At least 145 records · Page 8

Investigation of the structure and chemical nature of Pd fission product agglomerations in irradiated TRISO particle SiC

Tristructural-isotropic (TRISO)-coated fuel particles are used in high-temperature gas-cooled nuclear reactors. Although the polycrystalline 3C-SiC layer acts as the main barrier to fission product release, post-irradiation examinations have shown that certain metallic fission products are found outside of the TRISO coated particle, with no observable micro-cracks or other mechanical failure feature. In this study, an atomic resolution transmission electron microscopy investigation of a SiC layer of a neutron irradiated (19.38% fissions per initial metal atom average burnup; 1072°C time-averaged temperature) TRISO-coated particle from the first advanced gas reactor experiment at Idaho National Laboratory containing mainly Pd and U was conducted. The fission product Pd was found to be present at dislocation cores associated with twins, stacking faults, and their intersections. The Pd present at the dislocation cores were bonded to Si, suggesting that the diffusion of Pd along the SiC dislocation cores involves the formation of Pd-Si bonds. Evidence of single atom grain boundary migration was also found. Fission product agglomerations at grain boundaries most likely consist of a random solid solution containing Si-FP, Si-C, and C-C type bonding arrangements. No difference in the Si- or C-bonding environment is found for the unoccupied grain boundary adjacent to a fission product agglomeration compared to the bulk SiC.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Computation of Free Molecular Flow in Nuclear Materials

Generally the transport of gases and vapors in nuclear materials is adequately described by the diffusion equation with an effective diffusion coefficient. There are instances however, such as transport through porous or cracked media (nuclear fuels, cladding and coating materials, fuel-cladding gap, graphite, rocks, soil) where the diffusion description has limitations. In general, molecular transport is governed by intermolecular forces and collisions (interactions between multiple gas/vapor molecules) and by molecule-surface interactions. However, if nano-scale pathways exist within these materials, as has been suggested, then molecular transport can be characterized as being in the free-molecular flow regime where intermolecular interactions can be ignored and flow is determined entirely by molecule-surface collisions. Our purpose in this investigation is to focus on free molecular transport in fine capillaries of a range of shapes and to explore the effect of geometry on this transport. We have employed Monte Carlo techniques in our calculations, and for simple geometries we have benchmarked our results against some analytical and previously available results. We have used Mathematica® which has exceptional built-in symbolic and graphical capabilities, permitting easy handling of the complicated geometries and good visualization of the results. Our computations provide insights into the role of geometry in molecular transport in nuclear materials with narrow pathways for flows, and also will be useful in guiding computations that include intermolecular collisions and more realistic gas-surface collision operators.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Nanoscale Compositional Mapping of Commercial LiNi 0.8 Co 0.15 Al 0.05 O 2 Cathodes Using Atom Probe Tomography

Nickel-rich cathodes provide improved specific capacity that lead to higher gravimetric energy density, critical for electric vehicles. However, poor long-term capacity retention at elevated temperatures/high C-rates (the rate of charge and discharge on a battery) stem from material issues: surface phase changes, corrosive side reactions with the electrolyte, ion dissolution and propagation of cracks. Introducing dopants, developing nanoscale surface coatings and graded core-shell structures have all improved the electrochemical performance of nickel-rich cathodes. However, a material level understanding on the effect of Li composition and distribution in Ni-rich cathodes is limited, due to a lack of characterization methods available that can directly image Li at the nanoscale. Hence, it is critical to establish methods such as atom probe tomography (APT), having both nanometer scale spatial resolution and high compositional sensitivity to quantitatively analyze battery cathodes. To fully realize its potential as a method for quantitative compositional analysis of commercial Li-ion batteries, we provide a comprehensive description of the challenges in sample preparation and analyze the dependency of the analysis parameters, specifically laser pulse energy on the measured stoichiometry of elements in a high Ni content cathode material; LiNi 0.8 Co 0.15 Al 0.05 O 2 (NCA). In this work, our findings show the stoichiometry variations cannot be explained by charge state ratios or Ga implantation damage alone during FIB preparation, indicating that additional factors such as crystallographic orientation may need to be considered to achieve quantitative nanoscale compositional analysis of such battery cathodes using APT.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Inspection of plate weldments through an interposed layer of viscoelastic material using an elastic-electromagnetic scanning method

