99Tc immobilization from off-gas waste streams using nickel-doped iron spinel

Technetium-99 (99Tc) incorporation within stable spinel phases is a novel method for 99Tc removal and immobilization from waste streams. In this study, transformation of Ni-doped Fe(OH)2(s) to spinel minerals, e.g. trevorite (NiFe2O4), is explored as a method for removing 99Tc from Hanford Waste Treatment and Immobilization Plant (WTP) primary off-gas waste stream simulant. The Fe(OH)2(s) transformation process was found to reduce 99Tc(VII) to 99Tc(IV) and incorporate reduced Tc(VI) into the produced spinel simultaneously. Nickel doping was applied in the mineral transformation to inhibit potential reoxidation of 99Tc(IV). Solid phase characterization by XRD and XANES confirmed the formation of nickel substituted ferric-spinel, and suggest incorporation of 99Tc(IV) in the final spinel. Furthermore, in the primary off-gas stream, which contains both redox-sensitive contaminants Cr(VI) and 99Tc(VII), results from solution analysis and solid digestion indicate that nearly 100% Cr and over 80% 99Tc can be simultaneously removed by adding Fe(OH)2(s) to solution with a solid to solution ratio of 5 g/L under near neutral and alkaline conditions. The 99Tc removal approach developed herein provides an alternative treatment method to eliminate the proposed recycle process of the off-gas waste stream, which ultimately can reduce WTP mission cost and operation time.

Wang, Guohui↗

Unraveling Gibbsite Transformation Pathways into LiAl-LDH in Concentrated Lithium Hydroxide

The intercalation of lithium (Li+) ions into metallic hydroxides (e.g. gibbsite, Al(OH)3) facilitates the synthesis of layered double hydroxides. Caustic environments, such as in lithium hydroxide (LiOH) solutions, present additional pathways beyond the intercalation of ions, specifically dissolution/precipitation processes. Herein, the phase transformation Al(OH)3 to lithium aluminum hydroxide dihydrate, Li[Al(OH)3)]2OH•2H2O in partially deuterated LiOH solutions is tracked through multinuclear, magic angle spinning, high-field nuclear magnetic resonance spectroscopy (27Al and 6Li MAS-NMR) , X-ray diffraction, and scanning electron microscopy of harvested solids. At high magnetic fields (19.975 T), 27Al MAS-NMR enabled detection and quantification of the reactive interface between Al(OH)3 and Li[Al(OH)3)]2OH•2H2O. 6Li MAS-NMR spectra collected on the harvested solids exhibited exchange mediated narrowing as the reaction time progressed, consistent with transport of Li+ ions between the interface and the bulk Li[Al(OH)3)]2OH•2H2O. Complimentary in-situ 27Al MAS-NMR at lower magnetic fields (7.046 T) utilized unique rotors capable of simultaneous resolution of solution and solid state Al-species in caustic environments. The reaction between Al(OH)3 (0.5 M) and LiOH (3 M) initially exhibited greater dissolution and formation of Al(OH)4- than the precipitation. Over several hours, the supersaturated Al(OH)4- solution precipitated Li[Al(OH)3)]2OH•2H2O. Simultaneous, in-situ observations of the solid component tracked the formation of Li[Al(OH)3)]2OH•2H2O evident by an increase in signal and narrowing of the Oh resonance. These results provides insight into Al precipitation in alkaline media with applications ranging from the reduction of Al content in Hanford site, high-level radioactive waste (HLRW) to the precipitation of LDH materials for application as catalyst materials, drug delivery devices, and ion-ion exchangers.

Graham, Trenton R.↗

Toward an Understanding of Surface Layer Formation, Growth, and Transformation at the Glass–Fluid Interface

