At least 145 records · Page 8

The effect of phosphorus on precipitation in irradiated reactor pressure vessel (RPV) steels

Embrittlement of light water reactor pressure vessels (RPV) steels by fast neutron irradiation may limit extended nuclear plant life. Embrittlement, which is manifested as increases in various indexes of a ductile to brittle transition temperatures (ΔT), is primarily due to hardening by nanoscale precipitates containing Cu, Ni, Mn, and Si, which form under irradiation. In addition to these elements, P has also been found to play a role in embrittlement. While only slightly enriched in the precipitates, hardening and embrittlement increase with trace P concentrations in low-Cu steels. Here, we characterize the individual and synergistic irradiation precipitation and hardening mechanisms in a series of RPV steels containing no to low-Cu and with systematic variations in Ni and P. In this study, the steels were irradiated to a fluence of ~ 1.38 x 10 20 n/cm 2 at ~ 292 °C in the UCSB ATR-2 experiment. In Cu-free medium and high-Ni RPV steels, atom probe tomography shows that P and Ni promotes precipitation of P-Mn-Si-Ni and Mn-Si-Ni precipitates, respectively. The precipitate microstructure correlates with the observed irradiation hardening.

36 MATERIALS SCIENCE↗

Wide-band observations of LF hiss at Frobisher Bay /L = 14.6/

Temporal and spectral characteristics of LF hiss recorded at Frobisher Bay from October 30 to November 18, 1972 and from June 27, 1974 to June 26, 1975 using a wide-band (0-100 kHz) receiver are reported and discussed. The hiss occurs in bursts of about 1 to 30 min duration with a bandwidth of at least 30 kHz centered in the 20-30 kHz range. Its frequency may extend downward below 10 kHz with decreasing intensity and upward to 100 kHz with increasing intensity. There is a strong diurnal peak of occurrence centered on 21 hours LMT. Some events simultaneously recorded by a 30-MHz rapid response riometer directly follow LF hiss bursts. Apparently some electron precipitation events produce hiss bursts only, others produce hiss and then a riometer event as the precipitation flux hardens, and others, too hard to produce hiss, produce riometer events only. An examination of the present data together with previous results (Jorgensen et al., 1962; Laaspere et al., 1976) leads to the conclusion that the precipitating electrons causing ground-observed LF hiss are more energetic and have smaller pitch angles than most auroral hiss observed in the topside atmosphere with an electric dipole antenna.

Morgan, M. G.↗

Effects of chemical segregation on ductility-anisotropy in high strength Fe-Mn-Al-C lightweight austenitic steels

Ductile Fe-Mn-Al-C lightweight steels offer great potential as high specific strength materials for weight critical applications. In the present work, very high yield (~1 GPa) and ultimate tensile strength levels (~1.5 GPa) were obtained along the rolling and transverse directions of Fe-30Mn-8.5Al-0.9Si-0.9C-0.5Mo (wt.%), with high tensile elongation to failure of ~35%. This excellent mechanical behavior was attributed to the nanoscale, ordered κ-carbide precipitates formed during aging after rolling. However, tensile ductility was not isotropic through all directions of the rolled plate. In particular, the ductility was consistently lower than 5% true strain along the normal direction. Upon detailed microstructural investigations, micro-scale lamellar chemical micro-segregation bands were detected, which caused the observed anisotropic embrittlement along certain plate directions. These bands resulted in low failure strains along the normal direction since it is oriented perpendicular to these chemical segregation bands, resulting in a failure type reminiscent of delamination-induced cleavage fracture. Chemical segregation causes an inhomogeneous κ-carbide precipitate distribution upon aging, producing more pronounced mechanical anisotropy after peak-aging as compared to the solution heat treated samples. Surprisingly, deformation twinning was observed after tensile deformation of solution-heat treated specimens via electron-backscatter diffraction experiments, which is anomalous for a high stacking faulty energy (SFE) material. Further, it was proposed that chemical micro-segregation promotes locally different SFE regions, leading to deformation twinning in this nominally high SFE material. Overall, this work demonstrates the effects of chemical segregation on mechanical properties and microstructural evolution in a high performance, lightweight Fe-Mn-Al-C steel.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase field modeling of shearing processes of a dual-lobed γ"|γ'|γ" coprecipitate

