At least 145 records · Page 8

Surface Textures and Features Indicative of Endogenous Growth at the McCartys Flow Field, NM, as an Analog to Martian Volcanic Plains

Basaltic lavas typically form channels or tubes, which are recognized on the Earth and Mars. Although largely unrecognized in the planetary community, terrestrial inflated sheet flows also display morphologies that share many commonalities with lava plains on Mars. The McCartys lava flow field is among the youngest (approx.3000 yrs) basaltic flows in the continental United States. The southwest sections of the flow displays smooth, flat-topped plateaus with irregularly shaped pits and hummocky inter-plateau units that form a polygonal surface. Plateaus are typically elongate in map view, up to 20 m high and display lineations within the glassy crust. Lineated surfaces occasionally display small < 1m diameter lava coils. Lineations are generally straight and parallel each other, sometimes for over 100 meters. The boundaries between plateaus and depressions are also lineated and tilted to angles sometimes approaching vertical. Plateau-parallel cracks, sometimes containing squeeze-ups, mark the boundary between tilted crust and plateau. Some plateau depressions display level floors with hummocky surfaces, while some are bowl shaped with floors covered in broken lava slabs. The lower walls of pits sometimes display lateral, sagged lava wedges. Infrequently, pit floors display the upper portion of a tumulus from an older flow. In some places the surface crust has been disrupted forming a slabby texture. Slabs are typically on the scale of a meter or less across and no less than 7-10 cm thick. The slabs preserve the lineated textures of the undisturbed plateau crust. It appears that this style of terrain represents the emplacement of an extensive sheet that experiences inflation episodes within preferred regions where lateral spreading of the sheet is inhibited, thereby forming plateaus. Rough surfaces represent inflation-related disruption of pahoehoe lava and not a a lava. Depressions are often the result of non-inflation and can be clearly identified by lateral squeeze-outs along the pit walls that form when the rising crust exposes the still liquid core of the sheet. The plains of Tharsis and Elysium, Mars, display many analogous features

Bleacher, Jacob E.↗

Low and High-Power Inductive Pulsed Plasma Thruster Development Testing at NASA-MSFC

