Search NASA⌕ Search

SEARCH · Search NASA

Results for “LATHES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Laser Powder Deposition Parametric Optimization and Property Development for Ti-6Al-4V Alloy

In this study, Ti6Al4V alloy was produced via laser powder deposition (LPD). To obtain Ti6Al4V alloy with maximum density, LPD parameters for preparing Ti6Al4V samples were optimized using the Taguchi method. Results were analyzed on the basis of the signal-to-noise (S/N) ratios and analyses of variance. A high energy density should be used to achieve higher levels of densification. The optimal combination of parameters for density was a scanning speed of 550 mm/min, laser power of 160 W, powder feeding rate of 0.99 g/min, and shield gas flow of 8 L/min. An almost fully dense Ti6Al4V sample was prepared using the optimized LPD process, and the relative density was greater than 99%. In addition, the microstructure and properties of Ti6Al4V samples prepared by optimized LPD process were investigated. The microstructure investigation revealed that the LPD-prepared Ti6Al4V sample was predominantly composed of fine acicular α phase and lath-type α phase. Tensile and microhardness tests indicated that the LPD sample had higher mechanical properties than the traditional cast Ti6Al4V alloy because of the acicular martensitic phase and smaller grain size.

36 MATERIALS SCIENCE↗

Variation in Morphology and Kinetics of Granular Bainite with Welding Thermal Cycles in High-Nb Fire-Resistant Steel: Experiments and Theoretical Calculations

The microstructure and kinetics of granular bainite (GB) were investigated in novel fire-resistant steel containing high niobium and subjected to simulated welding thermal cycles. The dilatometric data were analyzed to determine the activation energy and Avrami exponents. It was observed that austenite transformed to GB over a wide range cooling rates of 0.5-100 K/s. Theoretical calculations indicated that Avrami exponent (n) decreased with increased transformed volume fraction (f{sub b}) and cooling rate. At a moderate cooling rate of 20-6 K/s, bainitic ferrite as sheaves formed from austenite and the corresponding Avrami exponent was 2 < n < 3. Martensite in martensite/austenite constituent formed with Avrami exponent n ~ 1. At the fastest cooling rate of 50 K/s, lath bainitic ferrite and film-like retained austenite (RA) were obtained with the corresponding Avrami exponent n ~ 1. At lower cooling of 1 and 0.5 K/s, plate-like bainitic ferrite and block-like microphase composed of lamellar RA and ferrite were obtained with Avrami exponent n > 3. The local activation energy for austenite transformation to bainitic ferrite decreased from ~ 198 to ~ 182 kJ/mol with increasing f{sub b} from 0.05 to 0.95, while the local activation energy for austenite transformation to martensite decreased from ~ 80 to ~ 71 kJ/mol with increasing f{sub b} from 0.05 to 0.95.

36 MATERIALS SCIENCE↗

Effect of Annealing on the Microstructure and Properties of Electron Beam Welded 4J34 Kovar Alloy

Electron beam welding of 4J34 Kovar alloy was conducted, and the microstructure and mechanical properties of the joints in as-welded and postweld annealing treatment (PWAT) states were investigated. The martensitic transformation occurred and led to the generation of α lath martensite due to the rapid cooling in the as-welded condition. After annealing treatment, part of the α martensite transformed to γ austenite and subsequently developed the bulk γ phase and α/γ lamellar microstructures in the fusion zone (FZ) of the postwelded joint. Grains in the heat-affected zone (HAZ) clearly developed and penetrated into the FZ, causing the disappearance of the fusion line between the FZ and the HAZ. All the joints in both the as-welded and PWAT conditions exhibited ductile fracture. The maximum tensile strength of 505 MPa was obtained in the as-welded joint with the welding speed of 150 mm/min. The linear expansion coefficients of the joint and base metal decreased with the increase in temperature. However, the decreasing rate of PWAT joints was lower than that of the as-welded joints.

