At least 145 records · Page 8

Impact decapitation from laboratory to basin scales

Although vertical hypervelocity impacts result in the annihilation (melting/vaporization) of the projectile, oblique impacts (less than 15 deg) fundamentally change the partitioning of energy with fragments as large as 10 percent of the original projectile surviving. Laboratory experiments reveal that both ductile and brittle projectiles produce very similar results where limiting disruption depends on stresses proportional to the vertical velocity component. Failure of the projectile at laboratory impact velocities (6 km/s) is largely controlled by stresses established before the projectile has penetrated a significant distance into the target. The planetary surface record exhibits numerous examples of oblique impacts with evidence fir projectile failure and downrange sibling collisions.

Schultz, P. H.↗

Transient Reliability Analysis Capability Developed for CARES/Life

The CARES/Life software developed at the NASA Glenn Research Center provides a general-purpose design tool that predicts the probability of the failure of a ceramic component as a function of its time in service. This award-winning software has been widely used by U.S. industry to establish the reliability and life of a brittle material (e.g., ceramic, intermetallic, and graphite) structures in a wide variety of 21st century applications.Present capabilities of the NASA CARES/Life code include probabilistic life prediction of ceramic components subjected to fast fracture, slow crack growth (stress corrosion), and cyclic fatigue failure modes. Currently, this code can compute the time-dependent reliability of ceramic structures subjected to simple time-dependent loading. For example, in slow crack growth failure conditions CARES/Life can handle sustained and linearly increasing time-dependent loads, whereas in cyclic fatigue applications various types of repetitive constant-amplitude loads can be accounted for. However, in real applications applied loads are rarely that simple but vary with time in more complex ways such as engine startup, shutdown, and dynamic and vibrational loads. In addition, when a given component is subjected to transient environmental and or thermal conditions, the material properties also vary with time. A methodology has now been developed to allow the CARES/Life computer code to perform reliability analysis of ceramic components undergoing transient thermal and mechanical loading. This means that CARES/Life will be able to analyze finite element models of ceramic components that simulate dynamic engine operating conditions. The methodology developed is generalized to account for material property variation (on strength distribution and fatigue) as a function of temperature. This allows CARES/Life to analyze components undergoing rapid temperature change in other words, components undergoing thermal shock. In addition, the capability has been developed to perform reliability analysis for components that undergo proof testing involving transient loads. This methodology was developed for environmentally assisted crack growth (crack growth as a function of time and loading), but it will be extended to account for cyclic fatigue (crack growth as a function of load cycles) as well.

Nemeth, Noel N.↗

An elastic failure model of indentation damage

A mechanistically consistent model for indentation damage based on elastic failure at tensile or shear overloads, is proposed. The model accommodates arbitrary crack orientation, stress relaxation, reduction and recovery of stiffness due to crack opening and closure, and interfacial friction due to backward sliding of closed cracks. This elastic failure model was implemented by an axisymmetric finite element program which was used to simulate progressive damage in a silicon nitride plate indented by a tungsten carbide sphere. The predicted damage patterns and the permanent impression matched those observed experimentally. The validation of this elastic failure model shows that the plastic deformation postulated by others is not necessary to replicate the indentation damage of brittle structural ceramics.

Liaw, B. M.↗

Proof Test Diagrams for a Lithia-Alumina-Silica Glass-Ceramic

The glass-ceramic (Zerodur, Schott Glaswerke, Mainz, Germany) contains 70% to 78% by weight crystalline phase of high-quartz structure with a mean crystal size of 50-55 nm. The vitreous phase has a positive thermal expansion coefficient which is practically balanced by the negative coefficient of the crystalline phase. This results in a material which can maintain longitudinal stability during thermal cycling. This was one of the reasons for its choice as the material for the grazing incidence mirrors for the Chandra X-Ray Facility. Brittle materials such as glass and glass-ceramics which exhibit slow crack growth and subsequent fast fracture to failure exhibit a time dependence in strength. The decrease in strength for a constant applied load is known as static fatigue. In many cases, environment plays a major role in the material lifetime. It has been shown for silicate glasses that crack velocity will increase as the amount of water vapor in the environment surface finish and rate of loading. A rough surface finish leads to a lower tensile strength than for an optically polished surface. The strength of glass is observed in general to increase with increasing load rate. This phenomena is known as dynamic fatigue. This was observed for Zerodur by Tucker and Gent and Tucker in previous dynamic fatigue studies, in which lifetimes were obtained. All of the above named factors need to be considered when glass is to be used in load bearing applications.