The Ni-based superalloy IN718 is one of the most widely used commercial alloy in the aerospace industry since its development in 1960s. The excellent mechanical properties have been attributed in a great deal to strengthening by coherent γ' and γ" precipitates. The deformation mechanisms of these two phases have been well studied individually. Recent experimental characterization has shown coprecipitates of these two phases in a variety of morphologies and it was argued that these coprecipitates may lead to improved strengthening as compared to their monolithic counterparts. However, the deformation mechanisms of these coprecipitates are still not well understood. In this study, we performed microscopic phase field simulations, with generalized-stacking-fault (GSF) energy surfaces from ab initio calculations as inputs, to systematically study the shearing processes of a periodical array of dual-lobed coprecipitates as well as monolithic precipitates. We found that the coupling between the γ' and γ" phases in the coprecipitates forces dislocations to take high energy shearing pathways in both phases that would not occur if they were in monolithic forms. The coupling also creates stacking fault configurations in the coprecipitates that require high stress to form. Thus, the presence of coprecipitates in general should increase the resistance to dislocation shearing and lead to higher strength levels. Various fault configurations observed during the shearing process are documented as a reference for future comparison with experimental observations. The link between stacking fault shearing and microtwinning is also discussed. Here, the mechanisms analyzed in this study deepens our understanding of coprecipitation effects on alloy strength and may form a cornerstone for multi-precipitate strengthened alloy design strategies.

36 MATERIALS SCIENCE↗

The role of cellular structure, non-equilibrium eutectic phases and precipitates on quasi-static strengthening mechanisms of as-built AlSi10Mg parts 3D printed via laser powder bed fusion

The quasi-static loading strengthening mechanism in the as-built state of an AlSi10Mg alloy 3D-printed via Laser Powder Bed Fusion (LPBF) was thoroughly identified and quantified using state-of-the-art electron microscopy and synchrotron X-ray diffraction techniques. The yield strength was comprehensively modelled through an in-depth characterization and quantification of the microstructural features as well as their effective volumes for strengthening. In particular, the non-equilibrium eutectic network was characterized with a two-fold structure: cell boundary particles as well as intracellular lamellar/fibrous networks, each consisting of discrete phases exhibiting a thru-thickness compositional gradient, a semi-coherent interface with the matrix and an abundance of crystal defects such as nano-sized sub-grains, microstrains and stacking faults. Further, these altogether made the eutectic phase the most potent contributor to the yield strength accounting for ~30–40% of the estimated value (i.e., cell boundary and eutectic network strengthening combined). Precipitates strengthening was identified as the second most potent mechanism via a shearing process only. Moreover, the presented methodology was able to capture the effect of LPBF processing variables on the individual strengthening contributions, e.g., the effect of a lower laser scanning speed on increasing the cell size as well as the mean precipitate size, which are shown to exhibit opposing impacts on strengthening.

36 MATERIALS SCIENCE↗

Influence of Mo Content on the Precipitation Behavior of 13Ni Maraging Ultra-High Strength Steels

This study offers valuable insights into the precipitation behavior of 13Ni maraging steels, emphasizing the role of molybdenum content in their microstructure, strengthening, and precipitate evolution. Precipitate morphology and crystallography were examined using a combination of high-resolution transmission electron microscopy and selected area electron diffraction. Strengthening mechanisms were assessed through Vickers hardness measurements. All the examined samples exhibited a lath martensite microstructure and displayed an increasing hardness over the aging time. The molybdenum content not only influenced the presence of retained austenite in the initial microstructure but also affected the type of precipitates formed during the early aging stages. Initially, Ni 3 Mo precipitates were formed, succeeded by the formation of more stable Fe 2 (Mo,Ti) Laves precipitates. The ultra-high strength of 13Ni maraging steels arises from the combination of the precipitate type and size distribution. The base composition of 13Ni maraging steels achieved a peak hardness of 798 HV1 through the precipitation of Laves Fe 2 (Mo,Ti) phases ranging from 3 to 14 nm in diameter.

