Search NASA⌕ Search

SEARCH · Search NASA

Results for “CASTING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Cast Stone Formulation At Higher Sodium Concentrations

A low temperature waste form known as Cast Stone is being considered to provide supplemental Low Activity Waste (LAW) immobilization capacity for the Hanford site. Formulation of Cast Stone at high sodium concentrations is of interest since a significant reduction in the necessary volume of Cast Stone and subsequent disposal costs could be achieved if an acceptable waste form can be produced with a high sodium molarity salt solution combined with a high water to premix (or dry blend) ratio. The objectives of this study were to evaluate the factors involved with increasing the sodium concentration in Cast Stone, including production and performance properties and the retention and release of specific components of interest. Three factors were identified for the experimental matrix: the concentration of sodium in the simulated salt solution, the water to premix ratio, and the blast furnace slag portion of the premix. The salt solution simulants used in this study were formulated to represent the overall average waste composition. The cement, blast furnace slag, and fly ash were sourced from a supplier in the Hanford area in order to be representative. The test mixes were prepared in the laboratory and fresh properties were measured. Fresh density increased with increasing sodium molarity and with decreasing water to premix ratio, as expected given the individual densities of these components. Rheology measurements showed that all of the test mixes produced very fluid slurries. The fresh density and rheology data are of potential value in designing a future Cast Stone production facility. Standing water and density gradient testing showed that settling is not of particular concern for the high sodium compositions studied. Heat of hydration measurements may provide some insight into the reactions that occur within the test mixes, which may in turn be related to the properties and performance of the waste form. These measurements showed that increased sodium concentration in the salt solution reduced the time to peak heat flow, and reducing the amount of slag in the premix increased the time to peak heat flow. These observations may help to describe some of the cured properties of the samples, in particular the differences in compressive strength observed after 28 and 90 days of curing. Samples were cured for at least 28 days at ambient temperature in the laboratory prior to cured properties analyses. The low activity waste form for disposal at the Hanford Site is required to have a compressive strength of at least 500 psi. After 28 days of curing, several of the test mixes had mean compressive strengths that were below the 500 psi requirement. Higher sodium concentrations and higher water to premix ratios led to reduced compressive strength. Higher fly ash concentrations decreased the compressive strength after 28 days of curing. This may be explained in that the cementitious phases matured more quickly in the mixes with higher concentrations of slag, as evidenced by the data for the time to peak heat generation. All of the test mixes exhibited higher mean compressive strengths after 90 days of curing, with only one composition having a mean compressive strength of less than 500 psi. Leach indices were determined for the test mixes for contaminants of interest. The leaching performance of the mixes evaluated in this study was not particularly sensitive to the factors used in the experimental design. This may be beneficial in demonstrating that the performance of the waste form is robust with respect to changes in the mix composition. The results of this study demonstrate the potential to achieve significantly higher waste loadings in Cast Stone and other low temperature, cementitious waste forms. Additional work is needed to elucidate the hydration mechanisms occurring in Cast Stone formulated with highly concentrated salt solutions since these reactions are responsible for determining the performance of the cured waste form. The thermal analyses completed in this study provide some preliminary insight, although the limited range of the factors in the test matrix hindered the identification of individual component effects. Future work should involve broader factor ranges to identify the roles played by each of the components in the mix via thermal analyses, analytical microscopy, and characterization of phase formation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Cast Stone Formulation At Higher Sodium Concentrations

