Work updates for Prof. Lee
I want to update my work which I have done so far in INL, including matlab GUI for neutron radiography and some fuel EBSD works.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
I want to update my work which I have done so far in INL, including matlab GUI for neutron radiography and some fuel EBSD works.
This is the poster for intern poster session on 08/12, including the EBSD analysis result of UO2 fuel.
Functionally graded material (FGM) ZnO is made via spark plasma sintering/field-assisted sintering technique (SPS/FAST) by varying the Al dopant content along the z-axis or pressing direction. A wide range of Al content (0–5 wt%) is used by adding Al powder to nanosized ZnO powder. Thermoelectric (TE) measurements are done on the FGM and individual layers made separately. X-ray diffraction (XRD) shows two phases, ZnO and spinel phase (ZnAl 2 O 4 ). High-resolution Raman spectroscopy reveals doped ZnO and spinel phase (ZnAl 2 O 4 ) spatially and shows segregation in the layer with highest Al content. Electron backscatter diffraction (EBSD) reveals noticeable grain growth with decreasing Al content, and there is a common, random preferred orientation in all layers. The tested properties are used to simulate efficiency curves for a discretely graded, five-layer FGM as well as a homogenous material, where both graded structures provide an opportunity to widen the current density ranges and therefore the temperature range of useful energy conversion.
Here, this study systematically investigates the effects of shielding gas, bead spacing, weld mode, and travel speed on the phase balance, porosity, and hardness of wire arc additively manufactured (WAAM) super duplex stainless steel (ER2594). Robotic WAAM was employed to fabricate multilayer walls under systematically varied process conditions, followed by phase transformation simulations, X-ray computed tomography (XCT), electron backscatter diffraction (EBSD), and microhardness evaluation. Thermodynamic simulations predicted rapid cooling of AM process can suppress the potential formation of deleterious precipitates which was later validated via cross-sectional microstructure analyses of printed samples. XCT revealed porosity levels below 0.2% for all deposits, with reduced travel speed significantly lowering defect volume. Microstructural analyses revealed the evolution of various austenite precipitates, including grain boundary austenite (GBA), Widmanstätten austenite (WA), and intergranular austenite (IGA), sequentially upon cooling of the ferrite phase. Among all process parameters, weld transfer mode exhibited the strongest influence on phase balance; pulsed mode promoted higher ferrite retention (~ 36%) compared to RapidX mode. No consistent relationship between stabilized phase fraction and captured microhardness was observed. This work provides critical insights for optimizing WAAM parameters to control phase balance and mechanical performance, which is essential for producing high-integrity super duplex stainless-steel components for nuclear and marine applications.
Serpentine minerals have received a lot of attention because of their unique crystal structures, their wide occurrence in orogenic belts and their potential role in contributing seismic anisotropy in subducting slabs. Several studies have investigated crystal preferred orientation (CPO) in high temperature antigorite serpentinites from Japan, the Alps, Spain, Cuba and Tibet, documenting significant crystal alignment. However, only a limited number of lower grade serpentines have been explored to date. Mainly because of submicroscopic microstructural heterogeneities CPO cannot be measured with conventional methods such as optical microscopy and EBSD. In this study 15 serpentinites from different tectonic settings in California, the Central Alps and Northern Spain have been investigated, mainly with high energy synchrotron X-ray diffraction, to quantify bulk crystal alignment. We find that CPO is strong on sheared surfaces of fractured blocks and secondary veins but the bulk of most serpentinite samples, except high-grade recrystallized antigorite serpentinite, show only weak crystal alignment. Correspondingly calculated seismic anisotropy based on CPO is not very significant. This is supported by very heterogeneous microstructures as documented with SEM and TEM analyses.
The effects of internal hydrogen on the deformation microstructures of 304L austenitic stainless steel have been characterized using electron backscattered diffraction (EBSD), transmission Kikuchi diffraction (TKD), high-resolution scanning transmission electron microscopy (HRSTEM), and nanoprobe diffraction. Samples, both thermally precharged with hydrogen and without thermal precharging, were subjected to tensile deformation of 5 and 20 pct true strain followed by multiple microscopic interrogations. Internal hydrogen produced widespread stacking faults within the as-forged initially unstrained material. While planar deformation bands developed with tensile strain in both the hydrogen-precharged and non-precharged material, the character of these bands changed with the presence of internal hydrogen. As shown by nanobeam diffraction and HRSTEM observations, in the absence of internal hydrogen, the bands were predominantly composed of twins, whereas for samples deformed in the presence of internal hydrogen, ε -martensite became more pronounced and the density of deformation bands increased. For the 20 pct strain condition, α '-martensite was observed at the intersection of ε -martensite bands in hydrogen-precharged samples, whereas in non-precharged samples α '-martensite was only observed along grain boundaries. We hypothesize that the increased prevalence of α '-martensite is a secondary effect of increased ε -martensite and deformation band density due to internal hydrogen and is not a signature of internal hydrogen itself.
