Search NASA⌕ Search

SEARCH · Search NASA

Results for “crystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,405 records · Page 78

Imaging System For Measuring Macromolecule Crystal Growth Rates in Microgravity

In order to determine how macromolecule crystal quality improvement in microgravity is related to crystal growth characteristics, a team of scientists and engineers at NASA's Marshal Space Flight Center (MSFC) developed flight hardware capable of measuring the crystal growth rates of a population of crystals growing under the same conditions. As crystal growth rate is defined as the change or delta in a defined dimension or length (L) of crystal over time, the hardware was named Delta-L. Delta-L consists of three sub assemblies: a fluid unit including a temperature-controlled growth cell, an imaging unit, and a control unit (consisting of a Data Acquisition and Control Unit (DACU), and a thermal control unit). Delta-L will be used in connection with the Glovebox Integrated Microgravity Isolation Technology (g-LIMIT) inside the Microgravity Science Glovebox (MSG), onboard the International Space Station. This paper will describe the Delta-L imaging system. The Delta-L imaging system was designed to locate, resolve, and capture images of up to 10 individual crystals ranging in size from 10 to 500 microns with a point-to-point accuracy of +/- 2.0 microns within a quartz growth cell observation area of 20 mm x 10 mm x 1 mm. The optical imaging system is comprised of a video microscope camera mounted on computer controlled translation stages. The 3-axis translation stages and control units provide crewmembers the ability to search throughout the growth cell observation area for crystals forming in size of approximately 10 microns. Once the crewmember has selected ten crystals of interest, the growth of these crystals is tracked until the size reaches approximately 500 microns. In order to resolve these crystals an optical system with a magnification of 10X was designed. A black and white NTSC camera was utilized with a 20X microscope objective and a 0.5X custom designed relay lens with an inline light to meet the magnification requirement. The design allows a 500 pm crystal to be viewed in the vertical dimension on a standard NTSC monitor (4:3 aspect ratio). Images of the 10 crystals are collected periodically and stored in sets by the DACU.

Corder, Eric L.↗

Rotating Vessels for Growing Protein Crystals

Rotating vessels have been proposed as means of growing larger, more nearly uniform protein crystals than would otherwise be possible in the presence of normal Earth gravitation. Heretofore, nonrotating vessels have been used. It is difficult to grow high-quality protein crystals in the terrestrial gravitational field because of convection plumes created by the interaction between gravitation and density gradients in protein-solution depletion layers around growing crystals. The density gradients and the associated convection plumes cause the surfaces of growing crystals to be exposed to nonuniform solution densities, thereby causing the crystals to form in irregular shapes. The microgravitational environment of outer space has been utilized to eliminate gravitation-induced convection, but this approach is generally not favorable because of the high cost and limited availability of space flight. The use of a rotating vessel according to the proposal is intended to ameliorate the effects of gravitation and the resultant convection, relative to the corresponding effects in a non-rotating vessel. The rotation would exert an averaging effect over time, distributing the convective force on the depletion layer. Therefore, the depletion layer would be more nearly uniform and, as a result, the growing crystal would be more nearly perfect. The proposal admits of variations (see figure), including the following: The growing crystal could be rotated about its own central axis or an external axis. The crystal-growth vessel could be of any of various shapes, including cylindrical, hemispherical, conical, and combinations thereof. The crystal-growth vessel could be suspended in a viscous fluid in an outer vessel to isolate the growing crystal from both ambient vibrations and vibrations induced by a mechanism that drives the rotation. The rotation could be coupled to the crystal-growth vessel by viscous or magnetic means. The crystal-growth vessel could be supported within the outer vessel by use of a magnetic field. The crystal-growth vessel and the outer vessel could be configured in a variety of ways to facilitate heat transfer, instrumentation, and rotation.

