Search NASA⌕ Search

SEARCH · Search NASA

Results for “GASKETS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

The COMPRES/GSECARS gas-loading system for diamond anvil cells at the Advanced Photon Source

We have designed and constructed a new system for loading gases at high pressure into diamond anvil cells at pressures up to 200 MPa. The gases are used either as quasi-hydrostatic pressure media surrounding the sample or as the sample itself. The diamond cell is sealed using a clamping mechanism, which permits nearly any type of diamond anvil cell to be used. Online ruby fluorescence and video imaging systems allow in situ monitoring of the pressure and gasket deformation as the cell is sealed, resulting in a very high success rate in loading cells. The system includes interlocks and computer control that allow it to be safely and easily operated by visiting users at the Advanced Photon Source. We present preliminary X-ray diffraction data on volume compression of single-crystal magnesium oxide (MgO) in helium up to 110 GPa.

43 PARTICLE ACCELERATORS↗

WH[eta] under pressure

An initial observation of the formation of WH under pressure from W gaskets surrounding hydrogen in diamond anvil cells led to a theoretical study of tungsten hydride phases. At P = 1 atm no stoichiometry is found to be stable with respect to separation into the elements, but as the pressure is raised WH{sub n} (n = 1-6, 8) stoichiometries are metastable or stable. WH and WH{sub 4} are calculated to be stable at P > 15 GPa, WH{sub 2} becomes stable at P > 100 GPa and WH{sub 6} at P > 150 GPa. In agreement with experiment, the structure computed for WH is anti-NiAs. WH{sub 2} shares with WH a hexagonal arrangement of tungsten atoms, with hydrogen atoms occupying octahedral and tetrahedral holes. For WH{sub 4} the W atoms are in a distorted fcc arrangement. As the number of hydrogens rises, the coordination of W by H increases correspondingly, leading to a twelve-coordinated W in WH{sub 6}. In WH{sub 8} H{sub 2} units also develop. All of the hydrides considered should be metallic at high pressure, though the Fermi levels of WH{sub 4} and WH{sub 6} lie in a deep pseudogap. Prodded by these theoretical studies, experiments were then undertaken to seek phases other than WH, exploring a variety of experimental conditions that would favor further reaction. Though a better preparation and characterization of WH resulted, no higher hydrides have as yet been found.

08 HYDROGEN↗

Design considerations for concentrating solar power tower systems employing molten salt.

The Solar Two Project was a United States Department of Energy sponsored project operated from 1996 to 1999 to demonstrate the coupling of a solar power tower with a molten nitrate salt as a heat transfer media and for thermal storage. Over all, the Solar Two Project was very successful; however many operational challenges were encountered. In this work, the major problems encountered in operation of the Solar Two facility were evaluated and alternative technologies identified for use in a future solar power tower operating with a steam Rankine power cycle. Many of the major problems encountered can be addressed with new technologies that were not available a decade ago. These new technologies include better thermal insulation, analytical equipment, pumps and values specifically designed for molten nitrate salts, and gaskets resistant to thermal cycling and advanced equipment designs.

25 ENERGY STORAGE↗

Fluidized Bed Asbestos Sampler Design and Testing

A large number of samples are required to characterize a site contaminated with asbestos from previous mine or other industrial operations. Current methods, such as EPA Region 10’s glovebox method, or the Berman Elutriator method are time consuming and costly primarily because the equipment is difficult to decontaminate between samples. EPA desires a shorter and less costly method for characterizing soil samples for asbestos. The objective of this was to design and test a qualitative asbestos sampler that operates as a fluidized bed. The proposed sampler employs a conical spouted bed to vigorously mix the soil and separate fine particulate including asbestos fibers on filters. The filters are then analyzed using transmission electron microscopy for presence of asbestos. During initial testing of a glass prototype using ASTM 20/30 sand and clay fines as asbestos surrogates, fine particulate adhered to the sides of the glass vessel and the tubing to the collection filter – presumably due to static charge on the fine particulate. This limited the fines recovery to ~5% of the amount added to the sand surrogate. A second prototype was constructed of stainless steel, which improved fines recovery to about 10%. Fines recovery was increased to 15% by either humidifying the inlet air or introducing a voltage probe in the air space above the sample. Since this was not a substantial improvement, testing using the steel prototype proceeded without using these techniques. Final testing of the second prototype using asbestos suggests that the fluidized bed is considerably more sensitive than the Berman elutriator method. Using a sand/tremolite mixture with 0.005% tremolite, the Berman elutriator did not segregate any asbestos structures while the fluidized bed segregated an average of 11.7. The fluidized bed was also able to segregate structures in samples containing asbestos at a 0.0001% concentration, while the Berman elutriator method did not detect any fibers at this concentration. Opportunities for improvement with the fluidized bed include improving reproducibility among replicates, increasing mass recovery, improving the lid gasket seal.

