Search NASA⌕ Search

SEARCH · Search NASA

Results for “SLIDING CONTACT”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Bearing material

A composite material is described which will provide low friction surfaces for materials in rolling or sliding contact and is self-lubricating and oxidation resistant up to and in excess of about 930 C. The composite is comprised of a metal component which lends strength and elasticity to the structure, a fluoride salt component which provides lubrication and, lastly, a glass component which not only provides oxidation protection to the metal but may also enhance the lubrication qualities of the composite.

Sliney, H. E.↗

Rapid interface flaw extension with friction

An idealized two-dimensional example of rapid interface flow extension is described. Initially undisturbed dissimilar isotropic, homogeneous, linearly elastic half-spaces are perfectly bonded along the interface y=0. Quantities associated with the half-space or = to 0 are denoted by the prime superscript or the subscripts 3 or 4 while those in y or = to 0 carry the subscripts 1 or 2. At time t=0 adjacent material points at x=0, y= + or - 0 are forced apart horizontally with a constant relative velocity delta v. This results in a zone of bond failure which extends symmetrically along the interface at a constant rate c. The newly created flaw surfaces are in sliding contact resisted by Coulomb friction. The friction coefficient is gamma.

Brock, L. M.↗

Microstructural and wear properties of sputtered carbides and silicides

Sputtered Cr3C2, Cr3Si2, and MoSi2 wear-resistant films (0.05 to 3.5 microns thick) were deposited on metal and glass surfaces. Electron transmission, electron diffraction, and scanning electron microscopy were used to determine the microstructural appearance. Strong adherence was obtained with these sputtered films. Internal stresses and defect crystallographic growth structures of various configurations within the film have progressively more undesirable effects for film thicknesses greater than 1.5 microns. Sliding contact and rolling element bearing tests were performed with these sputtered films. Bearings sputtered with a duplex coating (0.1-micron-thick undercoating of Cr3Si2 and subsequently 0.6-micron coating of MoS2) produced marked improvement over straight MoS2 films.

Spalvins, T.↗

Friction and deformation behavior of single-crystal silicon carbide

Friction and deformation studies were conducted with single-crystal silicon carbide in sliding contact with diamond. When the radius of curvature of the spherical diamond rider was large (0.3), deformation of silicon carbide was primarily elastic. Under these conditions the friction coefficient was low and did not show a dependence on the silicon carbide orientation. Further, there was no detectable cracking of the silicon carbide surfaces. When smaller radii of curvature of the spherical diamond riders (0.15 and 0.02 mm) or a conical diamond rider was used, plastic grooving occured and the silicon carbide exhibited anisotropic friction and deformation behavior. Under these conditions the friction coefficient depended on load. Anisotropic friction and deformation of the basal plane of silicon carbide was controlled by the slip system. 10101120and cleavage of1010.

Miyoshi, K.↗

Microstructural and wear properties of sputtered carbides and silicides

Sputtered Cr3C2, Cr3Si2, and MoSi2 wear-resistant films (0.05 to 3.5 microns thick) were deposited on metal and glass surfaces. Electron transmission, electron diffraction, and scanning electron microscopy were used to determine the microstructural appearance. Strong adherence was obtained with these sputtered films. Internal stresses and defect crystallographic growth structures of various configurations within the film have progressively more undesirable effects for film thicknesses greater than 1.5 microns. Sliding contact and rolling-element bearing tests were also performed with these sputtered films.

Spalvins, T.↗

Method of making bearing materials

A method is described for making a composite material which provides low friction surfaces for materials in rolling or sliding contact. The composite material which is self-lubricating and oxidation resistant up to and in excess of about 930 C is comprised of a metal component which lends strength and elasticity to the structure and a fluorine salt component which provides oxidation protection to the metal but may also enhance the lubrication qualities of the composite.

Sliney, H. E.↗

Plasma-sprayed coatings for lubrication of a titanium alloy in air at 430 deg C

Plasma sprayed coatings of pure silver and of composite materials containing silver were investigated as possible self lubricating coatings for titanium alloys in air at 430 C. Pure silver provided low friction but was prone to severe plastic deformation and excessive transfer except in coating thicknesses of 0.02 mm or less. Additions of nichrome, calcium fluoride, and glass to silver were all beneficial in reducing plastic deformation and otherwise improving the coatings. The longest coating wear life, low wear of Ti alloy pins in sliding contact with the coatings, and a steady friction coefficient of 0.19 were obtained with a four component coating of 0.17 mm thickness. The coating composition, in weight percent is 30 nichrome-30 Ag-25 CaF2-15 glass.