Silicate glass is a metastable and durable solid that has application to a number of energy and environmental challenges (e.g., microelectronics, fiber optics, and nuclear waste storage). If allowed to react with water over time silicate glass develops an altered layer at the solid-fluid interface. In this study, we used borosilicate glass (LAWB45) as model material to develop a robust understanding of altered layer formation (i.e., amorphous hydrated surface layer and crystalline reaction products). Experiments were conducted at high surface area-to-volume ratio (~200,000 m-1) and 90 °C in the pressurized unsaturated flow (PUF) apparatus for 1.5-years to facilitate the formation of thick altered layers and allow for the effluent solution chemistry to be monitored continuously. A variety of microscopy techniques were used to characterized reacted grains and suggest the average altered layer thickness is 13.2 ± 8.3 μm with the hydrated and clay layer representing 74.8% and 25.2% of the total altered layer, respectively. This estimate is within the experimental error of the value estimated from the B release rate data (~10 ±1 μm/yr) over the 1.5-year duration. PeakForce® quantitative nanomechanical mapping results suggest the hydrated layer has a modulus that ranges between ~20 to 40 GPa, which is in the range of porous silica that contains from ~20 to ~50% porosity, yet significantly lower than dense silica (~70 to 80 GPa). Scanning transmission electron microscopy (STEM) images confirm the presence of pores and an analysis of a higher resolution image of a region provides a qualitative estimate of ≥ 22% porosity in this layer with variations in the hydrated layer in void volume with increasing distance from the unaltered glass. Chemical composition analyses, based on a combination of time-of-flight secondary-ion mass spectrometry (ToF-SIMS) and scanning electron microscopy with X-ray energy dispersive spectroscopy (EDS) and STEM-EDS, clearly show that the altered layer is mainly composed of Al, H, Si, and O with the clay layer being enriched in Li, Zn, Fe, and Mg. The amorphous hydrated layer is enriched in Ca, H, and Zr with a minor amount of K. Furthermore, ToF-SIMS results also suggest the B profile is anti-correlated with the H profile in the hydrated layer. Our selected-area electron diffraction results suggest the structure of the hydrated layer closely resembles opal-AG (amorphous gel-like) with an average crystallite size of ~0.7 nm which is smaller than the critical nucleus for silica nanoparticles (i.e., 1.4 to 3 nm). These results suggest the hydrated layer is more consistent with a polymeric gel rather than a colloidal gel and is comprised of molecular units (<1 nm in size) that result from the difficult to hydrolyze bonds, such as Si—O—Zr units, during the glass corrosion process. The size of individual particles or molecular units is a function of formation conditions (e.g., pH, ionic strength, nano-confinement, solute composition) in the hydrated layer.

36 MATERIALS SCIENCE↗

Hydrogenation and Deuteration of C{sub 2}H{sub 2} and C{sub 2}H{sub 4} on Cold Grains: A Clue to the Formation Mechanism of C{sub 2}H{sub 6} with Astronomical Interest

We quantitatively investigated the hydrogen addition reactions of acetylene (C{sub 2}H{sub 2}) and ethylene (C{sub 2}H{sub 4}) on amorphous solid water (ASW) at 10 and 20 K relevant to the formation of ethane (C{sub 2}H{sub 6}) on interstellar icy grains. We found that the ASW surface enhances the reaction rates for C{sub 2}H{sub 2} and C{sub 2}H{sub 4} by approximately a factor of 2 compared to those on the pure-solid C{sub 2}H{sub 2} and C{sub 2}H{sub 4} at 10 K, probably due to an increase in the sticking coefficient and adsorption energy of the H atoms on ASW. In contrast to the previous proposal that the hydrogenation rate of C{sub 2}H{sub 4} is orders of magnitude larger than that of C{sub 2}H{sub 2}, the present results show that the difference in hydrogenation rates of C{sub 2}H{sub 2} and C{sub 2}H{sub 4} is only within a factor of 3 on both the surfaces of pure solids and ASW. In addition, we found the small kinetic isotope effect for hydrogenation/deuteration of C{sub 2}H{sub 2} and C{sub 2}H{sub 4} at 10 K, despite the requirement of quantum tunneling. At 20 K, the reaction rate of deuteration becomes even larger than that of hydrogenation. These unusual isotope effects might originate from a slightly larger number density of D atoms than H atoms on ASW at 20 K. The hydrogenation of C{sub 2}H{sub 2} is four times faster than CO hydrogenation and can produce C{sub 2}H{sub 6} efficiently through C{sub 2}H{sub 4} even in the environment of a dark molecular cloud.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

NUCLEOSYNTHETIC TUNGSTEN ISOTOPE ANOMALIES IN ACID LEACHATES OF THE MURCHISON CHONDRITE: IMPLICATIONS FOR HAFNIUM-TUNGSTEN CHRONOMETRY

