Search NASA⌕ Search

SEARCH · Search NASA

Results for “CLAD”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

The response of accident tolerant fuel cladding to LOCA burst testing: A comparative study of leading concepts

Accident tolerant fuel claddings seek to improve safety margins during loss-of-coolant accident (LOCA) scenarios by reducing cladding steam oxidation rates, hydrogen production, delaying or mitigating cladding burst, and reducing cladding deformation. After rapid and extensive progress in recent years, Cr coated Zr-based alloys, ferritic FeCrAl, and SiC/SiC ceramic matrix composites (CMCs) have emerged as the most promising cladding concepts, but there are few studies comparing the accident tolerance of all three concepts simultaneously. Here, in this study, LOCA burst testing has been conducted on Cr high impulse power magnetron sputtered Zry-4 (Cr/Zry-4), C26M (FeCrAl), and SiC/SiC SiGA (CMC). Experimental observations indicate Cr/Zry-4 burst at higher temperatures than Zry-4 however the effectiveness of the coating on mitigating ZrO 2 formation via Cr 2 O 3 formation depended on physical proximity to the burst opening. No dramatic improvement in diametrical strain nor opening geometry was observed. C26M burst at higher temperatures than Zry-4 at lower pressures, exhibiting small amounts of strain and smaller openings, and formed slow-growing Al 2 O 3 regardless of location. The CMCs did not burst or show any macroscopic signs of deformation, all the way up to an internal cladding pressure of 15.2 MPa. High temperature expanding Nb plug testing indicated that CMC room temperature strength may persist up to 1650°C, with an approximately 40% loss of strength at 1900°C. CMC steam oxidation was also compared to reference chemically vapor deposited SiC up to 1700°C, and CMCs were found to oxidize at slightly accelerated rates that were still orders of magnitude lower than bare Zry-4. Projected H 2 generation during LOCA burst testing showed that when accounting for cladding burst exposing inner diameters to steam, Cr coated Zry-4 reduced H 2 generation by a factor of two compared with bare Zry-4, while both C26M and SiC/SiC reduced H 2 generation by orders of magnitude relative to bare Zry-4.

36 MATERIALS SCIENCE↗

Annealing induced interfacial layers in niobium-clad stainless steel developed as a bipolar plate material for polymer electrolyte membrane fuel cell stacks

Niobium (Nb)-clad 304L stainless steel (SS) manufactured by cold rolling is currently under consideration for use as a bipolar plate material in polymer electrolyte membrane fuel cell (PEMFC) stacks. To make the fabrication of bipolar plates using the Nb-clad SS feasible, annealing may be necessary for the Nb-clad SS to reduce the springback induced by cold rolling. However, the annealing can develop an interfacial layer between the Nb cladding and the SS core and the interfacial layer plays a key role in the failure of the Nb-clad SS as reported earlier [JPS our work]. In this investigation, the Nb-clad SS specimens in as-rolled condition were annealed at different combinations of temperature and time. Based on the results of scanning electron microscope (SEM) analysis, an annealing process map for the Nb-clad SS was obtained. The results of SEM analysis and Transmission Electron Microscope (TEM) analysis also suggest that different interfacial layers occurred based on the given annealing conditions.

annealing↗

Interfacial microstructure and properties of copper clad steel produced using friction stir welding versus gas metal arc welding

A preliminary study compares the feasibility and microstructures of pure copper claddings produced on a pressure vessel A516 Gr. 70 steel plate, using friction stir welding versus gas metal arc welding. A combination of optical and scanning electron microscopy is used to characterize the grain structures in both the copper cladding and heat affected zone in the steel near the fusion line. The friction stir welding technique produces copper cladding with a grain size of around 25 μm, and no evidence of liquid copper penetration into the steel. The gas metal arc welding of copper cladding exhibits grain sizes over 1 mm, and with surface microcracks as well as penetration of liquid copper up to 50 μm into the steel substrate. Transmission electron microscopy reveals that metallurgical bonding is produced in both processes. Increased diffusion of Mn and Si into the copper cladding occurs when using gas metal arc welding, although some nano-pores were detected in the FSW joint interface. - Highlights: • Cladding of steel with pure copper is possible using either FSW or GMAW. • The FSW yielded a finer grain structure in the copper, with no evidence of cracking. • The FSW joint contains some evidence of nano-pores at the interface of the steel/copper. • Copper cladding by GMAW contained surface cracks attributed to high thermal stresses. • The steel adjacent to the fusion line maintained a hardness value below 248 HV.

