Search NASA⌕ Search

SEARCH · Search NASA

Results for “SINTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,423 records · Page 79

Production of cerium dioxide microspheres by an internal gelation sol–gel method

An internal gelation sol-gel technique was used to prepare cerium dioxide microspheres with uniform diameters near 100 µm. In this process, chilled aqueous solutions containing cerium, hexamethylenetetramine (HMTA), and urea are transformed into a solid gel by heat addition and are subsequently washed, dried, and sintered to produce pure cerium dioxide. Cerous nitrate and ceric ammonium nitrate solutions were compared for their usefulness in microsphere production. Gelation experiments were performed with both cerous nitrate and ceric ammonium nitrate to determine desirable concentrations of cerium, HMTA, and urea in feed solutions as well as the necessary quantity of ammonium hydroxide added to cerium solutions. Analysis of the pH before and after sample gelation was found to provide a quantitative metric for optimal parameter selection along with subjective evaluations of gel qualities. The time necessary for chilled solutions to gel upon inserting into a hot water bath was determined for samples with a variety of parameters and also used to determine desirable formulations for microsphere production. A technique for choosing the optimal mixture of ceric ammonium nitrate, HMTA, and urea was determined using gelation experiments and used to produce microspheres by dispersion of the feed solution into heated silicone oil. Gelled spheres were washed to remove excess reactants and reaction products before being dried and sintered. X-ray diffraction of air-dried microspheres, sintered microspheres, and commercial CeO 2 powders indicated that air-dried and sintered spheres were pure CeO 2 .

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Phase Field Modeling of Pressure Induced Densification in Solid Electrolytes

Adoption of dense and homogeneous solid electrolytes can possibly mitigate the propagation of lithium dendrites and enable lithium metal anodes. Application of external pressure helps to minimize the sintering temperature in oxide ceramics and can potentially densify softer sulfide electrolytes even under room temperature conditions. Here, a previously developed phase field-based computational scheme for predicting the high-temperature sintering-induced densification of oxide ceramic solid electrolytes is extended in the present context to capture the influence of external pressure for densifying solid electrolytes. Two different bulk deformation mechanisms, namely, "reorganization" and "creep deformation," are dominant under external pressure, which is different from the surface and grain-boundary diffusion-induced densification of solid electrolytes that occurs during high temperature sintering. External pressure also increases the points of contact between the particles, which further enhances the propensity of diffusion-induced sintering process. Results obtained from simulations indicate that densification under external pressure is independent of the solid electrolyte particle morphology. Finally, a phase map is generated between applied pressure and temperature for achieving complete densification of oxide ceramics, which can possibly guide the synthesis of thin and dense solid electrolyte separators.

25 ENERGY STORAGE↗

Ultrahigh temperature in situ transmission electron microscopy based bicrystal coble creep in Zirconia II: Interfacial thermodynamics and transport mechanisms

This work uses a combination of stress dependent single grain boundary Coble creep and zero-creep experiments to measure interfacial energies, along with grain boundary point defect formation and migration volumes in cubic ZrO 2 . These data, along with interfacial diffusivities measured in a companion paper are then applied to analyzing two-particle sintering. The analysis presented here indicates that the large activation volume, v * = v f + v m primarily derives from a large migration volume and suggests that the grain boundary rate limiting defects are delocalized, possibly due to electrostatic interactions between charge compensating defects. The discrete nature of the sintering and creep process observed in the small-scale experiments supports the hypothesis that grain boundary dislocations serve as sources and sinks for grain boundary point defects and facilitate strain during sintering and Coble creep. Model two-particle sintering experiments demonstrate that initial-stage densification follows interface reaction rate-limited kinetics.