The inductive pulsed plasma thruster (IPPT) is an electromagnetic plasma accelerator that has been identified in NASA roadmaps as an enabling propulsion technology for some niche low-power missions and for high-power in-space propulsion needs. The IPPT is an electrodeless space propulsion device where a capacitor is charged to an initial voltage and then discharged producing a high current pulse through a coil. The field produced by this pulse ionizes propellant, inductively driving current in a plasma located near the face of the coil. Once the plasma is formed it can be accelerated and expelled at a high exhaust velocity by the electromagnetic Lorentz body force arising from the interaction of the induced plasma current and the magnetic field produced by the current in the coil. Thrusters of this type possess many demonstrated and potential benefits that make them worthy of continued investigation. The electrodeless nature of these thrusters eliminates the lifetime and contamination issues associated with electrode erosion in conventional electric thrusters. Also, a wider variety of propellants are accessible when compatibility with metallic electrodes in no longer an issue. IPPTs have been successfully operated using propellants like ammonia, hydrazine, and CO2, and there is no fundamental reason why they would not operate on other in situ propellants like H2O. It is well-known that pulsed accelerators can maintain constant specific impulse (I(sub sp)) and thrust efficiency (eta(sub t)) over a wide range of input power levels by adjusting the pulse rate to hold the discharge energy per pulse constant. It has also been demonstrated that an inductive pulsed plasma thruster can operate in a regime where eta(sub t) is relatively constant over a wide range of I(sub sp) values (3000-8000 s). Finally, thrusters in this class have operated in single-pulse mode at high energy per pulse, and by increasing the pulse rate they offer the potential to process very high levels of power using a single thruster. There has been significant previous research on IPPTs designed around a planar-coil (flat-plate) geometry. The most notable of these was the Pulsed Inductive Thruster (PIT), with the PIT MkV presently representing the state-of- the-art in pulsed high-power IPPT technological development. In this paper, we focus on two planar-geometry devices that operate at significantly different power levels. Most work performed at NASA-Marshall Space Flight Center (MSFC) has, to date, focused on lower power thruster operation (approx. = 10s to 100s of J/pulse, up to 2-2.5 kW average power throughput) and previously described. The most recent work aimed to assemble a device that could be tested in cyclic mode on a thrust-stand, and which could augment the existing data set for IPPTs. In addition, the thruster was designed to serve as a test-bed for solid state switching circuitry and pulsed gas valves, with the modular design of the device allowing for variation in or upgrades to test configuration. Recently, MSFC obtained on loan from the Georgia Institute of Technology (Atlanta, GA) the PIT MkVI, successor to the PIT MkV. The MkV and MkVI are similar in design with much of the hardware from the former, specifically the capacitors and spark-gap switches, being reused in the latter. The coil is similar in geometry but has bent copper rods used in the latest iteration in place of the Litz wire windings found in the MkV. The MkVI master switch for the spark gaps is located in the vacuum chamber contained within a sealed, pressurized vessel fastened to the back of the thruster. This is different from the MkV where many capacitor charging lines and spark gap-triggering delay lines ran to the thruster from a master trigger located outside the vacuum chamber. The MkVI was damaged during testing soon after its fabrication was completed. The thruster arrived at MSFC still-damaged and mostly disassembled into many individual pieces. The device has been repaired, with a few additional design changes implemented after discussions with the late Prof. Lovberg regarding the initial testing results and issues encountered. In the present work, we present results from testing of both the small IPPT and the larger MkVI thruster. The smaller device (Fig. 1) is tested on a thrust stand on multiple gases to demonstrate its capability to operate in a repetition-rate mode and serve as a IPPT technology-development testbed. The larger MkVI (Fig. 2) is operated for the first time in its newly reconstituted state, demonstrating full-power pulsed operation and, for the first time, repetition-rate operation of a high-power IPPT. The additional upgrades required for synchronous operation of all the pulsed systems in single-pulse and repetition-rate mode are described in detail.

