Ferrimagnetic and spin-glass transition in the Aurivillius compound SrBi{sub 5}Ti{sub 4}Cr{sub 0.5}Co{sub 0.5}O{sub 18}
Single-phase polycrystalline SrBi{sub 5}Ti{sub 4}CrO{sub 18} and SrBi{sub 5}Ti{sub 4}Cr{sub 0.5}Co{sub 0.5}O{sub 18} were synthesized by a modified Pechini method. Both samples have an orthorhombic structure with the space group B2cb. The valence state of Cr is suggested to be +3 and the Co ions exist in the form of Co{sup 2+} and Co{sup 3+} based on the results of x-ray photoelectron spectroscopy. The sample SrBi{sub 5}Ti{sub 4}CrO{sub 18} exhibits the paramagnetic state, whereas SrBi{sub 5}Ti{sub 4}Cr{sub 0.5}Co{sub 0.5}O{sub 18} undergoes a ferrimagnetic transition at 89 K originating from the antiferromagnetic coupling of Cr-based and Co-based sublattices. In addition, SrBi{sub 5}Ti{sub 4}Cr{sub 0.5}Co{sub 0.5}O{sub 18} shows a typical spin-glass behavior below 89 K with zν = 6.02 and τ{sub 0} = (1.75 ± 0.33) × 10{sup −14} s as evidenced by the results of the frequency dependence of ac susceptibility and magnetic relaxation measurements. In particular, both the dielectric constant and dielectric loss of SrBi{sub 5}Ti{sub 4}Cr{sub 0.5}Co{sub 0.5}O{sub 18} exhibit the characteristics of dielectric relaxation around 89 K with the activation energy of (0.14 ± 0.02) eV, which can be ascribed to the electron hopping of Co{sup 2+}-V{sub O}-Co{sup 3+} through the bridging oxygen vacancies.