Search NASA⌕ Search

SEARCH · Search NASA

Results for “CRYSTAL DISLOCATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Carboxylic and Dicarboxylic Acids Extracted from Crushed Magnesium Oxide Single Crystals

Carboxylic and dicarboxylic acids (glycolic, oxalic, malonic and succinic) have been extracted with tetrahydrofuran (THE) and H2O from large synthetic MgO crystals, crushed to a medium fine powder. The extracts were characterized by infrared spectroscopy and (sup 1)H-NMR (Nuclear Magnetic Resonance). The THF extracts were derivatized with tert-butyldimethylsilyl (t-BDMS) for GC-MS (Gas Chromatography - Mass Spectroscopy) analysis. A single crystal separated from the extract was used for an x-ray structure analysis, giving the monoclinic unit cell, space group P2(sub 1)/c with a(sub o) = 5.543 A, b(sub o) = 8.845 A, c(sub o) = 5.086 A, and beta = 91.9 degrees, consistent with beta-succinic acid, HOOC(CH2)COOH. The amount of extracted acids is estimated to be of the order of 0.1 to 0.5 mg/g MgO. The MgO crystals from which these organic acids were extracted grew from the 2360 C hot melt, saturated with CO/CO2 and H2O, thereby incorporating small amounts of the gaseous components to form a solid solution (ss) with MgO. Upon cooling, the ss becomes supersaturated, causing solute carbon and other solute species to segregate not only to the surface but also internally, to dislocations and subgrain boundaries. The organic acids extracted from the MgO crystals after crushing appear to derive from these segregated solutes that formed C-C, C-H, and C-O bonds along dislocations and other defects in the MgO structure, leading to entities that can generically be described as (HxCyOz)(sup n-). The processes underlying the formation of these precursors are fundamental in nature and expected to be operational in any minerals, preferentially those with dense structures, that crystallized in H2O-CO2-laden environments. This opens the possibility that common magmatic and metamorphic rocks when weathering at the surface of a tectonically active planet like Earth may be an important source of abiogenically formed complex organic compounds.

Freund, Friedemann↗

Carboxylic and dicarboxylic acids extracted from crushed magnesium oxide single crystals

Carboxylic and dicarboxylic acids (glycolic, oxalic, malonic and succinic) have been extracted with tetrahydrofuran (THF) and H2O from large synthetic MgO crystals, crushed to a medium fine powder. The extracts were characterized by infrared spectroscopy and 1H-NMR. The THF extracts were derivatized with tert-butyldimethylsilyl (t-BDMS) for GC-MS analysis. A single crystal separated from the extract was used for an x-ray structure analysis, giving the monoclinic unit cell, space group P21/c with ao = 5.543 A, bo = 8.845 A, co = 5.086 A, and beta = 91.9 degrees, consistent with beta-succinic acid, HOOC(CH2)COOH. The amount of extracted acids is estimated to be of the order of 0.1 to 0.5 mg g-1 MgO. The MgO crystals from which these organic acids were extracted grew from the 2860 degrees C hot melt, saturated with CO/CO2 and H2O, thereby incorporating small amounts of the gaseous components to form a solid solution (ss) with MgO. Upon cooling, the ss becomes supersaturated, causing solute carbon and other solute species to segregate not only to the surface but also internally, to dislocations and subgrain boundaries. The organic acids extracted from the MgO crystals after crushing appear to derive from these segregated solutes that formed C-C, C-H and C-O bonds along dislocations and other defects in the MgO structure, leading to entities that can generically be described as (HxCyOz)n-. The processes underlying the formation of these precursors are fundamental in nature and expected to be operational in any minerals, preferentially those with dense structures, that crystallized in H2O-CO2-laden environments. This opens the possibility that common magmatic and metamorphic rocks when weathering at the surface of a tectonically active planet like Earth may be an important source of abiogenically formed complex organic compounds.