Tucker, Dennis S.↗

A bilinear failure criterion for mixed-mode delamination

Many different failure criteria have been suggested for mixed-mode delamination toughness, but few sets of mixed-mode data exist that are consistent over the full range of Mode 1 opening load to Mode 2 shear load range. The mixed-mode bending (MMB) test was used to measure the delamination toughness of a brittle epoxy composite, a state-of-the-art toughened epoxy composite, and a tough thermoplastic composite over the full mixed-mode range. To gain insight into the different failure responses of the different materials, the delamination fracture surfaces were also examined. An evaluation of several failure criteria that have been reported in the literature was performed, and the range of responses modeled by each criterion was analyzed. A bilinear failure criterion was introduced based on a change in the failure mechanism observed from the delamination surfaces. The different criteria were compared to the failure response of the three materials tested. The responses of the two epoxies were best modeled with the new bilinear failure criterion. The failure response of the tough thermoplastic composite could be modeled well with the bilinear criterion but could also be modeled with the more simple linear failure criterion. Since the materials differed in their mixed-mode failure response, mixed-mode delamination testing will be needed to characterize a composite material. This paper presents consistent sets of mixed-mode data, provides a critical evaluation of the mixed-mode failure criteria, and should provide general guidance for selecting an appropriate criterion for other materials.

Reeder, James R.↗

A review and assessment of the stress-intensity factors for surface cracks

The stress-intensity factor solutions proposed for a surface crack in a finite plate subjected to uniform tension are reviewed. Fourteen different solutions for the stress-intensity factors are compared. These solutions were obtained over the past 16 years using approximate analytical methods, experimental methods, and engineering estimates. The accuracy is assessed of the various solutions by correlating fracture data on surface-cracked tension specimens made of a brittle epoxy material. Fracture of the epoxy material was characterized by a constant value of stress-intensity factor at failure. Thus, the correctness of the various solutions is judged by the variations in the stress-intensity factors at failure. The solutions were ranked in order of minimum standard deviation. The highest ranking solutions correlated 95 percent of data analyzed within + or - 10 percent, whereas the lowest ranking solutions correlated 95 percent of data analyzed within + or - 20 percent. However, some solutions could be applied to all data considered, whereas others are limited with respect to crack shapes and crack sizes that could be analyzed.

Newman, J. C., Jr.↗

A review and assessment of the stress-intensity factors for surface cracks

The stress-intensity factor solutions proposed for a surface crack in a finite plate subjected to uniform tension are reviewed. Fourteen different solutions obtained over the past 16 years using approximate analytical methods, experimental methods, and engineering estimates are compared. The accuracy of the various solutions is assessed by correlating fracture data on surface-cracked tension specimens made of a brittle epoxy material. Fracture of the epoxy material was characterized by a constant value of stress-intensity factor as failure. Thus, the correctness of various solutions is judged by the variations in the stress-intensity factors at failure. The solutions were ranked in order of minimum standard deviation. The highest ranking solutions correlated 95% of data analyzed within + or - 10% whereas the lowest ranking solutions correlated 95% of data analyzed within + or - 20%. Some solutions could be applied to all data considered, whereas others were limited with respect to crack shapes and crack sizes that could be analyzed.

Newman, J. C., Jr.↗

Design and development of ceramic components

The development of the AGT 100 turbine components in structural ceramic materials is described. Development is defined as the complete and iterative cycle from design, analysis, test, and design refinement culminating in successful demonstration of the design requirements. The components are analyzed by a linear elastic probabilistic approach, which involves finite element (three- and/or two-dimensional) simulation of the component combined with a Weibull characterization of the brittle ceramic material strength distribution to calculate a probability of survival for the component in the operating environment. Component test failure investigation has resulted in design modifications, and an improvement in component reliability has been demonstrated. Engine testing (over 570 h to date) continues to assess design/development of structural ceramic components.