Progressive dissolution of the Murchison carbonaceous chondrite with acids of increasing strengths reveals large internal W isotope variations that reflect a heterogeneous distribution of s- and r-process W isotopes among the components of primitive chondrites. At least two distinct carriers of nucleosynthetic W isotope anomalies must be present, which were produced in different nucleosynthetic environments. The co-variation of {sup 182}W/{sup 184}W and {sup 183}W/{sup 184}W in the leachates follows a linear trend that is consistent with a mixing line between terrestrial W and a presumed s-process-enriched component. The composition of the s-enriched component agrees reasonably well with that predicted by the stellar model of s-process nucleosynthesis. The co-variation of {sup 182}W/{sup 184}W and {sup 183}W/{sup 184}W in the leachates provides a means for correcting the measured {sup 182}W/{sup 184}W and {sup 182}W/{sup 183}W of Ca-Al-rich inclusions (CAI) for nucleosynthetic anomalies using the isotopic variations in {sup 183}W/{sup 184}W. This new correction procedure is different from that used previously, and results in a downward shift of the initial {epsilon}{sup 182}W of CAI to -3.51 {+-} 0.10 (where {epsilon}{sup 182}W is the variation in 0.01% of the {sup 182}W/{sup 183}W ratio relative to Earth's mantle). This revision leads to Hf-W model ages of core formation in iron meteorite parent bodies that are {approx}2 Myr younger than previously calculated. The revised Hf-W model ages are consistent with CAI being the oldest solids formed in the solar system, and indicate that core formation in some planetesimals occurred within {approx}2 Myr of the beginning of the solar system.

79 ASTRONOMY AND ASTROPHYSICS↗

Investigation of phase evolution of CaCu{sub 3}Ti{sub 4}O{sub 12} (CCTO) by in situ synchrotron high-temperature powder diffraction

In situ synchrotron X-ray powder diffraction was used to study the high-temperature phase evolution of CaCu{sub 3}Ti{sub 4}O{sub 12} (CCTO) precursors prepared via solid-state and sol–gel methods. After the precursors are heated to 1225 °C, the CCTO phase is the main phase observed in the calcined powder, with the presence of some minor impurities. Comparing the two precursors, we found that the onset temperature for the CCTO phase formation is 800 °C in the sol–gel precursor, lower than that in the solid-state precursor (875 °C). Intermediate phases were only observed in the sol–gel precursor. Both precursors are able to be calcined to sub-micrometric sized powders. Based on the synchrotron data along with differential scanning calorimetry (DSC) and thermal gravimetric analysis (TGA), the phase formation sequence and mechanism during calcination are proposed in this study. -- Graphical abstract: The in situ synchrotron HT-XRD patterns of CCTO sol–gel and solid-state precursor. Highlights: • Phase formation sequence/mechanism in two CCTO precursors has been established. • Formation temperature of CCTO via sol–gel method is lower than solid-state method. • Intermediate phases are only observed in the sol–gel precursor. • Both precursors are able to be calcined into sub-micrometric sized powders.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The physics of planetesimal formation

Physical processes involved in the planetesimal formation are discussed with special attention given to the nature of aerodynamic interactions between solid bodies and gas in the solar nebula. It is emphasized that the model of planetesimal formation by gravitational instability of a dust layer yields predictions that are simple but almost certainly wrong. It is suggested instead that the formation of planetesimals began with the process of coagulation of grains into larger aggregates, and that gravitational forces became more important than gas drag only after objects as large as many meters in diameter had formed.

Weidenschilling, Stuart J.↗

Understanding the solidification and microstructure evolution during CSC-MIG welding of Fe–Cr–B-based alloy

The present is a study of the solidification and microstructure of Fe–28.2%Cr–3.8%B–1.5%Si–1.5%Mn (wt.%) alloy deposited onto a 1020 plain carbon steel substrate using the controlled short-circuit metal inert gas welding process. The as-solidified alloy was a metal matrix composite with a hypereutectic microstructure. Thermodynamic calculation based on the Scheil–Gulliver model showed that a primary (Cr,Fe){sub 2}B phase formed first during solidification, followed by an eutectic formation of the (Cr,Fe){sub 2}B phase and a body-centered cubic Fe-based solid solution matrix, which contained Cr, Mn and Si. Microstructure analysis confirmed the formation of these phases and showed that the shape of the (Cr,Fe){sub 2}B phase was irregular plate. As the welding heat input increased, the weld dilution increased and thus the volume fraction of the (Cr,Fe){sub 2}B plates decreased while other microstructural characteristics were similar. - Highlights: • We deposit Fe–Cr–B-based alloy onto plain carbon steel using the CSC-MIG process. • We model the solidification behavior using thermodynamic calculation. • As deposited alloy consists of (Cr,Fe){sub 2}B plates embedded in Fe-based matrix. • We study the effect of the welding heat input on the microstructure.

