Search NASA⌕ Search

SEARCH · Search NASA

Results for “Powder”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,333 records · Page 74

Large-scale synthesis of ear-like Si{sub 3}N{sub 4} dendrites from SiO{sub 2}/Fe composites and Si powders

Large-scale ear-like Si{sub 3}N{sub 4} dendrites were prepared by the reaction of SiO{sub 2}/Fe composites and Si powders in N{sub 2} atmosphere. The product was characterized by field emission scanning electron microscopy, X-ray diffraction, and transmission electron microscopy. The results reveal that the product mainly consists of ear-like Si{sub 3}N{sub 4} dendrites with crystal structures, which have a length of several microns and a diameter of 100-200 nm. Nanosized ladder-like Si{sub 3}N{sub 4} was also obtained when changing the Fe content in the SiO{sub 2}/Fe composites. The Si{sub 3}N{sub 4} nanoladders have a length of hundreds nanometers to several microns and a width of 100-300 nm. The ear-like Si{sub 3}N{sub 4} dendrites are formed from a two-step growth process, the formation of inner stem structures followed by the epitaxial growth of secondary branches.

36 MATERIALS SCIENCE↗

Electroless coating of tungsten oxide on the surface of copper powder

Tungsten oxide was successfully deposited on the surface of copper powder and the thickness of coating layer was dependent on deposition time. Because a spontaneous reaction occurred on the interface between copper and tungsten-peroxo electrolyte, there was a maximum thickness that could be obtained, as confirmed from XRD and EDX results. Mesoporous tungsten oxide was also deposited using SDS as a structure directing agent. As-synthesized tungsten oxide was amorphous and, after calcination at 450 deg. C, crystallized tungsten oxide was produced. Compared to pure tungsten oxide, the tungsten oxide coated copper oxide showed enhanced absorption in the visible region.

36 MATERIALS SCIENCE↗

Synthesis and upconversion luminescence properties of Yb{sup 3+}/Er{sup 3+} codoped BaGd{sub 2}(MoO{sub 4}){sub 4} powder

Synthesis and upconversion luminescence properties of the new BaGd{sub 2}(MoO{sub 4}){sub 4}:Yb{sup 3+},Er{sup 3+} phosphor were reported in this paper. The phosphor powder was obtained by the traditional high temperature solid-state method, and its phase structure was characterized by the XRD pattern. Based on the upconversion luminescence properties studies, it is found that, under 980 nm semiconductor laser excitation, BaGd{sub 2}(MoO{sub 4}){sub 4}:Yb{sup 3+},Er{sup 3+} phosphor exhibits intense green upconversion luminescence, which is ascribed to {sup 2}H{sub 11/2} {yields} {sup 4}I{sub 15/2} and {sup 4}S{sub 3/2} {yields} {sup 4}I{sub 15/2} transition of Er{sup 3+}. While the observed much weaker red emission is due to the non-radiative relaxation process of {sup 4}S{sub 3/2} {yields} {sup 4}F{sub 9/2} and {sup 4}F{sub 9/2} {yields} {sup 4}I{sub 15/2} transition originating from the same Er{sup 3+}. The concentration quenching effects for both Yb{sup 3+} and Er{sup 3+} were found, and the optimum doping concentrations of 0.5 mol% Yb{sup 3+} and 0.08 mol% Er{sup 3+} in the new BaGd{sub 2}(MoO{sub 4}){sub 4} Gd{sup 3+} host were established.

36 MATERIALS SCIENCE↗

A facile method for nickel catalyst immobilization on ultra fine Al{sub 2}O{sub 3} powders

A pure nickel coating has been successfully plated on the surface of ultra fine Al{sub 2}O{sub 3} particles via a facile electroless plating method. Coating morphology and crystallite size can be tailored by pH values. Dense coating with the maximum crystallite size of 24 nm was obtained at pH 11.0 and porous coating with the minimum crystallite size of 15 nm was obtained at pH value 12.5. The plated powders have been demonstrated to be an effective catalyst for growing boron nitride nanotubes.