Holtman, R. L.↗

Indigenous lunar construction materials

The utilization of local resources for the construction and operation of a lunar base can significantly reduce the cost of transporting materials and supplies from Earth. The feasibility of processing lunar regolith to form construction materials and structural components is investigated. A preliminary review of potential processing methods such as sintering, hot-pressing, liquification, and cast basalt techniques, was completed. The processing method proposed is a variation on the cast basalt technique. It involves liquification of the regolith at 1200-1300 C, casting the liquid into a form, and controlled cooling. While the process temperature is higher than that for sintering or hot-pressing (1000-1100 C), this method is expected to yield a true engineering material with low variability in properties, high strength, and the potential to form large structural components. A scenario for this processing method was integrated with a design for a representative lunar base structure and potential construction techniques. The lunar shelter design is for a modular, segmented, pressurized, hemispherical dome which could serve as habitation and laboratory space. Based on this design, estimates of requirements for power, processing equipment, and construction equipment were made. This proposed combination of material processing method, structural design, and support requirements will help to establish the feasibility of lunar base construction using indigenous materials. Future work will refine the steps of the processing method. Specific areas where more information is needed are: furnace characteristics in vacuum; heat transfer during liquification; viscosity, pouring and forming behavior of molten regolith; design of high temperature forms; heat transfer during cooling; recrystallization of basalt; and refinement of estimates of elastic moduli, compressive and tensile strength, thermal expansion coefficient, thermal conductivity, and heat capacity. The preliminary design of the lunar shelter showed us that joining is a critical technology needed for building a structure from large segments. The problem of joining is important to the design of any structure that is not completely prefabricated. It is especially important when the structure is subjected to tensile loading by an internal pressure. For a lunar shelter constructed from large segments the joints between these large segments must be strong, and they must permit automated construction. With a cast basalt building material which is brittle, there is the additional problem of connecting the joint with the material and avoiding stress concentration that would cause failure. Thus, a well-defined project which we intend to pursue during this coming year is the design of joints for cast basalt structural elements.

Rogers, Wayne P.↗

An experimental study of the mechanism of failure of rocks under borehole jack loading

Laboratory and field tests with an experimental jack and an NX-borehole jack are reported. The following conclusions were made: Under borehole jack loading, a circular opening in a brittle solid fails by tensile fracturing when the bearing plate width is not too small. Two proposed contact stress distributions can explain the mechanism of tensile fracturing. The contact stress distribution factor is a material property which can be determined experimentally. The borehole tensile strength is larger than the rupture flexural strength. Knowing the magnitude and orientation of the in situ stress field, borehole jack test results can be used to determine the borehole tensile strength. Knowing the orientation of the in situ stress field and the flexural strength of the rock substance, the magnitude of the in situ stress components can be calculated. The detection of very small cracks is essential for the accurate determination of the failure loads which are used in the calculation of strengths and stress components.

Van, T. K.↗

Hot tensile tests of Inconel 718

The physical metallurgy of near-solidus integranular cracking in Inconel 718 welds was investigated. The data, although inconclusive, suggest at least two mechanisms which might explain intergranular cracking (microfissuring) in the heat-affected zone of several high temperature alloys. One theory is based on the separation of intergranular liquid while the other involves mechanical failure of solid ligaments surrounded by intergranular liquid. Both mechanisms concentrate strain in the grain boundaries resulting in low strain (1%) intergranular brittleness. The mechanisms reported might also pertain to the physical metallurgy of casting, powder metallurgy sintering and hot isostatic pressing.

Source record↗

Influence of the resin on interlaminar mixed-mode fracture

Both literature review data and new data on toughness behavior of seven matrix and adhesive systems in four types of tests were studied in order to assess the influence of the resin on interlaminar fracture. Mixed mode (i.e., various combinations of opening mode 1, G sub 1, and shearing mode 2; G sub 2) fracture toughness data showed that the mixed mode relationship for failure appears to be linear in terms of G sub 1 and G sub 2. The study further indicates that fracture of brittle resins is controlled by the G sub 1 component, and that fracture of many tough resins is controlled by total strain-energy release rate, G sub T. Regarding the relation of polymer structure and the mixed mode fracture: high mode 1 toughness requires resin dilatation; dilatation is low in unmodified epoxies at room temperature/dry conditions; dilatation is higher in plasticized epoxies, heated epoxies, and in modified epoxies; modification improves mode 2 toughness only slightly compared with mode 1 improvements. Analytical aspects of the cracked lap shear test specimen were explored.