Polzin, Kurt A.↗

Inductive Pulsed Plasma Thruster Development Testing at NASA-MSFC

The inductive pulsed plasma thruster (IPPT) is an electromagnetic plasma accelerator that has been identified in NASA roadmaps as an enabling propulsion technology for some niche low-power missions and for high-power in-space propulsion needs. The IPPT is an electrodeless space propulsion device where a capacitor is charged to an initial voltage and then discharged producing a high current pulse through a coil. The field produced by this pulse ionizes propellant, inductively driving current in a plasma located near the face of the coil. Once the plasma is formed it can be accelerated and expelled at a high exhaust velocity by the electromagnetic Lorentz body force arising from the interaction of the induced plasma current and the magnetic field produced by the current in the coil. Thrusters of this type possess many demonstrated and potential benefits that make them worthy of continued investigation. The electrodeless nature of these thrusters eliminates the lifetime and contamination issues associated with electrode erosion in conventional electric thrusters. Also, a wider variety of propellants are accessible when compatibility with metallic electrodes in no longer an issue. IPPTs have been successfully operated using propellants like ammonia, hydrazine, and CO2, and there is no fundamental reason why they would not operate on other in situ propellants like H2O. It is well-known that pulsed accelerators can maintain constant specific impulse (I(sub sp)) and thrust efficiency (η(sub t)) over a wide range of input power levels by adjusting the pulse rate to hold the discharge energy per pulse constant. It has also been demonstrated that an inductive pulsed plasma thruster can operate in a regime where η(sub t) is relatively constant over a wide range of I(sub sp) values (3000-8000 s). Finally, thrusters in this class have operated in single-pulse mode at high energy per pulse, and by increasing the pulse rate they offer the potential to process very high levels of power using a single thruster. There has been significant previous research on IPPTs designed around a planar-coil (flat-plate) geometry. The most notable of these was the Pulsed Inductive Thruster (PIT), with the PIT MkV presently representing the state of- the-art in pulsed high-power IPPT technological development. In this paper, we focus on two planar-geometry devices that operate at significantly different power levels. Most work performed at NASA-Marshall Space Flight Center (MSFC) has, to date, focused on lower power thruster operation (≈ 10s to 100s of J/pulse, up to 2-2.5 kW average power throughput) and previously described in Refs. [5,6]. The most recent work aimed to assemble a device that could be tested in cyclic mode on a thrust-stand, and which could augment the existing data set for IPPTs. In addition, the thruster was designed to serve as a test-bed for solid state switching circuitry and pulsed gas valves, with the modular design of the device allowing for variation in or upgrades to test configuration. Recently, MSFC obtained on loan from the Georgia Institute of Technology (Atlanta, GA) the PIT MkVI, successor to the PIT MkV. The MkV and MkVI are similar in design with much of the hardware from the former, specifically the capacitors and spark-gap switches, being reused in the latter. The coil is simliar in geometry but has bent copper rods used in the latest iteration in place of the Litz wire windings found in the MkV. The MkVI master switch for the spark gaps is located in the vacuum chamber contained within a sealed, pressurized vessel fastened to the back of the thruster. This is different from the MkV where many capacitor charging lines and spark gap-triggering delay lines ran to the thruster from a master trigger located outside the vacuum chamber. The MkVI was damaged during testing soon after its fabrication was completed. The thruster arrived at MSFC still-damaged and mostly disassembled into many individual pieces. The device has been repaired, with a few additional design changes implemented after discussions with the late Prof. Lovberg regarding the initial testing results and issues encountered.

Polzin, Kurt A.↗

Microcraters on lunar rocks.

Lunar microcraters may consist of a central, glass-lined pit, a halo of microfractured material surrounding the pit and a larger, generally concentric, spall area. A classification of microcraters is based on the presence or absence of a pit and a spall. The change from one crater type to another is gradational. Comparison with laboratory experiments indicates that a primary microcrater may be identified by the presence of melted host rock associated with the crater. Most microcraters are the result of the high-speed impact of primary, extralunar particles. Microcratering represents the small-scale end of a continuum of impact cratering as a process.

Hartung, J. B.↗

Microcraters on lunar rocks.

Microcrater frequency distributions have been obtained for nine Apollo rocks and an exterior chip of an Apollo 12 rock. The frequency distributions indicate that five of the Apollo 14 rocks were tumbled more than once exposing different rock faces whereas four were not tumbled and represent a single exposure interval. The cumulative frequency of craters per square centimeter was extended below optical resolution limits using a SEM scan of an exterior chip of breccia 12073. No craters with central pit diameters less than 15 microns were seen in a total area of 0.44 sq cm. A detailed SEM scan of crystal faces and glassy crater liners revealed no microcraters equal to or larger than the resolution limit of 5 microns. An upper limit of 170 craters per sq cm with central pit diameters larger than 5 microns was set. The slope of the cumulative frequency curve for craters with central pit diameters less than about 75 microns is less than that obtained by other workers.

Morrison, D. A.↗

Crater populations on lunar rocks

Approximately 10,000 microcraters were investigated using binocular microscope techniques on fifteen Apollo 16 rocks: crystalline rocks 60315, 60335, 61156, 62235, 62295, and 68415; breccias 60016, 61015, 61175, 66075, and 69935; and glass surfaces 60015, 60095, 60135, and 64455. Diameter measurements of the central glass-lined pits and surrounding spall zones were made. Ratios of spall to pit diameters may range from 3.0 to 4.5 for different rock surfaces. Crater size distributions obtained for production surfaces confirm and extend to larger crater sizes data published previously. The crater size distribution on lunar rocks in the pit diameter range, 10 to 1000 microns, is shown to depend on the average angle of impact which is a function of the exposure geometry. In contrast to results of earlier studies, a wide range of crater densities was observed on relatively heavily cratered surfaces.