13Ni maraging steels↗

The effect of heat treatment on microfissuring in alloy 718

Changes in the microfissuring susceptibility of alloy 718 due to solution annealing and age hardening are studied. The effects of Ni3Nb (delta) precipitation during solution annealing and gamma-prime + gamma-double-prime precipitation during age hardening on microfissuring are investigated. It is observed that solution annealing reduces microfissuring and age hardening increases it, and the two precipitates do not affect microfissuring susceptibility. Potential causes for the detected intergranular segregation of the alloy are discussed.

Thompson, R. G.↗

Effect of Heat Treatments on the Tensile Properties of Additively Manufactured 15-5 Ph Stainless Steel

This study investigated the effect of post-manufacture heat treatments on the microstructure and mechanical properties of 15-5 PH stainless steel (SS) fabricated by laser powder-directed energy deposition (LP-DED). Various heat treatment procedures (CA-H900 and CA-H1150) were conducted to evaluate their effects on the tensile behavior of LP-DED 15-5 PH SS. Scanning electron microscopy was used to characterize the microstructural features and the fracture surfaces. Tensile tests were performed to evaluate the mechanical properties at cryogenic and room temperatures. Reduction in area of CA-H1150 treated specimens after tensile tests was significantly higher than CA-H900 ones, while the ultimate tensile and yield strengths of CA-H900 specimens were higher compared to the CA-H1150 ones. The mechanical behavior of the LP-DED 15-5 PH SS in various heat treatment conditions is discussed based on their microstructures and fracture surfaces.

Laser powder directed energy deposition (LP-DED)↗

Fracture-tough, corrosion-resistant bearing steels

The fundamental principles allowing design of stainless bearing steels with enhanced toughness and stress corrosion resistance has involved both investigation of basic phenomena in model alloys and evaluation of a prototype bearing steel based on a conceptual design exercise. Progress in model studies has included a scanning Auger microprobe (SAM) study of the kinetics of interfacial segregation of embrittling impurities which compete with the kinetics of alloy carbide precipitation in secondary hardening steels. These results can define minimum allowable carbide precipitation rates and/or maximum allowable free impurity contents in these ultrahigh strength steels. Characterization of the prototype bearing steel designed to combine precipitated austenite transformation toughening with secondary hardening shows good agreement between predicted and observed solution treatment response including the nature of the high temperature carbides. An approximate equilibrium constraint applied in the preliminary design calculations to maintain a high martensitic temperature proved inadequate, and the solution treated alloy remained fully austenitic down to liquid nitrogen temperature rather than transforming above 200 C. The alloy can be martensitically transformed by cryogenic deformation, and material so processed will be studied further to test predicted carbide and austenite precipitation behavior. A mechanistically-based martensitic kinetic model was developed and parameters are being evaluated from available kinetic data to allow precise control of martensitic temperatures of high alloy steels in future designs. Preliminary calculations incorporating the prototype stability results suggest that the transformation-toughened secondary-hardening martensitic-stainless design concept is still viable, but may require lowering Cr content to 9 wt. pct. and adding 0.5 to 1.0 wt. pct. Al. An alternative design approach based on strain-induced martensitic transformation during cryogenic forming, thus removing the high martensitic constraint, may permit alloy compositions offering higher fracture roughness.