36 MATERIALS SCIENCE↗

Designing an impedance-based technique for studying corrosion on cladding materials

In nuclear cladding materials, changes in structure and chemistry over the lifetime of claddings can have a significant impact on fuel and reactor performance. Currently, chemical evolution over the lifetime of the fuel and cladding materials can only be inferred using post-irradiation examination. As an alternative to post-irradiation measurements, electrochemical impedance spectroscopy (EIS) can provide an in-pile measurement of changes in chemistry in oxides and hydrides. The objective of this study is to develop an impedance based sensing technology for measuring spatial- and time-resolved in-pile changes in cladding chemistry in order to understand the mechanisms of hydride formation, hydride dealloying and associated cladding corrosion so that a mitigation strategy and technology can be developed for reactor safe operation. Two prototype impedance-based sensors were designed and assembled using Zr-4 as working electrode and Pt as counter and reference electrode. One sensor is tubular type and the other one is plate-type. These sensors will be tested in static autoclave to investigate the effects of various environmental conditions (including temperature, pressure, and water chemistry) on cladding material corrosion mechanisms. These in-situ EIS sensors would provide corrosion-layer parameters in high-temperature water, such as (1) total layer thickness, (2) the evolution of oxide structures as uniform layer dielectric or sublayer(s), and (3) the possible electrochemistry of the volume corrosion process and the solid/liquid interface, such as the cyclic nature of corrosion of Zr alloys in high-temperature water. This work was focused on electrochemical sensor development, targeting cladding oxides/hydrides under thermodynamic equilibria; characterization of samples using Kelvin probe force microscopy (SKPFM), Raman spectroscopy, and scanning electron microscopy (SEM) with energy-dispersive X-ray spectroscopy (EDS) to provide high-resolution co-localized characterization of zirconium oxide and metal/oxide interface.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effects of chemistry and microstructure on corrosion performance of Zircaloy-2-based BWR cladding - 2016-0066

In boiling water reactors (BWRs), Zircaloy-2 is typically the material of choice for fuel cladding. With increased focus on fuel performance and reliability, consistent cladding corrosion performance under varying BWR conditions has become an acknowledged requirement for modern BWR fuel. To support optimization of corrosion performance, modifications to alloy chemistry and manufacture conditions can be made, supported by ex-reactor corrosion testing and demonstrated through in-reactor operation. In this work, the combined effects of alloy chemistry and fabrication process were investigated. The effect of alloy chemistry is often complicated by variation within a production ingot. In this work, additional measurements were intentionally taken at the tube-shell stage (before cold pilgering) so that chemistry more representative of the final cladding could be obtained and the effect of iron, nickel, and tin could be examined more closely. Although chemistry range of Zircaloy-2 was the primary focus, the effect of iron above the ASTM limit in a new alloy was also explored. Three types of cladding fabrication processes were considered. Two types included a heat treatment applied after the first cold pilgering and annealing, and the treatment was limited to the outer portion of the cladding and differed in the temperature of the heat treatment; the third type had no special heat treatments after the first cold pilgering and annealing. The weight gain of the three types of cladding with varying compositions under two corrosion test conditions (400 deg. C steam and 410/520 deg. C two-stage steam) are discussed in terms of the initial second-phase particle sizes obtained from transmission electron microscopy examinations. Based on poolside inspections and hot-cell examinations, the in-reactor corrosion performance of the two cladding types up to typical discharge exposures are discussed in the terms of corrosion margin, microstructure evolution, and correlation with ex-reactor corrosion test data. (authors)