42 ENGINEERING↗

Cryogenic Flange and Seal Evaluation

The assembly of flanges, seals, and pipes are used to carry cryogenic fluid from a storage tank to the vehicle at launch sites. However, after a certain amount of cycles these raised face flanges with glass-filled Teflon gaskets have been found to have torque relaxation and are as a result susceptible to cryogenic fluid leakage if not re-torqued. The intent of this project is to identify alternate combinations of flanges and seals which may improve thermal cycle performance and decrease re-torque requirements. The general approach is to design a test fixture to evaluate leak characteristics between spiral and concentric serrations and to test alternate flange and seal combinations. Due to insufficient time, it was not possible to evaluate these different types of combinations for the combination that improved thermal cycle performance the most. However, the necessary drawings for the test fixture were designed and assembled along with the collection of the necessary parts.

fluid↗

Development of a Forced-Convection Liquid-Fluoride-Salt Test Loop

A small forced-convection molten-fluoride-salt loop is being constructed at Oak Ridge National Laboratory to examine the heat transfer behavior of FLiNaK salt in a heated pebble bed. Objectives of the experiment include reestablishing infrastructure needed for fluoride-salt loop testing, developing a unique inductive heating technique for performing heat transfer (or other) experiments, measuring heat transfer characteristics in a liquid-fluoride-salt-cooled pebble bed, and demonstrating the use of silicon carbide (SiC) as a structural component for salt systems. The salt loop will consist of an Inconel 600 piping system, a sump-type pump, a SiC test section, and an air-cooled heat exchanger, as well as auxiliary systems needed to pre-heat the loop, transport salt into and out of the loop, and maintain an inert cover gas over the salt. A 30,000 Hz inductive heating system will be used to provide up to 250 kW of power to a 15 cm diameter SiC test section containing a packed bed of 3 cm graphite spheres. A SiC-to-Inconel 600 joint will use a conventional nickel/grafoil spiral wound gasket sandwiched between SiC and Inconel flanges. The loop system can provide up to 4.5 kg/s of salt flow at a head of 0.125 MPa and operate at a pressure just above atmospheric. Pebble Reynolds numbers of up to 2600 are possible with this configuration. A sump system is provided to drain and store the salt when not in use. Instrumentation on the loop will include pressure, temperature, and flow measurements, while the test section will be instrumented to provide pebble and FLiNaK temperatures.

36 MATERIALS SCIENCE↗

Development and Application of an Oversize Reusable DOT 7A Type A Overpack Container at the Y-12 National Security Complex - 13150

Waste Management personnel at the Y-12 National Security Complex (Y-12) are concluding a multi-year effort to dispose of a large backlog of low-level waste. Six containers presented a particularly difficult technical challenge in that they each contained large robust equipment (mostly salt baths) with elevated levels of highly enriched uranium (exceeding U.S. Department of Transportation (DOT) fissile-excepted quantities). The equipment was larger than the standard 1.2 m x 1.2 m x 1.8 m (4 ft x 4 ft x 6 ft) DOT Specification 7A Type A box and would have been very difficult to size-reduce because of several inches of steel plate (along with insulating block and concrete) in the equipment design. A critical breakthrough for the success of the project involved procuring and developing two oversize reusable DOT Specification 7A Type A (fissile tested) containers (referred to as the CTI Model 7AF-690-SC) that could be used as overpacks for the original boxes of equipment. The 7A Type A overpack containers are approximately 3.5 m long x 2.7 m wide x 2.8 m high (11.7 ft x 8.9 ft x 9.2 ft) with a maximum gross weight of 10,660 kg (23,500 lb) and a payload capacity of 6,804 kg (15,000 lbs). The boxes were designed and fabricated using a split cavity design that allowed the gasketed and bolted closure to lie along the horizontal centerline of the box. The central closure location in this design allows for strengthening of box corners that tend to be points of weakness or failure in 49CFR173.465 drop tests. By combining the split cavity design with large diameter tubing and diagonal cross bracing, drop test requirements of 49CFR173.465(1) and (2) were met and demonstrated through finite element analysis modeling. The development and use of this new container dramatically reduced the need for down-sizing the equipment and allowed the project to meet objectives within cost and schedule targets. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Assessment of Core Status of Fukushima Daiichi Nuclear Power Plant