Cottingham, Paul↗

Crystallization processes in Ge{sub 2}Sb{sub 2}Se{sub 4}Te glass

Highlights: • Crystallization kinetics of Ge{sub 2}Sb{sub 2}Se{sub 4}Te glass was studied in dependence on particle size by DSC. • All studied fractions were described in terms of the SB autocatalytic model. • Relatively high amount of Te enhances manifestation of bulk crystallization mechanisms. • XRD analysis of samples crystallized under different conditions showed correlation with DSC data. • XRD analysis revealed a new crystallization mechanism indistinguishable by DSC. - Abstract: Differential scanning calorimetry (DSC) and X-ray diffraction (XRD) analysis were used to study crystallization in Ge{sub 2}Sb{sub 2}Se{sub 4}Te glass under non-isothermal conditions as a function of the particle size. The crystallization kinetics was described in terms of the autocatalytic Šesták–Berggren model. An extensive discussion of all aspects of a full-scale kinetic study of a crystallization process was undertaken. Dominance of the crystallization process originating from mechanically induced strains and heterogeneities was confirmed. Substitution of Se by Te was found to enhance the manifestation of the bulk crystallization mechanisms (at the expense of surface crystallization). The XRD analysis showed significant dependence of the crystalline structural parameters on the crystallization conditions (initial particle size of the glassy grains and applied heating rate). Based on this information, a new microstructural crystallization mechanism, indistinguishable by DSC, was proposed.

36 MATERIALS SCIENCE↗

Solid-State Structure and Crystallization in Double-Crystalline Diblock Copolymers of Linear Polyethylene and Hydrogenated Polynorbornene

Double-crystalline diblock copolymers of linear polyethylene (LPE) and hydrogenated polynorbornene (hPN) are synthesized, and their crystallization behavior and morphology are examined using small-angle (SAXS) and wide-angle X-ray scattering (WAXS). In symmetric hPN/LPE diblocks with molecular weights above 50 kg/mol, the hPN block has previously been shown to crystallize first and set the solid-state microstructure. Two-dimensional WAXS on hand-drawn fiber specimens reveals that the LPE crystals formed in confinement stack orthogonally to the hPN crystals. By adjusting total molecular weight, the order of block crystallization may be reversed, even while holding the block length ratio fixed. At a diblock molecular weight of 20 kg/mol, simultaneous time-resolved SAXS/WAXS reveals that the LPE block crystallizes first, even when LPE is the minority component, and restricts hPN to crystallize between the LPE lamellae. The relative orientation of the LPE and hPN crystals in the lower molecular weight diblocks is examined by modeling changes in the SAXS primary peak intensity on cooling two diblocks through the hPN crystal-crystal transition, where hPN densifies as it adopts a rotationally ordered crystal structure. Only a perpendicular stacking of hPN and LPE crystals consistently yields the large reduction in primary SAXS peak intensity observed for both diblocks. Thus, even though the templating block switches from hPN to LPE as the diblock molecular weight is reduced, the orthogonal stacking motif is retained for both high- and low-molecular-weight copolymers.

36 MATERIALS SCIENCE↗

Crystallization and preliminary crystallographic analysis of latent, active and recombinantly expressed aurone synthase, a polyphenol oxidase, from Coreopsis grandiflora

Latent and active aurone synthase purified from petals of C. grandiflora (cgAUS1) were crystallized. The crystal quality of recombinantly expressed latent cgAUS1 was significantly improved by co-crystallization with the polyoxotungstate Na{sub 6}[TeW{sub 6}O{sub 24}] within the liquid–liquid phase-separation zone. Aurone synthase (AUS), a member of a novel group of plant polyphenol oxidases (PPOs), catalyzes the oxidative conversion of chalcones to aurones. Two active cgAUS1 (41.6 kDa) forms that differed in the level of phosphorylation or sulfation as well as the latent precursor form (58.9 kDa) were purified from the petals of Coreopsis grandiflora. The differing active cgAUS1 forms and the latent cgAUS1 as well as recombinantly expressed latent cgAUS1 were crystallized, resulting in six different crystal forms. The active forms crystallized in space groups P2{sub 1}2{sub 1}2{sub 1} and P12{sub 1}1 and diffracted to ∼1.65 Å resolution. Co-crystallization of active cgAUS1 with 1,4-resorcinol led to crystals belonging to space group P3{sub 1}21. The crystals of latent cgAUS1 belonged to space group P12{sub 1}1 and diffracted to 2.50 Å resolution. Co-crystallization of recombinantly expressed pro-AUS with the hexatungstotellurate(VI) salt Na{sub 6}[TeW{sub 6}O{sub 24}] within the liquid–liquid phase separation zone significantly improved the quality of the crystals compared with crystals obtained without hexatungstotellurate(VI)

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

CRYSTALLIZATION IN HIGH-LEVEL WASTE GLASSES U.S. DEPARTMENT OF ENERGY OFFICE OF RIVER PROTECTION WTP ENGINEERING DIVISION