The nanostructured ferritic alloy 14YWT is a promising candidate for in-core use in generation IV nuclear reactors, due to a dense dispersion of insoluble, ultrafine-scale Y-Ti-O nano-oxides, which provide a high degree of irradiation tolerance and thermal stability. This work investigates the effects of heat treatment on the workability of 14YWT, along with the effect of processing history on abnormal grain structures and radial microstructural uniformity. In this study, a 14YWT rod consolidated at 850 °C was heat treated in argon at 1100 °C, 1150 °C, 1200 °C, or 1250 °C for 1 or 8 hours and changes in mechanical properties and microstructure were examined using microhardness and electron backscattered diffraction (EBSD). Two distinct types of large abnormal grains were observed, each with unique processing origins, including one with high and the other with low strain energy. Consolidation via direct extrusion resulted in radial microstructural gradients, where the center of the rod was softer with larger grain sizes and lower strain energies. These gradients persisted and intensified throughout heat treatment. Based upon this work, the recommended heat treatment for increased workability with minimal microstructural change is 1150 °C for 1 hours.
Uranium alloyed with 10 wt% Mo (U-10Mo) undergoes discontinuous precipitation (DP) when subjected to sub-eutectoid heat-treatment. It is hypothesized that the crystallographic texture of the U-10Mo can be modified to minimize the degree of DP, however the evolution of texture throughout the manufacturing process is not well understood. Crystallographic textures of two U-10Mo samples homogenized at 900°C and 1000°C were studied after uniaxial rolling and annealing. A total of 6 samples were analyzed upon rolling using a combination of hot and cold rolling conditions to strains of 83%, 90% and 97% and subsequently annealed at 700°C for one hour. Microstructures and textures were analyzed via electron backscatter diffraction (EBSD) for each homogenization, strain and post-annealed states. Results show that the U-10Mo exhibits typical rolling textures seen in body-centered cubic materials with increasing intensities of both a- and ?-fibers with increasing strain. After recrystallization, the texture appeared to be effectively randomized in all samples. Homogenization temperature showed no effect on the rolling and recrystallization behavior. Potential factors leading to the randomization of texture are discussed along with the implications of textures on the minimization of DP.
A survey of cadmium plated field return hardware showed ubiquitous cadmium whisker growth. The most worn and debris-covered hardware showed the densest whisker growth. Whiskers were often found growing in agglomerates of nodules and whiskers. The hardware was rinsed with alcohol to transfer whiskers and debris from the hardware to a flat stub. Fifty whiskers were studied individually by scanning electron microscopy (SEM), including energy dispersive spectroscopy (EDS) and electron backscatter diffraction (EBSD). Most of the whiskers were single crystal, though three were found to contain grain boundaries at kinks. The whiskers ranged from 5 to 600 μm in length and 80 pct showed a $<\bar{1} 2 \bar{1} 0>$ type growth direction. This growth direction facilitates the development of low energy side faces of the whisker, (0001) and {1010}.
The competition between epitaxial vs. equiaxed solidification has been investigated in CMSX-4 single crystal superalloy during laser melting as practiced in additive manufacturing. Single-track laser scans were performed on a powder-free surface of directionally solidified CMSX-4 alloy with several combinations of laser power and scanning velocity. Electron backscattered diffraction (EBSD) mapping facilitated identification of new orientations, i.e., “stray grains” that nucleated within the fusion zone along with their area fraction and spatial distribution. Using high-fidelity computational fluid dynamics simulations, both the temperature and fluid velocity fields within the melt pool were estimated. This information was combined with a nucleation model to determine locations where nucleation has the highest probability to occur in melt pools. In conformance with general experience in metals additive manufacturing, the as-solidified microstructure of the laser-melted tracks is dominated by epitaxial grain growth; nevertheless, stray grains were evident in elongated melt pools. It was found that, though a higher laser scanning velocity and lower power are generally helpful in the reduction of stray grains, the combination of a stable keyhole and minimal fluid velocity further mitigates stray grains in laser single tracks.
