High-resolution electron microscopy in spin pumping NiFe/Pt interfaces

In order to understand the effect of the interface on the spin pumping and magnetic proximity effects, high resolution transmission electron microscopy and ferromagnetic resonance (FMR) were used to analyze Py/Pt bilayer and Pt/Py/Pt trilayer systems. The samples were deposited by dc magnetron sputtering at room temperature on Si (001) substrates. The Py layer thickness was fixed at 12 nm in all the samples and the Pt thickness was varied in a range of 0–23 nm. A diffusion zone of approximately 8 nm was found in the Py/Pt interfaces and confirmed by energy dispersive X-ray microanalysis. The FMR measurements show an increase in the linewidth and a shift in the ferromagnetic resonance field, which reach saturation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Initial growth process of Co (Pd) layers on a Pd (Co) surface

The deposition process of ultra-thin Co and Pd layers is studied using DC magnetron sputtering and ex situ atomic force microscopy (AFM). It is found that observation with AFM in the air atmosphere is reliable to discuss nucleation of Co and Pd crystallites. It is discussed that a Co ultra-thin layer is formed primarily through the process of two-dimensional island formation, whereas a Pd ultra-thin layer is formed through the process of mixed two- and three-dimensional island formation. On the basis of those results, Co/Pd multilayers having a flat top surface are prepared successfully.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Tailoring of absorption edge by thermal annealing in tin oxide thin films

Tin oxide (SnO{sub 2}) thin films were deposited by radio-frequency (RF) magnetron sputtering on silicon and glass substrates in different oxygen-to-argon gas-flow ratio (O{sub 2}-to-Ar = 0%, 10%, 50%). All films were deposited at room temperature and fixed working pressures, 10 mTorr. The X-ray diffraction (XRD) measurement suggests that all films were crystalline in nature except film deposited in argon environment. Thin films were annealed in air at 200 °C, 400 °C and 600 °C for two hours. All films were highly transparent except the film deposited only in the argon environment. It was also observed that transparency was improved with annealing due to decrease in oxygen vacancies. Atomic force microscopy (AFM), results showed that the surface of all the films were highly flat and smooth. Blue shift was observed in the absorption edge with annealing temperature. It was also observed that there was not big change in the absorption edge with annealing for films deposited in 10% and 50% oxygen-to-argon gas-flow ratio.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Effects on crystal structure of CZTS thin films owing to deionized water and sulfurization treatment

To condense the cost and increase the production, using abundantly obtainable non-toxic elements, Cu{sub 2}ZnSnS{sub 4} (CZTS) seem to be a strong contender among the photovoltaic thin film technologies. Cu{sub 2}ZnSnS{sub 4} thin films were fabricated by RF magnetron sputtering system. CZTS were sputtered on Molybdenum (Mo) coated soda lime glass (SLG) using a single target sputtering technique. The sputtering parameters (base pressure, working pressure, Argon (Ar) flow rate, RF power and sputtering time) were kept same for all three types of films. For sulfurization, the temperature used was 500 °C. Finally, As-deposited film was immersed in DIW before undergoing identical sulfurization profile. As-deposited film (Sample A), sulfurized films (Sample B) and sulfurized plus DIW treated (Sample C) were compared in terms of their structural properties by means of X-Ray Diffraction (XRD) measurement and Atomic Force Microscopy (AFM). Sample B and C showed peak of (1 1 2) planes of CZTS which are characteristics of stannite structure. Post deposition treatment on CZTS films proved to be beneficial as evident from the observed enhancement in the crystallinity and grain growth. Significant difference on grain size and area roughness could be observed from the AFM measurement. The roughness of Sample A, B and C increased from 5.007 nm to 20.509 nm and 14.183 nm accordingly. From XRD data secondary phases of Cu{sub x}MoS{sub x} could be observed.

