Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microprobe”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,387 records · Page 77

Microstructural characterization of nitrided beta Ti-Mo alloys at 1400 deg. C

In this work, the two Ti{sub 92}Mo{sub 8} and Ti{sub 84}Mo{sub 16} alloy compositions were gas nitrided at 1400 deg. C. The microstructure and the chemical composition of the gas nitrided surfaces were investigated by scanning electron microscopy and by electron probe microanalysis. Two internal needle-like nitride precipitates, {alpha}-(Ti,N) and {delta}-TiN{sub 0.3}, were observed. Their crystallographic orientation relationships in the {beta} matrix were determined by electron backscattering diffraction.

36 MATERIALS SCIENCE↗

Dendritic coarsening of {gamma}' phase in a directionally solidified superalloy during 24,000 h of exposure at 1173 K

Dendritic coarsening of {gamma}' was investigated in a directionally solidified Ni-base superalloy during exposure at 1173 K for 24,000 h. Chemical homogeneity along different directions and residual internal strain in the experimental superalloy were measured by electronic probe microanalysis (EPMA) and electron back-scattered diffraction (EBSD) technique. It was indicated that the gradient of element distribution was anisotropic and the inner strain between dendrite core and interdendritic regions was different even after 24,000 h of exposure at 1173 K, which influenced the kinetics for the dendrite coarsening of {gamma}' phase.

36 MATERIALS SCIENCE↗

Diffusion bonding of 410 stainless steel to copper using a nickel interlayer

In the present work, plates of stainless steel (grade 410) were joined to copper ones through a diffusion bonding process using a nickel interlayer at a temperature range of 800-950 deg. C. The bonding was performed through pressing the specimens under a 12-MPa compression load and a vacuum of 10{sup -4} torr for 60 min. The results indicated the formation of distinct diffusion zones at both Cu/Ni and Ni/SS interfaces during the diffusion bonding process. The thickness of the reaction layer in both interfaces was increased by raising the processing temperature. The phase constitutions and their related microstructure at the Cu/Ni and Ni/SS diffusion bonding interfaces were studied using optical microscopy, scanning electron microscopy, X-ray diffraction and elemental analyses through energy dispersive spectrometry. The resulted penetration profiles were examined using a calibrated electron probe micro-analyzer. The diffusion transition regions near the Cu/Ni and Ni/SS interfaces consist of a complete solid solution zone and of various phases based on (Fe, Ni), (Fe, Cr, Ni) and (Fe, Cr) chemical systems, respectively. The diffusion-bonded joint processed at 900 deg. C showed the maximum shear strength of about 145 MPa. The maximum hardness was obtained at the SS-Ni interface with a value of about 432 HV.

36 MATERIALS SCIENCE↗

Experimental study of the distribution of alloying elements after the formation of epitaxial ferrite upon cooling in a low-carbon steel

The distributions of carbon and substitutional elements in a low-carbon steel during the formation of epitaxial ferrite on cooling after intercritical annealing have been studied by electron probe microanalysis (EPMA). The analysis has shown that the formation of epitaxial ferrite takes place with a partial redistribution of alloying elements between the epitaxial ferrite and the austenite. This redistribution of alloying elements causes compositional gradients in the epitaxial ferrite that lead to a different etching behaviour with respect to the intercritical ferrite. Contrary to Thermo-Calc predictions, a distinct partitioning behaviour of silicon has been observed.