A low temperature waste form known as Cast Stone is being considered to provide supplemental Low Activity Waste (LAW) immobilization capacity for the Hanford site. Formulation of Cast Stone at high sodium concentrations is of interest since a significant reduction in the necessary volume of Cast Stone and subsequent disposal costs could be achieved if an acceptable waste form can be produced with a high sodium molarity salt solution combined with a high water to premix (or dry blend) ratio. The objectives of this study were to evaluate the factors involved with increasing the sodium concentration in Cast Stone, including production and performance properties and the retention and release of specific components of interest. Three factors were identified for the experimental matrix: the concentration of sodium in the simulated salt solution, the water to premix ratio, and the blast furnace slag portion of the premix. The salt solution simulants used in this study were formulated to represent the overall average waste composition. The cement, blast furnace slag, and fly ash were sourced from a supplier in the Hanford area in order to be representative. The test mixes were prepared in the laboratory and fresh properties were measured. Fresh density increased with increasing sodium molarity and with decreasing water to premix ratio, as expected given the individual densities of these components. Rheology measurements showed that all of the test mixes produced very fluid slurries. The fresh density and rheology data are of potential value in designing a future Cast Stone production facility. Standing water and density gradient testing showed that settling is not of particular concern for the high sodium compositions studied. Heat of hydration measurements may provide some insight into the reactions that occur within the test mixes, which may in turn be related to the properties and performance of the waste form. These measurements showed that increased sodium concentration in the salt solution reduced the time to peak heat flow, and reducing the amount of slag in the premix increased the time to peak heat flow. These observations may help to describe some of the cured properties of the samples, in particular the differences in compressive strength observed after 28 and 90 days of curing. Samples were cured for at least 28 days at ambient temperature in the laboratory prior to cured properties analyses. The low activity waste form for disposal at the Hanford Site is required to have a compressive strength of at least 500 psi. After 28 days of curing, several of the test mixes had mean compressive strengths that were below the 500 psi requirement. Higher sodium concentrations and higher water to premix ratios led to reduced compressive strength. Higher fly ash concentrations decreased the compressive strength after 28 days of curing. This may be explained in that the cementitious phases matured more quickly in the mixes with higher concentrations of slag, as evidenced by the data for the time to peak heat generation. All of the test mixes exhibited higher mean compressive strengths after 90 days of curing, with only one composition having a mean compressive strength of less than 500 psi. Leach indices were determined for the test mixes for contaminants of interest. The leaching performance of the mixes evaluated in this study was not particularly sensitive to the factors used in the experimental design. This may be beneficial in demonstrating that the performance of the waste form is robust with respect to changes in the mix composition. The results of this study demonstrate the potential to achieve significantly higher waste loadings in Cast Stone and other low temperature, cementitious waste forms. Additional work is needed to elucidate the hydration mechanisms occurring in Cast Stone formulated with highly concentrated salt solutions since these reactions are responsible for determining the performance of the cured waste form. The thermal analyses completed in this study provide some preliminary insight, although the limited range of the factors in the test matrix hindered the identification of individual component effects. Future work should involve broader factor ranges to identify the roles played by each of the components in the mix via thermal analyses, analytical microscopy, and characterization of phase formation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Characterization of Technetium Speciation in Cast Stone

This report describes the results from laboratory tests performed at Pacific Northwest National Laboratory (PNNL) for the U.S. Department of Energy (DOE) EM-31 Support Program (EMSP) subtask, “Production and Long-Term Performance of Low Temperature Waste Forms” to provide additional information on technetium (Tc) speciation characterization in the Cast Stone waste form. To support the use of Cast Stone as an alternative to vitrification for solidifying low-activity waste (LAW) and as the current baseline waste form for secondary waste streams at the Hanford Site, additional understanding of Tc speciation in Cast Stone is needed to predict the long-term Tc leachability from Cast Stone and to meet the regulatory disposal-facility performance requirements for the Integrated Disposal Facility (IDF). Characterizations of the Tc speciation within the Cast Stone after leaching under various conditions provide insights into how the Tc is retained and released. The data generated by the laboratory tests described in this report provide both empirical and more scientific information to increase our understanding of Tc speciation in Cast Stone and its release mechanism under relevant leaching processes for the purpose of filling data gaps and to support the long-term risk and performance assessments of Cast Stone in the IDF at the Hanford Site.