In this study, an elastic-microwave based non-destructive evaluation method is presented to inspect for cracks in weldments and thinning of coated steel plates. The approach uses a microwave interferometer operating at 94 GHz to record the total surface displacement of a coated steel plated as it is driven by an incident elastic field. These spatiotemporal data coupled with wavefield processing algorithms provide powerful detection and localization capabilities. From these wavefield data sets, a plate thickness mapping capability has been demonstrated that can detect thickness changes on the order of 0.79 mm (1/32 in.). It is also shown that a topological energy analysis of the wavefield data can detect and locate small flaws on the order of 5–10 mm (0.19–0.40 in.) in the welded joint. Note, all of these results are obtained through a 50.8 mm (2 in.) thick viscoelastic coating without disturbing the coating or the coating bond. At present the algorithm cannot resolve individual flaws within a grid space, just their cumulative effect. Even with the current limitations, this detection approach appears to be a promising alternative to traditional phased array imaging methods where the coating layer must be removed prior to inspection.

42 ENGINEERING↗

Corrosion-Resistant Coatings for Mitigation and Repair of Spent Nuclear Fuel Dry Storage Canisters

This report summarizes the results of a literature survey on coatings and surface treatments that are used to provide corrosion protection for exposed metal surfaces. The coatings are discussed in the context of being used on stainless steel spent nuclear fuel (SNF) dry storage canisters for potential prevention or repair of corrosion and stress corrosion cracking. The report summarizes the properties of different coating classes, including the mechanisms of protection, their physical properties, and modes of degradation (thermal, chemical, radiological). Also discussed are the current standard technologies for application of the coatings, including necessary surface pretreatments (degreasing, rust removal, grinding) and their effects on coating adhesion and performance. The coatings are also classified according their possible use for in situ repair; ex situ repair, requiring removal from the overpack; and ex situ prevention, or application prior to fuel loading to provide corrosion protection over the lifetime of the canister.

36 MATERIALS SCIENCE↗

Fuel performance analysis of fully-resolved TRISO compact

The TRi-structural ISOtropic (TRISO) fuel multilayered coating structure offers multiple barriers to fission product release, enhancing safety and performance. The heterogeneous nature of TRISO fuel compacts, comprising thousands of randomly distributed coated fuel particles embedded in a graphite matrix, creates intricate stress fields and thermal gradients that cannot be accurately modeled using simplified one-dimensional or homogenized approaches. Consequently, three-dimensional modeling enables the prediction of fuel compact dimensional changes, internal pressure buildup, and fission product transport pathways under diverse irradiation and thermal conditions. This capability facilitates detailed analysis of particle-to-particle interactions, matrix cracking mechanisms, and the statistical distribution of coating failures, which directly impact fuel performance and safety margins. This capability is particularly critical for advanced reactors, such as high-temperature gas-cooled reactors and other Generation IV reactor designs where TRISO fuel operates at elevated temperatures and burn-up levels. This work introduces a novel method to generate an optimized packing of TRISO compacts and a complete 3D mesh with random distribution of TRISO particles, which are discretized into each coating component layer.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Measurement of Interfacial Fracture Toughness of Surface Coatings Using Pulsed-Laser-Induced Ultrasonic Waves

This research develops a new technique for the measurement of interfacial fracture toughness of films/surface coatings using laser-induced ultrasonic waves. Using pulsed laser ablation on the bottom substrate surface, strong stress waves are generated leading to interfacial fractures and coating delamination. Simultaneously, a laser ultrasonic interferometer is used to measure the normal (out-of-plane) displacement of the top surface coating in order to detect coating delamination in a non-destructive manner. We can thus determine the critical laser energy for delamination, yielding the critical stress (that is, the interfacial strength). Subsequently, to examine the interfacial fracture toughness, additional pulsed laser irradiation is applied to a pre-delaminated specimen to show that the delamination area expands. This type of interfacial crack growth can be visualized using laser ultrasonic scanning. Furthermore, the calculation of elastic wave propagation was carried out using a finite-difference time-domain method) in order to accurately estimate the interfacial stress field. In this calculation, the stress distribution around the initial delamination is calculated to obtain the stress intensity factor. Based on the experimental and computational results, interfacial fracture toughness can be quantitatively evaluated. Since this technique relies on a two-laser system in a non-contact approach, it may be useful for a quantitative evaluation of adhesion/bonding quality (including both interfacial fracture strength and toughness) in various environments.

