Effects of Static Recrystallization and Precipitation on Mechanical Properties of 00Cr12 Ferritic Stainless Steel

The 00Cr12 ferritic stainless steel samples were isothermally held at different temperatures in the range of 700 °C to 1000 °C to investigate the effect of static recrystallization and precipitation on mechanical properties, such as microhardness, tensile strength, and yield strength. The results show that the formation of the fine recrystallized grain, as well as precipitation, coarsening, and dissolution of the second-phase particles, influences the mechanical properties remarkably. The fine recrystallized grain can provide a positive grain boundary-strengthening effect in the sample under a relatively high holding temperature. Coarsening and dissolution of M{sub 23}C{sub 6} result in partial depletion of precipitate hardening. In contrast, the size and number density of MX particles are almost constant, regardless of the holding temperature; therefore, it can provide a better precipitation-hardening effect.

36 MATERIALS SCIENCE↗

Stainless Steel Coating Test Report

A process was developed to coat 316L stainless steel pieces having very low levels of fixed contamination on their surface (~100 dpm/100 cm²). The coating process served to significantly decrease the likelihood of any fixed contamination becoming loose contamination due to physical shocks. Prior to coating, the stainless steel was etched with a commercial methane sulfonic acid (MSA) solution in a heated ultrasonic bath, rinsed with deionized water, cleaned with a basic detergent solution, and then rinsed with deionized water. The MSA etched the surface of the stainless-steel pieces, creating a more favorable surface on which the coating could adhere. Due to the short timeline of the project, only commercially available clear coating products were considered. The clear coating had to be wear-resistant, shock resistant, radiation resistant, and have high adhesion to the surface of the stainless steel. Adhesion of coatings to stainless steel is notoriously difficult. A commercial, high molecular weight polymer coating was found that met these requirements. The adhesion properties of this coating to stainless steel are very good, and are significantly improved by the etching process. The etching process results in a higher surface area that is free of debris and other residues, making the surface much more wetable, and at the same time creating a favorable surface topography for adhesion. The polymer in its uncured form is a low viscosity liquid. It can be applied by brush or pipette, and it cures in air alone, but heat is required to speed up curing and attain the highest performance of the cured polymer. As the project progressed, the project team became interested in the composition of the selected commercial polymer coating, and in ways that this polymer coating could be made more wear resistant and potentially more radiation resistant. Nano-particle addition was chosen as the preferred way to achieve higher performance. Therefore, a series of tests were planned and performed. This report summarizes these tests, and presents the results.

36 MATERIALS SCIENCE↗

Recrystallization and modification of the stainless-steel surface relief under photonic heat load in powerful plasma discharges

Targets made of ITER-grade 316L(N)-IG stainless steel and Russian-grade 12Cr18Ni10Ti stainless steel with a close composition were exposed at the QSPA-T plasma gun to plasma photonic radiation pulses simulating conditions of disruption mitigation in ITER. After a large number of pulses, modification of the stainless-steel surface was observed, such as the formation of a wavy structure, irregular roughness, and cracks on the target surface. X-ray and optic microscopic analyses of targets revealed changes in the orientation and dimensions of crystallites (grains) over a depth of up to 20 μm for 316L(N)-IG stainless steel after 200 pulses and up to 40 μm for 12Cr18Ni10Ti stainless steel after 50 pulses, which is significantly larger than the depth of the layer melted in one pulse (∼10 μm). In a series of 200 tests of ITER-grade 316L(N)-IG ITER stainless steel, a linear increase in the height of irregularity (roughness) with increasing number of pulses at a rate of up to ∼1 μm per pulse was observed. No alteration in the chemical composition of the stainless-steel surface in the series of tests was revealed. A model is developed that describes the formation of wavy irregularities on the melted metal surface with allowance for the nonlinear stage of instability of the melted layer with a vapor/plasma flow above it. A decisive factor in this case is the viscous flow of the melted metal from the troughs to tops of the wavy structure. The model predicts saturation of the growth of the wavy structure when its amplitude becomes comparable with its wavelength. Approaches to describing the observed stochastic relief and roughness of the stainless-steel surface formed in the series of tests are considered. The recurrence of the melting-solidification process in which mechanisms of the hill growth compete with the spreading of the material from the hills can result in the formation of a stochastic relief.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Marine Atmospheric Corrosion of Additively Manufactured Stainless Steels

Additively manufactured (AM) stainless steels exhibit numerous microstructural differences compared to their wrought counterparts, such as Cr enriched dislocation cell structures. The influence these unique features have on a SSs corrosion resistance are still under investigation with most current works limited to laboratory experiments. The work herein shows the first documented study of AM 304L and 316L exposed to a severe marine environment on the eastern coast of Florida with comparisons made to wrought counterparts. Coupons were exposed for 21 months and resulted in significant pitting corrosion to initiate after 1 month of exposure for all conditions. At all times, the AM coupons exhibited lower average and maximum pit depths than their wrought counterparts. After 21 months, pits on average were 4 μm deep for AM 316L specimen and 8 μm deep for wrought specimen. Pits on the wrought samples tended to be nearly hemispherical and polished with some pits showing crystallographic attack while pits on AM coupons exhibited preferential attack at melt pool boundaries and the cellular microstructure.