Various circumstances influence crystallization in glassmaking, for example: (1) crystals nucleate and grow before the glass-forming melt occurs; (2) crystals grow or dissolve in flowing melt and during changing temperature; (3) crystals move under the influence of gravity; (4) crystals agglomerate and interact with gas bubbles; (5) high-level wastes (HLW) are mixtures of a large number of components in unusual proportions; (6) melter processing of HLW and the slow cooling of HLW glass in canisters provides an opportunity for a variety of crystalline forms to precipitate; (7) settling of crystals in a HLW glass melter may produce undesirable sludge at the melter bottom; and (8) crystallization of the glass product may increase, but also ruin chemical durability. The conclusions are: (1) crystal growth and dissolution typically proceed in a convective medium at changing temperature; (2) to represent crystallization or dissolution the kinetics must be expressed in the form of rate equations, such as dC/dt = f(C,T) and the temperature dependence of kinetic coefficients and equilibrium concentrations must be accounted for; and (3) non-equilibrium phenomena commonly occur - metastable crystallization, periodic distribution of crystals; and dendritic crystal growth.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Growth and characterization of new semiorganic nonlinear optical and piezoelectric lithium sulfate monohydrate oxalate single crystals

Highlights: • A new semiorganic single crystal of LSO grown by slow evaporation technique. • Morphological studies of the LSO crystal deduced by BFDH law. • In the UV–vis spectrum wide transparent region and large band gap were found. • SHG is equal to KDP crystal and d{sub 33} was found to be equal to 6pC/N. • Grown crystal belongs to softer category. - Abstract: New semiorganic crystal of lithium sulfate monohydrate oxalate (LSO) for nonlinear application was synthesized by controlled slow evaporation method. The growth rate of various planes of the grown crystal was estimated by morphological study. Single crystal XRD analysis confirmed that the crystal belongs to triclinic lattice with space group P1. High transparency (∼95%) with large band gap (4.57 eV) was analyzed by UV–vis studies. FTIR and Raman spectroscopy were used to identify various functional groups present in the LSO crystal. SHG efficiency was found to be equal to the KDP crystal. Thermal stability (up to 117.54 °C) and melting point (242 °C) of the crystal were studied by TG-DTA. In dielectric measurements, the value of dielectric constant decreases with increase in frequency. Hardness studies confirmed soft nature of crystals. The piezoelectric coefficient was found to be 6pC/N along [0 0 1].

36 MATERIALS SCIENCE↗

Imaging of Protein Crystals with Two-Photon Microscopy

Second-order nonlinear optical imaging of chiral crystals (SONICC), which portrays second-harmonic generation (SHG) by noncentrosymmetric crystals, is emerging as a powerful imaging technique for protein crystals in media opaque to visible light because of its high signal-to-noise ratio. Here we report the incorporation of both SONICC and two-photon excited fluorescence (TPEF) into one imaging system that allows visualization of crystals as small as 10 {mu}m in their longest dimension. Using this system, we then documented an inverse correlation between the level of symmetry in examined crystals and the intensity of their SHG. Moreover, because of blue-green TPEF exhibited by most tested protein crystals, we also could identify and image SHG-silent protein crystals. Our experimental data suggest that the TPEF in protein crystals is mainly caused by the oxidation of tryptophan residues. Additionally, we found that unspecific fluorescent dyes are able to bind to lysozyme crystals and enhance their detection by TPEF. We finally confirmed that the observed fluorescence was generated by a two-photon rather than a three-photon process. The capability for imaging small protein crystals in turbid or opaque media with nondamaging infrared light in a single system makes the combination of SHG and intrinsic visible TPEF a powerful tool for nondestructive protein crystal identification and characterization during crystallization trials.

59 BASIC BIOLOGICAL SCIENCES↗

Wide-Angle X-ray Scattering Study on Shear-Induced Crystallization of Propylene-1-Butylene Random Copolymer: Experiment and Diffraction Pattern Simulation

Shear-induced crystallization of a propylene-1-butylene random copolymer with low butylene content (5.7 mol %) was studied using time-resolved wide-angle X-ray scattering (WAXS) techniques. Polymorphism, preferred crystal orientation, crystallization kinetics, and disorder effect were investigated based on WAXS 2D whole pattern analysis. It was found that at 100 C, the crystallite of P-B copolymer was a mixture of 80% {gamma}-form and 20% {alpha}-form of isotactic polypropylene (iPP) crystals. The application of a step shear (shear rate = 100 s{sup -1}, shear duration =3s) induced {gamma}-form crystals with c-axis oriented perpendicular to the shear direction. In contrast, the c-axis of {alpha}-form crystals was normally in parallel to the shear direction. Both crystallization kinetics and crystallinity were greatly enhanced by shear. The disorder effect was found to play an important role in the crystallization behavior of P-B copolymer. In the early stage crystallization, the chosen copolymer contained a large amount of structure defects, where crystals became more ordered upon annealing. The degree of crystal orientation was also found to decrease during crystallization due to the relaxation after shear.

