At least 145 records · Page 8

In–Depth Analysis of the Degradation Mechanisms of High–Nickel, Low/No–Cobalt Layered Oxide Cathodes for Lithium–Ion Batteries

A rational compositional design of high-nickel, cobalt-free layered oxide materials for high-energy and low-cost lithium-ion batteries would be expected to further propel the widespread adoption of electric vehicles (EVs), yet a composition with satisfactory electrochemical properties has yet to emerge. The previous work has demonstrated a promising LiNi 0.883 Mn 0.056 Al 0.061 O 2 (NMA-89) composition that outperformed high-nickel, cobalt-containing analogs in cycling stability and maintained a comparable rate performance and thermal stability. Herein, the capacity fading mechanism of NMA-89 in a pouch full cell with a 4.2 V cutoff is compared to that of its cobalt-containing analogs. The results reveal that particle cracking in LiNi 0.89 Mn 0.055 Co 0.055 O 2 (NMC-89) and LiNi 0.883 Co 0.053 Al 0.064 O 2 (NCA-89) leads to a loss of active material and an increase in surface area, thereby exacerbating structural and surface instabilities, accelerating impedance and polarization growth, and ultimately reducing their capacity retentions. LiNi 0.89 Mn 0.044 Co 0.042 Al 0.013 Mg 0.011 O 2 (NMCAM-89) and NMA-89 experience subdued surface reactions and maintain spherical particle structures, both of which are conducive to their capacity retentions during long-term cycling. Furthermore, this investigation offers insights into how specific transition-metal ions dictate the electrochemical stability of high-Ni layered oxide cathode materials, highlights the benefit of Mn-Al combination in NMA-89, and presents potential strategies to further enhance the performance of this novel class of cathode materials.

degradation mechanisms↗

Voltage-Based Strategies for Preventing Battery Degradation under Diverse Fast-Charging Conditions

Maintaining safe operating conditions is a key challenge for high-performance lithium-ion battery applications. The lithium-plating reaction remains a risk during charging, but limited studies consider the highly variable charging conditions possible in commercial cells. Here we combine pseudo-2D electrochemical modeling with data visualization methods to reveal important relationships between the measurable cell voltage and difficult-to-predict Li-plating onset criteria. An extensively validated model is used to compute Li plating for thousands of multistep charging conditions spanning diverse rates, temperatures, states-of-charge, and cell aging. Here we observe an empirical cell operating voltage limit below which plating does not occur across all conditions, and this limit varies with the battery state-of-charge and aging. A model sensitivity analysis also indicates that, when comparing two charging voltage profiles, the capacity difference at 4.0 V correlates well with the difference in the plating onset capacity. These results encourage simple strategies for Li-plating prevention that are complementary to existing battery controls.

25 ENERGY STORAGE↗

Quantitative Microstructural Characterization of Plutonium Oxalate Auto-Degradation and Evidence for PuO2 Nanocrystal Formation

It has been known since the 1950s that plutonium oxalate powders change color and lose mass over time when stored at room temperature in air. Despite several studies monitoring these changes, there are still discrepancies in the literature regarding the speciation of intermediate and final products that result from this decomposition. Presented here for the first time is a comprehensive series of time-resolved powder X-ray diffraction experiments coupled with solid-state optical spectroscopy and electron microscopy of aged plutonium (III) and (IV) oxalate powders. These data provide fresh insight into the chemical and structural changes that occur in these solids over time at room temperature and represent new evidence suggesting both plutonium (III) and plutonium (IV) oxalates decompose to form nanocrystalline plutonium oxide in the solid state.

Corbey, Jordan F.↗

Experimental and modeling study of calcium carbonate precipitation and its effects on the degradation of oil well cement during carbonated brine exposure

Decalcification of cement in solutions of carbonated brine is important to a host of engineering applications, especially in subsurface service environments where cementitious materials are frequently utilized as engineered barriers for wellbore seals, as well as shaft and drift seals and waste forms for nuclear waste disposal. Analysis of leaching simulations and experiments shows that, depending on solution compositions (dissolved CO{sub 2} concentration, pH, Ca ion concentration), calcite precipitation occurring during leaching of cement in contact with carbonated brine can have a significant impact on cement reactivity, in some instances leading to complete arrest of reactivity via calcium carbonate ''pore-clogging''. We present modeling and experimental results that examine the range of solution conditions that can lead to pore-clogging. Analysis of the results shows that distinct regimes of leaching behavior, based on pH and pCO2, can be used to form a framework to better understand the occurrence of pore-clogging.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