36 MATERIALS SCIENCE↗

Effect of Heat Input on M-A Constituent and Toughness of Coarse Grain Heat-Affected Zone in an X100 Pipeline Steel

The joining of 14.8 mm thick pipeline steels was achieved with developments in high-power fiber laser by laser welding or hybrid laser arc welding. However, there were few studies on the effects of single-pass welding heat input on the M-A component and impact toughness of the heat-affected zone. In this study, single-pass welding thermal cycle was performed on Gleeble 3800 thermal simulation tester; the effect of heat input on microstructure, M-A constituent, hardness, toughness and corrosion resistance of coarse-grained heat-affected zone of X100 pipeline steel was studied. The results showed: The microstructure was lath martensite with a heat input of less than 8 kJ/cm. When the heat input was 26-36 kJ/cm, the microstructure was granular bainite. The heat input had not obvious effect on hardness (only 16% hardness reduction in this heat input arrange). However, the impact toughness was strongly influenced by heat input, with an 88% hardness reduction compared to base metal, due to M-A constituent and prior austenite grain size. Few finer M-A constituent dispersing in austenite was obtained instead of necklace-like M-A constituent at the prior austenite grain boundary when the welding heat input was less than 15 kJ/cm, which was beneficial to improve the impact toughness and corrosion resistance of welded joints of X100 pipeline steels.

36 MATERIALS SCIENCE↗

Development of a High-Strength Low-Carbon Steel with Reasonable Ductility through Thermal Cycling

In this research work, cost-effective structural material synthesis routes have been adopted in the form of thermal cycling designed and applied on a low-cost material (AISI 1010 steel). The main synthesis route consists of two-step thermal cycling (designed with respect to iron–carbon phase diagram) combining short-duration holding in upper critical and intercritical temperature regimes and different cooling conditions (forced air cooling and ice-brine quenching). Accordingly, the adopted hierarchical design approach (from nanoscale onwards) with a combination of hard and soft phases (to attain an adequate balance between mutually exclusive strength and ductility properties) results in origin of a novel microstructure. The microstructure consists of dislocation-enriched martensite regions (possessing plate and lath morphologies in 1:4 ratio) containing nanosized cementite particles and α-ferrite regions containing submicroscopic cementite particles. As a consequence, an excellent combination of strength (UTS = 905 MPa) and ductility (%Elongation = 17) is achieved in the synthesized material.

36 MATERIALS SCIENCE↗

Relationship Between Microstructure and Marine Corrosion Resistance of Martensitic Stainless Steels: A Multiscale Approach

The electrochemical properties of martensitic stainless steels may depend on complex aspects of their microstructure. Three alloys were considered in this study: X30Cr13 (AISI 420), a martensitic stainless steel with a low content of alloying elements; X17CrNi16-2 (AISI 431), chosen for its strong resistance to corrosion; and X5CrNiCu15-5 (AISI 630), chosen for its good mechanical resistance. Voltammetry tests have shown the influence of carbon and chromium content on corrosion resistance. Resistance to pitting appears equivalent for the both. However, heterogeneous corrosion, in relation to δ-ferrite precipitation and chromium carbides at the lath boundaries, appears in the case of X17CrNi16-2. Conversely, non-preferential corrosion occurs in the case of the X5CrNiCu15-5, and a superior passive film stability during immersion in artificial seawater. This counterbalance negative effect of the microstructure. Thus, it achieves an equivalent “macroscopically” corrosion behavior between the two steels.

36 MATERIALS SCIENCE↗

Creep Deformation and Rupture Behavior of P92 Steel Weld Joint Fabricated by NG-TIG Welding Process