36 MATERIALS SCIENCE↗

Novel processing route for design and manufacturing of metal toughened nanoceramics: Al–Al 2 O 3 nanocermets

Monolithic alumina is a highly brittle ceramic with a very low fracture toughness, making it an unreliable material for mechanical and structural applications. Ceramic-metal composites (cermets) are the subject of intensive interest to obtain materials which can address the intrinsic brittleness of ceramics without compromising their high strength and light weight. In the present investigation, aluminium-alumina (Al–Al 2 O 3 ) nanocermets were developed. The nanocermets possessed the toughness of Al phase and the strength of reinforced nano Al 2 O 3 particles. Here, the nanocermets green bodies were prepared such that upon sintering each adjacent Al 2 O 3 grain was conformally coated with a continuous Al film. Mechanical milling via a combination of cryo-milling and ball-milling was used to prepare Al–Al 2 O 3 nano-powder mixture. Spark plasma sintering was used to consolidate the green nanocermets. Results show that specimens prepared from 35 h milled powders exhibited superior mechanical properties as compared to other nanocermets, with an improvement in microhardness, elastic modulus, compressive strength, and flexural strength by 88%, 78%, 69% and 40% with respect to sintered pure Al. The indentation toughness of 35 h milled nanocermet showed an increment of 12.5% with respect to sintered pure Al 2 O 3 . Characterization techniques such as XRD, SEM, HR-TEM, X-ray tomography were employed to investigate the phase evolution and structural morphology, while FEM simulations were performed for understanding the crack propagation mechanisms in nanocermets.

36 MATERIALS SCIENCE↗

Additive manufacturing of mullite ceramic by digital light processing

Mullite material was successfully additively manufactured using digital light processing (DLP). The printed geometry involves a one-step process of pyrolysis, de-binding, and sintering under a plain atmosphere to achieve an average of 76 % ceramic yield and linear shrinkage of 12 %. Furthermore, the thermal profile was carefully controlled to obtain consistent phases in which the XRD shows a mullite phase. Here, in addition, the Weibull analysis was conducted on the sintered flexural specimens, showing a Weibull modulus (m) of 13.05 with a characteristic strength (σ 0 ) of 94.96 MPa. Synchrotron microtomography was performed on the sintered specimens, which showed two distinct porosity distributions (small and large). Large porosity (non-spherical elongated) is the primary cause of decreased material strength, while small porosity (spherical) is the sintering product. The measured thermal conductivity of the specimens was in the range of 2.7–3.1 W/m∙k and decreased with an increase in temperature. Lastly, large-scale prototypes were printed concurrently with a fine resolution of 25 μm without any compromise on the predetermined design and structure.

Additive manufacturing↗

Copper-polydopamine composite derived from bioinspired polymer coating

Metal matrix composites with nanocarbon phases, such carbon nanotube (CNT) and graphene, have shown potentials to achieve improved mechanical, thermal, and electrical properties. However, incorporation of these nanocarbons into the metal matrix usually involves complicated processes. Here, this study explored a new processing method to fabricate copper (Cu) matrix composite by coating Cu powder particles with nanometer-thick polydopamine (PDA) thin films and sintering of the powder compacts. For sintering temperatures between 300°C and 750°C, the Cu-PDA composite samples showed higher electrical conductivity and thermal conductivity than the uncoated Cu samples, which is likely related to the higher mass densities of the composite samples. After being sintered at 950°C, the thermal conductivity of the Cu-PDA sample was approximately 12% higher than the Cu sample, while the electrical conductivity did not show significant difference. On the other hand, Knoop micro-hardness values were comparable between the Cu-PDA and Cu samples sintered at the same temperatures.

36 MATERIALS SCIENCE↗

Microstructural features underpinning the mechanical behavior of powder metallurgy Cr-based alloys

Refractory materials such as Cr-based alloys offer the potential of enhanced elevated temperature performance but have been limited by their poor formability. However, powder metallurgy has been shown to be a viable pathway to fabricate these alloys. Nanophase separation sintering (NPSS) in particular has been used in the literature to accelerate the densification of powder metallurgy Cr- and W-based alloys. Here, we explore microstructure evolution during NPSS in a binary Cr 85 Ni 15 alloy consolidated via (i) cold pressing & pressureless sintering and (ii) hot isostatic pressing followed by hot extrusion & hot upsetting, and the role of these different processing routes on resulting material properties. The alloy lacked room temperature tensile ductility regardless of consolidation process, with multi-length scale characterization, including scanning electron microscopy, transmission electron microscopy, atom probe tomography, X-ray diffraction, and uniaxial tensile testing, revealing that brittleness was due to intrinsically poor Cr grain boundary cohesion. Tensile testing conducted at 760 °C showed marked strength reduction for the extruded & upset (94 %) condition compared to the pressed & sintered (18 %). The formation of orthorhombic CrNi 2 intermetallics functioned as precipitate strengtheners and prevented elevated temperature softening in the pressed and sintered condition. The findings offer foundational insights into aiding the future development of Cr-based alloys.

