Search NASA⌕ Search

SEARCH · Search NASA

Results for “Polymer electrolyte”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Coupled continuum and network model framework to study catalyst layers of polymer electrolyte fuel cells

The nanostructured thin film (NSTF) catalyst layers which have demonstrated high power densities, mass activities, and exceptional metal and support stability can have limited operational robustness due to their thin thickness and the hydrophilicity of the metal-coated nano whiskers. The dispersed nanostructured thin film (dNSTF) catalyst layers have been developed by dispersing the NSTF Pt whiskers with ionomer and carbon support to increase the thickness and hydrophobicity. Continuum and network models (NM) are coupled through boundary conditions to study the polymer electrolyte fuel cell with a dNSTF cathode catalyst layer. The coupled model combines the computational efficiency of the continuum model with the pore-scale information in the dNSTF cathode catalyst layer of the NM. It captures the special morphology of the partially ionomer/water covered cylindrical whiskers, as well as water percolation through the pore structures and their impact on the cell performance. Here we observe optimal ionomer coverage on whiskers to be 0.5, ionomer to carbon ratio to be 0.9 and higher whisker to carbon ratios to be desired.

08 HYDROGEN↗

Role of Intra-Domain Heterogeneity on Ion and Polymer Dynamics in Block Polymer Electrolytes: An Approach for Spatially Resolving Dynamics and Ion Transport

The design of safe and high-performance, nanostructured, block polymer (BP) electrolytes for lithium-ion batteries requires a thorough understanding of the key parameters that govern local structure and dynamics. Yet, the interfaces between microphase separated domains can introduce complexities in this local behavior that can be challenging to quantify. Herein, the local polymer, cation (Li + ), and anion dynamics were described in salt-doped polystyrene block poly(oligo-oxyethylene methyl ether methacrylate) (PS-b-POEM) through a quantitative framework that considered the effects of polymer architecture, segmental mixing, chain stretching, and confinement on polymer mobility and ion transport. This framework was validated through nuclear magnetic resonance (NMR) spectroscopy measurements on solid (dry) polymer electrolyte samples. Notably, a mobility transition temperature (T mobility ) was identified through NMR spectroscopy that captured the local dynamics more accurately than the thermal glass transition temperature. Additionally, the approach quantitatively described the mobility gradient across a domain when segmental mixing effects were combined with chain stretching and confinement information, especially at higher segregation strengths – facilitating the assessment of local ion diffusion and conductivity. As a result, spatially averaged local ion diffusion predictions quantitatively matched NMR-measured ion diffusivities in the BP samples, while spatially summed ionic conductivity predictions across a domain qualitatively captured trends in the measured ionic conductivities.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Polymer electrolytes based on protic ionic liquids with perfluorinated anions for safe lithium-ion batteries

Here, the quest for safe and high-performance polymer electrolytes in lithium-ion batteries (LIBs) has led researchers to explore protic ionic liquids (PILs) as potential candidates to be entrapped in polymer matrices. In this context, we present an investigation into solid polymeric systems based on poly(methyl methacrylate) (PMMA) as a host for PILs, featuring 1,8-diazabicyclo-[5,4,0]-undec-7-ene (DBU) cation paired with three different anions: bis(trifluoromethanesulfonyl)imide (TFSI – ), trifluoromethanesulfonate (TFO – ), and (trifluoromethanesulfonyl-nonafluorobutylsulfonyl)imide (IM14 – ). Additionally, we explore the lithium-doped IM14-gel-like system to broaden our understanding of these intriguing materials. Through comprehensive thermal analysis, solid-state NMR, and diffusion NMR techniques, we delve into the interactions and structural features of these binary and ternary polymeric systems. Our investigation reveals unique dynamics and ion interactions within the PMMA matrix, shedding light on the potential of these materials for advanced energy storage technologies. Particularly, we highlight the distinctive features of DBUH-IM14 and its specific interaction with the polymeric matrix and the lithium ions, underscoring its significance in advancing safer and more efficient energy storage devices.