Neukum, G.↗

Effect of surface texture by ion beam sputtering on implant biocompatibility and soft tissue attachment

The objectives in this report were to use the ion beam sputtering technique to produce surface textures on polymers, metals, and ceramics. The morphology of the texture was altered by varying both the width and depth of the square pits which were formed by ion beam erosion. The width of the ribs separating the pits were defined by the mask used to produce the texture. The area of the surface containing pits varies as the width was changed. The biological parameters used to evaluate the biological response to the texture were: (1) fibrous capsule and inflammatory response in subcutaneous soft tissue; (2) strength of the mechanical attachment of the textured surface by the soft tissue; and (3) morphology of the epidermal layer interfacing the textured surface of percutaneous connectors. Because the sputter yield on teflon ribs was approximately an order of magnitude larger than any other material the majority of the measurements presented in the report were obtained with teflon.

Gibbons, D. F.↗

Long term storage test of titanium material with liquid fluorine propellant

The compatibility of 6AL-4V Ti with propellant grade GF2 and LF2 at 77 K for up to 3 years was investigated. Titanium double coupons, annealed or heat treated, with 16 or 64 RMS finishes, were immersed in F2 in individual Pyrex capsules and stored under LN2 for 29 and 39 months. Pre and post immersion tests were performed on the propellant and coupons. Chemical analysis of the propellant did not reveal any significant changes due to titanium corrosion. Gravimetric, visual, microscopic, and metallurgical examination with pitting analysis did not reveal gross corrosion of the titanium although pitting appears to be greater after 39 months exposure. The increase in pit size and number raises the possibility of unpredictable crack propagation instability. Fracture toughness tests are necessary to define this possibility.

Denson, J. R.↗

Pseudocraters on Mars

In the Cydonia region of southern Acidalium Planitia are small, low-relief, apparently volcanic domelike structures, whose size, morphology, and general occurrence suggest they are martian analogs of terrestrial pseudocraters, a type of phreatic eruption. Average base diameters are about 800 m, which is somewhat larger than typical Icelandic examples. All the domes have summit pits; elongate domes generally have elongate summit pits or, in extreme cases, double pits. The greatest concentration of these domes is in a region of subdued fractured plains which may be old volcanic flows. Pseudocraters on the earth are produced when lava flows over water-logged ground. On Mars surface or subsurface ice was the likley medium that produced the steam eruptions resulting in cratered domelike structures on the lava surfaces.

Frey, H.↗

Stabilizing platinum in phosphoric acid fuel cells

The cathode of the phosphoric acid fuel cell uses a high surface area platinum catalyst supported on a carbon substrate. During operation, the small platinum crystallites sinter, causing loss in cell performance. A support was developed that stabilizes platinum in the high surface area condition by retarding or preventing the sintering process. The approach is to form etch pits in the carbon by oxidizing the carbon in the presence of a metal oxide catalyst, remove the metal oxide by an acid wash, and then deposit platinum in these pits. Results confirm the formation of etch pits in each of the three supports chosen for investigation: Vulcan XC-72R, Vulcan XC-72 that was graphized at 2500 C, and Shawinigan Acetylene Black.

Remick, R. J.↗

On lunar evidence for a possible large increase in solar flare activity approximately 2 x 10 to the 4th years ago

Data from lunar materials which may be interpreted as suggesting an increase in solar cosmic ray activity approximately 20,000 years ago is examined. The evidence includes the iron track within pit data of Hartung and Storzer (1974), the lunar whole rock pit and track data, lunar C-14 radioactivity data, lunar Ni-59 radioactivity data, the impact pit and iron track data of Morrison and Zinner (1975, 1977) and the lunar thermoluminescence data. While numerous explanations are possible for each set of data, it is shown that the first four data sets may be explained by a past increase in solar cosmic ray activity, and the remaining data sets are not necessarily incompatible with solar activity a factor of 20 to 40 times higher than at present for several thousand years prior to about 20,000 years ago.

