Palladium-chromium static strain gages for high temperatures

An electrical resistance strain gage that can provide accurate static strain measurement to a temperature of 1500 F or above is being developed both in fine wire and thin film forms. The gage is designed to be temperature compensated on any substrate material. It has a dual element: the gage element is a special alloy, palladium-13wt percent chromium (PdCr), and the compensator element is platinum (Pt). Earlier results of a PdCr based wire gage indicated that the apparent strain of this gage can be minimized and the repeatability of the apparent strain can be improved by prestabilizing the gage on the substrate for a long period of time. However, this kind of prestabilization is not practical in many applications and therefore the development of a wire gage which is prestabilized before installation on the substrate is desirable. This paper will present our recent progress in the development of a prestabilized wire gage which can provide meaningful strain data for the first thermal cycle. A weldable PdCr gage is also being developed for field testing where conventional flame-spraying installation can not be applied. This weldable gage is narrower than a previously reported gage, thereby allowing the gage to be more resistant to buckling under compressive loads. Some preliminary results of a prestabilized wire gage flame-sprayed directly on IN100, an engine material, and a weldable gage spot-welded on IN100 and SCS-6/(beta)21-S Titanium Matrix Composite (TMC), a National Aero-Space Plane (NASP) structure material, will be reported. Progress on the development of a weldable thin film gage will also be addressed. The measurement technique and procedures and the lead wire effect will be discussed.

Lei, Jih-Fen↗

A Miniature Palladium-Iron Thermometer for Temperatures Down to 0.05 K

Magnetic thermometers are appealing at temperatures below about 0.1 Kelvin, because the avoid the noise self-heating problems associated with resistive thermometers. In practical, metallic dilute electronic thermometers add the advantages of chemical stability, high thermal conductivity, and easy in heat sinking work we describe a palladium-iron thermometer which was designed to be small and conveniently packaged and optimized for use at temperatures down to 0.05 Kelvin. The device showed Curie-Weiss behavior above about 0.06 Kelvin, and we achieve 41 nK/ square root of z temperature resolution at a temperature of 49 mK. We describe the design and operation of this thermometers and present the test results.

Tuttle, Jim↗

Raman and FTIR Studies of Silicon Carbide Surface Damage from Palladium Implantation in Presence of Hydrogen

The ion implantation in a crystal such as silicon carbide will cause both damage in the ion track and in the substrate at the end of the ion track. We used both keV, and MeV Pd ions in fabricating electronic chemical sensors in silicon carbide, which can operate at elevated temperatures. In order to study the feasibility of fabricating an optical chemical sensor (litmus sensor), we need to understand the optical behavior of the embedded damage in the presence of hydrogen, as well as the potential chemical interaction of silicon carbide broken lattice bonds with the hydrogen dissociated from gas by palladium. Implanted samples of silicon carbide were studied using both Raman spectroscopy and FTIR (Fourier Transform-Infrared). The results of this work will be presented during the meeting.

Muntele, I.↗

The Vapor Pressure of Palladium at Temperatures up to 1973K

Understanding high-temperature processes is imperative for modeling the formation of the solar system. It is unfortunate that since the 1950 s little has been done in the area of thermodynamics to continue gaining information on metals such as iron (Fe), nickel (Ni), cobalt (Co), palladium (Pd) and many others. Although the vapor pressures of these metals can be extrapolated to higher temperatures, the data is often limited to temperature ranges too low to be applicable to processes that occur during the formation of the solar system (T approx. 2000K). Experimental techniques inhibited the data in the past by restricting the testing of metals to temperatures below their melting point. Today, higher temperature testing is possible by using a Thermo- Cahn Thermogravimetric system that is able to reach temperatures up to 1973K in vacuo and measure a 10 gram change in a sample with mass of up to 100 grams.