The creep deformation and rupture behavior of P92 steel weld joint fabricated by narrow-gap TIG (NG-TIG) welding process have been investigated at 923 K over a stress range of 80-140 MPa. The prior-austenite grain size, M{sub 23}C{sub 6} precipitate size and hardness have been found to vary significantly in the weld joint. The reduction in hardness from weld metal to base metal with a trough at the outer edge of heat-affected zone (HAZ) has been observed. Coarsening of M{sub 23}C{sub 6} precipitate, recovery of martensite lath dislocation structure and formation of subgrain structure led to lower hardness in the intercritical HAZ. The creep rupture life of NG-TIG weld joint was lower than the base metal, the difference in creep rupture life between base metal and weld joint has been increased significantly with decrease in applied stress. The fracture location in the joint changed from base metal at high-stress regime to the fine grain (FG) HAZ (Type IV cracking) under lower stress level. Fracture in the FGHAZ evidenced the significant reduction in ductility, localized deformation and extensive localized cavitation. Extensive Laves phase formation with significant loss of solution strengthening contribution from tungsten and coarsening of M{sub 23}C{sub 6} precipitate with prolonged creep exposure led to reduction in hardness and more extensive cavitation in the FGHAZ resulting in premature Type IV failure of the weld joint. Weld strength reduction factor about 0.59 has been evaluated for 10{sup 5} h at 923 K.

36 MATERIALS SCIENCE↗

Microstructural Evolution and Properties of 24CrNiMoY Alloy Steel Fabricated by Selective Laser Melting

24CrNiMoY alloy steel samples were fabricated by selective laser melting (SLM), and a phase transformation model was established to study the alloy steel microstructural evolution. Meanwhile, microhardness and tensile properties of 24CrNiMoY alloy steel prepared by different laser energy densities (E{sub v}) were investigated. Results indicate that the microstructural evolution of 24CrNiMoY alloy steel is consistent with the phase transformation model. The main microstructure changed from martensite to bainite with the increase in thermal cycle numbers. In addition, a suitable E{sub v} plays an important role in refining the bainite structure and improving the alloy steel properties. When the E{sub v} decreases from 210 to 140 J/mm{sup 3}, the bainite lath width reduces from 1.7 to 0.6 μm. Simultaneously, the relative density, tensile strength and microhardness of the fabricated samples increase first and decrease later. 24CrNiMoY alloy steel sample prepared by 160 J/mm{sup 3} has fine mechanical properties: The tensile strength is 850 MPa and microhardness is 360 HV{sub 0.2}.

36 MATERIALS SCIENCE↗

Effect of Chromium Content on Microstructure, Hardness, and Wear Resistance of As-Cast Fe-Cr-B Alloy

The effects of chromium content on microstructure, hardness and wear resistance of as-cast Fe-xCr-1.0B (x = 0, 4, 8, 12, 16, 20) alloys were investigated by means of optical microscope (OM), scanning electron microscope (SEM), x-ray diffractometer (XRD), hardness tester and ring block wear tester. The results showed that the microstructures of chromium-free alloy were mainly composed of pearlite, ferrite, and eutectic borocarbides, and the hardness was very low, only 18.8 HRC. With the increase in chromium content, the matrix of as-cast Fe-Cr-B alloy gradually began to transform from pearlite and ferrite to lath martensite, and the type of borocarbides changed from Fe{sub 2}(B, C) to M{sub 2}(B, C), M{sub 7}(C, B){sub 3} and M{sub 23}(C, B){sub 6} (M = Fe, Cr). When the chromium content was 12 wt.%, the hardness of alloy reached the highest value of 61.1 HRC, and the wear resistance of alloy was the best. The results of worn surface analysis showed that the wear failure of as-cast Fe-Cr-B alloy was mainly caused by multiple plastic deformation and micro-cutting.

36 MATERIALS SCIENCE↗

Significance of Finish Cooling Temperature to Microstructure and Property Relationship of Low-Carbon V-N-Cr Microalloyed High-Strength Steel

