Search NASA⌕ Search

SEARCH · Search NASA

Results for “MARTENSITE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Resolving the Martensitic Transformation in Q&P Steels In-Situ at Dynamic Strain Rates Using Synchrotron X-ray Diffraction

Herein the dynamic deformation response of two quenching and partitioning (Q&P) steels was investigated using a high strain rate tension pressure bar and in-situ synchrotron radiography and diffraction. This allowed for concurrent measurements of the martensitic transformation, the elastic strains/stresses on the martensite and ferrite, and the bulk mechanical behavior. The steel with the greater fraction of ferrite exhibited greater ductility and lower strength, suggesting that dislocation slip in ferrite enhanced the deformability. Meanwhile, the kinetics of the martensitic transformation appeared similar for both steels, although the steel with a greater ferrite fraction retained more austenite in the neck after fracture.

36 MATERIALS SCIENCE↗

Mechanical Properties and Strain-Induced Martensite Transformation in Cold Rolling of 304L Stainless Steel Plate

In this work, cold rolling behavior of stainless steel 304L is investigated and the effects of different process parameters on the occurrence of strain-induced martensite and mechanical properties are studied. The rolling experiments are conducted under different rolling speeds and reductions in which a set of samples is deformed at room temperature and the other set is first cooled to the temperature of − 10 °C and then rolled. Afterward, the developed microstructures and mechanical properties of the rolled steel are evaluated employing different testing techniques. In order to justify the results, mathematical modeling of cold rolling operation is also performed using Abaqus/Explicit to estimate the distribution of equivalent plastic strain and temperature rise during rolling. The results show that strain-induced martensite may occur during cold rolling and it efficiently alters microstructure and mechanical performance of the rolled plate. The amount of reduction, initial temperature, rolling layout, and, to a lesser extent, rolling speed can affect the kinetics of martensite transformation as well as microstructure and mechanical properties of the rolled steel.

36 MATERIALS SCIENCE↗

Creep-Resistant Ferritic-Martensitic Steels for Power Plant Applications

Creep-resistant ferritic-martensitic steels are essential materials used in power plants for electricity generation. The efficiency and emissions of the plant are closely related to the operating temperature. Materials used in the hottest sections are one of the main limiting factor for plant operation at 650 °C. This review describes the recent development of creep-resistant ferritic-martensitic steels from a large dataset of in-house research. The findings are tied to available literature for discussion. A first steel, CPJ-7, was developed with an operating temperature approaching 650 °C, and a refined design, JMP, showed the potential to operate at 650 °C. Approximately fifty different ingots, each weighing ~ 7 kg, were vacuum induction melted and processed. Overall, wrought and cast versions of CPJ-7 present superior creep properties when compared to wrought and cast versions of COST alloys for steam turbine and P91/92 for boiler applications. The prolonged creep life was attributed to slowing down the process of the destabilization of the MX and M 23 C 6 precipitates at 650 °C. The cast version of CPJ-7 also revealed superior mechanical performance, above commercially available cast 9% Cr martensitic steel or derivatives. Following the work on CPJ-7, the JMP steels were designed with higher Co for increased solid solution strengthening, Si for oxidation resistance and increased W for matrix strength and stability. The JMP steels showed increases in creep life compared to CPJ-7 between 118 and 150% at 650 °C for testing at various stresses between 138 and 207 MPa. On a Larson–Miller plot, the performance of the JMP steels surpasses that of state-of-the-art MARBN steel. The influence of various elements within the composition of the alloys on the microstructure and mechanical properties is discussed. This review presents approximately 420,000 h of in-house creep testing, the equivalent of almost 50 years of cumulative creep tests.

36 MATERIALS SCIENCE↗

Lüders-like martensitic transformation in a Cu/carbon-steel nanocomposite: An in situ synchrotron study

In this paper, a Cu/carbon-steel nanocomposite is fabricated by pressing, rolling and wire drawing. The average layer thickness is about 69 nm for steel and 67 nm for Cu. Cu suppresses the growth of prior austenite at elevated temperature, and thus the steel layer thickness barely increases during austenization. Subsequent quenching results in a large amount of metastable retained austenite within the steel layers. The martensitic transformation behavior of the composite during plastic deformation is investigated by in situ tensile test using synchrotron X-ray diffraction at room temperature. It is found that the retained austenite, rather than Cu, dominates the plastic deformation of the nanocomposite. Finally, in situ results verify that the transformation of retained austenite initiates in a manner of Lüders-like band due to stress-induced martensitic transformation, followed by strain-induced martensitic transformation until fracture.