36 MATERIALS SCIENCE↗

A study of the composition and microstructure of nanodispersed Cu-Ni alloys obtained by different routes from copper and nickel oxides

Mixtures of CuO and NiO were prepared by two different techniques, and then the oxides were reduced with H{sub 2}. Method A involved the preparation of mechanical mixtures of CuO and NiO using different milling and pelletizing processes. Method B involved the chemical synthesis of the mixture of CuO and NiO. The route used to prepare the copper and nickel oxide mixture was found to have great influence on the characteristics of bimetallic Cu-Ni particles obtained. Observations performed using the X-ray diffraction (XRD) technique showed that although both methods led to the Cu-Ni solid solution, the diffractogram of the alloy obtained with method A revealed the presence of NiO together with the alloy. The temperature-programmed reduction (TPR) experiments indicated that the alloy is formed at lower temperatures when using method B. The scanning electron microscopy (SEM) studies revealed notable differences in the morphology and size distribution of the bimetallic particles synthesized by different routes. The results of the electron probe microanalysis (EPMA) studies evidenced the existence of a small amount of oxygen in both cases and demonstrated that the alloy synthesized using method B presented a homogeneous composition with a Cu-Ni ratio close to 1:1. On the contrary, the alloy obtained using method A was not homogeneous in all the volume of the solid. The homogeneity depended on the mechanical treatment undergone by the mixture of the oxides. - Research Highlights: {yields}Study of the properties of Cu-Ni alloys synthesized by two different routes. {yields}Mixtures of Cu and Ni oxides prepared by two techniques were reduced with H{sub 2}. {yields}Mixtures of oxides were obtained by a mechanical process and the citrate-gel route. {yields}The characterizations were carried out by TPR, XRD, SEM and EPMA. {yields}The route used to prepare oxide mixtures influences on the Cu-Ni alloy obtained.

36 MATERIALS SCIENCE↗

Surface composition, microstructure and corrosion resistance of AZ31 magnesium alloy irradiated by high-intensity pulsed ion beam

High-intensity pulsed ion beam (HIPIB) irradiation of AZ31 magnesium alloy is performed and electrochemical corrosion experiment of irradiated samples is carried out by using potentiodynamic polarization technology in order to explore the effect of HIPIB irradiation on corrosion resistance of magnesium alloy. The surface composition, cross-sectional morphology and microstructure are characterized by using electron probe microanalyzer, optical microscope and transmission electron microscope, respectively. The results indicated that HIPIB irradiation leads to a significant improvement in corrosion resistance of magnesium alloy, in terms of the considerable increase in both corrosion potential and pitting breakdown potential. The microstructural refinement and surface purification induced by HIPIB irradiation are responsible for the improved corrosion resistance. - Research Highlights: {yields} A modified layer about 30 {mu}m thick is obtained by HIPIB irradiation. {yields} Selective ablation of element/impurity phase having lower melting point is observed. {yields} More importantly, microstructural refinement occurred on the irradiated surface. {yields} The modified layer exhibited a significantly improved corrosion resistance. {yields} Improved corrosion resistance is ascribed to the combined effect induced by HIPIB.

36 MATERIALS SCIENCE↗

Microstructure, mechanical properties and texture evolution of AZ31 alloy containing trace levels of strontium

The effect of low levels of Sr (0.01, 0.03, 0.05 wt.%) on the microstructure, mechanical properties and texture of AZ31 magnesium alloy has been investigated. Thermodynamic modeling has been used to study the effect of Sr on phase precipitation at different temperatures. Cooling curve analysis reveals a decrease in solidification superheat with the addition of 0.03 wt.% Sr to AZ31. The as-cast microstructures of the alloys have been studied using optical microscopy (OM) and electron probe micro analysis (EPMA). Results show the refining effect of Sr on the grain size and on the {beta}-Mg{sub 17}Al{sub 12} precipitates through growth poisoning and inoculation, respectively. To investigate the mechanical properties of the alloys, as-cast samples were compression tested at elevated temperatures. Hot compression peak stress ({sigma}{sub max}) and critical strain before recrystallization ({epsilon}{sub c}) initially drop but then increase. {sigma}{sub max} first decreases due to the depletion of Al from solid solution and then increases when the amount of the Al-Sr precipitates reach a significant amount. {epsilon}{sub c} drops due to the acceleration of dynamic recrystallization kinetics as a result of grain refinement. It increases with increasing Sr when the concentration Sr in solid solution is increased leading to dislocation pinning and retardation of recrystallization. X-ray texture measurements on the hot compressed and extruded samples show a decrease in maximum intensity of the basal pole figures with increasing Sr as a result of reduced twining and the changes in Al and Sr concentrations in solid solution. - Research Highlights: {yields} Microstructures/precipitates of AZ31+trace levels of Sr were examined by OM and EPMA. {yields} Thermodynamic calculations and cooling curve analysis were used to predict ppt formation. {yields} It has been shown that Sr refines the grains and Mg17Al12 precipitates. {yields} Mechanical properties and texture were studied using hot compression and X-ray diffraction. {yields} Different micro-mechanisms were responsible for mechanical and texture changes.