Zook, H. A.↗

Surface chemistry and wear behavior of single-crystal silicon carbide sliding against iron at temperatures to 1500 C in vacuum

X-ray photoelectron and Auger electron spectroscopy analyses and morphological studies of wear and metal transfer were conducted with a single-crystal silicon carbide 0001 surface in contact with iron at various temperatures to 1500 C in a vacuum of 10 to the minus 8th power pascal. The results indicate that below 800 C, carbide-carbon and silicon are primarily seen on the silicon carbide surface. Above 800 C the graphite increases rapidly with increase in temperature. The outermost surficial layer, which consists mostly of graphite and little silicon at temperatures above 1200 C is about 2 nm thick. A thicker layer, which consists of a mixture of graphite, carbide, and silicon is approximately 100 nm thick. The closer the surface sliding temperature is to 800 C, the more the metal transfer produced. Above 800 C, there was a transfer of rough, discontinuous, and thin iron debris instead of smooth, continuous and thin iron film which was observed to transfer below 800 C. Two kinds of fracture pits were observed on the silicon carbide surface: (1) a pit with a spherical asperity; and (2) multiangular shaped pits.

Miyoshi, K.↗

Hypervelocity impacts on Skylab IV/Apollo windows

A description is presented of some new observations of crater morphology on the Skylab IV/Apollo windows. Aluminum is detected as the only foreign component in six of the seven lined glassy pit craters so far examined by EDS analysis. The most probable source is from aluminum oxide spherules, exhaust effluent of solid fuel rocket motors. The seventh crater contains titanium which may have been derived from an impact of a chip of thermal paint. The size distribution of the lined glassy pit craters appears to be compatible with an origin by hypervelocity impacts of aluminum spherules. If the aluminum oxide spherules are in earth orbit, impact velocities largely in the range of 7 to 10 km/s should be expected. Thus, the impact velocities are well below those expected for most impacts by micrometeorites and these lower velocities may be significant in the development of the lined glassy pit craters. The results indicate that there is a significant population of man-induced micro-debris in earth orbit.

Clanton, U. S.↗

The stress-corrosion behavior of Al-Li-Cu alloys: A comparison of test methods

Two powder metallurgy processed (Al-Li-Cu) alloys with and without Mg addition were studied in aqueous 3.5% NaCl solution during the alternate immersion testing of tuning fork specimens, slow crack growth tests using fracture mechanics specimens, and the slow strain rate testing of straining electrode specimens. Scanning electron microscopy and optical metallography were used to demonstrate the character of the interaction between the Al-Li-Cu alloys and the selected environment. Both alloys are susceptible to SC in an aqueous 3.5% NaCl solution under the right electrochemical and microstructural conditions. Each test method yields important information on the character of the SC behavior. Under all conditions investigated, second phase particles strung out in rows along the extrusion direction in the alloys were rapidly attacked, and played principal role in the SC process. With time, larger pits developed from these rows of smaller pits and under certain electrochemical conditions surface cracks initiated from the larger pits and contributed directly to the fracture process. Evidence to support slow crack growth was observed in both the slow strain rate tests and the sustained immersion tests of precracked fracture mechanics specimens. The possible role of H2 in the stress corrosion cracking process is suggested.

Rizzo, P. P.↗

Observation of defects in mercury cadmium telluride crystals grown by chemical vapor transport

A mixture of nitric and hydrochloric acids was found to yield etch pits on mercury cadmium telluride crystals grown by chemical vapor transport using iodine or mercuric iodide as the transport agent. Two types of pits were observed by optical microscopy: triangular pyramidal and round saucer shaped pits. Transmission electron microscopy confirmed that two types of defects were present: dislocations and second phase occlusions. The present study suggests that the defects are near the crystal surface and therefore will probably not significantly affect the electrical characteristics.