Gardner, K. G.↗

Effects of Palladium Content, Quaternary Alloying, and Thermomechanical Processing on the Behavior of Ni-Ti-Pd Shape Memory Alloys for Actuator Applications

The need for compact, solid-state actuation systems for use in the aerospace, automotive, and other transportation industries is currently driving research in high-temperature shape memory alloys (HTSMA) having transformation temperatures above 100 C. One of the basic high temperature systems under investigation to fill this need is NiTiPd. Prior work on this alloy system has focused on phase transformations and respective temperatures, no-load shape memory behavior (strain recovery), and tensile behavior for selected alloys. In addition, a few tests have been done to determine the effect of boron additions and thermomechanical treatment on the aforementioned properties. The main properties that affect the performance of a solid state actuator, namely work output, transformation strain, and permanent deformation during thermal cycling under load have mainly been neglected. There is also no consistent data representing the mechanical behavior of this alloy system over a broad range of compositions. For this thesis, ternary NiTiPd alloys containing 15 to 46 at.% palladium were processed and the transformation temperatures, basic tensile properties, and work characteristics determined. However, testing reveals that at higher levels of alloying addition, the benefit of increased transformation temperature begins to be offset by lowered work output and permanent deformation or "walking" of the alloy during thermal cycling under load. In response to this dilemma, NiTiPd alloys have been further alloyed with gold, platinum, and hafnium additions to solid solution strengthen the martensite and parent austenite phases in order to improve the thermomechanical behavior of these materials. The tensile properties, work behavior, and dimensional stability during repeated thermal cycling under load for the ternary and quaternary alloys were compared and discussed. In addition, the benefits of more advanced thermomechanical processing or training on the dimensional stability of these alloys during repeated actuation were investigated. Finally, the effect of quaternary alloying on the thermal stability of NiTiPdX alloys is determined via thermal cycling of the materials to increasing temperatures under load. It was found that solid solution additions of platinum and gold resulted in about a 30 C increase in upper use temperature compared to the baseline NiTiPd alloy, providing an added measure of over-temperature protection.

Bigelow, Glen↗

Permeation Rate Equations for Hydrogen and Deuterium in a Palladium-Silver Alloy

Mass transfer of a gas through a selective, solid membrane is an effective method for separation of desired species. This selective permeability is evident in the flow of hydrogen and the isotope deuterium through palladium-silver metal alloy media. In this study, based upon Sieverts’s law and the Arrhenius diffusion equation, an empirical correlation was developed to determine the steady-state permeation rate R, dependence on media temperature T, gas supply pressure p(sub S), and gas backpressure p(sub B) on the lower pressure side. Because of an extensive range of experimental conditions and complete reporting of raw data, the research by Ackerman and Koskinas was used as a source for data allowing empirical equation fitting. Unfortunately, those authors reported best-fit equations that poorly represented their own results. To improve the modeling of the original data and demonstrate the quality of the measurements, the current study develops improved hydrogen and deuterium permeation rate equations: P = 4.22×10(exp −6) A[exp(−704/T)](sq. root p(sub S) − sq. root p(sub B))/t for hydrogen P = 2.12×10(exp −6) A[exp(−468/T )](sq. root p(sub S) − sq. root p(sub B))/t for deuterium for values of cross-sectional area A (sq.cm), medium thickness t (cm), pressure p (psia), and temperature T (Kelvin), giving a permeation rate in mole/minute. These equations model permeation rate data more closely than do several other existing literature sources.

Smith, Phillip J.↗

Transmutations Observed from Pressure Cycling Palladium Silver Metals with Deuterium Gas

Hydrogen, deuterium, and helium gases were separately cycled through a Johnson-Mattheypurifier containing coiled palladium silver alloy tubing: Pd25Ag (75 wt% Pd and 25 wt% Ag).During the cycling of D2 gas, evidence of anomalous heat production was observed. However,during the cycling of H2 and He,very little (H2) or no (He) unusual heat events were observed.After cycling the D2 gas through the coiled tubing for several months, Pd25Ag samples showedan increase in Cu and Fe compared with the amounts in unexposed Pd25Ag. Chromium,manganese, and zinc were detected in gas-cycled Pd25Ag samples, whereas they were notdetected in unexposed Pd25Ag samples. In particular, Zn was present in the gas-cycled Pd25Agmaterial in larger quantities than either Cr or Mn. Although a small amount of Cu was present inthe Pd25Ag coil before the D2 gas cycling, 7 times more was present after the cycling. Multiplematerial characterization techniques were used to obtain both pre-test and post-test elementalcomposition. The results indicate that novel post-test elements, primarily on the surface, werecreated by unknown nuclear mechanisms at low energy.