36 MATERIALS SCIENCE↗

Progress in development of SiC-based joints resistant to neutron irradiation

This study fills a knowledge gap regarding neutron-irradiation resistance of SiC joints for nuclear applications, by investigating high-dose neutron irradiation effects on the strength of selected joints and low-dose neutron irradiation effects on recently developed joints fabricated by state of the art processing methods. The joining methods used for the high-dose radiation study included pressure-assisted liquid-phase sintering (LPS) of SiC nanopowder, pressureless calcia-alumina glass ceramics joining, and reaction sintering of Ti-Si-C powders with hot-pressing. The joints were neutron-irradiated at 530 °C to 20 displacements per atom (dpa). Other joining methods included low-pressure LPS of cold-pressed SiC green body, pressureless reaction sintered Ti-Si-C powder joint, spark plasma–sintered Ti diffusion bond, and hot-pressed Ti diffusion bond, which were irradiated at ~500 °C to ~2 dpa. There was no notable degradation of torsional strengths of the joints following the high-dose irradiation. The irradiation-induced degradation at low neutron dose was highly dependent on joint type.

36 MATERIALS SCIENCE↗

Direct ink writing of boron carbide monoliths

Direct ink writing – an extrusion-based additive manufacturing process – followed by pressureless sintering was investigated to produce boron carbide monoliths. The effects of ceramic powder loading and Pluronic binder concentration on the rheology of boron carbide pastes were studied and linked to both processing behaviour and final outcome in terms of sintered density and hardness. The effects of printing parameters, in particular orifice diameter and printing speed, were also investigated. Reducing the size of the extrusion nozzle from 584 μm to 406 μm led to significantly better shape retention, lower surface roughness, as well as higher density and hardness. A 203 μm printing orifice was also trialled but was unsuccessful due to faster drying kinetics that occurred with smaller ceramic struts resulting in rapid warping and nozzle clogging. Carbon-black – 8 wt% relative to B 4 C – acted as an effective sintering aid to increase both density and hardness. After optimisation of feedstock and printing parameters, few-layer samples (3–5 layers) had a density as high as ~ 97 % TD and a hardness of ~ 30 GPa. On the other hand, 18-layer specimens had a sintered density of ~ 87 % TD, despite a fully dense microstructure, due to the formation of a 3D array of inter-strut pores. Nevertheless, several issues that arose during manufacturing and post-processing were detrimental to the density and structural integrity of printed specimens; these issues were identified, discussed, and suggestions for future work are provided in this report.

36 MATERIALS SCIENCE↗

Additive manufacturing of AISI M2 tool steel by binder jetting (BJ): Investigation of microstructural and mechanical properties

The presented research demonstrates for the first time the successful processing of AISI M2 tool steel by binder jetting, a promising additive manufacturing technique capable of producing complex shapes with minimal residual stresses and isotropic properties. The optimal printing parameters were explored by varying processing parameters such as the binder saturation (45 %–105 %), binder set time (0 to 10 s), targeted bed temperature (50–60 °C), oscillator (2600–2750 rpm), recoater (20–28 mm/s), and roller speeds (200–300 rpm). Microstructural characterization and evaluation of mechanical properties of binder jetted parts were performed using x-ray diffraction (XRD), scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS) to study their chemical composition, powder morphology, microstructure, carbide morphologies, relative density, hardness, compressive strength, and ductility. Two powder sizes (5 and 10 μm) were used, and sintering was performed at varying temperatures (1270, 1280, and 1300 °C) and durations (60 and 120 min), followed by a furnace, air, and water cooling. An optimum hardness of ~970 HV was obtained when parts were sintered at 1270 °C for 60 min, followed by water quenching. Impressive compressive strength of ~ 3580 MPa was observed in the sample sintered at 1280 °C for 60 min duration, followed by air cooling. Furnace-cooled parts showed the highest density of ~95 %, whereas the relative density of air- and water-cooled parts varied between ~91 to 93.50 %, respectively. The microstructure of sintered samples revealed the formation of M 6 C stable carbide, M 2 C metastable carbide, MC as a secondary carbide, and a-Fe matrix, which contributed to the observed increase in mechanical properties.