36 MATERIALS SCIENCE↗

Enhanced luminescence intensity and color purity of the red emitting LnVO{sub 4}:Eu{sup 3+}@ SiO{sub 2} (Ln = Gd, Y and Gd/Y) powder phosphors

Graphical abstract: Display Omitted Highlights: ► Tetragonal phase lanthanide vanadates doped with Eu{sup 3+} were synthesized. ► Luminescence enhancement was done by optimizing the host (Gd,Y) and SiO{sub 2} coatings. ► SiO{sub 2} coating was characterized by SEM-EDAX, FT-IR and PL techniques. ► {sup 5}D{sub 0} → {sup 7}F{sub 2} domination over {sup 5}D{sub 0} → {sup 7}F{sub 1} indicates the absence of an inversion symmetry. ► Y{sub 0.95}VO{sub 4}:Eu{sup 3+}@ SiO{sub 2}(10 vol.%) is found to be a novel enhanced red emitting phosphor. -- Abstract: An attempt was made to enhance the luminescence properties of LnVO{sub 4}:Eu{sup 3+}@ SiO{sub 2} (Ln = Gd, Y and Gd/Y) powder phosphors. Pure phase with tetragonal structure of the produced phosphors was confirmed by XRD profiles. Sub-micron sized phosphors have shown 35% more PL intensity than the bulk, which was further improved 20.22% with SiO{sub 2} shell coating. SiO{sub 2} shell coating was optimized by SEM-EDAX, FT-IR, PL and TEM measurements. Emission intensities of the transition, {sup 5}D{sub 0} → {sup 7}F{sub 2} have dominated {sup 5}D{sub 0} → {sup 7}F{sub 1}, which indicated the lowering of an inverse symmetry in the vicinity of Eu{sup 3+} ions. Luminescence intensity and color purity were enhanced with the host modification by substituting Gd{sup 3+} with Y{sup 3+} sites, followed by SiO{sub 2} coating. Based on the systematic investigations carried out, the phosphor Y{sub 0.95}VO{sub 4}:Eu{sup 3+}{sub 0.05}@ SiO{sub 2} is suggested to be a novel contender for its suitable red emission in certain displays or lighting.

36 MATERIALS SCIENCE↗

Investigation of structural and magnetic properties of Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} nano powders prepared by self combustion method

Graphical abstract: Display Omitted Highlights: ► Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} prepared by self combustion with uniform/nonuniform heating. ► Characterized using TEM, XRD, in-field Mössbauer and DC magnetometry. ► Leads to bimodal (S1) and very narrow size distribution (S2) type nano samples. ► S1 has magnetic properties of bulk Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4}. ► Although very even sized, S2 large magnetic anisotropy distribution. -- Abstract: Nano powders of Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} have been synthesized by the self-combustion method at a relatively low temperature of 473 K under conditions of non-uniform and uniform heating. Rietveld fitting of X-ray diffractograms confirm the formation of the pure spinel phase in both samples. Transmission electron microscopy indicates that the sample prepared under non-uniform heating has a bimodal particle size distribution (average values 16 nm and 6 nm) while the one prepared under uniform heating has a very narrow particle size distribution (average size 4 nm). Low temperature, in-field Mössbauer spectroscopic studies clearly show surface spin contributions. The hyperfine fields and Curie temperature of the non-uniformly heated sample are in good agreement with those reported for the corresponding bulk samples. Despite having a very narrow particle size distribution, the uniformly heated sample has a large anisotropy distribution which is evident in the broad transition visible in the temperature dependent magnetization curve. It is also corroborated by the fact that the experimental magnetization curve at room temperature requires two Langevin functions for satisfactory reproduction.