36 MATERIALS SCIENCE↗

Pellet Cladding Mechanical Interaction Modeling Using the Extended Finite Element Method

As a brittle material, the ceramic UO2 used as light water reactor fuel experiences significant fracturing throughout its life, beginning with the first rise to power of fresh fuel. This has multiple effects on the thermal and mechanical response of the fuel/cladding system. One such effect that is particularly important is that when there is mechanical contact between the fuel and cladding, cracks that extending from the outer surface of the fuel into the volume of the fuel cause elevated stresses in the adjacent cladding, which can potentially lead to cladding failure. Modeling the thermal and mechanical response of the cladding in the vicinity of these surface-breaking cracks in the fuel can provide important insights into this behavior to help avoid operating conditions that could lead to cladding failure. Such modeling has traditionally been done in the context of finite-element-based fuel performance analysis by modifying the fuel mesh to introduce discrete cracks. While this approach is effective in capturing the important behavior at the fuel/cladding interface, there are multiple drawbacks to explicitly incorporating the cracks in the finite element mesh. Because the cracks are incorporated in the original mesh, the mesh must be modified for cracks of specified location and depth, so it is difficult to account for crack propagation and the formation of new cracks at other locations. The extended finite element method (XFEM) has emerged in recent years as a powerful method to represent arbitrary, evolving, discrete discontinuities within the context of the finite element method. Development work is underway by the authors to implement XFEM in the BISON fuel performance code, and this capability has previously been demonstrated in simulations of fracture propagation in ceramic nuclear fuel. These preliminary demonstrations have included only the fuel, and excluded the cladding for simplicity. This paper presents initial results of efforts to apply XFEM to model stress concentrations induced by fuel fractures at the fuel/cladding interface during pellet cladding mechanical interaction (PCMI). This is accomplished by enhancing the thermal and mechanical contact enforcement algorithms employed by BISON to permit their use in conjunction with XFEM. The results from this methodology are demonstrated to be equivalent to those from using meshed discrete cracks. While the results of the two methods are equivalent for the case of a stationary crack, it is demonstrated that XFEM provides the additional flexibility of allowing arbitrary crack initiation and propagation during the analysis, and minimizes model setup effort for cases with stationary cracks.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Survivability of TREAT Zircaloy 3 Cladding

This chapter analyzes the effects of oxidation, growth, thermal stress, and fatigue on the Zircaloy-3 alloy used in TREAT fuel assembly cladding. The cladding surrounding the fuel is a protective shell which is used to prevent damage to the enclosed fuel. Therefore, its integrity is importance to guarantee this protection. All of the major factors which can affect the Zircaloy-3 cladding are considered in this chapter and investigated. Limits to operation are determined. The oxidation of Zircaloy-3 in air is of interest to air cooled reactors. The temperature range of interest is from room temperature where the fuel is stored for long periods of time, through the temperature range encountered in normal operation, to the highest temperatures which are possible in extreme accident situations. This temperature range is considered in this chapter to be from room temperature to 1100 C. Growth of the cladding can occur due to the buildup of the oxide layer which is less dense than the original metal and causes the metal to stretch. Thermal stress of the cladding can cause rupture of the cladding and therefore loss of protection to the fuel. Fatigue of the metal cladding occurs due to fuel handling.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Clad to coolant heat transfer during RIA in PWR conditions