There were some events and phenomena that occurred which have been deemed specific to the Fukushima Daiichi NPP. The primary issues were as follows: - Direct steam leakage from the reactor pressure vessels (RPVs) to the dry-wells through the gaskets of the safety relief valves and/or due to creep damage of the main steam line, and damage of the in-core monitor guide tubes due to buckling. - Direct corium leakage from the RPVs to the pedestal floors through the melt portions of the in-core monitor housings. - Alternative water injection by the fire trucks with large amount of leakages through the branch lines. - Partial load operation of the Reactor Core Isolation Cooling system and the High Pressure Coolant Injection system. - Gas leakage from the primary containment vessels to the reactor buildings due to over pressure than the design maximum value. - Thermal stratification in the suppression pool resulting in incomplete steam condensation in the pool. The accident progressions were analyzed with the newly developed physical models for the above issues. And also considering the qualitatively estimated core status based on the plant parameters measured after the accident, the current core status was assessed.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Polymer Lifetime in Plutonium Storage Containers - 18508

The plutonium facility at Los Alamos National Laboratory utilizes stainless steel containers for interim storage of plutonium compounds, metals, alloys, and process residues. Various polymer materials are used in these containers, including neoprene rubber gaskets, Viton O-rings, polytetrafluoroethylene membranes, and polyvinyl chloride bags. The DOE Manual, M441.1-1, requires storage containers to have a technically justified design life, and these polymer components play a key role in the determination of the overall design life for the containers. The capabilities at Los Alamos for monitoring degradation and estimating the design life of polymer materials used in plutonium storage containers will be described, along with the results of the lifetime determination studies for the polymer components used in SAVY-4000 and Hagan containers and some proposed alternatives. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Accelerated Aging and Evaluation of Hose-In-Hose Transfer Lines in the Hanford Waste Transfer System - 20312

Nonmetallic materials are used in the United States Department of Energy's Hanford Site Tank Farm waste transfer system. These materials include the inner primary hoses in the hose-in-hose transfer lines (HIHTLs), Garlock{sup R} gaskets, ethylene propylene diene monomer (EPDM) O-rings, and other nonmetallic materials. These nonmetallic materials are exposed to β and γ radiation, caustic solutions as well as high temperature and pressure stressors. How the nonmetallic components react to each of these stressors individually has been well established. However, simultaneous exposure of these stressors has not been evaluated and is of great concern to Hanford Site engineers. Florida International University's Applied Research Center engineers worked closely with key Hanford's Washington River Protection Solutions personnel to develop an experimental test plan that determines how these nonmetallic components react to various simultaneous stressor exposures. In this paper, research on the experimental testing of the hose-in-hose transfer lines used in the Hanford tank farm waste transfer system under simultaneous stressor exposures is presented. The stressor exposure experiments consisted of various combinations of simultaneous stressor exposure of caustic solution, high temperature and high pressure stressors. Research efforts focused on evaluating the aging behavior of EPDM by exposing samples of HIHTLs as well as EPDM dog bone shaped specimens to a 25% NaOH solution at (38 deg. C), operating (54 deg. C) and design temperatures (77 deg. C) for 6 months and 12 months. In addition, HIHTL and the EPDM dog-bone specimens were exposed to only hot water at 77 deg. C for a duration of one year. The mechanical and material properties of the samples were characterized and compared with those of the unexposed samples (baseline). Evaluations included burst pressure tests of the EPDM hose-in-hose transfer lines and material tensile strength test of EPDM dog-bone coupons. Both the tensile strength of the EPDM material dog bones and the burst pressure of the HIHTLs significantly decreased with the increasing temperature and increasing exposure time. When compared with the baseline samples, the burst pressure decreased by 28.75% for the sample aged at 77 deg. C after 12 months, in comparison to sample aged at 38 deg. C and 54 deg. C which had about 1.34% and 5.70% loss in burst pressures, respectively, after 12-month exposure. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Isothermal Martensitic and Pressure-Induced Delta to Alpha-Prime Phase Transformations in a Pu-Ga Alloy