36 MATERIALS SCIENCE↗

Comparison of powder bed fusion and directed energy deposition for tailoring mechanical properties of traditionally brittle alloys

The mechanical performance of an Fe-Co intermetallic alloy processed by laser powder bed fusion (L-PBF) and laser directed energy deposition (L-DED) additive manufacturing is compared. L-PBF material was characterized by high strength (500–550 MPa) and high ductility (35%) in tension, corresponding to a ~250% increase in strength and an order-of-magnitude improvement in ductility relative to conventional material. Conversely, L-DED material exhibited similarly poor tensile properties to the conventional wrought alloy, with low strength (200–300 MPa) and low ductility (0–2.7%). Finally, the disparity in properties between L-PBF and L-DED material is discussed in the context of the fundamental differences between manufacturing methods.

36 MATERIALS SCIENCE↗

Pressure-Induced Structural Evolution and Elastic Behaviour of Na{6}Cs{2}Ga{6}Ge{6}O{24} Variant of Cancrinite: A Synchrotron Powder Diffraction Study

The elastic behaviour and the pressure (P) induced structural evolution of Na6Cs2Ga6Ge6O24 Ge(OH)6, a synthetic compound isotypic with cancrinite (CAN topology), have been investigated up to 5.01(5) GPa by means of in situ X-ray synchrotron powder diffraction with a diamond anvil cell and using a nominally penetrating hydrous P-transmitting medium (methanol:ethanol:water = 16:3:1). No evidence of phase-transition was observed within the P-range investigated.

43 PARTICLE ACCELERATORS↗

Variation of elastic mechanical properties with texture, porosity, and defect characteristics in laser powder bed fusion 316L stainless steel

Elastic mechanical properties of 316 L stainless steel samples fabricated using laser powder bed fusion were studied non-destructively through resonant ultrasound spectroscopy. Samples in five different conditions were obtained by varying the laser power from 103 W (the highest density condition) to 68 W (the lowest density condition) at constant laser speed, producing samples with a volume energy density in the 24.5–16.5 J/mm 3 range and volumetric porosity in the 0.1–10% range. The observed elastic mechanical properties are discussed taking into consideration the bulk texture developed and quantitative pore characteristics studied using high-energy high-resolution synchrotron X-ray diffraction and X-ray computed micro-tomography, respectively. Furthermore, empirical exponential relationships are provided to express the functional dependence of Young's and shear moduli with porosity.

36 MATERIALS SCIENCE↗

Plasticity and fracture behavior of Inconel 625 manufactured by laser powder bed fusion: Comparison between as-built and stress relieved conditions

In this work, the influence of stress relief on the plasticity and fracture behavior of Inconel 625 fabricated through laser powder bed fusion additive manufacturing (AM) was investigated. The as-built versus stress relieved microstructures were compared, showing similar grain structures but the presence of ~10 vol % δ phase in the stress relieved condition, and no δ phase in the as-built condition. Mechanical tests under plane strain tension were performed on the stress relieved samples, and an anisotropic plasticity model was calibrated and validated using finite element simulations. Uniaxial and notched tension tests were performed on both as-built and stress relieved samples to probe the effect of stress relief on stress state- and direction-dependent fracture behavior. It was found that on average, the fracture strain of the stress relieved samples along the build direction was 30% higher than that along the perpendicular build direction in the stress state range studied, and the stress relief heat treatment resulted in a 45% decrease in fracture strain. The fracture strain in stress relieved samples was more strongly dependent on stress state than in as-built samples.

36 MATERIALS SCIENCE↗

Optimization of direct aging temperature of Ti free grade 300 maraging steel manufactured using laser powder bed fusion (LPBF)

Maraging steels are of interest to the tool and die industry owing to their high strength, toughness and machinability. Additive manufacturing technologies like laser powder bed fusion (LPBF) can result in a paradigm shift in the design of maraging steel tools. Here, the lack of precipitates, in combination with solute segregation and non-equilibrium microstructure in Grade 300 maraging steel fabricated via LPBF makes the steel amenable to strengthening via direct aging post fabrication instead of the conventional solution treatment and aging. In this study we have focused on optimizing the direct aging temperature for a Ti-free Grade 300 maraging steel fabricated via LPBF for two different aging times. Through strain hardening analysis and detailed microstructural characterization, we show that direct aging at a temperature of 440 °C for 6 h resulted in the best strength-ductility combination. Aging samples at a lower temperature or shorter time resulted in no strain hardening prior to necking as a result of lower fraction of reverted austenite, whereas aging samples at a higher temperature resulted in extensive recrystallization of martensite, coarsening of precipitates, and extensive austenite reversion, resulting in softening of the fabricated parts.

