) cm(exp -3) and 1.6 x 10(exp 18) cm(exp -3) and (2) the activation energy for the cubic site was 0.113 and 0.126 eV corresponding to doping concentrations of 4.2 x 10(exp 17) cm(exp -3) and 5.4 x 10(exp 18) cm(exp -3).

Lempner, Stephen E.↗

Off axis loading of silicon carbide fibers in a titanium aluminide matrix

Silicon carbide SCS-6 fibers in a Ti24A1 + 11Nb matrix were subjected to off axis loading in a 'thin-slice' pushout test, resulting in various combinations of shear, radial compression, and tension along the fibers as a function of orientation angle. The load necessary for debonding decreased as the orientation angle increased, whereas the average frictional sliding stress after 60 s of sliding remained relatively constant for orientation angles less than 30 deg. Analyses of the specimen bending stresses and of the contact stresses by finite element modeling and thin plate theory are presented.

Kennefick, C. M.↗

Power MOSFETs Formed In Silicon Carbide

High-performance power metal/oxide/semiconductor field-effect transistors (MOSFETs) fabricated in silicon carbide. Devices offer potential advantages over silicon-based MOSFETs, including lower "on" - state resistances at same rated voltages, ability to operate at higher temperatures, and higher thermal conductivity. Also more resistant to damage by ionizing radiation, an advantage for switching appications in nuclear facilities.

Palmour, John W.↗

Photoelectrochemical etching of silicon carbide (SiC) and its characterization

Silicon carbide (SiC) is an attractive semiconductor material for high speed, high density, and high temperature device applications due to its wide bandgap (2.2-3.2 eV), high thermal conductivity, and high breakdown electric field (4 x 10(exp 6) V/cm). An instrumental process in the fabrication of semiconductor devices is the ability to etch in a highly controlled and selective manner for direct patterning techniques. A novel technique in etching using electrochemistry is described. This procedure involves the ultraviolet (UV) lamp-assisted photoelectrochemical etching of n-type 3C- and 6H-SiC to enhance the processing capability of device structures in SiC. While under UV illumination, the samples are anodically biased in an HF based aqueous solution since SiC has photoconductive properties. In order for this method to be effective, the UV light must be able to enhance the production of holes in the SiC during the etching process thus providing larger currents with light from the photocurrents generated than those currents with no light. Otherwise dark methods would be used as in the case of p-type 3C-SiC. Experiments have shown that the I/V characteristics of the SiC-electrolyte interface reveal a minimum etch voltage of 3 V and 4 V for n- and p-type 3C-SiC, respectively. Hence it is possible for etch-stops to occur. Etch rates calculated have been as high as 0.67 micrometer/min for p-type, 1.4 micrometer/min for n-type, and 1.1 micrometer/min for pn layer. On n-type 3C- SiC, an oxide formation is present where after etching a yellowish layer corresponds to a low Si/C ratio and a white layer corresponds to a high Si/C ratio. P-type 3C-SiC shows a grayish layer. Additionally, n-type 6H-SiC shows a brown layer with a minimum etch voltage of 3 V.

Collins, D. M.↗

Silicon Carbide-Based Hydrogen and Hydrocarbon Gas Detection

Hydrogen and hydrocarbon detection in aeronautical applications is important for reasons of safety and emissions control. The use of silicon carbide as a semiconductor in a metal-semiconductor or metal-insulator-semiconductor structure opens opportunities to measure hydrogen and hydrocarbons in high temperature environments beyond the capabilities of silicon-based devices. The purpose of this paper is to explore the response and stability of Pd-SiC Schottky diodes as gas sensors in the temperature range from 100 to 400 C. The effect of heat treating on the diode properties as measured at 100 C is explored. Subsequent operation at 400 C demonstrates the diodes' sensitivity to hydrogen and hydrocarbons. It is concluded that the Pd-SiC Schottky diode has potential as a hydrogen and hydrocarbon sensor over a wide range of temperatures but further studies are necessary to determine the diodes' long term stability.

Hunter, Gary W.↗

Silicon carbide sewing thread

Composite flexible multilayer insulation systems (MLI) were evaluated for thermal performance and compared with currently used fibrous silica (baseline) insulation system. The systems described are multilayer insulations consisting of alternating layers of metal foil and scrim ceramic cloth or vacuum metallized polymeric films quilted together using ceramic thread. A silicon carbide thread for use in the quilting and the method of making it are also described. These systems provide lightweight thermal insulation for a variety of uses, particularly on the surface of aerospace vehicles subject to very high temperatures during flight.

Sawko, Paul M.↗

Elastic Moduli and Damping of Vibrational Modes of Aluminum/Silicon Carbide Composite Beams

Elastic and shear moduli were determined for two aluminum matrix composites containing 20 and 40 volume percent discontinuous silicon carbide, respectively, using transverse, longitudinal, and torsional vibrational modes of specimens prepared as thin beams. These moduli are consistent with those determined from stress-strain measurements. The damping factors for these modes were also determined. Thermal properties are used to show that part of the damping of transverse modes is caused by the transverse thermal currents discussed by C. Zener (thermo-elastic damping); this damping is frequency-dependent with a maximum damping factor of approximately 0.002. The remaining damping is frequency-independent, and has roughly similar values in transverse, longitudinal, and torsional modes: approximately 0.0001.