Olson, Gregory B.↗

Enhanced work hardening from oxygen-stabilized ω precipitates in an aged metastable β Ti-Nb alloy

High levels of oxygen in solid solution in Ti alloys are considered detrimental to mechanical properties because of embrittlement concerns. In metastable β titanium alloys, the formation of isothermal ω precipitates is also known to cause severe embrittlement and ductility reduction. However, oxygen has been shown to partition to the ω phase during ageing, and this partitioning behavior may potentially impact ω’s mechanical contribution. Using micropillar compression, we compared the deformation behavior of Ti-20Nb (at. %) with oxygen-stabilized ω precipitates to the behavior of oxygen-free specimens. The oxygen-stabilized microstructures showed increased compressive yield strength and enhanced work hardening behavior compared to oxygen-free specimens. In the absence of oxygen, the compressed pillars showed slip band formation and catastrophic failure, and transmission electron microscopy imaging revealed that ω precipitates were sheared within the continuous deformation channels resulting in slip localization. In contrast, oxygen-stabilized ω precipitates were harder to shear and the formation of continuous deformation channels was suppressed during compression, leading to improved work hardening behavior up to 15% strain. Furthermore, this counter-intuitive role of oxygen may offer design strategies to address the significant embrittlement and loss of ductility observed for ω-strengthened β Ti alloys without oxygen and avenues to expand the use of β Ti alloys.

36 MATERIALS SCIENCE↗

Hardenability and microstructural evolution of a precipitation strengthened Ni 50 Ti 21 Hf 25 Al 4 alloy

NiTi-based quaternary alloys are used in a variety of mechanical components, such as bearings, actuators, and dampers, owing to their good hardenability, wear resistance, and corrosion resistance. Additionally, one of the most notable characteristics of NiTi-based alloys is their shape memory effect and pseudoelastic properties. Connecting the macroscopic processing parameters employed in the design of new intermetallic alloys to the nanoscale structural characteristics dictating their behavior is crucial for improving their mechanical properties and expanding the spectrum of potential applications. Here, in this work, an arc melted Ni 50 Ti 21 Hf 25 Al 4 (at%) alloy was solution treated at 1050 °C followed by quenching and aging at 600 °C to investigate the effect of aging time on the microstructure and mechanical properties. Two types of nano-sized precipitates were observed and determined as face-centered orthorhombic H-phase (TiHf)Ni and L2 1 Heusler precipitates Ni 2 TiAl. The morphology and orientation of the H-phase were investigated using scanning and transmission electron microscopy (SEM and TEM), elucidating the coarsening kinetics and strengthening contribution of that phase to the intermetallic mechanical behavior. Following coarsening, the presence of Heusler nanoprecipitates was detected under overaged conditions through TEM imaging and nanobeam electron diffraction patterns. A peak hardness condition of 756 HV was achieved after 70 h of aging, indicating that the co-precipitation of H-phase and Heusler precipitates through a well-designed aging treatment can lead to optimal mechanical performance, thus elevating the alloy’s potential as a viable material for industrial applications.

36 MATERIALS SCIENCE↗

On massive carbide precipitation during high temperature low cycle fatigue in alloy 800H

The effect of strain rate on massive precipitation and the mechanism for the occurrence of massive precipitation of M23C6 in alloy 800H is investigated during elevated temperature low cycle fatigue testing. It was observed that large M23C6 platelets were in the vicinity of grain and incoherent twin boundaries. The strain controlled fatigue testing at higher strain rates that promoted cyclic hardening enabled massive precipitation to occur more easily.