36 MATERIALS SCIENCE↗

On the thermal coarsening and transformation of nanoscale oxide inclusions in 316L stainless steel manufactured by laser powder bed fusion and its influence on impact toughness

The thermal evolution of nanoscale oxide inclusions in 316L stainless steel (SS) manufactured by laser powder bed fusion additive manufacturing (AM) was explored. The size, chemical composition, morphology, and distribution of the oxides were characterized as the function of heat treatment conditions. The study revealed the mechanistic driving force of the rapid oxide coarsening during recrystallization. Ostwald ripening governs oxide coarsening. The active grain boundary-oxide interaction at the early stage of recrystallization accelerated oxide coarsening via enhanced solute diffusion along grain boundaries. Pipe diffusion along dislocation cellular boundaries has a negligible contribution to oxide coarsening. At high temperatures (T> 1065 °C), although lattice diffusion primarily controlled the oxide growth, the contribution from the grain-boundary diffusion was necessary. The transformation from MnSiO 3 to CrMn 2 O 4 took place in the un-recrystallized grains but was not observed when recrystallization started. The interaction of grain boundary and oxides during recrystallization resulted in a high fraction of oxides accumulated at grain boundaries. While oxide coarsening does not significantly alter the toughness value, grain-boundary oxides promote microvoid formation and intergranular fracture under Charpy impact in the recrystallized AM 316L SS.

36 MATERIALS SCIENCE↗

A lightweight Fe–Mn–Al–C austenitic steel with ultra-high strength and ductility fabricated via laser powder bed fusion

Lightweight Fe–Mn–Al–C steels have become a topic of significant interest for the defense and automotive industries. These alloys can maintain high strength and ductility while also reducing weight in structural applications. Conventionally processed Fe–Mn–Al–C austenitic steels with high Al content (~9 wt%) demonstrate greater than 1.5 GPa strength with 35% elongation. Several recent studies have demonstrated success in fabricating steel parts using laser powder bed fusion (L-PBF) additive manufacturing (AM), which can generate near-net-shape components with complex geometries and is capable of local microstructural control. However, studies on L-PBF processing of Fe–Mn–Al–C alloys have focused on low Al content (<5 wt%) compositional regimes representing alloys that undergo transformation-induced plasticity (TRIP) and twinning-induced plasticity (TWIP). Here, in this study, we present the effects of L-PBF processing on the microstructure and mechanical properties of an Fe–30Mn–9Al–1Si-0.5Mo-0.9C austenitic steel. A process optimization framework is employed to determine an ideal L-PBF processing space that will result in >99% density parts. Implementing this framework resulted in near-fully dense specimens fabricated over a broad range of process parameters. Additionally, two bi-directional scan rotation strategies (90° and 67°) were applied to understand their effects on texture and anisotropy in this material. As-printed specimens displayed considerable work-hardening characteristics with average strengths of up to 1.3 GPa and 36% elongation in the build direction. However, solidification microcracks oriented in the build direction resulted in anisotropy in tensile strength and ductility resulting in average strengths of 1.1 GPa and 20% elongation perpendicular to the build direction. The successful L-PBF fabrication of Fe–30Mn–9Al–1Si-0.5Mo-0.9C presented here is expected to open new avenues for weight reduction in structural applications with a high degree of control over part topology.