36 MATERIALS SCIENCE↗

Electrical and photovoltaic characteristics of MoS{sub 2}/Si p-n junctions

Bulk-like molybdenum disulfide (MoS{sub 2}) thin films were deposited on the surface of p-type Si substrates using dc magnetron sputtering technique and MoS{sub 2}/Si p-n junctions were formed. The vibrating modes of E{sup 1}{sub 2g} and A{sub 1g} were observed from the Raman spectrum of the MoS{sub 2} films. The current density versus voltage (J-V) characteristics of the junction were investigated. A typical J-V rectifying effect with a turn-on voltage of 0.2 V was shown. In different voltage range, the electrical transporting of the junction was dominated by diffusion current and recombination current, respectively. Under the light illumination of 15 mW cm{sup −2}, the p-n junction exhibited obvious photovoltaic characteristics with a short-circuit current density of 3.2 mA cm{sup −2} and open-circuit voltage of 0.14 V. The fill factor and energy conversion efficiency were 42.4% and 1.3%, respectively. According to the determination of the Fermi-energy level (∼4.65 eV) and energy-band gap (∼1.45 eV) of the MoS{sub 2} films by capacitance-voltage curve and ultraviolet-visible transmission spectra, the mechanisms of the electrical and photovoltaic characteristics were discussed in terms of the energy-band structure of the MoS{sub 2}/Si p-n junctions. The results hold the promise for the integration of MoS{sub 2} thin films with commercially available Si-based electronics in high-efficient photovoltaic devices.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Synthesis and magnetic properties of Ta/NdFeB-based composite microwires

Magnetic NdFeB-based microwire composites have been prepared by the direct current magnetron sputtering technique in a specifically designed sputtering chamber for thin-film deposition in wire geometry. As substrate wire material, we have employed steel and Ta. Annealing of the substrate wires during the deposition process was performed by ohmic heating through the application of a direct current. Samples were characterized by means of vibrating sample magnetometry (VSM) and scanning electron microscopy. Best properties have been encountered when using Ta wires as core (substrate) material. The VSM data show a dramatic impact of the current applied during the deposition process on the magnetic properties. For higher current values, i.e., higher annealing temperatures, the wires exhibit a reversal process that is typical for a two-phase system. Moreover, an increase of the coercive field (and remanent magnetization) is observed, which is ascribed to a modification of the magnetic phase present in the sample due to the annealing. We find an indication for the formation of a magnetic easy-axis direction which is azimuthally oriented around the wire axis.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Intrinsic Gilbert damping constant in epitaxial Co{sub 2}Fe{sub 0.4}Mn{sub 0.6}Si Heusler alloys films

The (001)-oriented and (110)-oriented epitaxial grown Co{sub 2}Fe{sub 0.4}Mn{sub 0.6}Si films were fabricated by magnetron sputtering technique in order to investigate the annealing temperature dependence of the intrinsic Gilbert damping constant (α). The stuck films, deposited on MgO and Al{sub 2}O{sub 3} a-plane substrates, respectively, were annealed at various temperatures ranging from 400 °C to 550 °C. The X-ray diffraction analysis was conducted to confirm that all the films were epitaxially grown. In addition, the ferromagnetic resonance measurements as well as the vibrating sample magnetometer were carried out to determine their magnetic properties. A small α of 0.004 was recorded for the sample with 001-oriented Co{sub 2}Fe{sub 0.4}Mn{sub 0.6}Si (CFMS (001)) and 110-oriented CFMS (CFMS (110)) annealed at 450 °C.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Temperature dependent exchange bias training effect in single-crystalline BiFeO{sub 3}/Co bilayers

Single-crystalline BiFeO{sub 3} (BFO)/Co bilayers were prepared by combined pulsed laser deposition and magnetron sputtering on (001) SrTiO{sub 3} substrates. Exchange bias (EB) and accompanying training effect have been studied as a function of temperature (T) between 5 K and 300 K. A non-monotonic exchange field variation with sharp increase below 100 K has been observed. In the meanwhile, strong training effect was recorded when T < 100 K and it weakens monotonically with increasing T up to 300 K. These temperature dependent EB and training effect may be caused by the uncompensated spins in both the interfacial spin-glass (SG) phase at low temperature and the antiferromagnetic BFO layer at higher temperature. The low temperature EB training results can be well fitted by a modified Binek's model considering asymmetric changes of the pinning SG spins at the descending and the ascending branches.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic properties and anisotropic magnetoresistance of antiperovskite nitride Mn{sub 3}GaN/Co{sub 3}FeN exchange-coupled bilayers