Sliney, H. E.↗

Evaluation and auger analysis of a zinc-dialkyl-dithiophosphate antiwear additive in several diester lubricants

The wear of pure iron in sliding contact with hardened M-2 tool steel was measured for a series of synthetic diester fluids, both with and without a zinc dialkyl dithiophosphate (ZDP) antiwear additive, as test lubricants. Selected wear scars were analyzed by an Auger emission spectroscopy (AES) depth profiling technique in order to assess the surface film elemental composition. The ZDP was an effective antiwear additive for all the diesters except dibutyl oxalate and dibutyl sebacate. The high wear measured for the additive-containing oxalate was related to corrosion; the higher wear measured for the additive-containing sebacate was due to an oxygen interaction. The AES of dibutyl sebacate surfaces run in dry air and in dry nitrogen showed large differences only in the amount of oxygen present. The AES of worn surfaces where the additive was effective showed no zinc, only a little phosphorus, and large amounts of sulfur.

Brainard, W. A.↗

Development of surface coatings for air-lubricated, compliant journal bearings to 650 C

Surface coatings for an air-lubricated, compliant journal for an automotive gas turbine engine were tested to find those capable of withstanding temperatures of either 540 C (1000 F) or 650 C (1200 F). Also, the coatings have to be capable of surviving the start-stop sliding contact cycles prior to rotor lift-off and at touchdown. Selected coating combinations were tested in start-stop tests at 14 kPa (2 psi) loading for 2000 cycles at room and maximum temperatures. Specific coating recommendations are: Cdo and graphite on foil versus chrome carbide on journal up to 370 C (700 F); NASA PS-120 (Tribaloy 400, silver, and CaF2) on journal versus uncoated foil up to 540 C (1000 F); and chemically adherent Cr2O3 on journal and foil up to 650 C (1200 F). The chemically adherent Cr2O3 coating system was further tested successfully at 35 kPa (5 psi) loading for 2000 start-stop cycles.

Bhushan, B.↗

Method of making bearing material

A composite material is described which will provide low friction surfaces for materials in rolling or sliding contact and is self lubricating and oxidation resistant up to and in excess of about 930 C. The composite is comprised of a metal component which lends strength and elasticity to the structure, a fluoride salt component which provides lubrication and, lastly, a glass component which not only provides oxidation protection to the metal but may also enhance the lubrication qualities of the composite.

Sliney, H. E.↗

Rotary Transformer Seals Power In

Rotary transformer originally developed for spacecraft transfers electrical power from stationary primary winding to rotating secondary without sliding contacts and very little leakage of electromagnetic radiation. Transformer has two stationary primary windings connected in parallel. Secondary, mounted on a shaft that extends out of housing, rotates between two windings of primary. Shaft of secondary is composed of electrically conducting inner and outer parts separated by an insulator. Electrical contact is made from secondary winding, through shaft, to external leads.

Studer, P. A.↗

Evaluation of boundary lubricants using steady-state wear and friction

A friction and wear study was made at 20 C to establish operating limits and procedures for obtaining improved reproducibility and reliability in boundary lubrication testing. Ester base and C-other base fluids were used to lubricate a pure iron rider in sliding contact with a rotating M-50 steel disk in a pin-on-disk apparatus. Results of a parametric study with varying loads and speeds slowed that satisfactory test conditions for studying the direction and wear characteristics in the boundary lubrication regime with this test device were found to be 1 kilogram load; 7 to 9 meters-per-minute (50 rpm) surface speed; dry air test atmosphere (less than 100 ppm H2O); and use of a time stepwise procedure for measuring wear. Highly reproducible steady-state wear rates resulted from the two fluid studies which had a linearity of about 99 percent after initially higher wear rates and friction coefficients during run-in periods of 20 to 40 minutes.

Loomis, W. R.↗

Temperature gradients through EHD films and molecular alignment evidenced by infrared spectroscopy

Partial and complete emission band reversals have been observed in the infrared emission spectra from portions of operating sliding contacts. An elementary analysis has been carried out to show that partial reversals are due to temperature gradients in the fluid film - the film acts both as a radiation-emitter and absorber, and that total reversals - an emission spectrum appears as an absorption spectrum are likely to be due to a continuum source, such as hot solid asperities. The total energy radiated under the latter conditions exceeds that under the others. A decrease in gap width with increased load was accompanied by a dramatic spectral change in the case of 5P4E polyphenyl ether, which is indicative of molecular alignment.

King, V. W.↗

Surface chemistry, microstructure and friction properties of some ferrous-base metallic glasses at temperatures to 750 C

X-ray photoelectron spectroscopy analysis, transmission electron microscopy, diffraction studies, and sliding friction experiments were conducted with ferrous-base metallic glasses in sliding contact with aluminum oxide at temperatures from room to 750 C in a vacuum of 30 nPa. The results indicate that there is a significant temperature influence on the friction properties, surface chemistry, and microstructure of metallic glasses. The relative concentrations of the various constituents at the surface of the sputtered specimens were very different from the normal bulk compositions. Contaminants can come from the bulk of the material to the surface upon heating and impart boric oxide and silicon oxide at 350 C and boron nitride above 500 C. The coefficient of friction increased with increasing temperature to 350 C. Above 500 C the coefficient of friction decreased rapidly. The segregation of contaminants may be responsible for the friction behavior.