36 MATERIALS SCIENCE↗

Laser powder bed fusion of oxide dispersion-strengthened IN718 alloys: A complementary study on microstructure and mechanical properties

In this study, two new grades of oxide dispersion strengthened (ODS) Inconel 718 (IN718) alloys were designed by the thermochemical CALPHAD method and produced by laser powder bed fusion (LPBF) technique. Alloys designated as IN718-YF and IN718-YFH, that consist Y 2 O 3 –FeO and Y 2 O 3 –FeO–Hf, respectively, were fabricated with >99.9 % densification using optimized process parameters. CALPHAD calculations were highly consistent with experimental findings, highlighting the formation of Al-containing Y–Ti–O and Y–Hf–O nano-oxides in both alloy types. Texture analyzes revealed no significant texture development in as-built (AB) or heat-treated (HT) alloys. Heat treatment was applied at 1050 °C for 1 h to enhance nano-oxide density. Further, the nano-oxide number density remained similar in IN718-YF while it decreased in IN718-YFH alloy as a result of carbide formation after the heat treatment. Besides, formation of secondary γ' particles was observed in the IN718-YFH/HT alloy. Even though the yield strengths of IN718-YF and IN718-YFH alloys in both AB and HT conditions were similar, the ductility of IN718-YFH was ~50 % less in almost all conditions compared to the ductility of IN718-YF. This has been shown to be as a result of irregular shaped micron-sized Y-Hf-O oxides, martensite formation in AB condition, increased amount of carbides and existence of secondary γ' particles in HT condition in IN718-YFH. High density of stacking faults (SF) forming at the interface of the nano-oxides have been detected in IN718-YF alloys. Besides dislocation/nanoparticle interactions, SFs which are responsible for the delocalization of the deformation improve the ductility of IN718-YF alloys. Overall, high temperature mechanical tests exhibit that both alloys have higher strength with improved ductility compared to the standard IN718 alloys, indicating the contribution of the nano-oxides.

36 MATERIALS SCIENCE↗

Precipitation hardening of laser powder bed fusion Ti-6Al-4V

Here, the laser powder bed fusion (PBF-L) additive manufacturing (AM) community has dedicated significant efforts into process optimization and control for defect-free Ti-6Al-4V. As defects become less of an issue for PBF-L Ti-6Al-4V, the processing-structure-properties (PSP) relationships between AM microstructures can now be explored to optimize mechanical properties. Lower temperature aging treatments around 550 °C in wrought Ti-6A-4V have been historically understood to precipitation harden the α phase with an ordered, hexagonal close packed (HCP) α 2 phase. The α 2 phase existed as nanoscale Ti 3 Al precipitates coherent with the parent α phase. The goal of the present investigation was to implement a vacuum heat treatment of 545 °C for 100 hours on PBF-L Ti-6Al-4V. This vacuum heat treatment took place after an initial hot isostatic pressure (HIP) treatment that decomposed the as-built, martensitic microstructure. The vacuum aging successfully produced nanoscale precipitates of α 2 phase within α-laths, confirmed via atom probe tomography (APT). Microstructural-length scale and quasi-static mechanical properties were investigated by nanoindentation and uniaxial tensile tests of miniaturized test specimens. Given the sensitivity of Ti-6Al-4V mechanical properties to small changes in chemistry, all test specimens originated from the same build. The α 2 precipitation resulted in significantly harder α-laths (≈ 2 GPa) as measured via nanoindentation, as well as a relative yield and ultimate tensile strength increase of 60 MPa and 38 MPa, respectively. Analysis of Variance (ANOVA) of the datasets revealed no statistical differences in total elongation between the HIPed and HIPed + aged specimens, indicative of the aging treatment producing a net benefit of strength with no loss in ductility.

36 MATERIALS SCIENCE↗

Laser powder bed fusion of ODS Fe–Cr–Al (0.3Zr, 0.3Y 2 O 3 ): Unveiling processing-microstructure- mechanical property relationships

