Synthesis and effect of Ba2+ ions on the dielectric properties of the layered-perovskite KSr2NaNb4O13 ceramics
Highlights: • 25 mol% excess K{sub 2}O was added to densify the pure K(Sr{sub 2}Na)Nb{sub 4}O{sub 13} ceramic at 1275 °C. • K(Sr{sub 2}Na)Nb{sub 4}O{sub 13} ceramic has an increased ε{sub r} compared with that of KSr{sub 2}Nb{sub 3}O{sub 10} ceramic. • K(Sr{sub 0.8}Ba{sub 0.2}){sub 2}NaNb{sub 4}O{sub 13} ceramic has a highest ε{sub r} of 67.4 with a small tan δ of 0.14. • Large ε{sub r} is explained by the increased dipole moment and NbO{sub 6} octahedron distortion. - Abstract: The 25 mol% K{sub 2}O-added K(Sr{sub 2}Na)Nb{sub 4}O{sub 13} ceramic sintered at 1275 °C exhibited a pure and dense K(Sr{sub 2}Na)Nb{sub 4}O{sub 13} phase, which had four octahedral layers. Synthesis of a pure K(Sr{sub 2}Na)Nb{sub 4}O{sub 13} ceramic was not possible without excess K{sub 2}O, due to the formation of a Na-deficient K(Sr{sub 2}Na{sub 2})Nb{sub 5}O{sub 16} secondary phase, because of K{sub 2}O evaporation during sintering. The dielectric constant (ε{sub r}) of the K(Sr{sub 2}Na)Nb{sub 4}O{sub 13} ceramic was 43.8 at 100 kHz, two times higher compared to the KSr{sub 2}Nb{sub 3}O{sub 10} ceramic, which has three octahedral layers. The increased ε{sub r} can be explained by the increased number of octahedral layers. Some of the Sr{sup 2+} ions in K(Sr{sub 2}Na)Nb{sub 4}O{sub 13} ceramic were replaced by Ba{sup 2+} ions, which have high ionic polarizability, to further increase ε{sub r}. The 25 mol% K{sub 2}O-excess K(Sr{sub 0.8}Ba{sub 0.2}){sub 2}NaNb{sub 4}O{sub 13} ceramic sintered at 1250 °C showed a high ε{sub r} of 67.4 at 100 kHz, which can be explained by the increased dipole moments and distortion of the NbO{sub 6} octahedra.