Cast Stone↗

Cast Stone Formulation At Higher Sodium Concentrations

A low temperature waste form known as Cast Stone is being considered to provide supplemental Low Activity Waste (LAW) immobilization capacity for the Hanford site. Formulation of Cast Stone at high sodium concentrations is of interest since a significant reduction in the necessary volume of Cast Stone and subsequent disposal costs could be achieved if an acceptable waste form can be produced with a high sodium molarity salt solution combined with a high water to premix (or dry blend) ratio. The objectives of this study were to evaluate the factors involved with increasing the sodium concentration in Cast Stone, including production and performance properties and the retention and release of specific components of interest. Three factors were identified for the experimental matrix: the concentration of sodium in the simulated salt solution, the water to premix ratio, and the blast furnace slag portion of the premix. The salt solution simulants used in this study were formulated to represent the overall average waste composition. The cement, blast furnace slag, and fly ash were sourced from a supplier in the Hanford area in order to be representative. The test mixes were prepared in the laboratory and fresh properties were measured. Fresh density increased with increasing sodium molarity and with decreasing water to premix ratio, as expected given the individual densities of these components. Rheology measurements showed that all of the test mixes produced very fluid slurries. The fresh density and rheology data are of potential value in designing a future Cast Stone production facility. Standing water and density gradient testing showed that settling is not of particular concern for the high sodium compositions studied. Heat of hydration measurements may provide some insight into the reactions that occur within the test mixes, which may in turn be related to the properties and performance of the waste form. These measurements showed that increased sodium concentration in the salt solution reduced the time to peak heat flow, and reducing the amount of slag in the premix increased the time to peak heat flow. These observations may help to describe some of the cured properties of the samples, in particular the differences in compressive strength observed after 28 and 90 days of curing. Samples were cured for at least 28 days at ambient temperature in the laboratory prior to cured properties analyses. The low activity waste form for disposal at the Hanford Site is required to have a compressive strength of at least 500 psi. After 28 days of curing, several of the test mixes had mean compressive strengths that were below the 500 psi requirement. Higher sodium concentrations and higher water to premix ratios led to reduced compressive strength. Higher fly ash concentrations decreased the compressive strength after 28 days of curing. This may be explained in that the cementitious phases matured more quickly in the mixes with higher concentrations of slag, as evidenced by the data for the time to peak heat generation. All of the test mixes exhibited higher mean compressive strengths after 90 days of curing, with only one composition having a mean compressive strength of less than 500 psi. Leachability indices were determined for the test mixes for contaminants of interest. The leaching performance of the mixes evaluated in this study was not particularly sensitive to the factors used in the experimental design. This may be beneficial in demonstrating that the performance of the waste form is robust with respect to changes in the mix composition. The results of this study demonstrate the potential to achieve significantly higher waste loadings in Cast Stone and other low temperature, cementitious waste forms. Additional work is needed to elucidate the hydration mechanisms occurring in Cast Stone formulated with highly concentrated salt solutions since these reactions are responsible for determining the performance of the cured waste form. The thermal analyses completed in this study provide some preliminary insight, although the limited range of the factors in the test matrix hindered the identification of individual component effects. Future work should involve broader factor ranges to identify the roles played by each of the components in the mix via thermal analyses, analytical microscopy, and characterization of phase formation.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Nuclear Metal Fuel Casting Modeling (Annual Report 2012)