The power pulse during an insertion of reactivity accident (RIA) leads to a transient heating of the fuel. Heat transfer toward the coolant through the clad and associated temperature transient of the clad is of safety significance since it may largely impact the risk of clad failure. For sufficiently large enthalpy deposited within the fuel, clad temperature increases rapidly and this can lead to coolant boiling. This paper concerns the critical review of the present understanding and of the models for the clad to coolant heat transfer in RIA for PWR conditions. The results of past experiments are reviewed and the reliability of current models dedicated to these conditions is analyzed. It appears that the use of classical models for wall to fluid heat transfer does not allow predicting the clad temperature transient as measured in RIA-related experiments. The deviation is all the more large when film boiling conditions are reached. To reproduce the experimental data, some correlations of heat transfer can be fitted but the reliability of such model out of the range of conditions of the experimental data is low. It is mainly due to a rather low level of understanding of the heat transfer in very transient conditions (i.e. when the time scale of variation of the main heat transfer parameters, like a wall temperature, is less than the typical internal time scale of the heat transfer process itself). It results in a very large scattering in the numerical simulation of clad temperature when several fuel codes are considered. To improve the reliability of these calculations, it is believed that the study of transient boiling heat transfer thanks to devoted experimental facilities is required.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Breakaway oxidation of ZIRLO and optimized ZIRLO cladding per 10CFR50.46c criteria

The United States Nuclear Regulatory Commission (NRC) in 10CFR50.46c proposed changes to the loss of coolant accident (LOCA) criteria for LWR licensees including a new requirement to test cladding materials for breakaway oxidation. Cladding materials must be shown to resist breakaway oxidation long enough for the LOCA transient to be terminated. The onset of breakaway oxidation is characterized by a rapidly increasing rate of oxidation and the absorption of hydrogen resulting in a loss of cladding integrity. The proposed rule changes effectively require some manner of periodic and on-going testing to monitor the population of cladding for breakaway resistance. More than 200 lots of production cladding material have been tested in accordance with the draft regulatory guidelines. Testing has been conducted in a steam environment at the critical temperature for breakaway oxidation for durations that exceed the analytical endurance limit required to comply with the breakaway oxidation test criteria. The alloys that have been tested include both ZIRLO cladding and Optimized ZIRLO cladding. Breakaway oxidation testing consisted of three basic steps: preparation of test specimens, high temperature steam oxidation and post-test specimen evaluation. The results show there is a high probability that all ZIRLO and Optimized ZIRLO lots will pass production certification testing. Variations in response to breakaway oxidation testing were observed only in testing that ran well beyond the maximum LOCA duration of 2000 seconds. No indications of early breakaway oxidation were observed in the testing of production material that has been completed thus far. This provides confidence that a sampling approach to breakaway oxidation testing and monitoring remains a sound approach.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Zircaloy Cladding as Starting Precursor for Ceramic Waste-Forms - 15562

Zircaloy cladding of spent fuel is regular waste-stream related to the process of reprocessing. It remains in the apparatus after spent fuel dissolution. The most common technique of zircaloy cladding treatment is cementation and disposal in metallic containers. In view of the high cost of the cladding material (mainly zirconium), there have been a number of proposals for this material to be recovered and re-used. However, the residual contamination of the claddings following the dissolution of the fuel and the chemical stability of the zirconium militate against any proposal for a recycling process that might be economically reasonable. At the same time there is a lot of information available about synthesis of mineral-like materials based on zirconium for immobilization of long-lived radionuclides. The object of this work was to study experimentally electrochemical dissolution of fuel rod cladding for further obtaining starting precursor for the synthesis of ceramic-waste forms. The results of experiments on electrochemical dissolution of zirconium and zirconium alloy (fuel rod cladding) in nitric acid solutions are presented. The peak dissolution rate of specimens is shown to be observed in dilute nitric acid at elevated temperatures. The rate of dissolution rises with temperature, reaching ∼40-70 mg/cm{sup 2}.h at 90 deg. C. The current yield at this point is 0.6-0.7 g/A.h. The results of analysis of the surface oxide film on specimens and residues formed during dissolution are also presented. An electrochemical dissolution of zircaloy claddings is the common technique for preparation of zirconium solutions to be used for ceramic waste form synthesis. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Advancements in FeCrAl Alloys for Enhanced Accident Tolerant Fuel Cladding for Light Water Reactors