Irene, E. A.↗

Ceramic wear in indentation and sliding

The various wear mechanisms involved with single-crystal ceramic materials in indentation and in sliding contacts. Experiments simulating interfacial events have been conducted with hemispherical, conical and pyramidal indenters (riders). With spherical riders, under either abrasive or adhesive conditions, two types of fracture pits have been observed. First, spherical-shaped fracture pits and wear particles are found as a result of either indenting or sliding. These are shown to be due to a spherical-shaped fracture along the circular or spherical stress trajectories. Second, polyhedral fracture pits and debris, produced by anisotropic fracture, and also found both during indenting and sliding. These are primarily controlled by surface and subsurface cracking along cleavage planes. Several quantitative results have also been obtained from this work. For example, using a pyramidal diamond, crack length of Mn-Zn ferrite in the indentation process grows linearly with increasing normal load. Moreover, the critical load to fracture both in indentation and sliding is essentially isotropic and is found to be directly proportional to the indenter radius.

Miyoshi, K.↗

Ceramic wear in indentation and sliding contact

The various wear mechanisms involved with single-crystal ceramic materials in indentation and in sliding contacts. Experiments simulating interfacial events have been conducted with hemispherical, conical and pyramidal indenters (riders). With spherical riders, under either abrasive or adhesive conditions, two types of fracture pits have been observed. First, spherical-shaped fracture pits and wear particles are found as a result of either indenting or sliding. These are shown to be due to a spherical-shaped fracture along the circular or spherical stress trajectories. Second, polyhedral fracture pits and debris, produced by anisotropic fracture, and also found both during indenting and sliding. These are primarily controlled by surface and subsurface cracking along cleavage planes. Several quantitative results have also been obtained from this work. For example, using a pyramidal diamond, crack length of Mn-Zn ferrite in the indentation process grows linearly with increasing normal load. Moreover, the critical load to fracture both in indentation and sliding is essentially isotropic and is found to be directly proportional to the indenter radius.

Miyoshi, K.↗

Compatibility of grain-stabilized platinum with candidate propellants for resistojets

Resistojets are candidates for space station auxiliary propulsion, and should be characterized by both long life and multipropellant operations, requirements limited by available materials. Grain stabilized platinum is examined for use as a resistojet thruster material. Use of platinum in other applications indicates it can be used at moderately high temperatures for extended periods of time. Past results indicate that grain-stabilized platinum should be sufficiently inert in candidate propellant environments. Therefore, compatibility of platinum-yttria (P/Y2O3) and platinum-zirconia (Pt/ZrO2) with carbon dioxide, methane, hydrogen and ammonia is examined. A series of 1000 hr tests in CO2, H2, and NH3 is conducted at 1400 C and a series of 1000 hr tests in CH4 is conducted at about 500 C. Scanning electron microscopy, Auger electron spectroscopy and depth profiling analysis are then used to determine the effects of propellants on the material surface, to evaluate possible material contamination and to evaluate grain growth. The results indicate that there is carbon deposition on the surface of the Pt/Y2O3 and Pt/ZrO2 in both the CO2 and CH4 environments. In the H2 environment, the Pt/Y2O3 and Pt/ZrO2 specimen surfaces are roughened. After exposure to the NH3 environment, the Pt/Y2O3 and Pt/ZrO2 are roughened and pitted over the entire heated area with some pitted areas along the grain boundaries. SEM photos show grain growth in cross-sectional views of all the Pt/Y2O3 samples and the Pt/ZrO2 samples, except that tested in methane. Mass loss measurements indicate that Pt/Y2O3 and Pt/ZrO2 would last in excess of 200,000 hr in each propellant environment. However, in NH3 both Pt/Y2O3 and Pt/ZrO2 are severely pitted, with voids up to 50 percent into the material. Pt/Y2O3 and Pt/ZrO2 are not recommended for high temperature service in NH3.

Whalen, M. V.↗