36 MATERIALS SCIENCE↗

Characterisation of Ga-coated and Ga-brazed aluminium

This work is devoted to the brazing of aluminium using liquid gallium. Gallium was deposited on aluminium samples at {approx} 50 Degree-Sign C using a liquid gallium 'polishing' technique. Brazing was undertaken for 30 min at 500 Degree-Sign C in air. EDS (Energy Dispersive X-ray Spectroscopy) and AES (Auger Electron Spectroscopy) characterisation of Ga-coated samples has shown that the Ga surface layer thickness is of ten (or a few tens of) nanometres. Furthermore, aluminium oxide layer (Al{sub 2}O{sub 3}) was shown to be 'descaled' during Ga deposition, which ensures good conditions for further brazing. Cross-section examination of Ga-coated samples shows that liquid gallium penetrates into the aluminium grain boundaries during deposition. The thickness of the grain boundary gallium film was measured using an original EDS technique and is found to be of a few tens of nanometres. The depth of gallium grain boundary penetration is about 300 {mu}m at the deposition temperature. The fracture stress of the brazed joints was measured from tensile tests and was determined to be 33 MPa. Cross-section examination of brazed joints shows that gallium has fully dissolved into the bulk and that the joint is really autogenous. - Highlights: Black-Right-Pointing-Pointer Aluminium can be brazed using liquid gallium deposited by a 'polishing' technique. Black-Right-Pointing-Pointer The aluminium oxide layer is 'descaled' during liquid Ga 'polishing' deposition. Black-Right-Pointing-Pointer EDS can be used for determination of surface and grain boundary Ga film thickness. Black-Right-Pointing-Pointer The surface and grain boundary Ga film thickness is of a few tens of nm. Black-Right-Pointing-Pointer Surface and grain boundary gallium dissolves in the bulk during brazing.

36 MATERIALS SCIENCE↗

Microstructural and compositional characterization of terbium-doped Nd-Fe-B sintered magnets

Anisotropic sintered magnets based on the Nd{sub 2}Fe{sub 14}B phase doped with Tb were prepared using a grain-boundary diffusion process (GBDP) in order to enhance their coercivity. A FEGSEM microstructural analysis revealed that these GBDP magnets had a core-shell structure, where thin, Tb-rich, (NdTb){sub 2}Fe{sub 14}B shells are formed on the original matrix Nd{sub 2}Fe{sub 14}B grains after diffusion of the Tb. This shell thickness varies from a few tens of nanometres in the middle of the magnet up to a few micrometers near the edge. The exact chemical composition of these shells was determined using EDS and WDS electron-probe microanalyses, which were modified and optimized for submicrometer scale analyses. When analyzing the common Nd-L{alpha}, Tb-L{alpha} and Fe-K{alpha} lines a mutual multiple overlap in the EDS spectra is present and, as a result, an accurate quantitative analysis was only feasible when using WDS. Using this technique we were able to achieve a lateral analytical resolution of 0.4 {mu}m. A further improvement in resolution, down to 0.15 {mu}m, was realized with a dedicated set-up using low-voltage EDS, analyzing the 'atypical' low-energy Nd-M{alpha}, Tb-M{alpha} and Fe-L{alpha} lines. Quantitative analyses confirmed that the reaction phase (Nd{sub x}Tb{sub 1} {sub -x}){sub 2}Fe{sub 14}B is formed after the diffusion of Tb with the equilibrium concentration of Tb being equal to x Almost-Equal-To 0.5, i.e., with the atomic ratio of Nd/Tb equal to 1/1. We also found that a relatively sharp Tb concentration gradient from the shell to the core occurs within a length of Almost-Equal-To 0.5 {mu}m, while the Fe concentration remains unchanged. In terms of magnetic properties, the Tb-doping significantly increased coercivity by Almost-Equal-To 30% while the remanence remained at the same value as in the undoped Nd-Fe-B. - Highlights: Black-Right-Pointing-Pointer Nd-Fe-B sintered magnets were doped with Tb using grain-boundary diffusion process. Black-Right-Pointing-Pointer A tiny core-shell reaction phase was formed around the Nd{sub 2}Fe{sub 14}B matrix grains. Black-Right-Pointing-Pointer EDS and WDS analyses confirmed (Nd{sub 0.5}Tb{sub 0.5}){sub 2}Fe{sub 14}B equilibrium shell composition. Black-Right-Pointing-Pointer Coercivity of Tb-doped Nd-Fe-B increases by 30% without a drop in remanence.