NASA Discipline Exobiology↗

Low-threshold photonic crystal laser

We have fabricated photonic crystal nanocavity lasers, based on a new high-quality factor design that incorporates fractional edge dislocations.

photonic↗

Electrical Impact of SiC Structural Crystal Defects on High Electric Field Devices

Commercial epilayers are known to contain a variety of crystallographic imperfections. including micropipes, closed core screw dislocations. low-angle boundaries, basal plane dislocations, heteropolytypic inclusions, and non-ideal surface features like step bunching and pits. This paper reviews the limited present understanding of the operational impact of various crystal defects on SiC electrical devices. Aside from micropipes and triangular inclusions whose densities have been shrinking towards manageably small values in recent years, many of these defects appear to have little adverse operational and/or yield impact on SiC-based sensors, high-frequency RF, and signal conditioning electronics. However high-power switching devices used in power management and distribution circuits have historically (in silicon experience) demanded the highest material quality for prolonged safe operation, and are thus more susceptible to operational reliability problems that arise from electrical property nonuniformities likely to occur at extended crystal defects. A particular emphasis is placed on the impact of closed-core screw dislocations on high-power switching devices, because these difficult to observe defects are present in densities of thousands per cm,in commercial SiC epilayers. and their reduction to acceptable levels seems the most problematic at the present time.

Neudeck, Philip G.↗

Rolling-contact deformation of MgO single crystals

Magnesium oxide single crystals were used as a model bearing material and deformed by rolling contact with a steel ball 0.64 cm in diameter. A dependence of depth of slip on rolling velocity which persisted with increasing numbers of rolling-contact cycles was discovered. The track width, track hardness and dislocation interactions as observed by transmission electron microscopy all increased in a consistent manner with increasing cycles. The rolling-contact state of stress produces a high density of dislocations in a localized zone. Dislocation interaction in this zone produces cleavage-type cracks after a large number of rolling-contact cycles. The orientation of the crystal influences the character of dislocation accumulation.

Dufrane, K. F.↗

Advances in large-diameter liquid encapsulated Czochralski GaAs

The purity, crystalline perfection, and electrical properties of n- and p-type GaAs crystals grown by the liquid encapsulated Czochralski (LEC) technique are evaluated. The determination of the dislocation density, incidence of twinning, microstructure, background purity, mobility, and minority carrier diffusion length is included. The properties of the LEC GaAs crystals are generally comparable to, if not superior to those of small-diameter GaAs material grown by conventional bulk growth techniques. As a result, LEC GaAs is suitable for application to minority carrier devices requiring high-quality and large-area substrates.

Chen, R. T.↗

Pulsed Molecular Beams For Growth Of InAs On GaAs

Pauses for annealing reduce number of defects. Deposition process that includes pulsed molecular beams produces high-quality epitaxial layers of indium arsenide on gallium arsenide substrates. Layers made as much as 30 atoms thick without introducing excessive numbers of dislocations, despite 7.4-percent mismatch between InAs and GaAs crystal lattices. Layers offer superior electrical properties in such devices as optically addressed light modulators, infrared sensors, semiconductor lasers, and high-electron-mobility transistors. Technique applicable to other epitaxial systems in which lattices highly mismatched.

Grunthaner, Frank J.↗

Electron Backscatter Diffraction (EBSD) Analysis and U-Pb Geochronology of the Oldest Lunar Zircon: Constraining Early Lunar Differentiation and Dating Impact-Related Deformation

The evolution of the early moon was dominated by two processes (i) crystallization of the Lunar Magma Ocean (LMO) and differentiation of potassium-rare earth element-phosphorous-rich residual magma reservoir referred to as KREEP, and (ii) an intense meteorite bombardment referred to as lunar cataclysm . The exact timing of these processes is disputed, and resolution relies on collection and interpretation of precise age data. This study examines the microstructure and geochronology of zircon from lunar impact breccias collected during the Apollo 17 mission. A large zircon clast within lunar breccia 72215,195 shows sector zoning in optical microscopy, cathodoluminescence (CL) imaging and Raman mapping, and indicates that it was a relict fragment of a much larger magmatic grain. Sensitive high resolution ion microprobe (SHRIMP) U-Pb analysis of the zircon shows that U and Th concentration correlate with sector zoning, with darkest CL domains corresponding with high-U and Th (approx.150 and approx.100 ppm respectively), and the brightest-CL sectors containing approx.30-50 ppm U and approx.10-20 ppm Th. This indicates that variations in optical CL and Raman properties correspond to differential accumulation of alpha-radiation damage in each sector. Electron backscatter diffraction (EBSD) mapping shows that the quality of electron backscatter patterns (band contrast) varies with sector zoning, with the poorest quality patterns obtained from high-U and Th, dark-CL zones. EBSD mapping also reveals a deformation microstructure that is cryptic in optical, CL and Raman imaging. Two orthogonal sets of straight discrete and gradational low-angle boundaries accommodate approx.12 misorientation across the grain. The deformation bands are parallel to the crystallographic {a}-planes of the zircon, have misorientation axes parallel to the c-axis, and are geometrically consistent with formation by dislocation creep associated with <100>{010} slip. The deformation bands are unlike curved morphology of crystal-plastic microstructures in tectonically deformed terrestrial zircon, and geometrically similar to dislocation microstructures reported in experimentally shocked zircon. We interpret these crystal-plastic deformation microstructures to have resulted from a significant impact, either directly from impact shock, or during ductile flow directly following the impact. The deformation bands appear to continue undeflected through the non-indexed, radiation-damaged areas of the grain, which suggests that the orientation variation predates any significant mechanical weakening from radiation damage in the grain, and therefore occurred early in its history.