Epitaxial bilayers of antiferromagnetic Mn{sub 3}GaN/ferromagnetic Co{sub 3}FeN with an antiperovskite structure were grown by reactive magnetron sputtering, and their structural, magnetic, and electrical properties were investigated. Exchange coupling with an exchange field H{sub ex} of 0.4 kOe at 4 K was observed for Mn{sub 3}GaN (20 nm)/Co{sub 3}FeN (5 nm) bilayers. Negative anisotropic magnetoresistance (AMR) effect in Co{sub 3}FeN was observed and utilized to detect magnetization reversal in exchange-coupled Mn{sub 3}GaN/Co{sub 3}FeN bilayers. The AMR results showed evidence for current-induced spin transfer torque in antiferromagnetic Mn{sub 3}GaN.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Investigation of optical and interfacial properties of Ag/Ta{sub 2}O{sub 5} metal dielectric multilayer structure

One-dimensional periodic metal-dielectric multilayer thin film structures consisting of Ag and Ta{sub 2}O{sub 5} alternating layers are deposited on glass substrate using RF magnetron sputtering technique. The spectral property of the multilayers has been investigated using spectrophotometry technique. The optical parameters such as refractive index, extinction coefficient, band gap etc., along with film thickness as well as the interfacial layer properties which influence these properties have been probed with spectroscopic ellipsometry technique. Atomic force microscopy has been employed to characterize morphological properties of this metal-dielectric multilayer.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Studies on VO{sub x} thin films deposited over Si{sub 3}N{sub 4} coated Si substrates

Vanadium oxide (VO{sub x}) thin films were deposited on to the silicon nitride (Si{sub 3}N{sub 4}) coated silicon (Si) substrate using reactive direct current magnetron sputtering at different substrate temperatures (T{sub s}). The deposited films were characterized for their structural, morphological, optical and electrical properties. The average grain size of the deposited films was in the range of 95 to 178 nm and the strain varied from 0.071 to 0.054 %. The optical bandgap values of the films were evaluated using UV-Vis spectroscopy and lies in the range of 2.46 to 3.88 eV. The temperature coefficient of resistance (TCR) for the film deposited at 125 °C was -1.23%/°C with the sheet resistivity of 2.7 Ω.cm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Interface study and performance of large layer pair ultra-short period W/B{sub 4}C X-ray multilayer

The nature of interfaces in ultra short period W/B{sub 4}C multilayers (MLs) is studied using hard x-ray reflectivity and cross sectional transmission electron microscope. W/B{sub 4}C MLs are fabricated using magnetron sputtering system with systematic varying thickness of both W and B{sub 4}C layers from ∼5 to 30 Å keeping number of layer pairs fixed at 10. It is observed that in low period W/B{sub 4}C ML, as the layer thickness decreases, the interdiffusion plays a significant role because of the discontinuous nature of film. This gives variation of density and roughness of the layer as well as generates thickness errors in the ML structure due to volume changes which is originated by interdifusion process. Finally, W/B{sub 4}C MLs with large number of layer pairs (300) are fabricated with periodicity d= 20 Å which gives ∼54 % of reflectivity at energy 8.047 keV.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Comparative study of structural, optical and impedance measurements on V{sub 2}O{sub 5} and V-Ce mixed oxide thin films

Vanadium pentoxide (V{sub 2}O{sub 5}) and Vanadium-Cerium mixed oxide thin films at different molar ratios of V{sub 2}O{sub 5} and CeO{sub 2} have been deposited at 200 W rf power by rf planar magnetron sputtering in pure argon atmosphere. The structural and optical properties were studied by taking X-ray diffraction and transmittance and absorption spectra respectively. The amorphous thin films show an increase in transmittance and optical bandgap with increase in CeO{sub 2} content in as-prepared thin films. The impedance measurements for as-deposited thin films show an increase in electrical conductivity with increase in CeO{sub 2} material.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Influence of calcium on structural and morphological properties of BiMnO{sub 3} thin films