36 MATERIALS SCIENCE↗

Characterisation of titanium-titanium boride composites processed by powder metallurgy techniques

In this work, a detailed characterisation of titanium-titanium boride composites processed by three powder metallurgy techniques, namely, hot isostatic pressing, spark plasma sintering and vacuum sintering, was conducted. Two composites with different volume percents of titanium boride reinforcement were used for the investigation. One was titanium with 20% titanium boride, and the other was titanium with 40% titanium boride (by volume). Characterisation was performed using X-ray diffraction, electron probe micro analysis - energy dispersive spectroscopy and wavelength dispersive spectroscopy, image analysis and scanning electron microscopy. The characterisation results confirm the completion of the titanium boride reaction. The results reveal the presence of titanium boride reinforcement in different morphologies such as needle-shaped whiskers, short agglomerated whiskers and fine plates. The paper also discusses how mechanical properties such as microhardness, elastic modulus and Poisson's ratio are influenced by the processing techniques as well as the volume fraction of the titanium boride reinforcement. - Highlights: Black-Right-Pointing-Pointer Ti-TiB composites were processed by HIP, SPS and vacuum sintering. Black-Right-Pointing-Pointer The completion of Ti-TiB{sub 2} reaction was confirmed by XRD, SEM and EPMA studies. Black-Right-Pointing-Pointer Hardness and elastic properties of Ti-TiB composites were discussed. Black-Right-Pointing-Pointer Processing techniques were compared with respect to their microstructure.

36 MATERIALS SCIENCE↗

Chemical banding revealed by chemical etching in a cold-rolled metastable stainless steel

The current work describes the metallographic characterization of the initial microstructure of a cold rolled precipitation hardening semi-austenitic stainless steel (12Cr–9Ni–4Mo–2Cu–1Ti, in wt.%). The use of the Lichtenegger and Blöch (L–B) color etching solution has been shown to reveal not only the phases present in the microstructure, but also the existence of chemical banding along the rolling direction. The L–B reagent has been found to color the microstructure in bands depending on what alloying elements have segregated to each band. Two-dimensional electron probe microanalysis (EPMA) maps have shown that Ni, Cu and Ti segregate together in the bands, while Cr has an opposite behavior. Mo has a mixed segregation behavior although much weaker than the other elements and more prompt to segregate like Ni does. A direct comparison of light optical micrographs with the EPMA maps of the same area of the microstructure has enable to establish a direct relationship between the alloying element band concentration and the resulting etching color contrast obtained with the L–B reagent. Thermodynamic calculations predict that solidification in this steel takes place with ferrite as the primary phase. Equilibrium partitioning coefficient calculations seem to support the observed segregation patterns. - Highlights: • A cold rolled metastable stainless steel has been characterized thoroughly. • EPMA shows that Ni, Cu and Ti segregate together; Cr in an opposite way. • L–B color etching is sensitive to the segregation of these chemical elements. • This chemical banding has been reduced by applying a homogenization heat treatment. • Partitioning coefficient calculations agree with the observed segregation patterns.