In fiscal year 2012, FLOW3D was used to develop an understanding of the metallic nuclear fuel casting processes. There were two major accomplishments for FY12, 1) a rank-order list of the most important material properties to measure, 2) simulation of alternative mold-fill methods. We performed a design of experiments study to quantify several material properties and their impact on effective mold fill, for both circular and annular fuel rod geometries. The most important fuel material property to be measured is the wetting angle of the molten metal on the coated mold material (coated graphite). The second most important property to measure is the surface tension of the molten metal in argon gas at the design mold pressure. The magnitude of these material properties had the largest effect on whether the mold casting processes produced large voids in the fuel rods. The nominal mold fill method used in the above study was the gravity assisted top-fill method of the Idaho National Laboratory Bench Scale Casting facility. Alternative mold fill methods were investigated and using a bottom-fill method shows promise. In the bottom-fill method, the molten metal is injected into the bottom of the mold and the argon cover gas is allowed to escape through vents at the top of the mold. This allows for a smooth, uniform fill of the mold, where as the top-fill geometry has a counter-flow condition of the molten metal and argon cover gas. The mold is initially filled with argon, and using a top fill method, the molten metal must flow downward into the mold and the argon is displaced by the metal and must flow upward out of the mold. This counter-flow condition creates large voids in the cast because bubbles of argon get trapped as the metal flows into the mold. We also investigated various venting schemes for the top fill casting process and this also shows some promise to mitigate the void formation. In fiscal year 2013, we will continue to investigate mold fill approaches. We will use the results of the FY2012 work and begin investigating the segregation of binary alloys for these casting approaches and recommend separate effects testing requirements. If data becomes available from the BSC, we will calibrate the computational models and identify optimum casting parameters. Finally, we will study the feasibility of extending the calibrated model to ternary flow problem by developing appropriate scaled models.

1.02.02.02↗

Improving the Mechanical Properties of Cast Aluminum Via Ultrasonication-Induced Microstructural Refinement

One barrier to the broader use of cast aluminum alloys in automotive applications is their poor mechanical properties, especially compared to wrought materials. This study investigates the use of ultrasound to refine the microstructure of cast aluminum alloys during solidification and thus improve their mechanical properties. An A356 aluminum alloy (Al-Si-Mg) with added Fe (to mimic a recycle-grade alloy) was cast in a graphite mold with the simultaneous application of ultrasound. Tensile specimens were extracted from the castings and heat treated to a T6 temper. Ultrasonication during casting transformed the morphology of primary aluminum grains from dendritic (~140 microns in size) to globular (~36 microns in size), increased the ultimate tensile strength by 10 %, and tripled the ductility compared to casting without ultrasound. This improvement in strength and ductility demonstrates the potential for ultrasonic processing to improve the performance of cast aluminum alloys without altering their chemistry or additional post-processing.

Aluminum, Solidification, Ultrasound, Grain refinm↗

Microstructural Evolution and Mechanical Behavior of Lead-Free Silicon Brass Manufactured by Low-Pressure Die Casting

Low-pressure die casting (LPDC) has been widely used to process aluminum and magnesium alloys; however, it has yet to be applied to manufacture brass alloys. This study investigates the microstructural evolution and mechanical behavior of a lead-free CuZnSiAl silicon brass via a variable-controlling approach on the basis of a faucet casting by LPDC. The manufactured silicon brass castings are predominantly composed of bcc β-CuZn(Si, Al) and minor fcc α-Cu(Zn, Si) solid solutions. The silicon brass castings also predominantly exhibit short rod-like or granular α phases, which distinctly differ from the acicular α morphology obtained by conventional gravity casting. The manufactured silicon brass castings which contain finer β grains and short rod-like or granular α phase exhibit superior mechanical properties. Their optimal mechanical properties—elongation of 15.0%, yield strength of 359.8 MPa, and ultimate tensile strength of 598.9 MPa—are far superior to those of the typical lead brass HPb59-1. The results obtained in this study provide insight into the manufacture and design of lead-free silicon brass castings by LDPC.