Herein, three final cooling temperatures were employed to achieve high strength and toughness communication in the V-N-Cr microalloyed steels. This study shows that V-N-Cr microalloyed steel primarily consisted of ferrite, granular bainite, acicular ferrite, and a small quantity of M/A phase at the final cooling temperature of 600 °C, while the polygonal ferrite, lamellar bainite, granular bainite, and a small fraction of acicular ferrite were obtained at 450 °C. The width of lamellar bainite was ~ 200-400 nm, and acicular ferrite was composed of fine non-parallel ferrite platelet structures with high dislocations densities. As the final cooling temperature decreased further, the microstructure included granular bainite and lath bainite at 350 °C. The nanoscale precipitates of V-N-Cr microalloyed steel were divided into two types, large-scale precipitates near the grain boundary that precipitated at high temperatures and small precipitates of diameter 5-10 nm at low temperatures, which significantly contributed toward strength. The hot rolled low-carbon V-N-Cr microalloy steel exhibited optimal mechanical properties at the final rolling temperature of 830 °C, as well the final cooling temperature was 450 °C. The highest yield strength and tensile strength of V-N-Cr microalloyed steel were 835 MPa and 989 MPa, respectively. The outstanding impact toughness of 161 J tested at − 60 °C was received. The transformation strengthening and precipitation hardening played a crucial role in affecting the thermo-mechanical properties.

36 MATERIALS SCIENCE↗

A Comparative Analysis on Microstructure and Fracture Mechanism of X100 Pipeline Steel CGHAZ Between Laser Welding and Arc Welding

The objective of this study is to compare and contrast the differences in microstructure and fracture mechanism between CGHAZ of laser welding and submerged arc welding in X100 pipeline steel. The single-pass welding thermal simulation test of laser welding and submerged arc welding was carried out in MMS-200 thermal simulation test machine using self-made fixtures. The results indicated that the microstructure of laser welding CGHAZ and submerged arc welding CGHAZ was lath martensite and granular bainite, respectively. The impact energy of laser welding CGHAZ was 27 J, and the fracture mode was ductile fracture; the impact energy of submerged arc welding CGHAZ was 7.7 J, and the fracture mode was brittle fracture. The nucleation and propagation mechanism of cracks in different welding modes was established. Microcracks nucleated at the position of dislocation accumulation and remained austenite suppressed crack nucleation in laser welding CGHAZ. The nucleation site was at the M–A constituents in submerged arc welding CGHAZ. The main crack of laser welding CGHAZ was formed by one or a small number of microcracks. The main crack in submerged arc welding CGHAZ was formed by a large number of microcracks. The difference between crack nucleation and propagation mechanism is the reason why the impact energy of laser welding CGHAZ is higher than of submerged arc welding CGHAZ.

36 MATERIALS SCIENCE↗

Nanoscale Solute Partitioning and Carbide Precipitation in a Multiphase TRIP Steel Analyzed by Atom Probe Tomography

Nanoscale solute partitioning across multiple constituent phases in a 980-grade quenched and partitioned (Q&P) steel was analyzed using atom probe tomography (APT). The Q&P process was used to increase the C content in the retained austenite phase thereby improving its stability under plastic straining. Significant carbon enrichment of austenite was measured with decreased levels of C in martensite and almost depleted C content in ferrite, supporting the C partitioning mechanism in the literature. The APT analysis of retained austenite surrounded by martensite demonstrated a higher amount of C content compared with retained austenite surrounded by the ferrite phase. Lath and discrete carbide particle precipitation was also observed inside martensite colonies, tying up C and reducing the total amount of C available for austenite stabilization. In addition, the partitioning of Mn and other minor elements was quantitatively investigated by correlating APT and SEM-EBSD. Furthermore, these techniques provide a robust methodology for analyzing nanoscale compositional partitioning in multiphase steels, TRIP steels in particular, which can be used to better explain their microstructure-mechanical property relationships.

36 MATERIALS SCIENCE↗

Investigation of Magnetic Signatures and Microstructures for Heat-Treated Ferritic/Martensitic HT-9 Alloy

There is increased interest in improved methods for in-situ nondestructive interrogation of materials for nuclear reactors in order to ensure reactor safety and quantify material degradation (particularly embrittlement) prior to failure. Therefore, a prototypical ferritic/martensitic alloy, HT-9, of interest to the nuclear materials community was investigated to assess microstructure effects on micromagnetics measurements – Barkhausen noise emission, magnetic hysteresis measurements, and first-order reversal curve analysis – for samples with three different heat-treatments. Microstructural and physical measurements consisted of high-precision density, resonant ultrasound elastic constant determination, Vickers microhardness, grain size, and texture. These were varied in the HT-9 alloy samples and related to various magnetic signatures. In parallel, a meso-scale microstructure model was created for alpha iron and effects of polycrystallinity and demagnetization factor were explored. It was observed that Barkhausen noise emission decreased with increasing hardness and decreasing grain size (lath spacing) while coercivity increased. The results are discussed in terms of the use of magnetic signatures for nondestructive interrogation of radiation damage and other microstructural changes in ferritic/martensitic alloys.