25 ENERGY STORAGE↗

High Temperature Polymer Electrolyte Membrane Fuel Cells with High Phosphoric Acid Retention

Phosphoric acid loss poses immense hurdles for the durability of high-temperature polymer electrolyte membrane fuel cells (HT-PEMFCs). Here we report quaternary ammonium-biphosphate ion-pair HT-PEMFCs that do not lose phosphoric acids under normal and accelerated stress conditions. Additionally, our energetics study explains the acid loss behavior of the conventional phosphoric acid-polybenzimidazole (PA-PBI) system by two mechanisms. If PA loss occurs via acid evaporation, the acid loss is constant over time. On the other hand, when water activity in the PA-PBI system is high, exponential decay of PA loss occurs via the water replacement mechanism. Combined 31 P NMR and computational studies show that the proposed ion-pair system has six times higher interaction energy, which allows for containing all PAs in the membrane electrode assemblies under a broad range of operating conditions. In addition, polar interactions between the phosphonic acid ionomer and phosphoric acid explain acid retention in the electrodes of the ion-pair HT-PEMFCs.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Experimental Performance Evaluation of a Hyper-Branched Polymer Electrolyte for Rechargeable Li-Air Batteries

A hyper-branched polymer (HBP) electrolyte is synthesized for rechargeable lithium-air (Li-air) battery cell and experimentally evaluated its performance in actual battery cell environment. Several real-world battery cells were fabricated with synthesized HBP electrolyte, pure lithium metal as anode and an oxygen permeable air cathode to evaluate reproducibility of the rechargeable Li-air battery cell. The effect of various conditions such as various HBP based electrolytes, discharge current -0.1~0.5 mA, cathode preparation processes and carbon contents on the battery cell performance were experimentally evaluated using the fabricated battery cells under dry air condition. Detailed HBP electrolyte synthesis procedures and experimental performance evaluation of Li-air battery cell for various conditions are presented. The experimental results showed that different conditions and processes significantly affect the Li-air battery performance. Upon taking into account the effect of different conditions and processes, optimized HBP electrolyte materials, cathode process and conditions were determined. Several Li-air battery cells were fabricated with optimized conditions and optimized battery cell materials to determine the reproducibility and performance consistency. Experimental results showed that over 55–65 h of discharge occurred over 2.5 V terminal cell voltage with all three optimized Li-air battery cells. It implied that the optimized Li-air battery cells were reproducible and were able to hold charge over 2.5 V for more than 2 days. Experimental results of the Li-air battery cell with further refined optimized materials revealed that the battery cell can discharge more than 10 days (i.e., more than 250 h) at or above 2.0 V. The experimental results also showed that the Li-air battery discharge time got shorter as the discharge-charge cycle increases due to increase in internal resistances of battery cell materials. The experimental results confirmed that the lithium-air battery cell can be reproduced without loss of performance and can hold charge more than 10 days at or over 2.0 V. The investigation results obtained may usher a pathway to manufacture a long-life rechargeable Li-air battery cell in the near future.

25 ENERGY STORAGE↗

Understanding Platinum Ionomer Interface Properties of Polymer Electrolyte Fuel Cells

A well-designed cathode catalyst layer with optimal ionomer distribution is critical to minimizing amount of Platinum (Pt) content in polymer electrolyte fuel cells (PEFCs). The impact of Pt loading, ionomer content and carbon support types on the catalyst/ionomer interface were also investigated at dry and wet conditions. Higher Pt loadings resulted in higher double layer capacity (C dl ) and similar electrochemical surface area (ECSA) due to well dispersed ionic phase material. Higher ionomer content resulted in higher ionic conductivity but also showed similar SO 3 − group coverage. High surface area (HSA) carbon support had larger ECSA and C dl at both dry and wet conditions, as less agglomerated Pt was well dispersed in the meso-pores of the support. Lower SO 3 − group coverages were observed for HSA carbon than for Vulcan carbon due to Pt particles being buried within the porous HSA carbon support. The effect of cell conditioning and voltage recovery on the PEFC cathode catalyst layer was shown to have minimal impact on SO 3 − group coverage despite a decrease in C dl and ECSA due to the size increase of Pt particles. At dry condition, a significant increases in SO 3 − group coverage were observed for all MEAs due to higher adsorptivity of ionomer in dry conditions.