36 MATERIALS SCIENCE↗

Effect of heat treatment on microstructure and interface of SiC particle reinforced 2124 Al matrix composite

The microstructure and interface between metal matrix and ceramic reinforcement of a composite play an important role in improving its properties. In the present investigation, the interface and intermetallic compound present in the samples were characterized to understand structural stability at an elevated temperature. Aluminum based 2124 alloy with 10 wt.% silicon carbide (SiC) particle reinforced composite was prepared through vortex method and the solid ingot was deformed by hot rolling for better particle distribution. Heat treatment of the composite was carried out at 575 °C with varying holding time from 1 to 48 h followed by water quenching. In this study, the microstructure and interface of the SiC particle reinforced Al based composites have been studied using optical microscopy, scanning electron microscopy (SEM) coupled with energy dispersive X-ray spectroscopy (EDS), electron probe micro-analyzer (EPMA) associated with wavelength dispersive spectroscopy (WDS) and transmission electron microscopy (TEM) to identify the precipitate and intermetallic phases that are formed during heat treatment. The SiC particles are uniformly distributed in the aluminum matrix. The microstructure analyses of Al–SiC composite after heat treatment reveal that a wide range of dispersed phases are formed at grain boundary and surrounding the SiC particles. The energy dispersive X-ray spectroscopy and wavelength dispersive spectroscopy analyses confirm that finely dispersed phases are CuAl{sub 2} and CuMgAl{sub 2} intermetallic and large spherical phases are Fe{sub 2}SiAl{sub 8} or Al{sub 15}(Fe,Mn){sub 3}Si. It is also observed that a continuous layer enriched with Cu and Mg of thickness 50–80 nm is formed at the interface in between Al and SiC particles. EDS analysis also confirms that Cu and Mg are segregated at the interface of the composite while no carbide is identified at the interface. - Highlights: • The composite was successfully heat treated at 575°C for 1-48 hrs. • A layer of 50-75 nm is formed at interface after heat treatment. • No Carbide formation and SiC dissolution is observed at this temperature. • MgAl{sub 2}O{sub 4}, CuMgAl{sub 2} phases are segregated at interface of Al-SiC composite. • Mg and Cu are also segregated at near to the grain boundary.

36 MATERIALS SCIENCE↗

Detection of secondary phases in duplex stainless steel by magnetic force microscopy and scanning Kelvin probe force microscopy

The secondary phase transformations in a commercial super duplex stainless steel were investigated by micro-chemical analyses and high resolution scanning probe microscopy. Energy dispersive X-ray and electron probe detected ferrite and austenite as well as secondary phases in unetched aged duplex stainless steel type 25Cr-7Ni-3Mo. Volta potential indicated that nitride and sigma appeared more active than ferrite, while secondary austenite and austenite presented a nobler potential. Reversal order in nobility is thought to be attributable to the potential ranking provided by oxide nature diversity as a result of secondary phase surface compositions on steel. After eutectoid transformation, secondary austenite was detected by electron probe microanalysis, whereas atomic force microscopy distinguished this phase from former austenite by image contrast. Magnetic force microscopy revealed a “ghosted” effect on the latter microstructure probably derived from metal memory reminiscence of mechanical polishing at passivity and long range magnetic forces of ferrite phase. - Highlights: • Nobility detection of secondary phases by SKPFM in DSS particles is not a straightforward procedure. • As Volta potential and contrast are not always consistent SKPFM surface oxides is thought played an important role in detection. • AFM distinguished secondary austenite from former austenite by image contrast though SEM required EPMA.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of diffusion bonded W/steel joint using V/Ni composite interlayer