Timms, Nick↗

Determining the Molecular Growth Mechanisms of Tetragonal Lysozyme Crystals

Studies of the growth of tetragonal lysozyme crystals employing atomic force microscopy (AFM) have shown the advantages of this technique in investigating the growth mechanisms of protein crystals [1]. The resolution of these studies was in the micron range, which revealed surface features such as the occurrence of dislocations and 2D nucleation islands, similar to those found in inorganic systems. They clearly showed that the crystals grew by these surface growth mechanisms. However, the studies also revealed some surprising features, such as bimolecular growth step heights and pronounced growth anisotropies on the (110) face, which could not be explained. In previous studies we employed Periodic Bond Chain (PBC) theory to tetragonal lysozyme crystal growth and found that the crystals were constructed by strongly bonded molecular chains forming helices about the 43 axes [2,3]. The helices were connected to each other with weaker bonds. The growth process was shown to proceed by the formation of these 43 helices, resulting in bimolecular growth steps on the (110) face. It was also shown to explain many other observations on tetragonal lysozyme crystal growth. Although PBC analysis is not a new technique [4], it has not been widely used as the mechanisms predicted from it could not be experimentally verified. In this study the growth process of these crystals was investigated, particularly for the (110) face, employing some newly developed high resolution AFM techniques. These techniques allowed individual lysozyme molecules on the crystal faces to be resolved and predictions from PBC analyses to be tested. The analyses had shown that of the two possible packing arrangements on (110) faces, only one would actually occur. Employing the first of the newly developed techniques, these faces were scanned by high resolution AFM. The resulting images were then compared with the theoretically constructed images for the two possible packing arrangements on the (110) face. The theoretical images were constructed by convolution of the crystal surface shape obtained from crystallographic data with the AFM tip shape. The comparison confirmed the prediction that the molecular packing arrangement of these faces corresponded to that for complete 43 helices. The second AFM technique that was developed was used to follow the growth process by measuring the dimensions of individual growth units on the (110) face. Linescans across a growth step, performed near the saturation limit of the crystals, allowed the growth unit dimensions to be measured. These measurements showed that growth on the (110) face proceeded by the formation of new 43 helices from the addition of at least tetramer units in the [110] direction. In the [001] direction growth proceeded by the addition of various aggregate units corresponding to the 4(sub 3) helices.

Li, Huayu↗

Grain Size-Dependent Crystal Plasticity Constitutive Model for Polycrystal Materials

A new method to introduce grain size-dependence in classical crystal plasticity constitutive model is developed by considering the resistance to dislocation motion in the grain boundary influence region as equivalent to that of a work hardening. A general framework for the size-dependent constitutive model is derived by implementing this method on a core and mantle model. The work hardening, equivalent to grain boundary effect, is realized by introducing a fictitious, pre-existing, plastic strain grain boundary influence region (mantle) following the principles of classical crystal plasticity. This fictitious plastic strain, in effect, increases the yield strength and decreases the initial hardening coefficient of the grain. With the thickness of grain boundary influence region and the distribution of introduced plastic strain remaining the same, the grain boundary effect increased as the grain size becomes smaller. A simplified model that considers the grain boundary effect on a grain average sense is also developed under this general framework. Implementation of this general framework to the specific cases of crystal plasticity constitutive models is demonstrated by considering the case of power law flow rule and hyperbolic-secant hardening rule. Finally, the grain size-dependent constitutive model is validated by comparing the predicted stress-strain behavior of polycrystal samples with different average grain sizes under uniaxial loading with the experimental results.