Gustave C Fralick↗

Highly Active and Stable Palladium Catalysts on Novel Ceria–Alumina Supports for Efficient Oxidation of Carbon Monoxide and Hydrocarbons

Precious metal catalysts with superior low-temperature activity and excellent thermal stability are highly needed in environmental catalysis field. In this study, a novel two-step incipient wetness impregnation (T-IWI) method was developed for the fabrication of a unique and highly stable CeO 2 /Al 2 O 3 support (CA-T). Pd anchored on CA-T exhibited a much higher low-temperature catalytic activity and superior thermal stability in carbon monoxide (CO) and hydrocarbon (HC) oxidations, compared to Pd anchored on conventional CeO 2 /Al 2 O 3 (CA), which was prepared by a one-step IWI method. After aging treatment at 800 °C, the CO oxidation rate on Pd/CA-T (1.69 mmol/(g Pd s)) at 120 °C was 4.1 and 84.5 times of those on Pd/CA (0.41 mmol/(g Pd s)) and Pd/Al 2 O 3 (0.02 mmol/(g Pd s)), respectively. It was revealed that the CA-T support with well-controlled small CeO 2 particles (ca. 12 nm) possessed abundant defects for Pd anchoring, which created rich Pd-CeO 2 interfaces with strengthened interaction between Pd and CeO 2 where oxygen could be efficiently activated. This resulted in the significantly improved oxidation activity and thermal stability of Pd/CA-T catalysts. The T-IWI method developed herein can be applied as a universal approach to prepare highly stable metal oxide-alumina-based supports, which have broad application in environmental catalyst design, especially for automobile exhaust aftertreatment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Σ3(111) Grain Boundaries Accelerate Hydrogen Insertion into Palladium Nanostructures

Grain boundaries (GBs) are frequently implicated as key defect structures facilitating metal hydride formation, yet their specific role remains poorly understood due to their structural complexity. Here, we investigate hydrogen insertion in Pd nanostructures enriched with well-defined Σ3(111) GBs (Pd GB ) synthesized via electrolysis-driven nanoparticle assembly. In situ synchrotron X-ray diffraction reveals that Pd GB exhibits dramatically accelerated hydriding and dehydriding kinetics compared with ligand-free and ligand-capped Pd nanoparticles with similar crystallite sizes. Strain mapping using environmental transmission electron microscopy shows that strain is highly localized at GBs and intensifies upon hydrogen exposure, indicating preferential hydrogen insertion along GB sites. Density functional theory calculations provide mechanistic insight supporting these findings, showing that hydrogen insertion near Σ3(111) GBs is energetically more favorable and that tensile strain lowers insertion barriers. Furthermore, these results provide atomic-level insights into the role of GBs in hydride formation and suggest new design strategies for GB-engineered Pd-based functional materials.

Anions↗

Dynamic Evolution of Palladium Single Atoms on Anatase Titania Support Determines the Reverse Water–Gas Shift Activity