Leidecker, Henning↗

Silicon Carbide Transistor For Detecting Hydrocarbon Gases

Proposed silicon carbide variable-potential insulated-gate field-effect transistor specially designed for use in measuring concentrations of hydrocarbon gases. Devices like this prove useful numerous automotive, industrial, aeronautical, and environmental monitoring applications.

Shields, Virgil B.↗

Radial variation of elastic properties of SCS-6 silicon carbide fiber

The upper and lower bounds of the bulk, shear, and Young's moduli are calculated point-by-point along the radius of SCS-6 silicon carbide fibers using the Hashin-Shtrikman equations from considerations of the Auger spectra along the fiber radius. The calculated values are in agreement with measurements of the average Young modulus obtained over relatively large radial regions of the fiber using scanning acoustic microscopy (SAM). The validity of the Hashin-Shtrikman bounds calculations is enhanced by the agreement found between experimental SAM V(z) curves for fixed z along the fiber radius and the theoretical bounds of such curves obtained from the bounds of the calculated bulk and shear moduli.

Sathish, Shamachary↗

High temperature brush seal tuft testing of metallic bristles versus chrome carbide

The tribology of brush seals is of considerable interest to turbine engine designers because bristle wear continues to limit long term seal performance and life. To provide better materials characterization and foster the development of improved seals, NASA Lewis has developed a brush seal tuft tester. In this test, a 'paintbrush' sample tuft is loaded under constant contact pressure against the outside diameter of a rotating journal. With this configuration a direct measurement of load and friction is made. Accurate wear rate measurements are possible due to the known contact pressure. Previously reported baseline research using this facility showed good data repeatability and wear morphology similar to published seal data. This paper extends and expands the database for candidate brush seal materials. A series of tuft tests were completed to evaluate the performance of five high temperature superalloy wires sliding against plasma sprayed nichrome-bonded chrome carbide. Wire materials were either nickel-chrome or cobalt-chrome based superalloys. Good corroboration of the tuft results with dynamic seal rig tests was observed; giving additional confidence in the tuft test as a screening and development tool.

Fellenstein, James A.↗

High-temperature oxidation behavior of reaction-formed silicon carbide ceramics

The oxidation behavior of reaction-formed silicon carbide (RFSC) ceramics was investigated in the temperature range of 1100 to 1400 C. The oxidation weight change was recorded by TGA; the oxidized materials were examined by light and electron microscopy, and the oxidation product by x-ray diffraction analysis (XRD). The materials exhibited initial weight loss, followed by passive weight gain (with enhanced parabolic rates, k(sub p)), and ending with a negative (logarithmic) deviation from the parabolic law. The weight loss arose from the oxidation of residual carbon, and the enhanced k(sub p) values from internal oxidation and the oxidation of residual silicon, while the logarithmic kinetics is thought to have resulted from crystallization of the oxide. The presence of a small amount of MoSi, in the RFSC material caused a further increase in the oxidation rate. The only solid oxidation product for all temperatures studied was silica.

Ogbuji, Linus U. J. T.↗

Joining of Silicon Carbide-Based Ceramics by Reaction Forming Method

Recently, there has been a surge of interest in the development and testing of silicon-based ceramics and composite components for a number of aerospace and ground based systems. The designs often require fabrication of complex shaped parts which can be quite expensive. One attractive way of achieving this goal is to build up complex shapes by joining together geometrically simple shapes. However, the joints should have good mechanical strength and environmental stability comparable to the bulk materials. These joints should also be able to maintain their structural integrity at high temperatures. In addition, the joining technique should be practical, reliable, and affordable. Thus, joining has been recognized as one of the enabling technologies for the successful utilization of silicon carbide based ceramic components in high temperature applications. Overviews of various joining techniques, i.e., mechanical fastening, adhesive bonding, welding, brazing, and soldering have been provided in recent publications. The majority of the techniques used today are based on the joining of monolithic ceramics with metals either by diffusion bonding, metal brazing, brazing with oxides and oxynitrides, or diffusion welding. These techniques need either very high temperatures for processing or hot pressing (high pressures). The joints produced by these techniques have different thermal expansion coefficients than the ceramic materials, which creates a stress concentration in the joint area. The use temperatures for these joints are around 700 C. Ceramic joint interlayers have been developed as a means of obtaining high temperature joints. These joint interlayers have been produced via pre-ceramic polymers, in-situ displacement reactions, and reaction bonding techniques. Joints produced by the pre-ceramic polymer approach exhibit a large amounts of porosity and poor mechanical properties. On the other hand, hot pressing or high pressures are needed for in-situ displacement reactions and reaction bonding techniques. Due to the equipment required, these techniques are impractical for joining large or complex shaped components.

Singh, M.↗