36 MATERIALS SCIENCE↗

Ageless Aluminum-Cerium-Based Alloys in High-Volume Die Casting for Improved Energy Efficiency

Strong chemical reactions between Al and Ce lead to the formation of intermetallics with exceptional thermal stability. The rapid formation of intermetallics directly from the liquid phase during solidification of Al-Ce alloys leads to an ultrafine microconstituent structure that effectively strengthens as-cast alloys without further microstructural optimization via thermal processing. Die casting is a high-volume manufacturing technology that accounts for greater than 40% of all cast Al products, whereas Ce is highly overproduced as a waste product of other rare earth element (REE) mining. Reducing heat treatments would stimulate significant improvements in manufacturing energy efficiency, exceeding (megatonnes/year) per large-scale heat-treatment line. In this study, multiple compositions were evaluated with wedge mold castings to test the sensitivity of alloys to the variable solidification rate inherent in high-pressure die casting. Once a suitable composition was determined, it was successfully demonstrated at 800 lbs/h in a 600-ton die caster, after which the as-die cast parts performed similarly to ubiquitous A380 in the same geometry without requiring heat treatment. Furthermore, this work demonstrates the compatibility of Al REE alloys with high-volume die-casting applications with minimal heat treatments.

36 MATERIALS SCIENCE↗

Low Temperature Age Hardening in Cast Uranium-6 wt. pct. Niobium

An investigation to determine whether cast U-6Nb would exhibit low temperature (<250°C) age hardening behavior, which has been well-documented in wrought U-6Nb, was performed using a 6 year old near-cylindrical U-6Nb casting, courtesy of AWE, UK. The casting was sectioned, and metallographic cubes and tensile bars were machined and subjected to a variety of heat treatments. Our results indicate that the cast U-6Nb has a larger grain size than wrought U-6Nb, ranging from ~200-500 μm, and that these grains are equiaxed. A significant quantity of inclusions are present at the <10 μm size range and appear to be carbides, based on their morphology (faceted) and color (dark gray). There does not appear to be significant porosity present and the few pores observed were <40 μm in size and spherical. Tensile bars (TBs) were lathe machined, solutionized, then water quenched prior to testing. A group of TBs were subjected to low temperature artificial aging heat treatments consisting of a hold at 200°C for 1 or 2h, followed by furnace cooling, all under a helium backfill. Mechanical testing confirms that cast U-6Nb TBs exhibit low temperature age hardening, with an increase in initial yield stress (Y1) of >425 MPa—a significant increase over wrought U-6Nb yield stress of 100-200 MPa for the same heat treatment. This increase is accompanied by a reduction in failure strain, which is indicative of a reduction in ductility. Modifying the heat treatment temperature and/or time may allow the properties to be tailored to the requirements. This study is intended as a preliminary investigation. Overall, this high impurity content casting exhibits a reasonable mechanical response which can be tailored in a consistent manner through low temperature heat treatment. As the result, a more comprehensive investigation of low temperature aging in cleaner cast U-6Nb, better representative of the state-of-the-art, shall be performed in FY19.

36 MATERIALS SCIENCE↗

Advanced Characterization of Microwave Melt Cast Uranium

For the last decade, the use of microwave (MW) melting and casting technology for processing uranium (U) has been under development at Y-12 National Security Complex in Oak Ridge, TN [2] . Their objective has been to determine if MW is a viable option to replace conventional vacuum induction melting (VIM) for some U part types. Some of the benefits of using MW technology are minimizing processing steps and decreasing impurity content by changing crucible material, which will help to lower costs and improve machinability, respectively. While Y-12 has shown success using a MW melting and casting process to make U parts [4, 5], it is still a relatively new technology for casting metals, and there are several unknowns with respect to how the material properties compare to conventional VIM cast U. One major concern, associated with MW casting of metals, is superheating, which can cause arcing or plasma formation in a part and result in non-uniform material properties. Therefore, studying the anisotropy in MW cast metals in terms of pertinent properties is highly relevant. Specifically, the properties of interest here are deformation behavior and mechanical properties of U tested at different strain rates and weldability of thin wall sections. In order to address concerns about high strain rate mechanical properties, prototype MW-U parts (processed in 2009) were sent to LLNL in 2015 for advanced materials testing. The parts received had relatively thin walls (~6 mm), so Split Hopkinson Pressure Bar was selected as a method for dynamic mechanical testing (strain rate of ~103s-1) since most other high-rate (HR) tests require much larger sample dimensions. A VIM-U part from Y-12 was not available at the time of the study, so a VIM part from Idaho National Laboratory, cast into a rectangular block, was used here for comparison.