Grain Size↗

1100 to 1500 K Slow Plastic Compressive Behavior of NiAl-xCr Single Crystals

The compressive properties of near <001> and <111> oriented NiAl-2Cr single crystals and near <011> oriented NiAl-6Cr samples have been measured between 1100 and 1500 K. The 2Cr addition produced significant solid solution strengthening in NiAl, and the <111> and <001> single crystals possessed similar strengths. The 6Cr crystals were not stronger than the 2Cr versions. At 1100 and 1200 K plastic flow in all three Cr-modified materials was highly dependent on stress with exponents > 10. The <011> oriented 6Cr alloy exhibited a stress exponent of about 8 at 1400 and 1500 K; whereas both <001> and <111> NiAl-2Cr crystals possessed stress exponents near 3 which is indicative of a viscous dislocation glide creep mechanism. While the Cottrell-Jaswon solute drag model predicted creep rates within a factor of 3 at 1500 K for <001>-oriented NiAl-2Cr; this mechanism greatly over predicted creep rates for other orientations and at 1400 K for <001> crystals.

Whittenberger, J. Daniel↗

Homoepitaxial "Web Growth" of SiC to Terminate C-Axis Screw Dislocations and Enlarge Step-Free Surfaces

Homoepitaxial CVD growth of thin lateral cantilevers emanating from the edges of mesa patterns dry-etched into on-axis commercial 4H-SiC substrates prior to growth is reported. Cantilevers on the order of a micrometer thick extending tens of micrometers from the edge of a mesa have been grown. The termination of vertically propagating screw dislocations, including a micropipe, that are overgrown by the cantilevers has been demonstrated, in large part because the crystal structure of the cantilevers is established laterally from the mesa sidewalls. This technique could help reduce performance-degrading dislocations in SiC electrical devices.

Neudeck, Philip G.↗

Computed stress fields in GaAs during vertical Bridgman growth

The thermoelastic stress field of GaAs crystals grown by the vertical Bridgman method has been approximated using a linear elastic, axisymmetric stress model. The model included the effects due to the thermal field and the gravitational field, as well as the interaction with the ampoule, but did not fully account for the elastic anisotropy of the crystal. Realistic thermal fields for different furnace temperatures and insulation zone thicknesses were computed with a similar model. The difference between the Von Mises stress and the critical resolved shear stress (CRSS) was used as a measure of the number of dislocations present. Different sets of growth parameters were examined to determine which produced the lowest amount of stress in the crystal. Results show that the crystal-ampoule interaction is the most important parameter in dislocation generation. In addition, for the same sticking boundary conditions, concave interfaces have lower stress than convex interfaces.

Rosch, William↗

Protein crystal growth in low gravity

The solubility and growth of the protein canavalin, and the application of the schlieren technique to study fluid flow in protein crystal growth systems were investigated. These studies have resulted in the proposal of a model to describe protein crystal growth and the preliminary plans for a long-term space flight experiment. Canavalin, which may be crystallized from a basic solution by the addition of hydrogen (H+) ions, was shown to have normal solubility characteristics over the range of temperatures (5 to 25 C) and pH (5 to 7.5) studies. The solubility data combined with growth rate data gathered from the seeded growth of canavalin crystals indicated that the growth rate limiting step is a screw dislocation mechanism. A schlieren apparatus was constructed and flow patterns were observed in Rochelle salt (sodium potassium tartrate), lysozyme, and canavalin. The critical parameters were identified as the change in density with concentration (dp/dc) and the change in index of refraction with concentration (dn/dc). Some of these values were measured for the materials listed. The data for lyrozyme showed non-linearities in plots of optical properties and density vs. concentration. In conjunction with with W. A. Tiller, a model based on colloid stability theory was proposed to describe protein crystallization. The model was used to explain observations made by ourselves and others. The results of this research has lead to the development for a preliminary design for a long-term, low-g experiment. The proposed apparatus is univeral and capable of operation under microprocessor control.

Feigelson, Robert S.↗

Low-temperature solid-state phase transformations in 2H silicon carbide.

Study of the phase transformations taking place in 2H SiC single crystals at temperatures as low as 400 C. Some crystals transformed to a structure with one-dimensional disorder along the crystal c axis. Others transformed to a faulted cubic/6H structure. The transformation is time and temperature dependent, and is greatly enhanced by dislocations. The transformation takes place by means of a slip process perpendicular to the c axis. Cubic SiC crystals were observed to undergo a solid-state transformation above 1400 C.

Powell, J. A.↗