Advanced FeCrAl alloys are being considered as an enhanced accident tolerant fuel (ATF) cladding for light water reactor (LWR) applications as they can exhibit slower reaction kinetics with high temperature steam and have a reduced production of hydrogen during accident scenarios compared both to historic 304L cladding and Zircaloy. Both of these attributes are key towards producing a fuel-form with enhanced accident tolerance over the current Zr-based-UO{sub 2} fuel form in deployment. A multi-year, multi-laboratory effort has been established to rapidly advance FeCrAl alloys as an ATF concept. This effort has focused on optimizing the microstructure and composition of these alloys in an attempt to provide performance on-par with or better than the current Zr-based cladding in both normal operating conditions and under accident scenarios. To date, a significant database supporting key performance factors in both scenarios has been developed. Based on this database, a compositional and microstructural window has been identified providing the insight for an optimized, advanced nuclear-grade FeCrAl alloy for LWRs. This work will provide a comprehensive overview of the systematic effort to advance FeCrAl alloys as an enhanced ATF cladding in commercial LWRs. Efforts undertaken by this multi-year, multi-laboratory program have shown the viability of using FeCrAl alloys as an ATF cladding in LWRs. Most importantly, it has been shown the oxidation resistance, decreased hydrogen production, and reduced heat generation of FeCrAl alloys strongly contribute to its ATF capability. Furthermore, it has been shown that the normal operational performance of a FeCrAl cladding can rival that of Zr-based alloys. Finally, it was found that optimizing the performance of FeCrAl cladding materials requires balancing the starting composition and microstructure in order to satisfy key performance indicators such as oxidation resistance and radiation tolerance. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Reactivity impact of accident tolerant claddings in an equilibrium PWR core

The US DoE's Accident Tolerant Fuels (ATF) program aims to establish a process to evaluate the feasibility of several ATF concepts. The two main aspects of such a process are to evaluate the 3-D 'whole core' neutronics and fuel (thermal-mechanical) performance. Determining the best ATF candidate usually involves a compromise between these two performance aspects. The work presented in this paper focuses solely on the 3-D neutronics, looking specifically at the end of cycle (EOC) reactivity, and upon the establishment of a realistic and modern equilibrium PWR core to use as a test-bed. Both the lattice physics code CASMO-4 and the 3-D nodal simulator NESTLE were used in this study. Eventually, operational power histories are provided to our collaborating team to carry out fuel performance evaluations to be presented in a future article. Neutronically, a goal of a prospective ATF concept is to at least match the fuel cycle length of a core with standard Zircaloy/UO{sub 2} fuel, without having to significantly change the design of the fuel bundle; meaning, without changing pin pitch or outer clad diameter. Such a 'seamless' transition to another cladding type would greatly reduce the burden of all the nuclear energy stakeholders (regulators, vendors, utilities), from both an analysis and financial perspective. For cladding materials that are less transparent to neutrons, which for this study included all the ATF concepts, the two degrees of freedom with respect to fuel fabrication are the U-235 enrichment and cladding thickness. The latter involved changing only the fuel radius and inner clad radius while keeping the gap and outer clad radius constant. The thinnest cladding value was set to a generous estimate of the minimum iron-chromium-aluminum (FeCrAl) thickness that can be manufactured. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Mechanical response and microstructure evolution from multiaxial stress relaxation in textured zircaloy nuclear cladding