36 MATERIALS SCIENCE↗

IR Bandwidth and Crystal Thickness Effects on THG Efficiency and Temporal Shaping of Quasi-Rectangular UV Pulses: Part II - Incident IR Ripple

We have investigated the effect of incident ir spectral bandwidth and crystal thickness, on uv pulses produced by third harmonic generation (THG) in a crystal pair. Our focus is on the third harmonic generation efficiency and longitudinal uv intensity profile parameters of SNLO predictions that are evaluated for three incident ir spectral bandwidths and a range of crystal thicknesses. These results represent a continuation of earlier work in which the effects of the same selected ir bandwidths and range of crystal thicknesses were investigated using a pair of BBO Type I crystals in a simplistic geometry for which the longitudinal intensity plateau has a zero slope, 'flattop' profile. The current work is distinguished from the previous work by an imposed ripple on the ir intensity longitudinal profile and constitutes a portion of a Part II effort to which we have made reference. As with preceding work, all third harmonic data are net results at the exit of the second BBO crystal. Predictions are obtained with the modified SNLO code developed by Arlee Smith at the Sandia National Laboratories. This modification has allowed us to pursue the 'coupled' case in which the output of the first BBO crystal is used as input to the second one. This includes both the fundamental and second harmonic light. Defined parameters are consistent with previous work. The presented cases are best results. The criteria for selection of these reported cases are highest THG efficiency combined with minimum intensity ripple in the plateau. The incident ir pulse is quasi-rectangular with an imposed 5.2 % (rms) intensity ripple added to the plateau. The ir pulse bandwidth is centered at 800 nm. Second harmonic generation occurs in the first BBO crystal and THG occurs in the second crystal as a consequence of sum frequency generation. Type I phase matching is used throughout, so that for a negative uniaxial crystal: n{sub 2}{sup e}({theta}) = n{sub 1}{sup o};(SHG) (1.1) 3n{sub 3}{sup 3}({theta}) = 2n{sub 2}{sup o} + n{sub 1}{sup o};(THG) where n{sub 2}{sup e}({theta}) and n{sub 3}{sup e}({theta}) are the angle dependent extraordinary refractive indices for the second and third harmonics respectively, and n{sub 1}{sup 1} and n{sub 2}{sup o} are the ordinary refractive indices for the fundamental and second harmonic respectively. Although our goal at this stage has not been to comply with all the LCLS injector laser specifications, the results provided here represent a parameter study that can be used to determine candidate bandwidth dependent, crystal thickness combinations for the detailed design of compliant THG subsystems. This simplistic geometry better elucidates acceptance bandwidth limitations that are intrinsic to the crystal material.

43 PARTICLE ACCELERATORS↗

Non-isothermal Crystallization Kinetics of Mold Fluxes for Casting High-Aluminum Steels

This paper investigates the crystallization behavior of CaO-SiO{sub 2}- and CaO-Al{sub 2}O{sub 3}-based mold fluxes for casting high-aluminum steels using single hot thermocouple technology, developed kinetic models, and scanning electron microscope. The results showed that the crystallization ability of the typical CaO-SiO{sub 2}-based Flux A (CaO/SiO{sub 2} 0.62, Al{sub 2}O{sub 3} 2 mass pct) is weaker than that of CaO-Al{sub 2}O{sub 3}-based Flux B (CaO/SiO{sub 2} 4.11, Al{sub 2}O{sub 3} 31.9 mass pct) because of its higher initial crystallization temperature. The crystallization kinetics of Flux A was “surface nucleation and growth, interface reaction control” in the overall non-isothermal crystallization process, whereas that of Flux B was “constant nucleation rate, 1-dimensional growth, diffusion control, in the primary crystallization stage, and then transformed into constant nucleation rate, 3-dimensional growth, interface reaction control in the secondary crystallization stage.” The energy dispersive spectroscopy results for Flux B suggested that the variations in the crystallization kinetics for Flux B are due to different crystals precipitating in the primary (BaCa{sub 2}Al{sub 8}O{sub 15}) and secondary (CaAl{sub 2}O{sub 4}) crystallization periods during the non-isothermal crystallization process.