A well-homogenized Pu-2 at.% Ga alloy can be retained in the metastable face-centered cubic {delta} phase at room temperature. Ultimately, this metastable {delta} phase will decompose via a eutectoid transformation to the thermodynamically stable monoclinic {alpha} phase and the intermetallic compound Pu{sub 3}Ga over a period of approximately 10,000 years [1]. In addition, these low solute-containing {delta}-phase Pu alloys are metastable with respect to an isothermal martensitic phase transformation to the {alpha}{prime} phase during low temperature excursions [2, 3] and are also metastable with respect to a {delta} {yields} {alpha}{prime} phase transformation with increases in pressure [3-5]. The low temperature {delta} {yields} {alpha}{prime} isothermal martensitic phase transformation in the Pu-2 at.% Ga alloy only goes to {approx}25% completion with the resultant {approx}20 {micro}m long by 2 {micro}m wide lath-shaped {alpha}{prime} particles dispersed within the {delta} matrix. In recently reported studies, Faure et al. [4] have observed a {delta} {yields} {gamma} {yields} {alpha}{prime} pressure-induced phase transformation sequence during a diamond anvil cell investigation and, based on x-ray diffraction and density and compressibility experiments, Harbur [5] has concluded that both {alpha}{prime} and an amorphous phase are present in samples that were pressurized and recovered. In this work, a large volume moissanite anvil cell is constructed to permit the pressurization and recovery of specimens of a size suitable for TEM and electron diffraction studies. The cell, shown in Fig. 1, has an overall diameter of 101.6 mm, a moissanite anvil diameter of 9.00 mm, a culet size of 3 mm, and a spring steel gasket 0.5 mm thick with a hole diameter of 2.5 mm. A 2.3 mm diameter by 100 {micro}m thick sample of {delta}-phase Pu-2 at.% Ga is compressed at a rate of approximately 0.05 GPa/minute to {approx}1 GPa to induce the phase transformation to {alpha}{prime}. Optical microscopy of the recovered specimen reveals a very fine microstructure that appears to be single phase, although the resolution of this technique is insufficient to differentiate between single and multiple phases if the grain size is below approximately 1 {micro}m. X-ray diffraction, using a laboratory Cu K{sub {alpha}} source with wavelength of 1.542{angstrom}, shows the monoclinic reflections from the {alpha}{prime} phase, strong peaks from the aluminum specimen holder, and weak peaks from the face-centered cubic {delta} phase as shown in Fig. 2. The recovered specimen is prepared for TEM and electron diffraction studies as described in Moore et al. [6]. TEM reveals small regions of {delta} phase with a very high dislocation density interspersed between the 10-100's nm {alpha}{prime} grains as shown in Fig. 3. Electron diffraction, shown in the insert in Fig. 3, clearly reveals the presence of the {delta} phase. This microstructure is in contrast to the {alpha}{prime} particles that form as a result of the low-temperature isothermal martensite in which the {alpha}{prime} particles are lath-shaped and significantly larger as shown in the optical micrograph in Fig. 4 of a sample cooled to -120 C and held for 10 hours. In these preliminary results, there is no evidence of either an amorphous phase, as suggested by Harbur [5], or the presence of a {gamma} phase. We expected to observe an amorphous phase based on the similarity of this experiment to that of Harbur [5]. It is possible that the {gamma} phase, as reported by Faure et al. [4], does form as an intermediate, but it is not retained to ambient pressure.

36 MATERIALS SCIENCE↗

High-Temperature Experiments using a Resistively-Heated High-Pressure Membrane Diamond Anvil Cell

A reliable high-performance heating method using resistive heaters and a membrane driven diamond anvil cell (mDAC) is presented. Two micro-heaters are mounted in a mDAC and use electrical power of less than 150 W to achieve sample temperatures up to 1200 K. For temperature measurement we use two K-type thermocouples mounted near the sample. The approach can be used for in-situ Raman spectroscopy and x-ray diffraction at high pressures and temperatures. A W-Re alloy gasket material permits stable operation of mDAC at high temperature. Using this method, we made an isothermal compression at 900 K to pressures in excess of 100 GPa and isobaric heating at 95 GPa to temperatures in excess of 1000 K. As an example, we present high temperature Raman spectroscopy measurements of nitrogen at high pressures.

36 MATERIALS SCIENCE↗

Strong degradation of polycarbonate and polystyrene by the CO 2 capture solvent diethyl sebacate

Here, we report on observations of strong degradation of a polycarbonate vessel by a solvent being considered for a CO 2 capture process, diethyl sebacate. This degradation led to failure of a polymeric hollow fiber membrane unit. Additional tests showed rapid degradation of polycarbonate safety glasses and polystyrene-based petri dishes by exposure to diethyl sebacate at ambient conditions. We also report on safe operations with diethyl sebacate in extensive experiments studying the corrosion of steel in CO 2 -pressurized reactors lined with PTFE and using PTFE gaskets. Used diethyl sebacate was also stored for long time periods in bottles made from low-density polyethylene bottles without physical deterioration. These observations indicate that care must be taken in development of new contactors and processes for CO 2 capture with diethyl sebacate and related solvents and in the choice of material for storage.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