36 MATERIALS SCIENCE↗

Crystallographic stability of the BCC phase during quenching of metastable beta titanium alloy Ti-5553 and comparison of structural criteria for the predictive capability of α” martensite

This work evaluates the compositional standard currently developed for Ti-5553 powder and explores the metastable β region for sensitivity to martensitic formation during rapid quenching from the melt. Ti-5553 is a beta-stabilized titanium alloy that is increasingly being used in additive manufacturing applications. A series of alloys within the Ti-5553 compositional space was processed using two-piston spat quenching to perform rapid solidification and quenching for each of these alloy compositions. Typical empirical models such as molybdenum equivalency are not able to fully separate the retained BCC and martensitic compositions. Further, the use of thermodynamic data to estimate the transformation energy needed to form martensite can differentiate the alloys and provide a metric to further develop compositional limits for metastable beta titanium alloy development.

36 MATERIALS SCIENCE↗

Effect of homogenization temperature on the martensitic transformation kinetics in a Fe-32%Ni-0.4%Cr alloy

Kinetic, morphological and some thermal properties of thermally induced and deformation-induced martensite were studied in a Fe-32%Ni-0.4%Cr alloy. Scanning electron microscopy (SEM), differential scanning calorimetry (DSC) and compression deformation test techniques were used for these studies. SEM observations revealed the occurrence of both athermal and isothermal martensitic transformation kinetics for producing a lenticular martensite morphology for different homogenization conditions of the prior austenite phase. The DSC measurement results showed a fair agreement with those of previous studies on ferrous alloys.

36 MATERIALS SCIENCE↗

In-situ determination of austenite and martensite formation in 13Cr6Ni2Mo supermartensitic stainless steel

In-situ analysis of the phase transformations in a 13Cr6Ni2Mo supermartensitic stainless steel (X2CrNiMoV13-5-2) was carried out using a thermo-magnetic technique, dilatometry and high temperature X-ray diffractometry (HT-XRD). A combination of the results obtained by the three applied techniques gives a valuable insight in the phase transformations during the austenitization treatment, including subsequent cooling, of the 13Cr6Ni2Mo supermartensitic stainless steel, where the magnetic technique offers a high accuracy in monitoring the austenite fraction. It was found by dilatometry that the austenite formation during heating takes place in two stages, most likely caused by partitioning of Ni into austenite. The in-situ evolution of the austenite fraction is monitored by high-temperature XRD and dilatometry. The progress of martensite formation during cooling was described with a Koistinen-Marburger relation for the results obtained from the magnetic and dilatometer experiments. Enhanced martensite formation at the sample surface was detected by X-ray diffraction, which is assumed to be due to relaxation of transformation stresses at the sample surface. Due to the high alloy content and high thermodynamic stability of austenite at room temperature, 4 vol.% of austenite was found to be stable at room temperature after the austenitization treatment. - Highlights: Black-Right-Pointing-Pointer We in-situ analyzed phase transformations and fractions of a 13Cr6Ni2Mo SMSS. Black-Right-Pointing-Pointer Higher accuracy of the austenite fraction was obtained from magnetic technique. Black-Right-Pointing-Pointer Austenite formation during heating takes place in two stages. Black-Right-Pointing-Pointer Enhanced martensite formation at the sample surface detected by X-ray diffraction.

36 MATERIALS SCIENCE↗

Determination of dislocation density by electron backscatter diffraction and X-ray line profile analysis in ferrous lath martensite

The microstructure and the dislocation density in as-quenched ferrous lath martensite were studied by different methods. The blocks, packets and variants formed due to martensitic transformation were identified and their sizes were determined by electron backscatter diffraction (EBSD). Concomitant transmission electron microscopy (TEM) investigation revealed that the laths contain subgrains with the size between 50 and 100 nm. A novel evaluation procedure of EBSD images was elaborated for the determination of the density and the space distribution of geometrically necessary dislocations from the misorientation distribution. The total dislocation density obtained by X-ray diffraction line profile analysis was in good agreement with the value determined by EBSD, indicating that the majority of dislocations formed due to martensitic transformation during quenching are geometrically necessary dislocations.