Research interest in single-atom catalysts (SACs) has been continuously rising. However, the lack of understanding of the dynamic behaviors of SACs during applications hinder catalyst development and mechanistic understanding. Herein, we report on the evolution of active sites over Pd/TiO 2 -anatase SAC (Pd 1 /TiO 2 ) in the reverse water-gas shift (rWGS) reaction. Combining kinetics, in-situ characterization, and theory, we show that at T ≥ 350 °C, the reduction of TiO 2 by H 2 alters the coordination environment of Pd, creating Pd sites with partially cleaved Pd-O interfacial bonds and a unique electronic structure that exhibit high intrinsic rWGS activity through the carboxyl pathway. The activation by H 2 is accompanied by the partial sintering of single Pd atoms (Pd 1 ) into disordered, flat, ~1 nm diameter clusters (Pd n ). The highly active Pd sites in the new coordination environment under H 2 are eliminated by oxidation, which, when performed at high temperature, also re-disperses Pd n and facilitates the reduction of TiO 2 . In contrast, Pd 1 sinters into crystalline, ~5 nm particles (Pd NP ) during CO treatment, deactivating Pd 1 /TiO 2 . During the rWGS reaction, the two Pd evolution pathways co-exist. The activation by H 2 dominates, leading to the increasing rate with time-on-stream, and steady-state Pd active sites similar with the ones formed under H 2 . Finally, this work demonstrates how the coordination environment and nuclearity of metal sites on a SAC evolve during catalysis and pre-treatments, and how their activity is modulated by these behaviors. These insights on SAC dynamics and structure-function relationship are valuable to mechanistic understanding and catalyst design.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Facile Synthesis of Palladium-Based Nanocrystals with Different Crystal Phases and a Comparison of Their Catalytic Properties

A relatively unexplored aspect of noble-metal nanomaterials is polymorphism, or their ability to crystallize in different crystal phases. Here, in this work, a method is reported for the facile synthesis of Ru@Pd core–shell nanocrystals featuring polymorphism, with the core made of hexagonally close-packed (hcp)-Ru while the Pd shell takes either an hcp or face-centered cubic (fcc) phase. The polymorphism shows a dependence on the shell thickness, with shells thinner than ≈1.4 nm taking the hcp phase whereas the thicker ones revert to fcc. The injection rate provides an experimental knob for controlling the phase, with one-shot and drop-wise injection of the Pd precursor corresponding to fcc-Pd and hcp-Pd shells, respectively. When these nanocrystals are tested as catalysts toward formic acid oxidation, the Ru@Pd hcp nanocrystals outperform Ru@Pd fcc in terms of both specific activity and peak potential. Density functional theory calculations are also performed to elucidate the origin of this performance enhancement.

36 MATERIALS SCIENCE↗

Palladium/Ferrierite versus Palladium/SSZ-13 Passive NOx Adsorbers: Adsorbate-Controlled Location of Atomically Dispersed Palladium(II) in Ferrierite Determines High Activity and Stability**

Pd-loaded FER and SSZ-13 zeolites as low-temperature passive NOx adsorbers (PNA) are compared under practical conditions. Vehicle cold start exposes the material to CO under a range of concentrations, necessitating a systematic exploration of the effect of CO on the performance of isolated Pd ions in PNA. The NO release temperature of both adsorbers decreases gradually with an increase in CO concentration from a few hundred to a few thousand ppm. This beneficial effect results from local nano-“hot spot” formation during CO oxidation. Dissimilar to Pd/SSZ-13, increasing the CO concentration above ˜1000 ppm improves the NOx storage significantly for Pd/FER, which was attributed to the presence of Pd ions in FER sites that are shielded from NOx. CO mobilizes this Pd atom to the NOx accessible position where it becomes active for PNA. This behavior explains the very high resistance of Pd/FER to hydrothermal aging: Pd/FER materials survive hydrothermal aging at 800°C in 10% H 2 O vapor for 16 hours with no deterioration in NOx uptake/release behavior. Therefore, by allocating Pd ions to the specific microporous pockets in FER, we have produced (hydro)thermally stable and active PNA materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Heterogeneous Palladium Catalyst for the Polymerization of Olefins Prepared by Halide Abstraction Using Surface R 3 Si + Species