25 ENERGY STORAGE↗

Carbon Corrosion in Polymer Electrolyte Fuel Cells: A Complex Interplay between Morphological Changes and Electrochemical Performance

Due to the high gravimetric energy density of hydrogen, the focus of implementation of polymer electrolyte fuel cells (PEFCs) has shifted from light duty passenger vehicles to heavy duty vehicles such as buses, trucks, locomotives and marine vessels. A mechanistic understanding of degradation is therefore necessary to improve durability and efficiency. During start-up and shut-down (SUSD) of PEFC systems, the catalyst (Pt nanoparticles embedded on carbon support) undergoes local potentials ~ 1 - 1.5 V caused by a combination of fuel (H 2 ) starvation, mixed fuel region and cell reversal. This leads to a series of degradation phenomenon including reduction in cathode catalyst layer (cCL) thickness and porosity, loss in electrochemical surface area (ECSA), ionomer degradation and loss in electrical contact, therefore resulting in severe performance loss. The convoluted relationship between these individual degradation mechanisms, their chronology and their effects on electrochemical performance are yet unresolved. Here, the complex interplay between morphological changes due to carbon corrosion and its effects on the electrochemical performance were analyzed using a combination of detailed electrochemical characterization, spectroscopy, and electron microscopy techniques.

25 ENERGY STORAGE↗

Contaminant Cation Effect on Oxygen Transport through the Ionomers of Polymer Electrolyte Membrane Fuel Cells

We characterized the effects of cobalt (Co 2+ ) and other cation contaminants on the oxygen (O 2 ) transport properties of the PFSA ionomer used in polymer electrolyte membrane fuel cells (PEMFCs) and gained insight into the mechanisms by which contaminant cations inhibit O 2 transport. Such cations can be released by alloy catalysts and environmental conditions and pose a significant challenge to maintaining high current density performance with low platinum (Pt) loadings. We used a test cell capable of isolating the ionomer from the membrane electrode assembly (MEA), allowing for O 2 transport resistance (R O2 ) measurements using a limiting current technique. We contaminated ionomer membranes with Li + , Na + , Ni 2+ , Co 2+ , and Ce 3+ and found a general increase in R O2 for increased contamination levels and decreased water activity. In addition, our Co 2+ results indicated distinct concentration-dependent regimes. The other cation-form ionomers allowed us to separate the impacts of ion pair strength, multivalency, and reduced water uptake. We believe that these factors cause a more compressed hydrophilic domain and tortuous O 2 diffusion path, and a commensurate increase in R O2 . Lastly, we studied the impact of Co 2+ on an operating PEMFC and found an increase in R O2 consistent with the results of our isolated membrane tests.

25 ENERGY STORAGE↗

Polymer Electrolyte Membrane Fuel Cell Electrode Compositions

This Snapshot summarizes several inventions made at Los Alamos National Laboratory that are believed to promise high power density and extended durability in a Polymer Electrolyte Membrane (PEM) fuel cell Membrane Electrode Assembly (MEA). In the laboratory these ion pair electrode and membrane innovations improve fuel cell performance under anhydrous conditions above 100 °C, and remain operable at lower temperatures as well

25 ENERGY STORAGE↗

Review—Development of Highly Active and Durable Hybrid Compressive Platinum Lattice Catalysts for Polymer Electrolyte Membrane Fuel Cells: Mathematical Modeling and Experimental Work

This review provides a comprehensive overview on the development of highly active and durable platinum catalysts with ultra-low Pt loadings for polymer electrolyte membrane fuel cells (PEMFCs) through a combined mathematical modeling and experimental work. First, simulation techniques were applied to evaluate the validity of the Tafel approximation for the calculation of the mass activity (MA) and specific activity (SA). A one-dimensional agglomeration model was developed and solved to understand the effects of exchange current density, porosity, agglomerate size, Nafion ® film thickness, and Pt loading on the MA and SA. High porosity (> 60%) and agglomerations at high Pt loadings cause the loss of the Tafel approximation and consequently the decrease in MA and SA. A new structure parameter was introduced to estimate the real porous structure using the fractal theory. The volumetric catalyst density was corrected by the fractal dimension (measured by Hg porosimetry), which gave a good agreement with the experimental values. The loading-dependent Tafel equation was then derived, which contains both the utilization and the non-linear scaling factor. Second, activated carbon composite support (ACCS) with optimized surface area, porosity, pore size, and pore size distribution was developed. The hydrophilic/hydrophobic ratio, structural properties (amorphous/crystalline ratio), and the number of active sites were optimized through metal-catalyzed pyrolysis. Stability of ACCS and Pt/ACCS were evaluated using an accelerated stress test (AST). The results indicated that Pt/ACCS showed no significant loss of MA and power density after 5,000 cycles at 1.0–1.5 V, while the commercial Pt/C catalysts showed drastic losses of MA and power density. Finally, monolayers of compressed Pt (core–shell-type Pt 3 Co 1 ) catalysts were structured by diffusing Co atoms (previously embedded in ACCS) into Pt. Compressive Pt lattice (Pt * ) catalysts were synthesized through an annealing procedure developed at the University of South Carolina (USC). The Pt * /ACCS catalyst showed high initial power density (rated) of 0.174 g Pt kW −1 and high stability (24 mV loss) at 0.8 A cm −2 after 30,000 cycles (0.6–1.0 V). The outstanding performance of Pt * /ACCS is due to the synergistic effect of ACCS and compressive Pt * lattice.