36 MATERIALS SCIENCE↗

Martensite crystal structure in Ru-based high temperature shape memory alloys

Highlights: • A three level twinned microstructure is recognized in the β″ phase. • Wavy contrast boundaries which are typical for translation interfaces • Displacements are translations of tetragonal β′ phase, lost during transformation. • Six times bigger monoclinic cell is characterized by the disappearance of 5 translations. - Abstract: High temperature shape memory alloys RuNb and RuTa were investigated by X-ray diffraction in order to determine the structure of the low temperature β” martensite. Powder X-ray diffraction and Rietveld analysis confirm the monoclinic symmetry and allow a precise determination of the atom positions. The low temperature microstructure is the result of a martensitic transformation from a tetragonal β′ martensite. The analysis of how it is controlled by the space groups of the two phases and by their relative orientation is performed by transmission electron microscopy. A three level twinned microstructure is recognized in the β” phase. The investigation at the smallest scale twins reveals the presence of wavy contrast boundaries which are typical for translation interfaces. High resolution transmission electron microscopy images, accompanied by phase contrast imaging analysis, have been used to determine the translation vectors associated to the interfaces. These displacements are the translations of the tetragonal β′ phase which are lost during the transformation. The combination of X-ray diffraction and transmission electron microscopy investigation allows the suggestion of a global distortion mechanism that explains the atomic displacements in the β” form.

36 MATERIALS SCIENCE↗

Suppressing heating rate-dependent martensitic stabilization in ductile Cu-Al-Mn shape memory alloys by Ni addition: An experimental and first-principles study

Highlights: • Additional nearest neighbor bond between Ni and Al atoms was produced theoretically in the Cu-Al-Mn-Ni (Ni≤2 at.%) alloys. • Shape memory effect of Cu-Al-Mn alloys heated at 20 K/min was improved from 85% to 92% after the addition of 2 at.% Ni. • Addition of 2 at.% Ni can suppress heating rate-dependent martensitic stabilization in Cu-Al-Mn alloys heated at 0.01 K/min. - Abstract: The present paper aims to suppress the heating rate-dependent martensitic stabilization of ductile Cu-Al-Mn shape memory alloys through restricting the mobility and thus the behavior of vacancies. A combined study based on first-principles calculation and experimental results were presented to unveil the effect of Ni addition into ternary Cu-Al-Mn alloys on the bonding force between atoms. The results showed that additional nearest neighbor bond between Ni and Al atoms in quaternary Cu-Al-Mn-Ni alloys can be produced. The addition of Ni (≤2 at.%) into ternary Cu-Al-Mn alloys can not only efficiently increase the shape memory effect, but also suppress the occurrence of heating rate-dependent martensitic stabilization. The addition of 2 at.% Ni improved the shape memory effect of ternary Cu-Al-Mn alloys from 85% to 92% when heated at 20 k/min. The shape memory effect of ternary Cu-Al-Mn alloys dropped to 10% as the heating rate decreased to 1 K/min, but it remain at 92% even when the heating rate was sufficiently lowered to 0.01 K/min after the addition of 2 at.% Ni.

36 MATERIALS SCIENCE↗

Elastic strain evolution and {epsilon}-martensite formation in individual austenite grains during in-situ loading of a metastable stainless steel.

The (hcp) {var_epsilon}-martensite formation and the elastic strain evolution of individual (fcc) austenite grains in metastable austenitic stainless steel AISI 301 has been investigated during in situ tensile loading up to 5% applied strain. The experiment was conducted using high-energy X-rays and the 3DXRD technique, enabling studies of individual grains embedded in the bulk of the steel. Out of the 47 probed austenite grains, one could be coupled with the formation of {var_epsilon}-martensite, using the reported orientation relationship between the two phases. The formation of ?-martensite occurred in the austenite grain with the highest Schmid factor for the active {l_brace}111{r_brace}<12{bar 1}> slip system.

36 MATERIALS SCIENCE↗

Creep of MARBN-type 9Cr martensitic steel in gaseous CO 2 environment

Here, with an interest in moving from steam to supercritical CO 2 as the working fluid in advanced energy systems, it is important to study the mechanical response of structural alloys to CO 2 -containing environments. MARBN-type 9Cr martensitic steel was originally developed for application in boilers for supercritical and ultra-supercritical power plants where the steam temperature reaches 650 °C. In this research, a MARBN-type 9Cr martensitic steel designed and manufactured at NETL was creep tested in a gaseous CO 2 environment (i.e., 0.1 MPa at 650 °C), and the results are directly compared to creep tests conducted in air. It was found that environmentally-assisted cracking facilitated by carbide formation beneath the growing oxide accelerated failure in gaseous CO 2 . This work indicates that creep-oxidation interactions in advanced martensitic steels represent an important consideration for materials selection in supercritical CO 2 power cycles. Furthermore, this work confirms that more oxidation-resistant alloys will be required for the highest temperature portions of these systems.

36 MATERIALS SCIENCE↗

In-situ neutron diffraction investigation of two-stage martensitic transformation in a 13%Mn steel with serrated deformation

Two stage austenite →ε-martensite →α-martensite phase transformation, phase-specific lattice strain evolution and load sharing during tensile deformation of a 13%Mn hot-rolled austenitic steel are revealed by in-situ neutron diffraction. In conclusion, direct evidence is provided that serrated deformation behavior is attributed to discontinuous martensitic transformation.