The silylium-like surface species [ i Pr 3 Si][(R F O) 3 Al-OSi≡)] activates (N^N)Pd(CH 3 )Cl (N^N=Ar-N=CMeMeC=N-Ar, Ar=2,6-bis(diphenylmethyl)-4-methylbenzene) by chloride ion abstraction to form [(N^N)Pd-CH 3 ][(R F O) 3 Al-OSi≡)] ( 1 ). A combination of FTIR, solid-state NMR spectroscopy, and reactions with CO or vinyl chloride establish that 1 shows similar reactivity patterns as (N^N)Pd(CH 3 )Cl activated with Na[B(Ar F ) 4 ]. Multinuclear 13 C{ 27 Al} RESPDOR and 1 H{ 19 F} S-REDOR experiments are consistent with a weakly coordinated ion-pair between (N^N)Pd-CH 3 + and [(R F O) 3 Al-OSi≡)]. 1 catalyzes the polymerization of ethylene with similar activities as [(N^N)Pd-CH 3 ] + in solution and incorporates up to 0.4% methyl acrylate in copolymerization reactions. 1 produces polymers with significantly higher molecular weight than the solution catalyst, and generates the highest molecular weight polymers currently reported in copolymerization reactions of ethylene and methylacrylate.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Revealing the Chemical State of Palladium in Operating In 2 O 3 Gas Sensors: Metallic Pd Enhances Sensing Response and Intermetallic In x Pd y Compound Blocks It

The sensing response of metal oxides activated with noble metal nanoparticles is significantly influenced by changes to the chemical state of corresponding elements under operating conditions. Here, a PdO/rh-In 2 O3 consisting of PdO nanoparticles loaded onto rhombohedral In 2 O 3 was studied as a gas sensor for H 2 gas (100–40000 ppm in an oxygen-free atmosphere) in the temperature range of 25–450 °C. The phase composition and chemical state of elements were examined by resistance measurements combined with synchrotron-based in situ X-ray diffraction and ex situ X-ray photoelectron spectroscopy. As found, PdO/rh-In 2 O 3 undergoes a series of structural and chemical transformations during operation: from PdO to Pd/PdH x and finally to the intermetallic In x Pd y phase. The maximal sensing response (R N2 /R H2 ) of ~5 · 10 7 towards 40000 ppm (4 vol %) H 2 at 70 °C is correlated with the formation of PdH 0.706 /Pd. The In x Pd y intermetallic compounds formed around 250 °C significantly decrease the sensing response.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Tuning the hydrogenation of CO 2 to CH 4 over mechano-chemically prepared palladium supported on ceria

CO 2 methanation reactivity, reaction mechanism, and surface structure were investigated on a mechanochemically prepared Pd/CeO 2 catalyst (PdAcCeO 2 -M), where an oxidative pretreatment (-o) increased methane yield by a factor of two compared to a reductive pretreatment (-h). Methanation rates were maintained for over 48 h and further increased upon oxidative regeneration treatments. The surface species of both PdAcCeO 2 -M-o and PdAcCeO 2 -M-h were explored via in situ CO 2 and CO hydrogenation DRIFTS, where CO hydrogenation effectively models the dissociative CO 2 mechanism (CO 2 → CO → CH 4 ). PdAcCeO 2 -M-o yielded distinct Pd-CO adsorption and the absence of monodentate carbonate at ~ 1400 cm -1 , while AP-XPS showed that PdAcCeO 2 -M-o yielded a unique Pd δ+ contribution at 335.9 eV. By gaining insights from various in situ spectroscopic techniques, and by breaking the CO 2 hydrogenation mechanism into piecewise steps, a deeper understanding of the direct CO 2 reduction towards methane and CO over mechanochemically prepared Pd/CeO 2 catalysts was obtained.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Silica modulated palladium catalyst with superior activity for the selective catalytic reduction of nitrogen oxides with hydrogen