Bi{sub 1-x}Ca{sub x}MnO{sub 3} (x = 0, 0.1, 0.2, 0.4) thin films were deposited on n–type silicon (100) substrate by RF magnetron sputtering. The X-ray diffraction pattern showed that the films were in monoclinic structure with C2 space group. The crystallite size and strain in the prepared films were measured by W-H plot. The surface morphology of the films was examined by atomic force microscope. The thickness of films was measured by thickness monitor in the sputtering system. From the analysis, it has been concluded that the optimum level for calcium doping is 20 at.% in the Bi site of BiMnO{sub 3} thin film, which will lead a way for further research in the Ca doped BiMnO{sub 3} system.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Resistance switching in polyvinylidene fluoride (PVDF) thin films

Polyvinylidene fluoride (PDVF), one of the best electrically active polymer material & an interesting candidate to address the electrical control of its functional properties like ferroelectricity, piezoelectricity, pyroelectricity etc. In the current work, with the help of spin coater and DC magnetron sputtering techniques, semi-crystallized PVDF thin films prominent in alpha phase is prepared in capacitor like structure and their electrical characterization is emphasized. In current-voltage (I-V) and resistance-voltage (R-V) measurements, clear nonlinearity and resistance switching has been observed for films prepared using 7 wt% 2-butanone and 7 wt% Dimethyl Sulfoxide (DMSO) solvents.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

High electron mobility ZnO film for high-performance inverted polymer solar cells

High-quality ZnO films (ZnO-MS) are prepared via magnetron sputtering deposition with a high mobility of about 2 cm{sup 2}/(V·s) and are used as electron transport layer for inverted polymer solar cells (PSCs) with polymer poly[4,8-bis(5-(2-ethylhexyl)thiophen-2-yl)benzo[1,2-b:4,5-b′] dithiophene-co-3-fluorothieno[3,4-b]thiophene-2-carboxylate]:[6,6]-phenyl C71-butyric acid methyl ester as the active layer. A significant improvement of J{sub SC}, about 20% enhancement in contrast to the devices built on sol-gel derived ZnO film (ZnO-Sol), is found in the ZnO-MS based device. High performance ZnO-MS based PSCs exhibit power conversion efficiency (PCE) up to 8.55%, which is much better than the device based on ZnO-Sol (PCE = 7.78%). Further research on cathode materials is promising to achieve higher performance.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Stress-induced anomalous shift of optical band gap in Ga-doped ZnO thin films: Experimental and first-principles study

In this work, highly c-axis oriented Ga-doped ZnO thin films have been deposited on glass substrates by RF magnetron sputtering under different sputtering times. The optical band gap is observed to shift linearly with the electron concentration and in-plane stress. The failure of fitting the shift of band gap as a function of electron concentration using the available theoretical models suggests the in-plane stress, instead of the electron concentration, be regarded as the dominant cause to this anomalous redshift of the optical band gap. And the mechanism of stress-dependent optical band gap is supported by the first-principles calculation based on density functional theory.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of L1{sub 2} ordering in antiferromagnetic Ir-Mn epitaxial layer on exchange bias of FePd films

Two series of samples of single-layer IrMn and IrMn/FePd bilayer films, deposited on a single-crystal MgO substrate at different IrMn deposition temperatures (T{sub s} = 300–700 °C), were investigated using magnetron sputtering. L1{sub 2} ordering was revealed for the 30 nm-thick IrMn epitaxial (001) films with T{sub s} ≥ 400 °C, determined by synchrotron radiation x-ray diffractometry (XRD). XRD results also provide evidence of the epitaxial growth of the IrMn films on MgO substrate. Increasing T{sub s} from 400 to 700 °C monotonically increases the ordering parameter of L1{sub 2} phases from 0.17 to 0.81. An in-plane exchange bias field (H{sub eb}) of 22 Oe is obtained in a 10 nm-thick FePd film that is deposited on the disordered IrMn films. As the L1{sub 2} ordering of the IrMn layers increases, the H{sub eb} gradually decreases to 0 Oe, meaning that the exchange bias behavior vanishes. The increased surface roughness, revealed by atomic force microscopy, of the epitaxial IrMn layers with increasing T{sub s} cannot be the main cause of the decrease in H{sub eb} due to the compensated surface spins regardless of the disordered and ordered (001) IrMn layers. The change of antiferromagnetic structure from the A1 to the L1{sub 2} phase was correlated with the evolution of H{sub eb}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