Modern energy markets provide motivation for nuclear reactors to increase operational flexibility and load following capacity of existing reactor designs. The operational power changes result in fuel pellet expansion and contraction resulting in pellet-cladding mechanical interaction (PCMI) and high cladding stresses that are strongly related to stressed corrosion cracking (SCC) which can lead to fuel rod failure. This work aims to quantify the stress fields in cladding with a focus on multiaxial stress relaxation response from an imposed strain and the resulting microstructure changes in textured zircaloy claddings. Stress relaxation tests resulting in multiaxial stress fields are performed to measure the material response of Zircaloy-4 nuclear cladding. Multiple experiments using samples from the same piece of cladding are performed so samples with the same processing history may be removed at strategic points throughout mechanical testing for microstructure characterization. The microstructure evolution is analyzed with mechanical response to evaluate the static recovery impact on crystallographic texture and grain morphology. Experiments are performed at Idaho National Laboratory using an experimental device capable of applying internal pressure and independent axial load to commercial nuclear cladding at elevated temperatures with stress- or strain-controlled experimental capability. X-ray diffraction and electron backscatter diffraction are used for microstructure analysis. Rheological models are used to visualize the multiaxial stress-strain relationships and isolate elastic, plastic, and viscoplastic material properties for analysis.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Mechanical Properties of Advanced Gas-Cooled Reactor Stainless Steel Cladding After Irradiation

The production of helium bubbles in advanced gas-cooled reactor (AGR) cladding could represent a significant hazard for both the mechanical stability and long-term storage of such materials. However, the high radioactivity of AGR cladding after operation presents a significant barrier to the scientific study of the mechanical properties of helium incorporation, said cladding typically being analyzed in industrial hot cells. An alternative non-active approach is to implant He{sup 2+} into unused AGR cladding material via an accelerator. Here, a feasibility study of such a process, using sequential implantations of helium in AGR cladding steel with decreasing energy is carried out to mimic the buildup of He (e.g., 50 appm) that would occur for in-reactor AGR clad in layers of the order of 10 µm in depth, is described. The implanted sample is subsequently analyzed by scanning electron microscopy, nanoindentation, atomic force and ultrasonic force microscopies. As expected, the irradiated zones were affected by implantation damage (< 1 dpa). Nonetheless, such zones undergo only nanoscopic swelling and a small hardness increase (~ 10%), with no appreciable decrease in fracture strength. Thus, for this fluence and applied conditions, the integrity of the steel cladding is retained despite He{sup 2+} implantation.

36 MATERIALS SCIENCE↗

Micro X-ray computed tomography examination of mini plate fuel with hot isostatic pressed aluminum cladding

In order to minimize proliferation risks and improve security of nuclear material, the United States high performance research and test reactors (USHPRR) program is tasked with converting nuclear reactors that are fueled with highly enriched uranium (HEU) fuels to operate with low-enriched uranium (LEU) nuclear fuels. One favorable LEU fuel configuration is plate fuel with a metallic uranium-molybdenum foil clad within an aluminum alloy (AA 6061). In this fuel, the aluminum cladding is bonded with a hot isostatic pressing (HIP) method to seal the cladding around the fuel meat. However, the HIP process parameters influence the cladding performance, as a defective or incomplete bond can cause a pathway for corrosion. Micro X-ray computed tomography (XCT), a nondestructive technique that provides volumetric imaging, can be applied to inspect fuel plate cladding at the engineering scale. In this work, XCT methodology was developed and successfully utilized to not only observe the bond line of unirradiated mini fuel plates, but to also identify subsurface abnormalities in the plates’ cladding. Importantly, in future work, this technique could be applied to fuel plates, pre- and post-irradiation, to quantify irradiation effects on cladding defects and bond line integrity.