36 MATERIALS SCIENCE↗

Characterization of Cast U-6Nb Sprue

Shape casting of uranium-6 wt. pct. niobium (U-6Nb) can produce near net shape components, providing a higher efficiency alternative to wrought processing. A substantial amount of materials characterization in support of direct casting process development has been performed and documented. This supplemental work describes the mechanical behavior of the hot top region of shape cast U-6Nb in order to determine and quantify the effect of casting defects, such as gas porosity and inclusions, on U-6Nb performance. The annular hot top region of a hollow cylindrical casting was sectioned and metallographic, bend, and tensile specimen blanks were machined from various locations around the part. Porosity ranging from 5-13% was observed, depending on the region sampled (i.e. top, bottom or outer portion of casting). Optical and scanning electron microscopy showed prior gamma grain size ranging from <10 up to 300 μm. There are uranium oxide and carbide inclusions present at the 50-150 μm size range; these were identified based on their morphology and color. Martensitic herringbone twinning and a lamellar structure was observed as well as what may be platelets of retained $γ$° in a matrix of $α$". The tensile test specimens were lathe machined and subjected to a low temperature artificial aging heat treatment consisting of a hold at 200°C for 2 hours, followed by furnace cooling in a helium atmosphere. Quasi-static mechanical tests showed a ductile void coalescence fracture mode with failure strains from 2-16% and a linear increase in stress up to approximately 400 MPa. Prior studies on low porosity regions sampled from a similar casting reported a failure strain of 15-21% in the artificially aged condition. The significant loss in ductility in the hot top region is attributed to increased porosity.

36 MATERIALS SCIENCE↗

VTR Casting Furnace Conceptual Design

This TEV describes the development of a conceptual design for a fuel casting system to be used in the development and demonstration of fuel designs for the new Versatile Test Reactor (VTR). This system will be installed in the Fuel Manufacturing Facility (FMF). The system will be in a shielded glovebox and will be used to melt fuel materials and injection cast these materials into fuel slugs, which will further be used to fabricate fuel elements for the VTR. This TEV covers only the injection casting system itself. Operations such as removing the castings from the injection molds, trimming of the castings, and installation of the castings into fuel element cladding are beyond the scope of the TEV. The conceptual design herein is principally concerned with the mechanical portion of the casting system and does not include details of the control or power supply systems.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Mitigate Stress Corrosion Cracking (SCC) in High-strength Al Castings (CRADA 508)