25 ENERGY STORAGE↗

Interpreting Ionic Conductivity for Polymer Electrolyte Fuel Cell Catalyst Layers with Electrochemical Impedance Spectroscopy and Transmission Line Modeling

A cathode catalyst layer containing optimally distributed ionomer is critical to reduce the platinum loading and increase its utilization in polymer electrolyte fuel cells. Here, electrochemical impedance spectroscopy (EIS) was used to measure effective ionic conductivity of pseudo catalyst layers (PCLs) at a relative humidity (RH) range of 50%-120%. These results are compared to previous work using the hydrogen pump (HP) method. EIS effective ionic conductivity results reported here are higher than those from the HP because in the HP set-up ionic pathways must be effectively connected through the PCL to be counted, whereas in the EIS measurement, ionomer segments that are in contact with the membrane but are not effectively connected all the way through the PCL can be detected. Double layer capacitances and effective ionic conductivities of Pt/C catalyst layers with various supports and ionomer to carbon (I/C) ratios were studied. High surface area carbon support resulted in a lower effective ionic conductivity compared to the graphitized carbon support due to worse ionomer dispersion. Effective ionic conductivities of Pt/C layers were compared to that of PCLs. On average, effective ionic conductivities of Pt/C layers were higher than PCLs because of possible carbon agglomeratio n within the PCLs.

25 ENERGY STORAGE↗

Process model for multilayer slide coating of polymer electrolyte membrane fuel cells

Slide coating is a precision method suitable for depositing multiple liquid-film layers simultaneously. Originally developed in the photographic film industry, it has been deployed for manufacturing of other products that benefit from multilayer coatings. One emerging application is the manufacture of polymer electrolyte membrane fuel cells (PEMFCs), which are used to produce electricity through electrochemical reactions of hydrogen and oxygen gas. The membrane-electrode assembly (MEA), in which key electrochemical reactions occur, consists of three layers that are typically deposited separately in serial fashion and then laminated together to form the three-layer MEA, i.e., three sequential steps of coat and dry. Adapting the process to simultaneous, multilayer slide coating of all three layers will save equipment cost and space while minimizing possible exposure to contaminants during transition between the steps. We are developing a three-layer slide coating model to aid the manufacturing process design of PEMFC. The model accounts for rheology of each layer, which typically exhibit shear thinning behavior. Model predictions are used to investigate simultaneous coatability of catalyst inks and to determine the best layer-by-layer ink selection.

25 ENERGY STORAGE↗

Nanotomography Investigation of 3D Printed Batteries with a Water-in-Salt Gel Polymer Electrolyte

3D printing, also known as additive manufacturing, has emerged as a promising strategy to design and fabricate future energy storage devices. Although significant progress has been reported, current 3D printed battery designs are still limited by the choice of the electrolyte, such as ceramic or conventional toxic organic electrolytes. Here, we incorporated the latest developments in aqueous batteries into a novel 3D printable battery that can be fabricated directly in an ambient environment that is also more environmentally friendly. Specifically, a gel polymer electrolyte with a water-in-salt concept was introduced in our 3D-printed batteries. Combining their advantages, the resulting 3D printable batteries show promise for much simplified processing conditions. Further, the structural, (electro-)chemical, and morphological evolution batteries are being investigated by synchrotron X-ray nanotomography and electrochemical analysis. Overall, our research explores the possibility of an easier and more environmentally friendly way to build 3D printable, customizable batteries for future technologies.

36 MATERIALS SCIENCE↗

Durability evaluation of a Fe–N–C catalyst in polymer electrolyte fuel cell environment via accelerated stress tests

In this work, an “atomically-dispersed” iron-nitrogen-carbon (Fe–N–C) catalyst was used to provide a systematic comparison of platinum group metal (PGM)-free electrocatalyst degradation as a function of accelerated stress tests (ASTs) in an acidic polymer electrolyte fuel cell (PEFC). It was determined that the majority of catalyst degradation was caused by cell operation in presence of O 2 . In contrast, potential cycling of the Fe–N–C-containing cathode under inert atmosphere over typical PEFC cathode operation from 0.95 to 0.6 V had little to no effect. The increase in kinetic overpotential is shown to be the major source of the PEFC performance decrease during the ASTs. These results continue to showcase the need for development of robust PGM-free electrocatalysts in concert with improved electrochemical performance.