Environmental Molecular Sciences Laboratory↗

High-pressure phase transitions in a laser directed energy deposited Fe-33Cu Alloy

Here, additively manufactured Fe-Cu alloys contain both equilibrium face-centered cubic (FCC) and metastable body-centered cubic (BCC) crystal structure Cu precipitates depending on their size. However, the stability of these nanoscale precipitates under extreme conditions such as high pressures has not been reported. This study investigates the phase transformations and microstructural stability of laser directed energy deposition (DED-LB) made Fe67Cu33 alloy (nominal composition in at.%) under high static pressure deformation using in-situ synchrotron X-ray diffraction under pressure, postmortem high-resolution scanning transmission electron microscopy (HR-STEM), and molecular dynamics (MD) simulations. In-situ XRD results reveal a reversible phase transformation from BCC to the hexagonal close-packed (HCP) structure in the Fe grains at an onset pressure of 16.4 GPa, significantly higher than reported in the literature for pure Fe. Although no high-pressure phase transition was observed in the FCC Cu grains through XRD, HR-STEM analysis uncovers a phase transition to the HCP structure in nanoscale metastable BCC Cu precipitates within the BCC Fe matrix. After decompression, the Fe matrix reverted back to the BCC structure with periodic lath martensite, while regions of the nanoscale BCC Cu precipitates retained the metastable HCP structure. MD simulations support the BCC → HCP transition in the embedded nanoscale coherent Cu precipitates, consistent with the classical Burgers mechanism. Thus, by leveraging in-situ XRD observation, postmortem high-resolution S/TEM microscopy, and MD simulations, this study offers profound insights into the distinctive phase transformations induced by high pressure in DED-LB Fe67Cu33 alloy, which is distinguished by its hierarchical microstructure.

36 MATERIALS SCIENCE↗

Fatigue performance of laser powder bed fusion hydride-dehydride Ti-6Al-4V powder

We report hydride-dehydride (HDH) Ti-6Al-4V alloy with particle size distribution of 50–120 µm is laser powder bed fusion (L-PBF) processed using optimum processing parameters and a near-fully dense structure with a density of 99.9 % is achieved. Microstructural observations and phase analyses indicate formation of columnar β grains with acicular α/α' phases in as-built condition. The roughness of the as-fabricated samples is significant with an average roughness of R a = 15.71 ± 3.96 µm and a root mean square roughness of R rms = 108.4 ± 24.9 µm, however, both values are reduced to R a = 0.19 ± 0.04 µm and R rms = 4.9 ± 0.6 µm after mechanical grinding. Mechanical tests are carried out on as-fabricated specimens followed by stress relief treatment. All samples are tested to failure in fatigue, under fully-reversed tension-compression conditions of R = –1. The as-built samples failed from the surface with crack initiation mainly at micro-notches, whereas after mechanically grinding, crack initiation changed to subsurface defects such as pores. Minimizing surface roughness by mechanically grinding eliminates surface micro-notches which improves fatigue strength in the high cycle fatigue region. Fatigue notch factor calculations showed that the effect of surface roughness was significantly lower when HDH powder is used compared to standard spherical powder. X-ray diffraction analysis revealed an in-plane compressive stress, micro-strain and grain refinement on the surface of the mechanically ground samples. Fractography observations (macroscale) revealed a fully brittle fracture in the first stage of crack growth with a transition to a dominantly ductile fracture in the third stage of crack growth. On the other hand, at the micro scale, even the brittle fracture regions showed evidence of ductile fracture within the α' martensite laths.