Diffusion bonding between W and steel using V/Ni composite interlayer was carried out in vacuum at 1050 °C and 10 MPa for 1 h. The microstructural examination and mechanical property evaluation of the joints show that the bonding of W to steel was successful. No intermetallic compound was observed at the steel/Ni and V/W interfaces for the joints bonded. The electron probe microanalysis and X-ray diffraction analysis revealed that Ni{sub 3}V, Ni{sub 2}V, Ni{sub 2}V{sub 3} and NiV{sub 3} were formed at the Ni/V interface. The tensile strength of about 362 MPa was obtained for as-bonded W/steel joint and the failure occurred at W near the V/W interface. The nano-indentation test across the joining interfaces demonstrated the effect of solid solution strengthening and intermetallic compound formation in the diffusion zone. - Highlights: • Diffusion bonding of W to steel was realized using V/Ni composite interlayer. • The interfacial microstructure of the joint was clarified. • Several V–Ni intermetallic compounds were formed in the interface region. • The application of V/Ni composite interlayer improved the joining quality.

36 MATERIALS SCIENCE↗

Characterization of the correlation between the interfaces and failure behaviors for particle reinforced Mg–Li composites

The interfacial microstructure of SiC{sub p} or YAl{sub 2p} reinforced Mg–14Li–3Al matrix composites was comparatively characterized by scanning electron microscopy and electron probe microanalysis. A nanoindentation combined with scanning electron microscopy technique was used to characterize the interfacial mechanical properties between the reinforcements and matrix. The interfacial strength and failure behaviors for the composites were analyzed from the load–penetration curves and corresponding images. In situ tensile tests were used to observe the fracture and deformation processes with the aid of scanning electron microscopy. The results show that both the chemical and mechanical compatibilities between the YAl{sub 2} particles and LA143 matrix are better than those between the SiC particles and LA143 matrix. The interfacial breakage load for the SiC/LA143 composite is lower than that for the YAl{sub 2}/LA143 composite because of the worse chemical and mechanical compatibilities between the ceramic particles and metal matrix. Interfacial breakage is the main failure mechanism for the SiC/LA143 composite, while the particle breakage and matrix crack are the main failure mechanism for the YAl{sub 2}/LA143 composite. These may be related to the stronger interfacial bonding between the intermetallic particles and metal matrix. - Highlights: • The compatibility for YAl{sub 2} particle with LA143 matrix is better than SiC particle. • The strength of the YAl{sub 2}/LA143 interface is higher than the SiC/LA143 interface. • The main failure behavior for the SiC/LA143 composite is interfacial breakage. • The main failure behavior for YAl{sub 2}/LA143 composite is particle and matrix breakage. • The interfacial strength plays an important role on the composite failure behavior.

36 MATERIALS SCIENCE↗

Heat-affected zone liquation crack on resistance spot welded TWIP steels

In this study, the heat affected zone (HAZ) liquation crack and segregation behavior of the resistance spot welded twinning induced plasticity (TWIP) steel have been reported. Cracks appeared in the post-welded joints that originated at the partially melted zone (PMZ) and propagated from the PMZ through the heat affected zone (HAZ) to the base metal (BM). The crack length and crack opening widths were observed increasing with heat input; and the welding current was identified to be the most influencing parameter for crack formation. Cracks appeared at the PMZ when nugget diameter reached at 4.50 mm or above; and the liquation cracks were found to occur along two sides of the notch tip in the sheet direction rather than in the electrode direction. Cracks were backfilled with the liquid films which has lamellar structure and supposed to be the eutectic constituent. Co-segregation of alloy elements such as, C and Mn were detected on the liquid films by electron-probe microanalysis (EPMA) line scanning and element map which suggests that the liquid film was enrich of Mn and C. The eutectic constituent was identified by analyzing the calculated phase diagram along with thermal temperature history of finite element simulation. Preliminary experimental results showed that cracks have less/no significant effect on the static cross-tensile strength (CTS) and the tensile-shear strength (TSS). In addition, possible ways to avoid cracking were discussed. - Highlights: • The HAZ liquation crack during resistance spot welding of TWIP steel was examined. • Cracks were completely backfilled and healed with divorced eutectic secondary phase. • Co-segregation of C and Mn was detected in the cracked zone. • Heat input was the most influencing factor to initiate liquation crack. • Cracks have less/no significant effect on static tensile properties.