Johnson, W. S.↗

Influence of the resin on interlaminar mixed-mode fracture

Both literature review data and new data on toughness behavior of seven matrix and adhesive systems in four types of tests were studied in order to assess the influence of the resin on interlaminar fracture. Mixed mode (i.e., various combinations of opening mode 1, G sub 1, and shearing mode 2; G sub 2) fracture toughness data showed that the mixed mode relationship for failure appears to be linear in terms of G sub 1 and G sub 2. The study further indicates that fracture of brittle resins is controlled by the G sub 1 component, and that fracture of many tough resins is controlled by total strain-energy release rate, G sub T. Regarding the relation of polymer structure and the mixed mode fracture: high mode 1 toughness requires resin dilatation; dilatation is low in unmodified epoxies at room temperature/dry conditions; dilatation is higher in plasticized epoxies, heated epoxies, and in modified epoxies; modification improves mode 2 toughness only slightly compared with mode 1 improvements. Analytical aspects of the cracked lap shear test specimen were explored.

Johnson, W. S.↗

Fracture surfaces of irradiated composites

Electron microscopy was used to analyze the fracture surfaces of T300/934 graphite/epoxy unidirectional off-axis tensile coupons which were subjected to 1.0-MeV electron radiation at a rate of 50 Mrad/h for a total dose of 10 Grad. Fracture surfaces from irradiated and nonirradiated specimens tested at 116 K, room temperature, and 394 K were analyzed to assess the influence of radiation and temperature on the mode of failure and variations in constituent material as a function of environmental exposure. Micrographs of fracture surfaces indicate that irradiated specimens are more brittle than nonirradiated specimens at low temperatures. However, at elevated temperatures the irradiated specimens exhibit significantly more plasticity than nonirradiated specimens.

Milkovich, Scott M.↗

The kinetic and mechanical aspects of hydrogen-induced failure in metals

Premature hydrogen-induced failure observed to occur in many metal systems involves three stages of fracture: (1) crack initiation, (2) stable slow crack growth, and (3) unstable rapid crack growth. The presence of hydrogen at some critical location on the metal surface or within the metal lattice was shown to influence one or both of the first two stages of brittle fracture but has a negligible effect on the unstable rapid crack growth stage. The relative influence of the applied parameters of time, temperature, etc., on the propensity of a metal to exhibit hydrogen induced premature failure was investigated.

Nelson, H. G.↗

Fabrication of Lanthanum Telluride 14-1-11 Zintl High-Temperature Thermoelectric Couple

The development of more efficient thermoelectric couple technology capable of operating with high-grade heat sources up to 1,275 K is key to improving the performance of radioisotope thermoelectric generators. Lanthanum telluride La3-xTe4 and 14-1-11 Zintls (Yb14MnSb11) have been identified as very promising materials. The fabrication of advanced high-temperature thermoelectric couples requires the joining of several dissimilar materials, typically including a number of diffusion bonding and brazing steps, to achieve a device capable of operating at elevated temperatures across a large temperature differential (up to 900 K). A thermoelectric couple typically comprises a heat collector/ exchanger, metallic interconnects on both hot and cold sides, n-type and ptype conductivity thermoelectric elements, and cold-side hardware to connect to the cold-side heat rejection and provide electrical connections. Differences in the physical, mechanical, and chemical properties of the materials that make up the thermoelectric couple, especially differences in the coefficients of thermal expansion (CTE), result in undesirable interfacial stresses that can lead to mechanical failure of the device. The problem is further complicated by the fact that the thermoelectric materials under consideration have large CTE values, are brittle, and cracks can propagate through them with minimal resistance. The inherent challenge of bonding brittle, high-thermal-expansion thermoelectric materials to a hot shoe material that is thick enough to carry the requisite electrical current was overcome. A critical advantage over prior art is that this device was constructed using all diffusion bonds and a minimum number of assembly steps. The fabrication process and the materials used are described in the following steps: (1) Applying a thin refractory metal foil to both sides of lanthanum telluride. To fabricate the n-type leg of the advanced thermoelectric couple, the pre-synthesized lanthanum telluride coupon was diffusion bonded to the metal foil using a thin adhesion layer. (2) Repeating a similar process for the 14-1-11 Zintl p-type leg of the advanced thermoelectric couple. (3) Bonding thick CTE-matched metal plates on the metallized lanthanum telluride and Yb14MnSb11 to form the hot and cold sides of the thermoelectric couple. The calculated conversion efficiency of such an advanced couple would be about 10.5 percent, about 35 percent better than heritage radioisotope thermoelectric technology that relies on Si-Ge alloys. In addition, unlike Si-Ge alloys, these materials can be combined with many other thermoelectric materials optimized for operation at lower temperatures to achieve conversion efficiency in excess of 15 percent (a factor of 2 increase over heritage technology).