36 MATERIALS SCIENCE↗

On phase equilibria and crystal structures in the systems Ce-Pd-B and Yb-Pd-B. Physical properties of R{sub 2}Pd{sub 13.6}B{sub 5} (R=Yb, Lu)

Phase equilibria and crystal structures of ternary compounds were determined in the systems Ce-Pd-B and Yb-Pd-B at 850 deg. C in the concentration ranges up to 45 and 33 at% of Ce and Yb, respectively, employing X-ray single crystal and powder diffraction. Phase relations in the Ce-Pd-B system at 850 deg. C are governed by formation of extended homogeneity fields, tau{sub 2}-CePd{sub 8}B{sub 2-x} (0.10<x<0.48); tau{sub 3}-Ce{sub 3}Pd{sub 25-x}B{sub 8-y} (1.06<x<1.87; 2.20<y<0.05), and CePd{sub 3}B{sub x} (0<x<0.65) the latter arising from binary CePd{sub 3}. Crystallographic parameters for the new structure type tau{sub 2}-CePd{sub 8}B{sub 2-x} (space group C2/c, a=1.78104(4) nm, b=1.03723(3) nm, c=1.16314(3), beta=118.515(1){sup o} for x=0.46) were established from X-ray single crystal diffraction. The crystal structures of tau{sub 2}-CePd{sub 8}B{sub 2-x} and tau{sub 3}-Ce{sub 3}Pd{sub 25-x}B{sub 3-y} are connected in a crystallographic group-subgroup relationship. Due to the lack of suitable single crystals, the novel structure of tau{sub 1}-Ce{sub 6}Pd{sub 47-x}B{sub 6} (x=0.2, C2/m space group, a=1.03594(2) nm, b=1.80782(3) nm, c=1.01997(2) nm, beta=108.321(1){sup o}) was determined from Rietveld refinement of X-ray powder diffraction data applying the structural model obtained from single crystals of homologous La{sub 6}Pd{sub 47-x}B{sub 6} (x=0.19) (X-ray single crystal diffraction, new structure type, space group C2/m, a=1.03988(2) nm, b=1.81941(5) nm, c=1.02418(2) nm, beta=108.168(1){sup o}). The Yb-Pd-B system is characterized by one ternary compound, tau{sub 1}-Yb{sub 2}Pd{sub 14}B{sub 5}, forming equilibria with extended solution YbPd{sub 3}B{sub x}, YbB{sub 6}, Pd{sub 5}B{sub 2} and Pd{sub 3}B. The crystal structures of both Yb{sub 2}Pd{sub 14}B{sub 5} and isotypic Lu{sub 2}Pd{sub 14}B{sub 5} were determined from X-ray Rietveld refinements and found to be closely related to the Y{sub 2}Pd{sub 14}B{sub 5}-type (I4{sub 1}/amd). The crystal structure of binary Yb{sub 5}Pd{sub 2-x} (Mn{sub 5}C{sub 2}-type) was confirmed from X-ray single crystal data and a slight defect on the Pd site (x=0.06) was established. The three structures tau{sub 1}-Ce{sub 6}Pd{sub 47-x}B{sub 6}, tau{sub 2}-CePd{sub 8}B{sub 2-x} and tau{sub 3}-Ce{sub 3}Pd{sub 25-x}B{sub 8-y} are related and can be considered as the packings of fragments observed in Nd{sub 2}Fe{sub 14}B structure with different stacking of common structural blocks. Physical properties for Yb{sub 2}Pd{sub 13.6}B{sub 5} (temperature dependent specific heat, electrical resistivity and magnetization) yielded a predominantly Yb-4f{sup 13} electronic configuration, presumably related with a magnetic instability below 2 K. Kondo interaction and crystalline electric field effects control the paramagnetic temperature domain. - Graphical Abstract: Crystal structure of CePd{sub 8}B{sub 2-x}.