36 MATERIALS SCIENCE↗

Binder-jetted AISI M2 tool steel during hot isostatic pressing: Densification and carbide transformation

Binder jetting (BJ) enables fabrication of complex components from high-alloy steels such as AISI M2; however, residual porosity after sintering limits mechanical performance. This study investigates the coupled effects of binder chemistry, sintering conditions, cooling rate, and subsequent hot isostatic pressing (HIP) on densification, microstructure, and mechanical response in binder-jetted M2 tool steel. HIP increased relative density from ∼93 to 95% to >99% and improved compressive strength by ∼40-70%. Densification was governed by initial pore morphology, where closed porosity was effectively eliminated, while interconnected porosity limited full consolidation. Microstructural analysis (XRD, EBSD, SEM) shows that HIP promotes dissolution of metastable carbides and redistribution of alloying elements (W, Mo, V), transforming heterogeneous carbide networks into finer and more uniformly distributed M 2 C, MC, and M 6 C phases through diffusion-assisted homogenization. Among the investigated conditions, the FluidFuse binder combined with sintering at 1270 °C for 60 min and furnace cooling produced the most balanced response, achieving ∼99.7% density, ∼855 HV hardness, ∼4130 MPa compressive strength, and ∼24% strain. In contrast, higher sintering temperatures promoted carbide coarsening, reducing ductility despite high density. HIP reduces microstructural heterogeneity and drives the system toward a near-equilibrium state with reduced sensitivity to prior processing history. A comparative assessment with conventional and additive manufacturing routes (LPBF, DED, EBM, FFF) shows that the BJ-HIP approach achieves competitive densification and mechanical performance. These findings provide a mechanistic basis for controlling densification and microstructure in high-alloy steels processed via BJAM.

AISI M2 tool steel↗

Efficacy of a Solution-Based Approach for Making Sodalite Waste Forms for an Oxide Reduction Salt Utilized in the Reprocessing of Used Uranium Oxide Fuel

This paper describes various approaches for making sodalite with a LiCl-Li2O oxide reduction salt used to recover uranium from used oxide fuel. The approaches include sol-gel and solution-based synthesis processes. As-made products were mixed with 5 and 10 mass% of a Na2O-B2O3-SiO2 glass binder and these, along with product without a binder, were heated using either a cold-press-and-sinter method or hot uniaxial pressing. The results demonstrate the limitation of sodalite yield due to the fast intermediate reactions between Na+ and Cl- to form halite in solution and Li2O and SiO2 to form lithium silicates (e.g., Li2SiO3 or Li2Si2O5) in the calcined and sintered pellets. The results show that pellets can be made with high sodalite fractions (~92 mass%) and low porosities using a solution-based approach and this LiCl-Li2O salt.

electrochemical↗

Irradiation resistance of silicon carbide joint at light water reactor–relevant temperature

We fabricated and irradiated monolithic silicon carbide (SiC) to SiC plate joints with neutrons at 270–310 °C to 8.7 dpa for SiC. The joining methods included solid state diffusion bonding using titanium and molybdenum interlayers, SiC nanopowder sintering, reaction sintering with a Ti-Si-C system, and hybrid processing of polymer pyrolysis and chemical vapor infiltration (CVI). All the irradiated joints exhibited apparent shear strength of more than 84 MPa on average. Significant irradiation-induced cracking was found in the bonding layers of the Ti and Mo diffusion bonds and Ti-Si-C reaction sintered bond. Furthermore, the SiC-based bonding layers of the SiC nanopowder sintered and hybrid polymer pyrolysis and CVI joints all showed stable microstructure following the irradiation.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Al{sub 2}TiO{sub 5}-Al{sub 2}O{sub 3}-TiO{sub 2} nanocomposite: Structure, mechanical property and bioactivity studies