In this study, prismatic geometries of GRCop-84 [Cu-8Cr-4Nb (at. pct)] were built with laser-powder bed fusion (L-PBF) process. The samples were sectioned parallel or perpendicular to the build direction and characterized in the as-built and after post-processing with a hot-isostatically pressing (HIP) treatment. The microstructure and phase evolutions were evaluated with optical microscopy, scanning electron microscopy (SEM), electron backscattered diffraction (EBSD), and high-temperature X-ray diffraction (HTXRD) up to 1223 K. The samples in the as-built conditions exhibited predominantly columnar epitaxial and misoriented Cu-FCC grains. The microstructure evolutions are discussed based on locations within the overall build geometry, the dynamics of small melt pool shape and sectioning effects. The above grain structure did not change significantly during post-process HIP treatment. The stability of this FCC grain structure is attributed to the formation of primary stable Cr 2 Nb (Laves phase) during L-PBF, even before the emergence of FCC grains from liquid. The stability of Cr 2 Nb in both as-built and HIPed samples were evaluated using high-temperature X-ray diffraction measurements and compared with that of gas-atomized powder. The significance of these results is discussed with reference to aerospace applications.
Abstract The Additive Manufacturing Benchmark Test Series (AM Bench) is a broad effort to produce rigorous measurement datasets for validating AM computer simulations across the range of processing, structure, and properties, for many additive manufacturing (AM) build methods and material classes. Here, the microstructures of nickel alloy 718 AM Bench 2022 test artifacts produced using laser-based powder bed fusion (PBF-LB), in both as-built and fully heat-treated conditions, are examined. Cross sections are primarily characterized using large area scanning electron microscopy (SEM) electron backscatter diffraction (EBSD) and example analyses of the crystallographic textures are described. These data are part of a large set of in situ and ex situ measurements from both three-dimensional builds and laser tracks on bare plates. All the measurement data are available online with download links at www.nist.gov/ambench .
A new wrought FeMnAl steel contains high Mn content and high Al content. This steel has high strength. When it is compared to conventional steels with the similar strength, its density is lower. FeMnAl steels can be used in armor vehicle manufacturing, in which welding is a common practice to join the steel plates together. The welding of FeMnAl steels has not been sufficiently studied before. Here, this work studied the weldability and weld microstructure of an FeMnAl steel and provided useful data for the welding practice of FeMnAl steels. The influences of weld filler metals and shielding gases were studied, using single-pass bead-on-plate gas metal arc welding (GMAW) and gas tungsten arc welding (GTAW) two processes. The optimal filler metals and shielding gases have been determined to achieve the better weldability. Autogenous GTAW and electron beam welding were also conducted. Cracks were found in the HAZ in the GMAW welds and electron beam welds. Fewer or no cracks were found in the HAZ of GTAW welds. SEM, SEM/EDX, TEM, TEM/EDX, and EBSD were used to analyze the grain boundaries in the HAZ and the cracks. The grain boundaries of FeMnAl base metal are mostly high angle grain boundaries (HAGBs), which attract impurity and solute atoms and cause intergranular cracking. The proposed cracking mechanisms are liquation cracking and ductility-dip cracking. It was found that GTAW provides much better weldability for the FeMnAl steel than GMAW and EBW.
Shear Assisted Processing and Extrusion (ShAPE) experimental setup and tooling were adopted for extruding thin-walled AA7075 aluminum tube from as-cast non-homogenized billet material in a single run. The mechanical and microstructural characterizations were performed on the extrudate in the as-extruded condition without subsequent heat treating. It was shown that the ShAPE process developed a significantly refined microstructure with uniform and almost equiaxed grain structure on both hoop and axial cross-sections of the extrudate as well as through the thickness of the material. The pole figures and inverse pole figures of the EBSD data showed an strong shear texture development, and it was found out that axial shear is the dominant deformation mechanism in the regions near the inner surface of the tube, while combined axial and torsional shears are the two dominant modes of deformation near the outer surface of the extrudate. As for the mechanical properties, there was an increase of 150% and 73% in the yield and ultimate strengths of the tube produced using ShAPE process, respectively, and a 18% decrease in maximum uniform plastic elongation compared to the conventionally extruded AA7075-O tube.
Developing a comprehensive understanding of the modification of material properties by neutron irradiation is important for the design of future fission and fusion power reactors. Self-ion implantation is commonly used to mimic neutron irradiation damage, however an interesting question concerns the effect of ion energy on the resulting damage structures. The reduction in the thickness of the implanted layer as the implantation energy is reduced results in the significant quandary: Does one attempt to match the primary knock-on atom energy produced during neutron irradiation or implant at a much higher energy, such that a thicker damage layer is produced? In this work, we address this question by measuring the full strain tensor for two ion implantation energies, 2 MeV and 20 MeV in self-ion implanted tungsten, a critical material for the first wall and divertor of fusion reactors. A comparison of 2 MeV and 20 MeV implanted samples is shown to result in similar lattice swelling. Multi-reflection Bragg coherent diffractive imaging (MBCDI) shows that implantation induced strain is in fact heterogeneous at the nanoscale, suggesting that there is a non-uniform distribution of defects, an observation that is not fully captured by micro-beam Laue diffraction. At the surface, MBCDI and high-resolution electron back-scattered diffraction (HR-EBSD) strain measurements agree quite well in terms of this clustering/non-uniformity of the strain distribution. However, MBCDI reveals that the heterogeneity at greater depths in the sample is much larger than at the surface. This combination of techniques provides a powerful method for detailed investigation of the microstructural damage caused by ion bombardment, and more generally of strain related phenomena in micro-volumes that are inaccessible via any other technique.