36 MATERIALS SCIENCE↗

Fracture toughness evaluation for Zr-4 clad tubing structure with pellet inserts

Applying fracture mechanics approach to spent nuclear fuel (SNF) system reliability investigation is warranted due to the inherent flaws and hydride structures existed in a SNF system after nuclear reactor operation. However, none of the existing fracture toughness data deal with fuel cladding specific geometry or spent fuel material conditions, such as cladding structure with the pellet-inserts and the associated pellet clad mechanical interactions induced mixed-mode damage mechanisms. Thus, the development of an intrinsic fracture mechanics approach that is suitable for SNF materials is needed. Due to thin wall and small dimension of clad tubing structure, the spiral notch torsion test (SNTT) method of small specimen approach was used to estimate the clad tubing structure fracture toughness. The estimated fracture toughness for Zr-4 cladding with alumina-pellet inserts are presented in this report. For SNTT samples with a short or medium crack length, between 5.4-mm and 8-mm, the estimate JIQ upon fracture initiation for the baseline Zr-4 cladding is at 50 kJ/m2 with 2-sigma uncertainty of 3.26 kJ/m2, and the associated KIQ is at 67.46 MPa√m. For SNTT samples with a long crack length, around 13-mm, the crack initialization is deviated from that of the Mode-I tensile fracture and appears to be a mixed-mode fracture of Mode I – tensile stress and Mode III – out of plane shear stress; the estimated JMQ is at 18.9 kJ/m2, the associated KMQ is at 41.4 MPa√m.

36 MATERIALS SCIENCE↗

Advanced Multiphysics Code Coupling for Cladding Surface Thermocouples During Two-Phase Heat Transfer from Nuclear Fuel

Transient testing of nuclear fuel involves the evaluation of fuel performance under off-normal and accident conditions and is essential for proving design performance. Instrumentation included in such experiments commonly includes thermocouples attached to the outer surface of the cladding to provide temperature measurements throughout the transient. However, the presence of thermocouples on the cladding surface can alter the local heat transfer characteristics with the surrounding coolant. These localized effects can influence the temperature of the nearby cladding surface and introduce uncertainties in interpreting the thermocouple data. Understanding the impact of thermocouples attached to the outer surface of the cladding is crucial for accurate data interpretation as well as its effect on the thermomechanical behavior of the cladding. This paper presents a novel methodology for simulating the impact of outer cladding thermocouples during transient testing of nuclear fuels. The simulation framework leverages the thermal-hydraulic capabilities of RELAP5-3D coupled to the BISON fuel performance code through the RELAPCouplingApp interface. The methodology is compared against Accident Tolerant Fuel Reactivity Initiated Accident-1-E experiment performed at Idaho National Laboratory. The results reveal approximately 100°C difference between thermocouple-altered temperature and virgin cladding surface. The model overpredicts surface rewet time due to conservative correlations.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Simulations of Failure via Three-Dimensional Cracking in Fuel Cladding for Advanced Nuclear Fuels

Enhancing performance of fuel cladding and duct alloys is a key means of increasing fuel burnup. This project will address the failure of fuel cladding via three-dimensional cracking models. Researchers will develop a simulation code for the failure of the fuel cladding and validate the code through experiments. The objective is to develop an algorithm to determine the failure of fuel cladding in the form of three-dimensional cracking due to prolonged exposure under varying conditions of pressure, temperature, chemical environment, and irradiation. This project encompasses the following tasks: 1. Simulate 3D crack initiation and growth under instantaneous and/or fatigue loads using a new variant of the material point method (MPM); 2. Simulate debonding of the materials in the crack path using cohesive elements, considering normal and shear traction separation laws; 3. Determine the crack propagation path, considering damage of the materials incorporated in the cohesive elements to allow the energy release rate to be minimized; 4. Simulate the three-dimensional fatigue crack growth as a function of loading histories; 5. Verify the simulation code by comparing results to theoretical and numerical studies available in the literature; 6. Conduct experiments to observe the crack path and surface profile in unused fuel cladding and validate against simulation results; and 7. Expand the adaptive mesh refinement infrastructure parallel processing environment to allow adaptive mesh refinement at the 3D crack fronts and adaptive mesh merging in the wake of cracks. Fuel cladding is made of materials such as stainless steels and ferritic steels with added alloying elements, which increase stability and durability under irradiation. As fuel cladding is subjected to water, chemicals, fission gas, pressure, high temperatures, and irradiation while in service, understanding performance is essential. In the fast fuel used in advanced burner reactors, simulations of the nuclear fuels are critical to understand the burnup, and thus the fuel efficiency.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