Here, this study investigates the fabrication of oxide dispersion strengthened (ODS) Fe-Cr-Al alloys via laser powder bed fusion (LPBF) with strategic additions of 0.3 wt% Zr and 0.3 wt% Y 2 O 3 for enhanced mechanical performance in nuclear applications. Systematic processing parameter optimization yielded three distinct conditions: one low-density product with significant defects and two near-full-density materials with improved consolidation. Comprehensive characterization confirmed single-phase α-ferrite matrix formation with successful incorporation of Y-, Zr-, O-, and C-rich precipitates characteristic of ODS alloys. However, precipitate density remained low (∼10 7 cm −3 ), resulting in sink strength values substantially below optimal levels for radiation resistance. Microhardness values (mid-200s HV) correlated inversely with grain size following the Hall-Petch relationship, indicating grain boundary strengthening as the dominant mechanism rather than precipitation strengthening. The optimized processing conditions achieved excellent mechanical properties with room temperature yield strength of approximately 500 MPa and 30 % elongation, demonstrating superior strength-ductility synergy compared to other additively manufactured ODS materials and performance consistent with literature values for LPBF-processed ODS-FeCrAl alloys. This investigation reveals both the potential and limitations of LPBF processing for ODS Fe-Cr-Al alloys. While successful defect-free fabrication was achieved, results highlight the critical need for systematic optimization of processing parameters and post-processing heat treatments to enhance precipitate density for effective dispersion strengthening and radiation resistance while maintaining additive manufacturing advantages.

Additive manufacturing↗

Controlling mechanical properties of laser powder bed fused AlSi10Mg through manipulation of laser scan rotation

The microstructure and mechanical properties of laser powder bed fused (LPBF) AlSi10Mg alloys can be controlled by many processing parameters. This study focuses on the scan rotation angle, α, between adjacent layers, and establishes the relationship between α and tensile behavior of the as-built LPBF-processed AlSi10Mg alloy. Near-full density cubic coupons were manufactured using the same processing parameters but with systematic variation of α from 0° to 90°. Microscopic observations and X-ray diffraction analysis showed that differences among various coupons mainly include orientations of the melt pools with respect to the build direction and development of the crystallographic texture. The α=0° coupon and α=30° coupon showed the highest and lowest texture index, although the overall crystallographic texture was mild. Tensile specimens were manufactured horizontally and vertically using either α=0° or α=30°, but with various first layer laser direction with respect to the build plate. Notably, the α=0° specimen that was tested along the laser scan direction showed the largest yield strength (283 MPa) and highest tensile ductility (10.1 %). Quantitative image analysis and fractography were performed on all specimens. Results showed that the melt pool orientation with respect to the tensile direction affected the tensile behavior across the different specimens. This was closely related to the localized strain distribution within the melt pool and along the melt pool boundary for the different melt pool orientations observed. Further, these results demonstrate that the laser scan rotation angle between layers can be used to fine tune the mechanical properties of LPBF AlSi10Mg alloy.

36 MATERIALS SCIENCE↗

Post-build stress-relief optimization for laser powder bed fusion 316H stainless steel

Nuclear energy remains a critical component of a diversified and efficient energy portfolio, offering reliable, high-capacity, and low-carbon power. However, in the U.S., aging infrastructure and the slow qualification and deployment of advanced materials and manufacturing techniques hinder progress in next-generation reactor technologies. This study explores the application of laser powder bed fusion (LPBF) additive manufacturing for stainless steel 316H, with a focus on optimizing post-build heat treatments to enhance material properties for high-temperature nuclear applications. The research targets the optimization of stress-relief temperatures to alleviate postbuild residual stresses, ensuring improvements in the microstructural corelated properties. A series of microstructural and mechanical evaluations were performed on LPBF-printed SS-316H samples which were subjected to annealing at temperatures varying between 650 °C and 850 °C. X-ray diffraction, scanning electron microscopy, and transmission electron microscopy analyses revealed that increasing the heattreatment temperature accelerated dislocation recovery. Vickers microhardness measurements showed an initial reduction in values, followed by stabilization over extended durations at all the temperatures. While higher temperatures facilitated faster recovery, they also promoted carbide precipitation along grain and solidification cell boundaries, narrowing the safe processing window. In contrast, heat treatment at 650°C preserved the cellular substructure and enabled controlled carbide precipitation over time. In conclusion, these findings highlight the importance of time–temperature optimization and suggest that 650°C for up to 2 h provides the most favorable balance between recovery and carbide control for a stress-relief treatment.

316 stainless steel↗