36 MATERIALS SCIENCE↗

Cohesive finite element modeling of the delamination of HTPB binder and HMX crystals under tensile loading

Accurately modeling the mechanical behavior of the polymer binders and the degradation of interfaces between binder and crystal is important to science-based understanding of the macro-scale response of polymer bonded explosives. The paper presents a description of relatively a simple bi-crystal HMX-HTPB specimen and associated tensile loading experiment including computed tomography imaging, the pertinent constitutive theory, and details of numerical simulations used to infer the behavior of the material during the delamination process. Within this work, mechanical testing and direct numerical simulation of this relatively simple bi-crystal system enabled reasonable isolation of binder-crystal interface delamination, in which the effects of the complicated thermomechanical response of explosive crystals were minimized. Cohesive finite element modeling of the degradation and delamination of the interface between a modified HTPB binder and HMX crystals was used to reproduce observed results from tensile loading experiments on bi-crystal specimens. Several comparisons are made with experimental measurements in order to identify appropriate constitutive behavior of the binder and appropriate parameters for the cohesive traction-separation behavior of the crystal-binder interface. This research demonstrates the utility of directly modeling the delamination between binder and crystal within crystal-binder-crystal tensile specimen towards characterizing the behavior of these interfaces in a manner amenable to larger scale simulation of polycrystalline PBX materials. One critical aspect of this approach is micro computed tomography imaging conducted during the experiments, which enabled comparison of delamination patterns between the direct numerical simulation and actual specimen. In addition to optimizing the cohesive interface parameters, one important finding from this investigation is that understanding and representing the strain-hardening plasticity of HTPB binder is important within the context of using a cohesive traction-separation model for the delamination of a crystal-binder system.

42 ENGINEERING↗

Unraveling the Determinant Mechanisms in Flow-Mediated Crystal Growth and Phase Behaviors

To uncover the critical mechanisms responsible for mesoscopic level development during flow-mediated crystal growth, we develop a semi-two-way hydrodynamic coupled structural phase-field crystal formalism (HXPFC-s2). The new formalism, inspired by previous attempts at coupling hydrodynamic and phase-field crystal (PFC) equations, allows for studying mesoscopic flow-mediated crystallization at diffusive timescales pertinent to industrial applications. Unlike previous efforts, the devised coupling to the structural PFC (XPFC) equations allows generalization to more complex crystal structures through explicit parameterization of the direct correlation function (DCF). Utilizing the HXPFC-s2 formalism, we seek to uncover the determinant physical mechanisms in crystallization under simple shear flows by comparing temperature-driven crystallization to flow-mediated crystallization under varying flow-strengths. Parallels and deviations of under-cooling and flow-strength effects on crystal growth are drawn using the crystal cluster-size and system ordering time evolutions. In doing so, we identify scaling behaviors with a Peclet-like number, Pe∼, a critical Peclet-like number, Pe∼*, and flow-field-crystal plane-dependent interactions. Our findings may be relevant for controlling crystal growth and phase behaviors in flow applications.

Willis, L. Connor (ORCID:0009000961321848)↗

Simulation of the temperature distribution in crystals grown by Czochralski method

Production of perfect crystals, free of residual strain and dislocations and with prescribed dopant concentration, by the Czochralski method is possible only if the complex, interacting phenomena that affect crystal growth in a Cz-puller are fully understood and quantified. Natural and forced convection in the melt, thermocapillary effect and heat transfer in and around the crystal affect its growth rate, the shape of the crystal-melt interface and the temperature gradients in the crystal. The heat transfer problem in the crystal and between the crystal and all other surfaces present in the crystal pulling apparatus are discussed at length. A simulation and computer algorithm are used, based on the following assumptions: (1) only conduction occurs in the crystal (experimentally determined conductivity as a function of temperature is used), (2) melt temperature and the melt-crystal heat transfer coefficient are available (either as constant values or functions of radial position), (3) pseudo-steady state is achieved with respect to temperature gradients, (4) crystal radius is fixed, and (5) both direct and reflected radiation exchange occurs among all surfaces at various temperatures in the crystal puller enclosure.

Dudokovic, M. P.↗

Total immersion crystal growth

Crystals of wide band gap materials are produced by positioning a holder receiving a seed crystal at the interface between a body of molten wide band gap material and an overlying layer of temperature-controlled, encapsulating liquid. The temperature of the layer decreases from the crystallization temperature of the crystal at the interface with the melt to a substantially lower temperature at which formation of crystal defects does not occur, suitably a temperature of 200 to 600 C. After initiation of crystal growth, the leading edge of the crystal is pulled through the layer until the leading edge of the crystal enters the ambient gas headspace which may also be temperature controlled. The length of the column of liquid encapsulant may exceed the length of the crystal such that the leading edge and trailing edge of the crystal are both simultaneously with the column of the crystal. The crystal can be pulled vertically by means of a pulling-rotation assembly or horizontally by means of a low-angle withdrawal mechanism.