Austenitic steel↗

Characterization of strain-induced martensite phase in austenitic stainless steel using a magnetic minor-loop scaling relation

We propose a combined magnetic method using a scaling power-law rule and initial permeability in magnetic minor hysteresis loops for characterization of ferromagnetic {alpha}{sup '} martensites in austenitic stainless steel. The scaling power law between the hysteresis loss and remanence is universal, being independent of volume fraction of strain-induced {alpha}{sup '} martensites. A coefficient of the power law largely decreases with volume fraction, while the initial permeability linearly increases, reflecting a change in the morphology and quantity of martensites, respectively. The present method is highly effective for integrity assessment of austenitic stainless steels because of the sensitivity and extremely low measurement field.

36 MATERIALS SCIENCE↗

Evidence of martensitic phase transitions in magnetic Ni-Mn-In thin films

Ni{sub 50}Mn{sub 35}In{sub 15} Heusler alloy thin films (with thicknesses of about 10 nm) have been grown on single crystal MgO and SrTiO{sub 3} (STO) (100) substrates using a laser-assisted molecular beam epitaxy method. Films of mixed austenitic and martensitic phases and of pure martensitic phase have been detected for those grown on MgO and STO substrates, respectively. Thermomagnetic curves were measured using a SQUID magnetometer and are consistent with those of off-stoichiometric In-based bulk Heusler alloys, including a martensitic transition at T = 315 K for films grown on MgO. The differences in the properties of the films grown on MgO and STO are discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Study of electroless Ni-W-P alloy coating on martensitic stainless steel

Electroless nickel phospor (Ni-P) is widely used in many industries due to their corrosion and wear resistance, coating uniformity, and ability to coat non-conductive surfaces. The unique properties of tungsten such as high hardness, higher melting point, lower coefficient of linear thermal expansion, and high tensile strength have created a lot of interest in developing ternary Ni-W-P alloys. This article presents the study of electroless Ni-W-P alloys coating using acid or alkaline bath on martensitic stainless steel. Nickel sulfate and sodium tungstate were used as nickel and tungsten sources, respectively, and sodium hypophosphite was used as a reducing agent. Acid or alkaline bath refer to bath pH condition was adjusted by adding sulfuric acid. Martensitic stainless steel was immersed in Ni-W-P bath for 15, 30, and 60 minutes. The substrate of martensitic stainless steel was subjected to pre-treatment (polishing and cleaning) and activation prior to electroless plating. The plating characteristics were investigated for concentration ratio of nickel and hypophosphite (1:3), sodium tungstate concentration 0,1 M, immersion time (15 min, 30 min, 60 min), and bath condition (acid, alkaline). The electroless Ni-W-P plating was heat treated at 400°C for 1 hour. Deposits were characterized using scanning electron microscope (SEM) and corrosion measurement system (CMS).

36 MATERIALS SCIENCE↗

Magnetostructural martensitic transformations with large volume changes and magneto-strains in all-d-metal Heusler alloys

The all-d-metal Mn{sub 2}-based Heusler ferromagnetic shape memory alloys Mn{sub 50}Ni{sub 40−x}Co{sub x}Ti{sub 10} (x = 8 and 9.5) are realized. With a generic comparison between d-metal Ti and main-group elements in lowering the transformation temperature, the magnetostructural martensitic transformations are established by further introducing Co to produce local ferromagnetic Mn-Co-Mn configurations. A 5-fold modulation and (3, −2) stacking of [00 10] of martensite are determined by X-ray diffraction and HRTEM analysis. Based on the transformation, a large magneto-strain of 6900 ppm and a large volume change of −2.54% are observed in polycrystalline samples, which makes the all-d-metal magnetic martensitic alloys of interest for magnetic/pressure multi-field driven applications.

36 MATERIALS SCIENCE↗

Phonon-deformational generalized ginzburg-landau functionals for describing martensite transitions between FCC and BCC structures in metals

A method is developed for theoretical description of martensite transitions between fcc and bcc phases of metals based on generalized Ginzburg-Landau functionals (GGLFs), in which the transformation parameters are the 'phonon' parameter describing relative slips of close-packed atomic planes and fcc lattice deformations in the region of a martensite inclusion. General expressions are proposed for calculating the deformational contributions to the GGLF. Local strains and local elastic moduli in the region of martensite inclusions are estimated numerically. The possibility of constructing phenomenological expressions for the GGLF using interpolations of available experimental data on the structure and elastic moduli in the fcc and bcc phases is discussed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