Development of high strength, corrosion resistant, aluminum alloys is important to a number of industries, including automotive, aerospace, power, etc. Understanding how processing methods such as casting, chemistry, additives and recycle content affect an alloy’s microstructure and performance in real world environments is crucial to their implementation. One major concern is how the repeated exposure to saline solutions can be detrimental to the structural integrity of aluminum alloy components. This study was undertaken as a collaboration between Eck Industries and PNNL to investigate the stress corrosion cracking (SCC) and corrosion behavior of aluminum alloys. This work examines the SCC response of three different materials set. First is cast A206 Al alloy produced by three different casting techniques (i.e., permanent mold, and sand casting with and without chill) and with or without nano forming additives as potential grain refiners. The second materials set comprises Al alloy tubes extruded by PNNL’s ShAPE process and produced using raw material with three different ratios of twitch and pre-consumer Al 6061 scrap. Finally, the third materials set comprises two Al-Si-Mg-Fe alloys with controlled Si% and Fe% to mimic recycle grade Al alloys. The corrosion behavior of these materials was characterized using SCC testing and scanning electrochemical cell microscopy (SECCM) technique; mechanical behavior was characterized using tensile testing, and microstructure was characterized using optical and electron microscopy techniques. Of the A206 Al alloys, the samples with nano forming additives performed poorly compared to those without. The best SCC performance (i.e. least degradation in mechanical properties) was demonstrated by A206 alloy sand cast with chill while the permanent mold sample showed the worst SCC performance. The SECCM was performed on A206 alloy sand cast with chill to understand the effect of microstructure and determine the location-dependent corrosion properties on grain boundaries (GB) and inside grains (IG) on the sample. The corrosion potential and current measured on GB and IG at various points on the sample established that the GB locations are more cathodic and corrosive than the IG locations. Further work needs to be conducted to investigate the mechanisms behind the observed dependence of SCC on casting technique and nano forming additives. Among the ShAPE extruded tubes, SECCM data suggests the decreasing order of tendency to corrode as follows: 100% twitch > 75% twitch > 50% twitch. Finally, both variants of the Al-Si-Mg-Fe alloys showed a large volume fraction of Fe- and Si-containing intermetallics and additional work is needed to discern differences in their respective corrosion responses. In summary, correlating local electrochemical behavior (e.g. via SECCM) with micro/nanostructure, in conjunction with bulk mechanical behavior, can help identify the right fabrication method and alloy chemistry to minimize SCC issues in Al alloys.

36 MATERIALS SCIENCE↗

Development of a CFD code for casting simulation

Because of high rejection rates for large structural castings (e.g., the Space Shuttle Main Engine Alternate Turbopump Design Program), a reliable casting simulation computer code is very desirable. This code would reduce both the development time and life cycle costs by allowing accurate modeling of the entire casting process. While this code could be used for other types of castings, the most significant reductions of time and cost would probably be realized in complex investment castings, where any reduction in the number of development castings would be of significant benefit. The casting process is conveniently divided into three distinct phases: (1) mold filling, where the melt is poured or forced into the mold cavity; (2) solidification, where the melt undergoes a phase change to the solid state; and (3) cool down, where the solidified part continues to cool to ambient conditions. While these phases may appear to be separate and distinct, temporal overlaps do exist between phases (e.g., local solidification occurring during mold filling), and some phenomenological events are affected by others (e.g., residual stresses depend on solidification and cooling rates). Therefore, a reliable code must accurately model all three phases and the interactions between each. While many codes have been developed (to various stages of complexity) to model the solidification and cool down phases, only a few codes have been developed to model mold filling.

Murph, Jesse E.↗

An investigation of squeeze-cast alloy 718

Alloy 718 billets produced by the squeeze-cast process have been evaluated for use as potential replacements for propulsion engine components which are normally produced from forgings. Alloy 718 billets were produced using various processing conditions. Structural characterizations were performed on 'as-cast' billets. As-cast billets were then homogenized and solution treated and aged according to conventional heat-treatment practices for this alloy. Mechanical property evaluations were performed on heat-treated billets. As-cast macrostructures and microstructures varied with squeeze-cast processing parameters. Mechanical properties varied with squeeze-cast processing parameters and heat treatments. One billet exhibited a defect free, refined microstructure, with mechanical properties approaching those of wrought alloy 718 bar, confirming the feasibility of squeeze-casting alloy 718. However, further process optimization is required, and further structural and mechanical property improvements are expected with process optimization.