Morrison, Andrew D.↗

Automated protein crystal growth facility

A customer for the protein crystal growth facility fills the specially designed chamber with the correct solutions, fills the syringes with their quenching solutions, and submits the data needed for the proper growth of their crystal. To make sure that the chambers and syringes are filled correctly, a NASA representative may assist the customer. The data needed is the approximate growth time, the growth temperature, and the desired crystal size, but this data can be changed anytime from the ground, if needed. The chambers are gathered and placed into numbered slots in special drawers. Then, data is entered into a computer for each of the chambers. Technicians map out when each chamber's growth should be activated so that all of the chambers have enough time to grow. All of this data is up-linked to the space station when the previous growth session is over. Anti-vibrational containers need to be constructed for the high forces encountered during the lift off and the landing of the space shuttle, and though our team has not designed these containers, we do not feel that there is any reason why a suitable one could not be made. When the shuttle reaches the space station, an astronaut removes a drawer of quenched chambers from the growth facility and inserts a drawer of new chambers. All twelve of the drawers can be replaced in this fashion. The optical disks can also be removed this way. The old drawers are stored for the trip back to earth. Once inside the growth facility, a chamber is removed by the robot and placed in one of 144 active sites at a time previously picked by a technician. Growth begins when the chamber is inserted into an active site. Then, the sensing system starts to determine the size of the protein crystal. All during the crystal's growth, the customer can view the crystal and read all of the crystal's data, such as growth rate and crystal size. When the sensing system determines that the crystal has reached the predetermined size, the robot is told to pick up a syringe filled with the correct quenchant solution and inject it into the chamber to stop the crystal growth. The chamber is then removed from the active site and placed into its original storage slot. Another chamber is then placed into the active site and the process is repeated in all of the active sites until all of the chambers have complted their growth. After ninety days (the scheduled time between shuttle visits), the crystal growth is completed, and the old drawers are replaced with new ones. Once the customer extracts the crystals, the chambers are retrieved for future customers.

Donald, Stacey↗

Ground Based Program for the Physical Analysis of Macromolecular Crystal Growth

During the past year we have focused on application of in situ Atomic Force Microscopy (AFM) for studies of the growth mechanisms and kinetics of crystallization for different macromolecular systems. Mechanisms of macrostep formation and their decay, which are important in understanding of defect formation, were studied on the surfaces of thaumatin, catalase, canavalin and lysozyme crystals. Experiments revealed that step bunching on crystalline surfaces occurred either due to two- or three-dimensional nucleation on the terraces of vicinal slopes or as a result of uneven step generation by complex dislocation sources. No step bunching arising from interaction of individual steps in the course of the experiment was observed. The molecular structure of the growth steps for thaumatin and lipase crystals were deduced. It was further shown that growth step advance occurs by incorporation of single protein molecules. In singular directions growth steps move by one-dimensional nucleation on step edges followed by lateral growth. One-dimensional nuclei have different sizes, less then a single unit cell, varying for different directions of step movement. There is no roughness due to thermal fluctuations, and each protein molecule which incorporated into the step remained. Growth kinetics for catalase crystals was investigated over wide supersaturation ranges. Strong directional kinetic anisotropy in the tangential step growth rates in different directions was seen. The influence of impurities on growth kinetics and cessation of macromolecular crystals was studied. Thus, for catalase, in addition to pronounced impurity effects on the kinetics of crystallization, we were also able to directly observe adsorption of some impurities. At low supersaturation we repeatedly observed filaments which formed from impurity molecules sedimenting on the surfaces. Similar filaments were observed on the surfaces of thaumatin, canavalin and STMV crystals as well, but the frequency was low compared with catalase crystallization. Cessation of growth of xylanase and lysozyme crystals was also observed and appeared to be a consequence of the formation of dense impurity adsorption layers. Attachment: "An in situ AFM investigation of catalase crystallization", "Atomic force microscopy studies of living cells: visualization of motility, division, aggregation, transformation, and apoptosis", AFM studies on mechanisms of nucleation and growth of macromolecular crystals", and "In situ atomic force microscopy studies of surface morphology, growth kinetics, defect structure and dissolution in macromolecular crystallization".

Malkin, Alexander J.↗