Here this study presents an in-depth characterization of the microstructures, crystallographic orientations, and dislocation characteristics beneath hydrogen-induced quasi-cleavage fracture features of an as-quenched, lath martensitic (α') 22MnB5 steel. The fracture surfaces of gaseous hydrogen-embrittled martensitic specimens were analyzed by a combination of multiple analytical tools: scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM), and transmission Kikuchi diffraction (TKD). The dominant fracture mode in the hydrogen-affected zones was quasi-cleavage fracture, which involved significant plasticity, evidenced by plastic zones near tear ridges and a high density of dislocations beneath the quasi-cleavage facets. The martensite constituent sizes, variant orientations, and boundaries influenced the quasi-cleavage surface morphologies. Fractography revealed the occurrence of {100} α' -type cleavage across martensitic laths, developing relatively “flat” quasi-cleavage surfaces, in addition to {110} α' -type cracking likely along lath and block boundaries, and fracture along non-cleavage planes. The likelihood of the formation of the relatively “flat” quasi-cleavage surfaces increased with increasing martensitic constituent sizes. Substantial dislocation bands formed on intersecting {112} α' slip planes within a martensite block below the hydrogen-induced cleavage fractures on {100} α' planes. River markings on the quasi-cleavage surfaces were found to originate from the complex, hierarchical lath martensitic microstructure. Steps and ridges on the quasi-cleavage facets generally linked with the various martensitic boundaries, suggesting that they were produced as a result of crack deviations at those boundaries. The fracture paths and martensite quasi-cleavage mechanisms are discussed in the context of the role of hydrogen and Cottrell cleavage model.
Here, a CrCoNi based medium entropy alloy with small additions of Ti, Al and Nb (denoted as (CrCoNi) 93 Al 4 Ti 2 Nb) in the as-quenched condition, exhibits tensile properties comparable to those of the equiatomic CrCoNi alloy at room temperature. Dark field transmission electron microscopy (TEM), atomic resolution high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM) together with atom probe tomography (APT) show that spatially-localized long range ordering (LRO) L1 2 domains exist in this alloy. The evolution of deformation substructure with plastic deformation in this alloy was characterized using electron backscatter diffraction (EBSD), electron channeling contrast imaging (ECCI) and STEM based techniques including the recently developed weak beam dark field STEM imaging. Plastic deformation occurs by the slip of a/2<110>dislocations, which are narrowly dissociated into Shockley partial dislocations on {111} slip planes. Their dissociation distances in the (CrCoNi) 93 Al 4 Ti 2 Nb alloy are much smaller than the widths of the corresponding partials in the equiatomic CrCoNi alloy due to one or more of the minor alloying elements (Al, Ti, Nb). Dislocation slip in this alloy has a pronounced planar character. The leading dislocations in slip bands glide as pairs due to the existence of LRO domains. Multipoles were formed through the slip of dislocations with opposite signs on adjacent {111} slip planes. Those multipoles serve as building blocks for the formation of subgrain structures consisting of fine slip bands. The distances between slip bands were continuously refined during plastic deformation and dynamic refinement of slip bands plays a crucial role in strain hardening. The effects of LRO domains on planar dislocation slip, the deactivation of deformation twinning and strain hardening of this alloy are discussed.
Predicting the failure of crystalline materials at high strain rates requires knowledge of the underlying failure mechanisms and their dependence on microstructure. However, little experimental consensus exists on the underlying micromechanics of spallation. In this study, a 3D-EBSD characterization experiment is performed on tantalum prior to and after partial spallation by plate impact, which allowed for the statistical assessment of the microstructural neighborhoods surrounding incipient voids. In analyzing the resulting dataset containing 5884 grains and 467 voids, it is observed that the voids were roughly spherical and consistent in size throughout the spalled material. The voids mostly resided at quadruple points, at triple junctions, at grain boundaries, and within grains, in decreasing order of prevalence. Moreover, voids tended to form at grain boundaries with high degrees of plastic incompatibility, growing into the plastically soft grain but orienting primarily with or perpendicular to the loading direction. Here, the statistics from these analyses of 3D microstructural data support dynamic cavitation models for ductile spallation.