Novel biomaterials are of prime importance in tissue engineering. Here, we developed novel nanostructured Al{sub 2}TiO{sub 5}-Al{sub 2}O{sub 3}-TiO{sub 2} composite as a biomaterial for bone repair. Initially, nanocrystalline Al{sub 2}O{sub 3}-TiO{sub 2} composite powder was synthesized by a sol-gel process. The powder was cold compacted and sintered at 1300-1500 {sup o}C to develop nanostructured Al{sub 2}TiO{sub 5}-Al{sub 2}O{sub 3}-TiO{sub 2} composite. Nano features were retained in the sintered structures while the grains showed irregular morphology. The grain-growth and microcracking were prominent at higher sintering temperatures. X-ray diffraction peak intensity of {beta}-Al{sub 2}TiO{sub 5} increased with increasing temperature. {beta}-Al{sub 2}TiO{sub 5} content increased from 91.67% at 1300 {sup o}C to 98.83% at 1500 {sup o}C, according to Rietveld refinement. The density of {beta}-Al{sub 2}TiO{sub 5} sintered at 1300 {sup o}C, 1400 {sup o}C and 1500 {sup o}C were computed to be 3.668 g cm{sup -3}, 3.685 g cm{sup -3} and 3.664 g cm{sup -3}, respectively. Nanocrystalline grains enhanced the flexural strength. The highest flexural strength of 43.2 MPa was achieved. Bioactivity and biomechanical properties were assessed in simulated body fluid. Electron microscopy confirmed the formation of apatite crystals on the surface of the nanocomposite. Spectroscopic analysis established the presence of Ca and P ions in the crystals. Results throw light on biocompatibility and bioactivity of {beta}-Al{sub 2}TiO{sub 5} phase, which has not been reported previously.

36 MATERIALS SCIENCE↗

Microstructural and electrical changes in nickel manganite powder induced by mechanical activation

Highlights: {yields} The influence of mechanical activation on microstructure evolution in the nickel manganite powder was investigated as well as electrical properties of the sintered samples. {yields} Structural refinement obtained by Topas-Academic software based on Rietveld analysis showed that the milling process remarkably changed the powder morphology and microstructure. {yields} SEM studies of sintered samples also revealed the strong influence of milling time on ceramics density (increases with milling time). {yields} The electrical properties of ceramic samples are clearly conditioned by terms of synthesis, in our case the time of mechanical activation. {yields} The highest density and higher values of dielectric constant were achieved at the sample activated for 45 min. -- Abstract: Nickel manganite powder synthesized by calcination of a stoichiometric mixture of manganese and nickel oxide was additionally mechanically activated in a high energy planetary ball mill for 5-60 min in order to obtain a pure NiMn{sub 2}O{sub 4} phase. The as-prepared powders were uniaxially pressed into disc shape pellets and then sintered for 60 min at 1200 {sup o}C. Changes in the particle morphology induced by mechanical activation were monitored using scanning electron microscopy, while changes in powder structural characteristics were followed using X-ray powder diffraction. The ac impedance spectroscopy was performed on sintered nickel manganite samples at 25 {sup o}C, 50 {sup o}C and 80 {sup o}C. It was shown that mechanical activation intensifies transport processes causing a decrease in the average crystallites size, while longer activation times can lead to the formation of aggregates, defects and increase of lattice microstrains. The observed changes in microstructures were correlated with measured electrical properties in order to define optimal processing conditions.

36 MATERIALS SCIENCE↗

High surface area neodymium phosphate nano particles by modified aqueous sol-gel method

Graphical abstract: Synthesis of nano rod shaped neodymium phosphate particles with specific surface area as high as 107 m{sup 2} g{sup -1} and particles could be compacted and sintered at as low as 1300 Degree-Sign C to a density of 98.5% (theoretical) with an average grain size of {approx}1 {mu}m. Highlights: Black-Right-Pointing-Pointer Nano size neodymium phosphate is synthesized and characterized using a novel modified aqueous sol gel process. Black-Right-Pointing-Pointer Specific surface area above 100 m{sup 2} g{sup -1} achieved without the addition of any complexing agents. Black-Right-Pointing-Pointer High sintered density reported than the density obtained for powder synthesized through conventional solid state reaction. Black-Right-Pointing-Pointer The particles are nano sized and have rod shape morphology and are retained at higher temperatures. Black-Right-Pointing-Pointer An average grain size of {approx}1 {mu}m obtained for sintered NdPO{sub 4} after thermal etching at 1400 Degree-Sign C. -- Abstract: Synthesis of nano rod shaped neodymium phosphate (NdPO{sub 4}) particles with specific surface area as high as 107 m{sup 2}g{sup -1} and an average length of 50 nm with aspect ratio 5 was achieved using modified sol gel method. Crystallite size calculated from the X-ray diffraction data by applying Scherer equation was 5 nm for the precursor gel after calcination at 400 Degree-Sign C. NdPO{sub 4} was first precipitated from neodymium nitrate solution using phosphoric acid followed by peptization using dilute nitric acid and further gelation in ammonia atmosphere. The calcined gel powders were further characterized by surface area (Brunauer-Emmet-Teller nitrogen adsorption analysis), Transmission electron microscopy, scanning electron microscopy, UV-vis and FT-IR analysis. Transmission electron microscopy confirms the formation of rod like morphology from the sol, gel and the calcined particles in nano size range. These particles could be compacted and sintered at as low as 1300 Degree-Sign C to a density of 98.5% (theoretical) with an average grain size of {approx}1 {mu}m.