A significant promotion effect of colloidal SiO 2 on Pd/TiO 2 catalyst for improving the activity and N 2 selectivity in the selective catalytic reduction of NO with H 2 (H 2 -SCR) was reported, both before and after hydrothermal aging. The SiO 2 addition not only benefited the formation of more oxygen vacancies but also increased Pd dispersion and created rich Pd-SiO 2 interfaces on Pd-SiO 2 /TiO 2 catalyst. The H 2 -SCR of NO on both Pd/TiO 2 and Pd-SiO 2 /TiO 2 followed a Langmuir-Hinshelwood mechanism, in which the adsorbed bridging bidentate nitrates on TiO 2 could react with dissociated H 2 species on Pd sites at Pd-TiO 2 interface. Particularly, on the promoted Pd-SiO 2 /TiO 2 , the Pd-TiO 2 interface could facilitate NO adsorption and activation, and the created Pd-SiO 2 interface could benefit H 2 adsorption and dissociation, thus contributing to its significantly improved H 2 -SCR activity. Additionally, the active Pd species (which should be Pd0 under reaction condition with higher surface concentration) within Pd-SiO 2 /TiO 2 could be well stabilized during long-term hydrothermal aging process through the formation of rich Pd-SiO 2 interfaces.

36 MATERIALS SCIENCE↗

Insights into palladium poisoning of Cu/SSZ-13 selective catalytic reduction catalysts

Here, the impacts of Pd poisoning to the activity, selectivity, and hydrothermal stability of Cu/SSZ-13 selective catalytic reduction (SCR) catalysts are reported. Pd lowers DeNOx efficiency of Cu/SSZ-13 via two mechanisms: (1) displacing SCR active sites in the form of isolated Pd-ions, and (2) catalyzing non-selective NH 3 oxidation in the form of PdO. The first mechanism works by the diffusion of isolated Pd-ions into chabazite cages to displace ZCu II OH SCR active species, and it occurs on Cu/SSZ-13 catalysts with and without external surface CuO clusters in similar fashion. In contrast, the second mechanism works differently with and without external surface CuO clusters. For Cu/SSZ-13 catalyst without external CuO clusters (i.e., primarily isolated Cu-ions), PdO leads to significant decrease of DeNOx efficiency at reaction temperatures above ~400°C due to its non-selective NH 3 oxidation activity at high temperatures. However, this poisoning effect becomes much less impactful on Cu/SSZ-13 catalyst containing CuO clusters. This is due to the formation of CuO-PdO solid solution via interactions between CuO and PdO, which reduces non-selective NH 3 oxidation potential. Furthermore, this solid solution formation even mitigates adverse effects caused by hydrothermal aging. Hence, the poisoning effects of Pd are closely related to Cu speciation and spatial distribution of a Cu/SSZ-13 catalyst. Finally, this study suggests a strategy in eliminating Pd poisoning, that is, the introduction of an oxide phase that effectively traps PdO but does not adversely influence SCR.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Promoting the oxidative coupling of methanol and dimethylamine using group 1 alkali metals on palladium-gold nanoparticles

PdAu/SiO 2 catalysts were synthesized by strong electrostatic adsorption (SEA) and characterized by TEM, DRIFTS, XRD, XAS, and O 2 -TPD. The use of group 1 alkali salt solutions to control pH during SEA syntheses led to uptake of alkali metals observed reductions in the densities of terminal silanol groups of the SiO 2 support. In the absence of alkali metals, PdAu/SiO 2 catalyzes oxidative C-N bond formation between methanol and dimethylamine (DMA), yielding dimethylformamide (DMF) with ∼95 % carbon selectivity (CO 2 ∼5 %) at temperatures below 413 K. When Na, K, and Cs were present on the catalyst, methyl formate (MF) and tetramethylurea (TMU) were observed as additional products (combined ∼30 % carbon selectivity) while only TMU was detected for the Li-promoted catalyst. Total coupling product rate increased for promoted samples in the order Li < Na < Cs < K, and the apparent kinetics over the Cs-promoted catalyst were distinct from those over the alkali-free catalyst as the apparent reaction order with respect to DMA decreased and the apparent activation energy increased. Finally, this work demonstrates the sensitivity of oxidative coupling reactions to alkali metal promoters and the opportunity to achieve alkali promotion of metal catalysts during SEA synthesis.