36 MATERIALS SCIENCE↗

One-pot generation of lignin microspheres and digestible substrate with a polyol-DES pretreatment in high solid loading

Previous lignin microspheres (LMS) preparation needs multiple steps with very low yield and high cost. Herein, we developed a high-solid deep eutectic solvent (DES) pretreatment for an effective lignin fractionation and enzymatic saccharification of moso bamboo under mild temperature (110 °C) with high-solid loading. Lignin was significantly removed from the plant cell wall, and cellulose properties (e.g., crystallinity and degree of polymerization) were also altered during the pretreatment. As a result, the enzymatic digestibility of the pretreated bamboo was dramatically increased. Uniform micro-spherical lignin was directly produced from the pretreatment system, and its particle size could be regulated by controlling the solid loadings and pretreatment temperatures. The lignin microspheres formation mechanism was investigated by analyzing the lignin's size distribution, molecular weight distribution, chemical structure, and hydrophobicity. The DES showed excellent recyclability, and the recycled DES could still remove 42.78% lignin even after 7th circulation associated with 100% glucan saccharification. Further, the mass balance based on 1000 g biomass showed that 196.28 g LMS was directly recovered, which exhibited a high RhB adsorption. Besides, 404.91 g glucose and 36.67 g xylose were obtained after the enzymatic saccharification process. Specifically, GAPI analysis exhibited a near total green and yellow portions of the pictogram, indicating our DES process was green enough to make this biorefinery sustainable. Overall, the proposed DES generated synergistic productions of digestible solid and LMS which could contribute to establish a green and sustainable biorefinery sequence with diverse outputs in one pot.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The initial stage of growth of crystalline nanowhiskers

The initial stage of formation of semiconductor nanowhiskers by the vapor-liquid-solid mechanism is studied theoretically and experimentally. It is shown that small-sized droplets either are overgrown or emerge together with the surface of the two-dimensional epitaxial layer. The geometric shape of the nanowhiskers at the initial stage of growth is calculated. Experimental data on the formation of GaAs nanowhiskers by molecular beam epitaxy on the GaAs(111)As substrates activated with Au are reported.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Defect energetics of concentrated solid-solution alloys from ab initio calculations: Ni 0.5 Co 0.5 , Ni 0.5 Fe 0.5 , Ni 0.8 Fe 0.2 and Ni 0.8 Cr 0.2

It has been shown that concentrated solid solution alloys possess unusual electronic, magnetic, transport, mechanical and radiation-resistant properties that are directly related to underlying chemical complexity. Because every atom experiences a different local atomic environment, the formation and migration energies of vacancies and interstitials in these alloys exhibit a distribution, rather than a single value as in a pure metal or dilute alloy. In this study, using ab initio calculations based on density functional theory and special quasirandom structure, we have characterized the distribution of defect formation energy and migration barrier in four Ni-based solid-solution alloys: Ni 0.5 Co 0.5 , Ni 0.5 Fe 0.5 , Ni 0.8 Fe 0.2 and Ni 0.8 Cr 0.2 . As defect formation energies in finite-size models depend sensitively on the elemental chemical potential, we have developed a computationally efficient method for determining it which takes into account the global composition and the local short-range order. In addition we have compared the results of our ab initio calculations to those obtained from available embedded atom method (EAM) potentials. Our results indicate that the defect formation and migration energies are closely related to the specific atomic size in the structure, which further determines the elemental diffusion properties. In conclusion, different EAM potentials yield different features of defect energetics in concentrated alloys, pointing to the need for additional potential development efforts in order to allow spatial and temporal scale-up of defect and simulations, beyond those accessible to ab initio methods.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Role of Manganese in Accelerating the Oxidation of Pb(II) Carbonate Solids to Pb(IV) Oxide at Drinking Water Conditions