36 MATERIALS SCIENCE↗

Composition, morphology and nanostructure of C-S-H in 70% white Portland cement-30% fly ash blends hydrated at 55 {sup o}C

Outer product C-S-H had a mixture of fibrillar and foil-like morphology in a 28-day-old water-activated paste, and foil- or lath-like morphology in an alkali-activated paste. It was not possible to determine the chemical composition of C-S-H using SEM-EDX because of fine-scale intermixing with other phases; TEM-EDX was necessary. The C-S-H formed in the alkali-activated paste had a lower mean Ca/(Al + Si) ratio than that formed with water. The mean length of the aluminosilicate anions in the C-S-H was similar in both systems and increased with age; those in the Op C-S-H were likely to be shorter than those present in the Ip C-S-H with water activation, but longer (and more protonated) with alkali. The potassium in the alkali-activated paste was present either within the C-S-H structure charge balancing the substitution of Al{sup 3+} for Si{sup 4+}, or adsorbed on the C-S-H charge balancing sulfate ions.

36 MATERIALS SCIENCE↗

High plasticity in refractory composite fabrication by ultrasonic additive manufacturing

Refractory metal composites are desirable for use in extreme environments that require materials with high specific strengths and resilience to external environments such as that found in nuclear and aerospace. However, due to the high melting temperature of refractories, liquid state joining processes such as welding remains difficult. Ultrasonic additive manufacturing (UAM) provides a potential route for processing refractory composites because it is a solid-state (i.e., no-melting) process and allows for intermittent machining operations to be performed between welds. Further, to demonstrate refractory composite fabrication, this study utilized UAM to machine a cavity to locate and sequester a Mo foil in a Zircaloy-4 (Zry-4) baseplate and additively build over the top with Zry-4 foils, thereby embedding the Mo in Zry-4 matrix. Significant deformation of the Zry-4 microstructure was observed: this deformation caused adiabatic heating and subsequent dynamic recrystallization through the transformation from α→β and then back to α as the material cooled. Flexural testing of the Zr–Mo composite revealed no delamination or failure, but the strength was not as expected, falling lower than a cold-worked Zry-4 sample. Finite element analysis supported that some bonding must have existed between the Zry-4 and Mo. There was indeed an interdiffusion zone at the Zry-4 foil–Mo foil interface, observing a metastable body-centered cubic β-Zr lathe. It was determined that sufficient strain energy was present to encourage the nucleation of the β-Zr grain along α-Zr grains. Future work is warranted to investigate UAM for refractory composite fabrication.

36 MATERIALS SCIENCE↗

The Effect of processing on the 455 C tensile and fatigue behavior of boron-modified Ti-6Al-4V

This work investigated the effect of nominal boron (B) additions of 0.1 wt.% and 1.0 wt.% on the elevated-temperature (455 C) fatigue deformation behavior of Ti-6Al-4V (wt.%) for maximum applied stresses between 250 and 550 MPa (R = 0.1, 5 Hz). The alloys were evaluated in the as-cast condition as well as the cast-and-extruded condition. Boron additions resulted in a dramatic refinement of the as-cast grain size, and larger boron additions resulted in larger titanium-boride (TiB) phase volume percents. For the as-cast alloys, the B-containing alloys exhibited longer average fatigue lives than those for Ti-6Al-4V, which was suggested to be related to their increased strength and stiffness due to the addition of the strong and stiff TiB phase. The longest average fatigue lives were exhibited by the Ti-6Al-4V-0.1B alloy, which also exhibited the greatest elongation-to-failure value. The extrusions, which were performed in the {beta}-phase field, resulted in a significantly smaller grain size, a smaller {alpha}-colony size, and finer {alpha}-lath width compared to that for the as-cast B-modified alloys. The TiB whiskers were aligned in the extrusion direction and the {alpha}-phase was also strongly textured such that the basal plane was predominately oriented perpendicular to the extrusion axis. Together these microstructural features were responsible for the significantly higher 455 C yield strength, ultimate tensile strength, and fatigue strength exhibited by the cast-and-extruded alloys compared with the as-cast alloys. In the extruded condition, B-addition did not improve the tensile or fatigue strength.

36 MATERIALS SCIENCE↗