42 ENGINEERING↗

Structural integrity of additively manufactured stainless steel with cold sprayed barrier coating under combined cyclic loading

Integration of metal additive manufacturing (AM) and cold spray (CS) technologies provide an unprecedented opportunity to manufacture coated material systems with complex geometrical features. The application of these material systems in functionally critical components requires adequate structural integrity, particularly in the presence of cyclic loading. This article researches the multiaxial fatigue (axial-torsional cyclic loading) behavior of a coated material system consisting of 15Cr-5Ni precipitation-hardening stainless steel (15-5 PH SS) substrate additively manufactured by direct metal laser sintering with a layer of chromium carbide nickel (CrC-Ni) barrier coating deposited by CS. The influence of AM and CS-induced residual stresses on fatigue performance of test specimens was thoroughly studied. Additionally, the effect of surface roughness and processes induced defects were considered to explain the crack growth mechanism. Stresses assessed by synchrotron X-ray diffraction indicated a substantial accumulation of residual stresses, particularly in the outer surface of the as-fabricated 155 PH SS specimens. The state of residual stress was changed notably following the deposition of CrC-Ni coating in the axial, hoop, and radial directions of the fatigue test specimen. Also, CS deposition of CrC-Ni coating caused significant improvement in the surface quality of the additively manufactured components. Fatigue test results indicated, CS deposition of CrC-Ni substantially enhances the fatigue life of the AM-produced 15-5 PH SS substrate in all loading conditions, particularly in the high cycle fatigue regime. The improvement in the fatigue life of the specimens with coating was associated with a reduction in equivalent residual stress at the substrate surface and improvement in the specimens' surface condition (i.e., reduced surface roughness). The fractographic analysis of the specimen indicated the cracks tend to initiate in the surface of both as-fabricated and cold-sprayed specimens. However, the mechanism of crack growth changed notably following the deposition of CrC-Ni coating. The cracks tended to propagate in the planes parallel or with a small deviation from the build layers of the AM-produced specimens. On the other hand, deposition of CrC-Ni coating increased the deviation of crack growth plane from the build layers of the substrate.

36 MATERIALS SCIENCE↗

On the failure mechanisms of Cr-coated 316 stainless steel in bending fatigue tests

Here, fully-reversed cyclic bending tests were conducted on uncoated and Cr-coated 316 stainless steel specimens. At high stresses, the uncoated specimens outperformed the Cr-coated ones, while the trend reversed at low stresses. For Cr-coated specimens subjected to high stress amplitude loading, experimental observations showed crack initiation at the Cr/substrate interface due to shear steps formed from dislocation activities in the substrate—a conclusion supported by accompanying finite element analysis. Interfacial crack initiation was not observed under low stress amplitudes. This difference in fatigue crack initiation mechanisms induced an opposite trend in fatigue life between high and low stress amplitudes.

36 MATERIALS SCIENCE↗

Enhanced condensation heat transfer using porous silica inverse opal coatings on copper tubes

Abstract Phase-change condensation is commonplace in nature and industry. Since the 1930s, it is well understood that vapor condenses in filmwise mode on clean metallic surfaces whereas it condenses by forming discrete droplets on surfaces coated with a promoter material. In both filmwise and dropwise modes, the condensate is removed when gravity overcomes pinning forces. In this work, we show rapid condensate transport through cracks that formed due to material shrinkage when a copper tube is coated with silica inverse opal structures. Importantly, the high hydraulic conductivity of the cracks promote axial condensate transport that is beneficial for condensation heat transfer. In our experiments, the cracks improved the heat transfer coefficient from ≈ 12 kW/m 2 K for laminar filmwise condensation on smooth clean copper tubes to ≈ 80 kW/m 2 K for inverse opal coated copper tubes; nearly a sevenfold increase from filmwise condensation and identical enhancement with state-of-the-art dropwise condensation. Furthermore, our results show that impregnating the porous structure with oil further improves the heat transfer coefficient by an additional 30% to ≈ 103 kW/m 2 K. Importantly, compared to the fast-degrading dropwise condensation, the inverse opal coated copper tubes maintained high heat transfer rates when the experiments were repeated > 20 times; each experiment lasting 3–4 h. In addition to the new coating approach, the insights gained from this work present a strategy to minimize oil depletion during condensation from lubricated surfaces.