36 MATERIALS SCIENCE↗

Potential and limitations of microanalysis SEM techniques to characterize borides in brazed Ni-based superalloys

Brazed Ni-based superalloys containing complex phases of different Boron contents remain difficult to characterize at the micrometer scale. Indeed Boron is a light element difficult to measure precisely. The state-of-the-art microanalysis systems have been tested on a single crystal MC2 based metal brazed with BNi-2 alloy to identify boride precipitates. Effort has been made to evaluate the accuracy in Boron quantitation. Energy-dispersive and wavelength-dispersive X-ray spectroscopy attached to a Scanning Electron Microscope have first been used to determine the elemental composition of Boron-free phases, and then applied to various types of borides. Results have been compared to the ones obtained using a dedicated electron probe microanalysis, considered here as the reference technique. The most accurate method to quantify Boron using EDS is definitely by composition difference. A precision of 5 at.% could be achieved with optimized data acquisition and post-processing schemes. Attempts that aimed at directly quantifying Boron with various standards using EDS or coupled EDS/WDS gave less accurate results. Ultimately, Electron Backscatter Diffraction combined with localized EDS analysis has proved invaluable in conclusively identifying micrometer sized boride precipitates; thus further improving the characterization of brazed Ni-based superalloys. - Highlights: • We attempt to accurately identify Boron-rich phases in Ni-based superalloys. • EDS, WDS, EBSD systems are tested for accurate identification of these borides. • Results are compared with those obtained by electron probe microanalysis. • Boron was measured with EDS by composition difference with a precision of 5 at. %. • Additional EBSD in phase identification mode conclusively identifies the borides.

36 MATERIALS SCIENCE↗

Oxidation and alpha-case formation in Ti–6Al–2Sn–4Zr–2Mo alloy

Isothermal heat treatments in ambient air were performed on wrought Ti–6Al–2Sn–4Zr–2Mo (Ti-6242) material at 500, 593 and 700°C for times up to 500 h. In the presence of oxygen at elevated temperatures simultaneous reactions occurred in Ti-6242 alloy, which resulted in the formation of an oxide scale and a layer with higher oxygen concentration (termed as alpha-case). Total weight gain analysis showed that there was a transition in the oxidation kinetics. At 500°C, the oxidation kinetics obeyed a cubic relationship up to 200 h and thereafter changed to parabolic at prolonged exposure times. At 593°C, it followed a parabolic relationship. After heat treatment at 700°C, the oxidation obeyed a parabolic relationship up to 200 h and thereafter changed to linear at prolonged exposure times. The observed transition is believed to be due to the differences observed in the oxide scale. The activation energy for parabolic oxidation was estimated to be 157 kJ/mol. In addition, alpha-case layer was evaluated using optical microscope, electron probe micro-analyser and microhardness tester. The thickness of the alpha-case layer was found to be a function of temperature and time, increasing proportionally, and following a parabolic relationship. The activation energy for the formation of alpha-case layer was estimated to be 153 kJ/mol. - Highlights: • Transition in oxidation kinetics was observed in Ti–6Al–2Sn–4Zr–2Mo alloy in the temperature range 500–700°C. • The activation energy for parabolic oxidation and for alpha-case formation is about 157 kJ/mol and 153 kJ/mol. • Thickness of alpha-case layer estimated by optical microscopy and electron probe microanalysis is comparable.

36 MATERIALS SCIENCE↗