CARBON SUPERSATURATION↗

Effect of metallurgical structure and properties on adhesion and friction behavior of cobalt alloys

The metallurgical structure and some of the mechanical properties of two cobalt alloys, cobalt-50% iron and cobalt-25% molybdenum-10% chromium, were determined under various heat treated conditions. The mechanical properties of the bcc disordered Co-50Fe alloy, which was found to be very brittle, indicated an exceedingly low fracture strength, low hardness, and very weak grain boundary strength. Ordering by suitable heat treatment only produced a more brittle material with a lower fracture strength and a slightly higher hardness value. Work hardening was found to produce a finer grain structure and a greater grain boundary strength. Tensile properties were examined. It was found that the Co-25Mo-10Cr alloy was difficult to place in the alpha Co solid solution condition, which limited the ability to use precipitation as a hardening reaction. Over two hundred adhesion cycles from zero contact load, to maximum load, to fracture were conducted between couples for each of the above alloys in an ultrahigh vacuum system which would permit the sample surfaces to be cleaned of all contaminant layers. In the Co-50Fe case, the calculated fracture stress from the adhesion tests showed values in the range of 80 to 150 k.s.i., which is about ten times greater than the values from tension tests.

Keller, D. V., Jr.↗

Effect of heavy ion irradiation dose rate and temperature on α' precipitation in high purity Fe-18%Cr alloy

Cr-rich alpha prime precipitates (CrRP) induce hardening and embrittlement of FeCr alloys, but the kinetics of CrRP formation due to particle irradiation are not well understood. In this study, Fe18wt.%Cr alloy in solid solution state and pre-aged to produce relatively coarse CrRP was irradiated with 8 MeV Fe ions. The irradiation conditions involved two midrange doses of 0.37 and 3.7 displacements per atom (dpa), a wide range of dose rates (10 -5 –10 -3 dpa/s) and temperatures (300–450 °C). The distributions of CrRP after irradiation were studied with atom probe tomography (APT). The critical irradiation conditions to suppress CrRP formation were identified as 300 °C and 10-3 dpa/s; CrRP formation occurred readily at lower dose rates or higher temperatures. From 0.37 to 3.7 dpa, CrRP were observed to slightly grow at 350 °C and strongly coarsen at 450 °C. Specimens with pre-existing CrRP evolved into a similar precipitate distribution as detected after ion irradiation on solution annealed specimens at 300–350 °C to 0.37 dpa, indicating that the precipitate microstructure approaches a quasi-equilibrium for doses <1 dpa. Limited shrinking of pre-existing CrRP was observed after irradiation at 450 °C to 0.37 dpa, indicating a higher recovery rate at this temperature. Additionally, the evolution of CrRP is quantitatively explained by employing corrections to the historic Nelson-Hudson-Mazey precipitate stability model, and a radiation modified precipitation mechanism is proposed to account for the competition between radiation enhanced diffusion and ballistic dissolution which results in the modifications on both size and solute concentration of CrRP.

36 MATERIALS SCIENCE↗

Directed energy deposition of Haynes 282 nickel superalloy

Laser powder directed energy deposition was employed to fabricate Haynes® 282 Ni-based superalloy for high temperature creep testing. Material was heat treated using a single-step aging heat treatment of 800 °C for 4 h. Microstructural analysis was conducted in the as-deposited, solution-annealed, and age-hardened conditions. γ′ precipitates were absent in the as-deposited and annealed condition but formed during aging with an average size of 48.5 ± 12 nm. γ’ denuded zones ranging in thickness from 73 to 469 nm were observed adjacent to an effectively continuous grain boundary carbide film that covered 72.5% of the measured boundary length. The heat-treated material contained a high-volume fraction of TiC carbides ranging in size from 38 to 457 nm. Electron backscatter diffraction showed partial recrystallization, with 77-83% recrystallized area and a heterogeneous grain-size distribution. Creep testing at 750 °C at 300, 320, and 350 MPa revealed significantly inferior performance compared to wrought material, with higher strain rates, earlier tertiary onset, and shorter rupture lives. Fractography shows that failure was dominated by intergranular rupture. Post rupture microstructural analysis results suggest that the creep behavior was primarily governed by the non-equilibrium interface network rather than the bulk γ/γ’ matrix. In conclusion, the findings indicate that achieving wrought-like creep performance necessitates substantial improvements in the additive process, specifically focusing on enhanced homogenization, full recrystallization, and precise control over the morphology and distribution of carbides.