Adera, Solomon↗

Microstructure Study on Initial Lithiation/Delithiation Cycle of Crystalline Silicon Wafer

In this work, we found that Si wafer has a preferential expansion along <110> directions during the initial lithiation/delithiation cycle, as the evidence of wider <110> cracks. These cracks also propagate much deep, at least 5 um. The morphology of the amorphous Si layer appearing after the initial cycle shows a dependence on the plane orientation, i.e., multi and deep layers on the {110} plane, where as a single layer with ~200nm on the {100} plane.A PAA coating layer on the Si wafer mitigates the cracks and reduces the thickness of the amorphous Si layer.

14 SOLAR ENERGY↗

Review of recent developments in the field of magnesium corrosion: Recent developments in Mg corrosion

This paper provides a review of recent developments in the field of Mg corrosion and puts those into context. This includes considerations of corrosion manifestations, material influences, surface treatment, anodization, coatings, inhibition, biodegradable medical applications, stress corrosion cracking, flammability, corrosion mechanisms for HP Mg, critical evaluation of corrosion mechanisms, and concluding remarks. There has been much research recently, and much research continues in this area. In conclusion, this is expected to produce significantly better, more-corrosion-resistant Mg alloys.

36 MATERIALS SCIENCE↗

Effects of a Pressurized Water Treatment on Internal Gelation Sol-Gel Microspheres

Based on previous observations that a pressurized water treatment (PWT) prevented cracking of sol-gel microspheres, we investigated the effects of a PWT on microsphere crystallinity, density, and specific surface area (SSA). Results were used to determine how a PWT alters the properties of microspheres upon drying and heating. Microspheres with diameters near 100-200 µm were prepared with and without a PWT and measured using x-ray diffraction (XRD), transmission electron microscopy (TEM), nitrogen adsorption (BET), and pycnometry. Properties of air-dried microspheres processed with and without a PWT are compared. Additionally, the properties of microspheres processed using a PWT are reported after heating to 150 °C, 450 °C, 750 °C, 1050 °C, and 1350 °C. X-ray diffraction measurements indicate that the PWT step improves the crystallinity of air-dried microspheres. XRD data was also used to calculate crystallite size, which increases with higher heat treatment temperatures. TEM images support crystallite size calculations from XRD data and provide an indication of the range of crystallite sizes, particularly for samples processed at higher temperatures where crystallite sizes are too large for estimation using the Scherrer formula. Density and SSA measurements performed as a function of heat treatment temperature indicate that a PWT increases the density of air-dried microspheres, creates a pore network, and that significant densification occurs between 450 - 750 °C. These results may be used to inform decisions on internal gelation flowsheet parameters to optimize the microsphere formation and gelation step, prevent microsphere cracking, and produce microspheres suitable for subsequent coating operations or pressing into pellets.

cerium oxide, TRISO, internal gelation, nuclear fu↗

Residual Stresses in Spent Nuclear Fuel Storage Canisters with Cold Spray Coatings

This report describes the development of cold spray (CS) process and its application to provide on overlay coating of metal welds with a surface crack in a spent nuclear fuel (SNF) storage canister and thereby remediate the canister from further propagation of the crack. This work informs aging management programs for the SNF canisters.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Detection and analysis of particles with failed SiC in AGR-1 fuel compacts