Pb(II) carbonate solids are corrosion products that form on the inner surfaces of lead service lines (LSLs) and can be oxidized by free chlorine to form Pb(IV) oxide (PbO 2 ). The formation of PbO 2 can maintain low dissolved lead concentrations in drinking water, but PbO 2 can dissolve if a free chlorine residual is not maintained. Experiments demonstrated that the oxidation of Pb(II) carbonate by free chlorine was faster with manganese (Mn). Without Mn(II), the oxidation of Pb(II) carbonate was an autocatalytic process. With Mn(II), the overall oxidation rate was 2 orders of magnitude faster than without Mn(II). X-ray diffraction and free chlorine consumption profiles indicated that δ-MnO 2 was formed within several minutes of the reaction of Mn(II) with free chlorine, and δ-MnO 2 catalyzed the oxidation of Pb(II) carbonate by free chlorine. Free chlorine consumption profiles for Pb(II) carbonate with and without Mn(II) were interpreted based on the kinetics and stoichiometry of the underlying chemical reactions. These findings highlight the importance of Mn in accelerating the formation of PbO 2 in water with Pb(II) carbonate solids and free chlorine, and it may help explain why PbO 2 is observed on LSLs of some but not all water systems that use free chlorine.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Wellbore cement alteration and roles of CO 2 and shale during underground hydrogen storage

To mitigate climate change and adopt renewable energy, energy storage is crucial and can be done in the form of hydrogen gas (H 2 ). Subsurface geologic reservoirs are positioned to store H 2 on the largest scales for the longest terms of all potential options. However, H 2 injection may boost reactions that consume hydrogen, generate undesired gases, and alter pore structures of geomedia. To explore the extent of H 2 -associated biotic reactions at a near wellbore location, four experiments were conducted under underground storage conditions with wellbore cement cores and, in most instances, shale samples submerged in synthetic formation brine. Post-reaction gas, aqueous, and solid phase samples were analyzed using olfactory screening and, later, gas chromatography (GC-MS), inductively coupled plasma optical emission spectroscopy (ICP-OES), scanning electron microscopy (SEM), and synchrotron micro-scale x-ray fluorescence (μ-XRF). Within a period of 16 weeks, hydrogen sulfide (H 2 S) was generated in systems containing both H 2 and shale. XRF mapping identified a zone enriched in iron(II) and reduced sulfur along the rim of cement cross sections that was largely associated with CO 2 -induced cement carbonation. Shale did not show noticeable alteration, but there is evidence it contributed to the initial inoculation of the system and provided nutrients for microbes via water-rock interactions. Here, this study considers both rock formations and wellbore cement not previously evaluated concurrently. Findings support understanding and modeling of H 2 -associated biogeochemical reactions during underground hydrogen storage.

36 MATERIALS SCIENCE↗

Infrared vibrational nano-crystallography and nano-imaging

Molecular solids and polymers can form low-symmetry crystal structures that exhibit anisotropic electron and ion mobility in engineered devices or biological systems. The distribution of molecular orientation and disorder then controls the macroscopic material response, yet it is difficult to image with conventional techniques on the nanoscale. We demonstrated a new form of optical nanocrystallography that combines scattering-type scanning near-field optical microscopy with both optical antenna and tip-selective infrared vibrational spectroscopy. From the symmetry-selective probing of molecular bond orientation with nanometer spatial resolution, we determined crystalline phases and orientation in aggregates and films of the organic electronic material perylenetetracarboxylic dianhydride. Mapping disorder within and between individual nanoscale domains, the correlative hybrid imaging of nanoscale heterogeneity provides insight into defect formation and propagation during growth in functional molecular solids.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Elaboration of Aggregated Polysulfide Phases: From Molecules to Large Clusters and Solid Phases

With the increasing strategies aimed at repressing shuttle problems in the lithium–sulfur battery, dissolved contents of polysulfides are significantly reduced. Except for solid-state Li 2 S 2 and Li 2 S, aggregated phases of polysulfides remain unexplored, especially in well confined cathode material systems. Here, we report a series of nanosize polysulfide clusters and solid phases from an atomic perspective. The calculated phase diagram and formation energy evolution process demonstrate their stabilities and cohesive tendency. It is interesting to find that Li 2 S 6 can stay in the solid state and contains short S 3 chains, further leading to the unique stability and dense structure. Simulated electronic properties indicate reduced band gaps when polysulfides are aggregated, especially for solid phase Li 2 S 6 with a band gap as low as 0.47 eV. In conclusion, their dissolution behavior and conversion process are also investigated, which provides a more realistic model and gives further suggestions on the future design of the lithium–sulfur battery.