Ravi, Vilupanur A.↗

Fracture toughness and the effects of stress state on fracture of nickel aluminides

The effects of stress state on the fracture behavior of Ni3Al, Ni3Al + B, and NiAl were determined using either notched or fatigue-precracked bend bars tested to failure at room temperature, in addition to testing specimens in tension under superposed hydrostatic pressure. Although Ni3Al is observed to fail in a macroscopically brittle intergranular manner in tension tests conducted at room temperature, the fracture toughnesses presently obtained on Ni3Al exceeded 20 MPam, and R-curve behavior was exhibited. In situ monitoring of the fracture experiments was utilized to aid in interpreting the source(s) of the high toughness in Ni3Al, while SEM fractography was utilized to determine the operative fracture modes. The superposition by hydrostatic pressure during tensile testing of NiAl specimens was observed to produce increased ductility without changing the fracture mode.

Lewandowski, John J.↗

Microstructure, Mechanical Properties, Hot-Die Forming, and Joining of 47XD Gamma TiAl Rolled Sheets

The microstructure and mechanical properties, along with the hot-die forming and joining of Ti-47Al-2Nb-2Mn-0.8 vol% TiB, sheets (known as 47XD), produced by a low-cost rolling process, were evaluated. A near-gamma microstructure was obtained in the as-rolled condition. The microstructures of heat-treated sheets ranged from a recrystallized equiaxed near-gamma microstructure at 1,200 to 1,310 C, to a duplex microstructure at 1,350 C, to a fully lamellar microstructure at 1,376 C. Tensile behavior was determined for unidirectionally rolled and cross-rolled sheets for room temperature (RT) to 816 C. Yield stress decreased gradually with increasing deformation temperature up to 704 C; above 704 C, it declined rapidly. Ultimate tensile strength exhibited a gradual decrease up to 537 C before peaking at 704 C, followed by a rapid decline at 816 C. The modulus showed a gradual decrease with temperature, reaching approximately 72% of the RT value at 816 C. Strain to failure increased slowly from RT to 537 C; between 537 C and 704 C it exhibited a phenomenal increase, suggesting that the ductile-brittle transition temperature was below 704 C. Fracture mode changed from transgranular fracture at low temperature, to a mixture of transgranular and intergranular fracture at intermediate temperature, to ductile fracture at 816 C, coupled with dynamic recrystallization at large strains. Creep rupture response was evaluated between 649 and 816 C over the stress range of 69 to 276 MPa. Deformation parameters for steady-state creep rate and time-to-rupture were similar: activation energies of approximately 350 kJ/mol and stress exponents of approximately 4.5. Hot-die forming of sheets into corrugations was done at elevated temperatures in vacuum. The process parameters to join sheets by diffusion bonding and brazing with TiCuNi 70 filler alloy were optimized for test coupons and successfully used to fabricate large truss-core and honeycomb structures. Nondestructive evaluation methods, e.g., ultrasonic C-scans and thermography along with metallography, were used to characterize bond quality. Microstructural evaluation during heat treatment, identification of phases at the braze/matrix interface, determination of shear strengths of brazed joints, and deformation mechanisms during tensile and creep processes will be discussed.

Das, G.↗