As the primary barrier to release of radioactive isotopes emitted from the fuel kernel, retention performance of the SiC layer in tristructural isotropic (TRISO) coated particles is critical to the overall safety of reactors that utilize this fuel design. Most isotopes are well-retained by intact SiC coatings, so pathways through this layer due to cracking, structural defects, or chemical attack can significantly contribute to radioisotope release. In the US TRISO fuel development effort, release of 134 Cs and 137 Cs are used to detect SiC failure during fuel compact irradiation and safety testing because the amount of cesium released by a compact containing one particle with failed SiC is typically ten or more times higher than that released by compacts without failed SiC. Compacts with particles that released cesium during irradiation testing or post-irradiation safety testing at 1600–1800 °C were identified, and individual particles with abnormally low cesium retention were sorted out with the Oak Ridge National Laboratory (ORNL) Irradiated Microsphere Gamma Analyzer (IMGA). X-ray tomography was used for three-dimensional imaging of the internal coating structure to locate low-density pathways through the SiC layer and guide subsequent materialography by optical and scanning electron microscopy. In addition, all three cesium-releasing particles recovered from as-irradiated compacts showed a region where the inner pyrocarbon (IPyC) had cracked due to radiation-induced dimensional changes in the shrinking buffer and the exposed SiC had experienced concentrated attack by palladium; SiC failures observed in particles subjected to safety testing were related to either fabrication defects or showed extensive Pd corrosion through the SiC where it had been exposed by similar IPyC cracking.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Silver (Ag) Transport Mechanisms in TRISO Coated Particles: A Critical Review

Transport of 110mAg in the intact SiC layer of TRISO coated particles has been studied for approximately 30 years without arriving at a satisfactory explanation of the transport mechanism. In this paper the possible mechanisms postulated in previous experimental studies, both in-reactor and out-of reactor research environment studies are critically reviewed and of particular interest are relevance to very high temperature gas reactor operating and accident conditions. Among the factors thought to influence Ag transport are grain boundary stoichiometry, SiC grain size and shape, the presence of free silicon, nano-cracks, thermal decomposition, palladium attack, transmutation products, layer thinning and coated particle shape. Additionally new insight to nature and location of fission products has been gained via recent post irradiation electron microscopy examination of TRISO coated particles from the DOE’s fuel development program. The combined effect of critical review and new analyses indicates a direction for investigating possible the Ag transport mechanism including the confidence level with which these mechanisms may be experimentally verified.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The Effect of HVOF Bond Coating with APS Flash Coating on TBC Performance

To study the benefit of ~ 50-µm-thick air-plasma-sprayed (APS) ‘flash’ bond coatings, NiCoCrAlYHfSi high-velocity oxygen fuel (HVOF) bond coatings were deposited on alloy 247 disk substrates with APS yttria-stabilized zirconia topcoatings. Using 1-h cycles at 1100 °C in air with 10% H 2 O and HVOF-only bond coatings as a baseline, APS flash coatings extended the average coating lifetime by > 10% using NiCoCrAlYHfSi and > 70% using NiCoCrAlY powder. Coatings were characterized after 0, 100 and 300 cycles and after failure. Residual stress in the thermally grown alumina scale was mapped every 100 cycles using photo-stimulated luminescence piezospectroscopy. The flash coating created an interlocked metal–alumina layer that appeared to inhibit critical crack formation, and the underlying HVOF layer prevented further internal oxidation and appeared to supply the APS flash coating with Al. Furthermore, the addition of Hf and Y to the flash coating increased internal oxidation and accelerated Al consumption, thereby reducing the benefit of the flash coating.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

In situ high-temperature 3D imaging of the damage evolution in a SiC nuclear fuel cladding material

Silicon carbide (SiC)-based nuclear fission fuel rod cladding has been considered as one of the possible designs for accident tolerant fuels. It is in the form of a SiC fibre reinforced SiC matrix composite tube (SiC f -SiC m ) with monolithic SiC outer and/or inner coating layers. This study focuses on the deformation and fracture processes in this material using in situ X-ray micro-computed tomography (XCT) at room temperature (RT) and 1200 °C in an inert gas environment in a C-ring compression loading configuration. Prior to testing, local properties and residual stresses were characterised using nanoindentation and Raman spectroscopy since they can impact the mechanical behaviour of the material. The 3D strain distribution, crack formation and propagation processes including the toughening mechanisms (e.g., crack deflection, micro-cracking, crack bridging and bifurcation) are investigated in the coating and underlying composites at RT and 1200 °C. There is no particular sequence which toughening mechanism occurs first – this is very different from the conventional toughening theory in ceramic-matrix composites under uniaxial tension loading. Indeed, no evidence of fibre pull-out or fibre fracture was observed in this SiC f -SiC m nuclear cladding material in the current C-ring compression configuration. The correlation between local measurements and bulk mechanical behaviour are discussed.

3D imaging↗