Miyoshi, K.↗

Tribological properties of sintered polycrystalline and single crystal silicon carbide

Tribological studies and X-ray photoelectron spectroscopy analyses were conducted with sintered polycrystalline and single crystal silicon carbide surfaces in sliding contact with iron at various temperatures to 1500 C in a vacuum of 30 nPa. The results indicate that there is a significant temperature influence on both the friction properties and the surface chemistry of silicon carbide. The main contaminants on the as received sintered polycrystalline silicon carbide surfaces are adsorbed carbon, oxygen, graphite, and silicon dioxide. The surface revealed a low coefficient of friction. This is due to the presence of the graphite on the surface. At temperatures of 400 to 600 C graphite and copious amount of silicon dioxide were observed on the polycrystalline silicon carbide surface in addition to silicon carbide. At 800 C, the amount of the silicon dioxide decreased rapidly and the silicon carbide type silicon and carbon peaks were at a maximum intensity in the XPS spectra. The coefficients of friction were high in the temperature range 400 to 800 C. Small amounts of carbon and oxygen contaminants were observed on the as received single crystal silicon carbide surface below 250 C. Silicon carbide type silicon and carbon peaks were seen on the silicon carbide in addition to very small amount of graphite and silicon dioxide at temperatures of 450 to 800 C.

Miyoshi, K.↗

Durable solid lubricant coatings for foil gas bearings to 315 deg C

The durability and friction characteristics of bonded solid lubricant films on compliant gas bearings were measured. Coating compositions, which were judged to be suitable for use to at least 315 C, were selected for this study. Most of the data were obtained with polyimide-bonded graphite fluoride coatings and with silicate-bonded graphite coatings. These coatings were applied to the bore of Inconel 750 foil bearings. The journals were A286 stainless steel, with a rms surface finish of 0.2 microns. The foils were subjected to repeated start/stop cycles under a 14 kPa (2 psi) bearing unit load. Sliding contact occurred during lift-off and coast down at surface velocities less than 6 m/s (3000 rpm). Testing continued until 9000 cycles were accumulated or until a rise in starting torque indicated that the coating had failed. The coatings were evaluated in the temperature range from 25 C to 315 C. Comparisons in coating performance as well as discussions of their properties and methods of application are given.

Wagner, R. C.↗

Effects of silver and group 2 fluorides addition to plasma sprayed chromium carbide high temperature solid lubricant for foil gas bearing to 650 deg C

A new self-lubricating coating composition of nickel aluminide-bonded chromium carbide formulated with silver and Group II fluorides was developed in a research program on high temperature solid lubricants. One of the proposed applications for this new coating composition is as a wide temperature spectrum solid lubricant for complaint foil gas bearings. Friction and wear properties were obtained using a foil gas bearing start/stop apparatus at temperatures from 25 to 650 C. The journals were Inconel 718. Some were coated with the plasma sprayed experimental coating, others with unmodified nickel aluminide/chromium carbide as a baseline for comparison. The addtitional components were provided to assist in achieving low friction over the temperature range of interest. Uncoated, preoxidized Inconel X-750 foil bearings were operated against these surfaces. The foils were subjected to repeated start/stop cycles under a 14-kPa (2-psi) bearing unit loading. Sliding contact occurred during lift-off and coastdown at surface velocities less than 6 m/s (3000 rpm). Testing continued until 9000 start/stop cycles were accumulated or until a rise in starting torque indicated the journal/bearing had failed. Comparison in coating performance as well as discussions of their properties and methods of application are given.

Wagner, R. C.↗

Analytical and experimental investigation of rubbing interaction in labyrinth seals for a liquid hydrogen fuel pump

Cracking of the titanium knife edges on the labyrinth seals of the liquid hydrogen fuel pump in the Space Shuttle main engine is considered. Finite element analysis of the thermal response of the knife edge in sliding contact with the wear ring surface shows that interfacial temperatures can be quite high and they are significantly influenced by the thermal conductivity of the surfaces in rubbing contact. Thermal shock experiments on a test specimen similar to the knife edge geometry demonstrate that cracking of the titanium alloy is possible in a situation involving repeated thermal cycles over a wide temperature range, as might be realized during a rub in the liquid hydrogen fuel pump. High-speed rub interaction tests were conducted using a representative knife edge and seal geometry over a broad range of interaction rates and alternate materials were experimentally evaluated. Plasma-sprayed aluminum-graphite was found to be significantly better than presently used aluminum alloy seals from the standpoint of rub performance. Ion nitriding the titanium alloy knife-edges also improved rub performance compared to the untreated baseline.

Dolan, F. X.↗