Gamwell, W. R.↗

AMCC casting development. Volume 1: Executive Summary

The Advanced Combustion Chamber Casting (AMCC) has been a technically challenging part due to its size, configuration, and alloy type. The height and weight of the wax pattern assembly necessitated the development of a hollow gating system to ensure structural integrity of the shell throughout the investment process. The complexity in the jacket area of the casting required the development of an innovative casting technology that PCC has termed 'TGC' or Thermal Gradient Control. This method, of setting up thermal gradients in the casting during solidification, represents a significant process improvement for PCC and has been successfully implemented on other programs. Metallurgical integrity of the final four castings was very good. Only the areas of the parts that utilized 'TGC Shape & Location System #2' showed any significant areas of microshrinkage when evaluated by non-destructive tests. Alumina oxides detected by FPI on the 'float' surfaces (top sid surfaces of the casting during solidification) of the part were almost entirely less than the acceptance criteria of .032 inches in diameter. Destructive chem mill of the castings was required to determine the effect of the process variables used during the processing of these last four parts (with the exception of the 'Shape & Location of TGC' variable).

Source record↗

Precision Casting via Advanced Simulation and Manufacturing

A two-year program was conducted to develop and commercially implement selected casting manufacturing technologies to enable significant reductions in the costs of castings, increase the complexity and dimensional accuracy of castings, and reduce the development times for delivery of high quality castings. The industry-led R&D project was cost shared with NASA's Aerospace Industry Technology Program (AITP). The Rocketdyne Division of Boeing North American, Inc. served as the team lead with participation from Lockheed Martin, Ford Motor Company, Howmet Corporation, PCC Airfoils, General Electric, UES, Inc., University of Alabama, Auburn University, Robinson, Inc., Aracor, and NASA-LeRC. The technical effort was organized into four distinct tasks. The accomplishments reported herein. Task 1.0 developed advanced simulation technology for core molding. Ford headed up this task. On this program, a specialized core machine was designed and built. Task 2.0 focused on intelligent process control for precision core molding. Howmet led this effort. The primary focus of these experimental efforts was to characterize the process parameters that have a strong impact on dimensional control issues of injection molded cores during their fabrication. Task 3.0 developed and applied rapid prototyping to produce near net shape castings. Rocketdyne was responsible for this task. CAD files were generated using reverse engineering, rapid prototype patterns were fabricated using SLS and SLA, and castings produced and evaluated. Task 4.0 was aimed at developing technology transfer. Rocketdyne coordinated this task. Casting related technology, explored and evaluated in the first three tasks of this program, was implemented into manufacturing processes.

Source record↗

Macrovoid Defect Growth during Evaporative Casting of Polymeric Membranes

Macrovoid (MV) formation is a significant problem in evaporatively cast polymeric membranes. MVs are large, elongated or teardrop-shaped pores (~10-50 micron) that can impair membrane structural integrity. Although MVs have been extensively studied, there is no general agreement on the mechanisms governing MV growth. Recently, our research group has formulated the solutocapillary convection (SC) hypothesis, which contends that MV growth involves three principal forces: a Marangoni force generated by surface tension gradients within the MV interface, a viscous drag force, and a gravitationally induced body force. Two sets of complementary experiments were conducted to test the SC hypothesis. Ground-based videomicroscopy flow-visualization (VMFV) was utilized to measure the flow velocities at the MV-casting solution interface and deep within the casting solution. The measurements were performed with casting solutions containing 10 wt% cellulose acetate (CA), 30 wt% H2O, 60 wt% acetone, and 200- ppm TiO2 particles for flow visualization, and the surface tension was controlled by surfactant addition. Qualitatively, the experiments indicated that MV growth occurs in three distinct phases: (1) a very rapid initial growth period, (2) a much slower growth phase, and (3) absorption of selected MVs into the expanding demixed region. The presence of tracer particles inside the MVs suggests the presence of a convective flow, which transfers the particles from the bulk solution to the MV interior. Although the VMFV experiments did not establish any surfactant effect on the interfacial velocities, a statistically significant effect on the MV number density was observed. In the second set of experiments, membranes were cast aboard a KC-135 aircraft under 0-g and 2-g conditions. Despite careful attention to the design and fabrication of the membrane casting apparatus (MCA), several problems were encountered, the most significant of which was the contamination of the casting solution by the activated carbon particles used for solvent absorption.

Greenberg, A. R.↗