25 ENERGY STORAGE↗

3D Printed Carbon Aerogels for Polymer-Electrolyte Fuel Cells

Carbon aerogels (CA) are known for ultra-low density, very high surface area, fine porous structure, and excellent electrical conductivity. Recent advances in high resolution 3D printing at LLNL enable the manufacturing of complex structured CA electrodes which have been demonstrated in electrolysis, flow battery, and supercapacitor applications. Polymer-electrolyte fuel cells (PEFC) may be an excellent candidate for these materials/methods as designers seek to optimize membrane-electrode assemblies to achieve higher efficiencies. A major challenge to PEFC design is two-phase flow due to water production which causes pore flooding and leads to cell instability and degradation. To mitigate these effects, groups have investigated the creation of liquid specific pathways in the porous layers to alleviate liquid buildup and enhance gas diffusion. While some progress has been made, traditionally manufactured GDLs, which consist of randomly distributed carbon fibers, are limiting. 3D printed CAs are a promising solution as complex macroporous electrode structures can be manufactured out of micro and nano porous filaments with a high level of control. Additionally, the process may allow for the consolidation of multiple layers (MPL, GDL, & flow channels) into a single printed architecture. In this work various CA lattice structures were printed using a direct ink write (DIW) method and liquid breakthrough pressures were measured to demonstrate the ability to tune the water pathways to achieve specific pressure thresholds. Furthermore, a discussion of the prospects for printed CA electrodes in PEFC will focus on material properties, synthesis techniques, and current challenges.

36 MATERIALS SCIENCE↗

Dynamic sparse x-ray nanotomography reveals ionomer hydration mechanism in polymer electrolyte fuel-cell catalyst

Tomographic imaging of time-evolving samples is a challenging yet important task for various research fields. At the nanoscale, current approaches face limitations of measurement speed or resolution due to lengthy acquisitions. We developed a dynamic nanotomography technique based on sparse dynamic imaging and 4D tomography modeling. We demonstrated the technique, using ptychographic x-ray computed tomography as its imaging modality, on resolving the in situ hydration process of polymer electrolyte fuel cell (PEFC) catalyst. The technique provides a 40-time increase in temporal resolution compared to conventional approaches, yielding 28 nm half-period spatial and 12 min temporal resolution. The results allow a quantitative characterization of the water intake process inside PEFC catalysts with nanoscale resolution, which is crucial for understanding their electrochemical mechanisms and optimizing their performance. Our technique enables high-speed operando nanotomography studies and paves the way for wider application of dynamic tomography at the nanoscale.

Science & Technology - Other Topics↗

Universal Relationship between Limiting Current and Electrochemical Transport Properties in Malonate-Based Polymer Electrolytes

There is considerable interest in developing high-performance electrolytes for rechargeable lithium batteries. For practical applications, the electrolyte must support large dc currents. However, the parameters most often reported in the literature, conductivity, κ, and current fraction, ρ + , reflect ion transport in the limit of infinitesimal currents. In this limit, the efficacy of an electrolyte is given by the product κρ + . The limiting current density, i lim , is the maximum current density that can be applied across an electrolyte; the cell voltage diverges if the applied current density exceeds ilim. This parameter reflects ion transport in the limit of large dc currents and is therefore of practical interest. It would therefore be convenient if i lim could be predicted from measurements of κρ + . In order to explore this possibility, we studied six malonate-based polymers and PEO at a fixed salt concentration (r = 0.08) and temperature (90°C) using symmetric cells with planar electrodes. Unfortunately, there is no correlation between ilim and κρ + . When the applied current density, i, is less than ilim, the cell voltage approaches a stable plateau, ϕ plateau . Here, we found a linear dependence between i and thickness-normalized plateau potential, ϕ plateau L –1 , irrespective of the magnitude of the applied current. In all seven polymer electrolytes, we found a linear correlation between ilim and the slopes of these lines, σ. In other words, measurements of σ can be used to predict the limiting current.

Jana, Rounak [Lawrence Berkeley National Laborator↗