Microstructure, magnetic properties and exchange-coupling interactions for one-dimensional hard/soft ferrite nanofibers
SrFe{sub 12}O{sub 19} (SFO)/Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} (NZFO) composite ferrite nanofibers with diameters about 120 nm have been prepared by the electrospinning and calcination process. The SFO/NZFO composite ferrites are formed after calcined at 700 Degree-Sign C for 2 h and the composite nanofibers with various mass ratios obtained at 900 Degree-Sign C are fabricated from NZFO grains about 16-40 nm and SFO grains of 19-45 nm with a uniform phase distribution. With the SFO ferrite content increasing, the coercivity (H{sub c}) and remanence (M{sub r}) for the composite ferrite nanofibers initially increase, reaching maximum values of 379.8 kA/m (297 K) and 242.2 kA/m (77 K), 39.1 Am{sup 2}/kg (297 K) and 53.5 Am{sup 2}/kg (77 K), respectively, at a mass ratio (SFO:NZFO) of 4, and then show a reduction tendency with a further increase of the mass ratio. This enhancement in magnetic properties is attributed to the competition of the exchange-coupling interaction and the dipolar interaction in the composite nanofibers. - Graphical abstract: SrFe{sub 12}O{sub 19} (SFO)/Ni{sub 0.5}Zn{sub 0.5}Fe{sub 2}O{sub 4} (NZFO) composite ferrite nanofibers with a uniform phase distribution show competition of the exchange-coupling interaction and the dipolar interaction in the composite nanofibers. Highlights: Black-Right-Pointing-Pointer Composite ferrite nanofibers have been prepared by the electrospinning. Black-Right-Pointing-Pointer Magnetic exchange-coupling interaction for these nanofibers were analyzed. Black-Right-Pointing-Pointer Nanofibers magnetic properties measured at 297 K and 77 K were discussed.