25 ENERGY STORAGE↗

Lamellar crystalline self-assembly behaviour and solid lipid nanoparticles of a palmityl prodrug analogue of Capecitabine—A chemotherapy agent

An amphiphile prodrug, 5'-deoxy-5-fluoro-N 4 -(palmityloxycarbonyl) cytidine or 5'-deoxy-5-fluoro-N 4 -(hexadecanaloxycarbonyl) cytidine (5-FCPal), consisting of the same head group as the commercially available chemotherapeutic agent Capecitabine, linked to a palmityl hydrocarbon chain via a carbamate bond is reported. Thermal analysis of this prodrug indicates that it melts at ~115 °C followed quickly by degradation beginning at ~120 °C. The neat solid 5-FCPal amphiphile acquires a lamellar crystalline arrangement with a d-spacing of 28.6 ± 0.3 Å, indicating interdigitation of the hydrocarbon chains. Under aqueous conditions, solid 5-FCPal is non-swelling and no lyotropic liquid crystalline phase formation is observed. In order to assess the in vitro toxicity and in vivo efficacy in colloidal form, solid lipid nanoparticles (SLNs) with an average size of ~700 nm were produced via high pressure homogenization. The in vitro toxicity of the 5-FCPal SLNs against several different cancer and normal cell types was assessed over a 48 h period, and IC 50 values were comparable to those observed for Capecitabine. The in vivo efficacy of the 5-FCPal SLNs was then assessed against the highly aggressive mouse 4T1 breast cancer model. To do so, the prodrug SLNs were administered orally at 3 different dosages (0.1, 0.25, 0.5 mmol/mouse/day) and compared to Capecitabine delivered at the same dosages. After 21 days of receiving the treatments, the 0.5 mmol dose of 5-FCPal exhibited the smallest average tumour volume. Since 5-FCPal is activated in a similar manner to Capecitabine via a 3 step enzymatic pathway with the final step occurring preferentially at the tumour site, formulation of the prodrug into SLNs combines the advantage of selective, localized activation with the sustained release properties of nanostructured amphiphile self-assembly and multiple payload materials thereby potentially creating a more effective anticancer agent.

60 APPLIED LIFE SCIENCES↗

Application of soot carbonization kinetics to deduce meaningful soot formation rates in premixed flat flames

Soot formation rates measured in fuel-rich premixed flat flames are frequently used to calibrate or validate chemical kinetic models of soot formation. Unfortunately, these flames feature an extended region of soot precursor particle inception and carbonization that complicates interpretation of soot measurements and leads to a fundamental inconsistency in the nature of the soot material that is modeled versus what is being measured when using non-intrusive, optical techniques. In the work presented here, previously reported data on two canonical sooting ethylene-air premixed flames at 1 atm pressure are interpreted via a new analysis approach that combines soot optical dispersion coefficient measurements with soot carbonization kinetics. This analytical approach explicitly accounts for the production of poorly ordered soot precursor particle mass and its carbonization over time in the flames, providing a clear distinction between the formation rate of precursor particles and their transformation into ordered, solid soot particulate mass. In particular, the results of the analysis show that the precursor particles form much earlier in the flame than the majority of the carbonized soot and their formation rate is two to three times faster than that of ordered soot. The results also show that particle agglomeration begins when the particles are at an intermediate state of carbonization. In conclusion, these results offer a valuable new interpretation of these important datasets and should lead to substantial improvements in the development and calibration of quantitative soot models.

Soot formation↗

PARTICLE CLUMPING AND PLANETESIMAL FORMATION DEPEND STRONGLY ON METALLICITY

We present three-dimensional numerical simulations of particle clumping and planetesimal formation in protoplanetary disks with varying amounts of solid material. As centimeter-size pebbles settle to the mid-plane, turbulence develops through vertical shearing and streaming instabilities. We find that when the pebble-to-gas column density ratio is 0.01, corresponding roughly to solar metallicity, clumping is weak, so the pebble density rarely exceeds the gas density. Doubling the column density ratio leads to a dramatic increase in clumping, with characteristic particle densities more than 10 times the gas density and maximum densities reaching several thousand times the gas density. This is consistent with unstratified simulations of the streaming instability that show strong clumping in particle-dominated flows. The clumps readily contract gravitationally into interacting planetesimals on the order of 100 km in radius. Our results suggest that the correlation between host star metallicity and exoplanets may reflect the early stages of planet formation. We further speculate that initially low-metallicity disks can be particle enriched during the gas dispersal phase, leading to a late burst of planetesimal formation.

79 ASTRONOMY AND ASTROPHYSICS↗