36 MATERIALS SCIENCE↗

Development of mixed conducting dense nickel/Ca-doped lanthanum zirconate cermet for gas separation application

Highlights: Black-Right-Pointing-Pointer Phase pure La{sub 1.95}Ca{sub 0.05}Zr{sub 2}O{sub 7-{delta}} (LCZ) material is prepared by combustion synthesis. Black-Right-Pointing-Pointer LCZ and Ni-LCZ bulk samples are prepared with theoretical density close to 100%. Black-Right-Pointing-Pointer Bulk electrical conductivity {approx}400 S/cm is obtained for Ni-LCZ cermet at 750 Degree-Sign C. -- Abstract: La{sub 1.95}Ca{sub 0.05}Zr{sub 2}O{sub 7-{delta}} (LCZ) and Ni-LCZ cermet have been prepared by combustion synthesis and conventional solid state mixing methods respectively. Both the materials are sintered in air and controlled atmosphere (5% H{sub 2} in Ar). The density obtained for the material sintered at 1400 Degree-Sign C in controlled atmosphere is found to be more than 99.5%. This sintering temperature (1400 Degree-Sign C) is considered to be much lower compared to the conventional sintering temperature. The corresponding total conductivity for such Ni-LCZ cermet materials is {approx}400 S/cm measured at 750 Degree-Sign C having 40 vol% of Ni and 60 vol% LCZ.

36 MATERIALS SCIENCE↗

Microstructure and photoluminescent properties of Sr{sub 2}SiO{sub 4}:Eu{sup 3+} phosphors with various NH{sub 4}Cl flux concentrations

Graphical abstract: This paper describes effects of NH{sub 4}Cl concentration on microstructural and luminescent characteristics of Sr{sub 2}SiO{sub 4}:Eu{sup 3+} phosphors using microwave assisted sintering at 1200 °C for 1 h. The results showed the improved photoluminescence properties of microwave sintered Sr{sub 2}SiO{sub 4}:Eu{sup 3+} phosphors by adding NH{sub 4}Cl flux. Highlights: ► NH{sub 4}Cl flux improved the luminescence properties of microwave sintered phosphors. ► The particle sizes were enlarged from 1 μm to 10 μm as the NH{sub 4}Cl flux was added. ► The maximum photoluminescence intensity was appeared as adding 1 wt% NH{sub 4}Cl flux. ► The decay times of Sr{sub 2}SiO{sub 4}:Eu{sup 3+} phosphors with NH{sub 4}Cl flux were around 2.47–2.52 ms. -- Abstract: In this paper, effect of NH{sub 4}Cl flux concentrations (0, 1, 2, 3 and 4 wt%) on the crystal structure, morphology and photoluminescent properties of Sr{sub 2}SiO{sub 4}:Eu{sup 3+} phosphors synthesized by a microwave sintering at 1200 °C for 1 h was investigated and discussed. X-ray powder diffraction analysis showed the crystal structure was not affected and the pure Sr{sub 2}SiO{sub 4} phase was formed without second phase or phases of starting materials when adding with the NH{sub 4}Cl flux. The SEM images indicated that increase of the NH{sub 4}Cl flux enlarged the particle size of the phosphor particles. The photo-luminescence results showed the addition of 1 wt% NH{sub 4}Cl flux much improved the emission intensity at λ{sub em} of 617 nm as the excitation spectrum at λ{sub ex} of 395 nm. The decay times of Sr{sub 2}SiO{sub 4}:Eu{sup 3+} phosphors with different NH{sub 4}Cl flux concentrations were obtained around 2.47–2.52 ms.

36 MATERIALS SCIENCE↗