36 MATERIALS SCIENCE↗

In-situ Characterization of Cast Stainless Steel Microstructures

Cast austenitic stainless steel (CASS) was commonly used in selected designs of nuclear power reactor systems for corrosion resistance and enhanced durability in service. CASS materials are generally coarse-grained and elastically anisotropic in nature, and are consequently difficult to inspect ultrasonically, largely due to detrimental effects of ultrasonic wave interactions with the coarse-grain microstructures. To address the inspection needs for these materials, new approaches that are robust to these phenomena are being developed. However, to enhance the probability of detecting flaws, knowledge of the microstructure and the corresponding acoustic properties of the material may be required. This paper discusses the application of ultrasonic backscatter measurement methods for classifying the microstructure of CASS components, when making measurements from the outside surface of the pipe or component. Results to date from laboratory experiments demonstrate the potential of these measurements to classify the material type of CASS for two homogeneous microstructures—equiaxed-grain material or columnar-grain material. Measurements on mixed or banded microstructures also show correlation with the estimated volume-fraction of columnar grains in the material. However, several operational issues will need to be addressed prior to applying this method for in-situ characterization of CASS microstructure.

CASS↗

Methods for the In-Situ Characterization of Cast Austenitic Stainless Steel Microstructures

Cast austenitic stainless steel (CASS) that was commonly used in U.S. nuclear power plants is a coarse-grained, elastically anisotropic material. Its engineering properties made it a material of choice for selected designs of nuclear power reactor systems. However, the fabrication processes result in a variety of coarse-grain microstructures that make current ultrasonic in-service inspection of components quite challenging. To address inspection needs, new ultrasonic inspection approaches are being sought. However, overcoming the deleterious and variable effects of the microstructure on the interrogating ultrasonic beam may require knowledge of the microstructure, for potential optimization of inspection parameters to enhance the probability of detection (POD). The ability to classify microstructure type (e.g. polycrystalline or columnar) has the potential to guide selection of optimal NDE approaches. This paper discusses the application of ultrasonic and electromagnetic methods for classifying CASS microstructures, when making measurements from the outside surface of the component. Results to date demonstrate the potential of these measurements to discriminate between two consistent microstructures - equiaxed-grain material versus columnar-grain material. The potential for fusion of ultrasonic and electromagnetic measurements for in-situ microstructure characterization in CASS materials will be explored.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Stainless Steel to Titanium Bimetallic Transitions

In order to use stainless steel piping in an LCLS-II (Linac Coherent Light Source Upgrade) cryomodule, stainless steel to titanium bimetallic transitions are needed to connect the stainless steel piping to the titanium cavity helium vessel. Explosion bonded stainless steel to titanium transition pieces and bimetallic transition material samples have been tested. A sample transition tube was subjected to tests and x-ray examinations between tests. Samples of the bonded joint material were impact and tensile tested at room temperature as well as liquid helium temperature. The joint has been used successfully in horizontal tests of LCLS-II cavity helium vessels and is planned to be used in LCLS-II cryomodules. Results of material sample and transition tube tests will be presented.

43 PARTICLE ACCELERATORS↗

Hydrogen effects on the deformation and slip localization in a single crystal austenitic stainless steel

Hydrogen is known to embrittle austenitic stainless steels, which are widely used in high-pressure hydrogen storage and delivery systems, but the mechanisms that lead to such material degradation are still being elucidated. The current work investigates the deformation behavior of single crystal austenitic stainless steel 316L through combined uniaxial tensile testing, characterization and atomistic simulations. Thermally precharged hydrogen is shown to increase the critical resolved shear stress (CRSS) without previously reported deviations from Schmid’s law. Molecular dynamics simulations further expose the statistical nature of the hydrogen and vacancy contributions to the CRSS in the presence of alloying. Slip distribution quantification over large in-plane distances (> 1 mm), achieved via atomic force microscopy (AFM), highlights the role of hydrogen increasing the degree of slip localization in both single and multiple slip configurations. The most active slip bands accumulate significantly more deformation in hydrogen precharged specimens, with potential implications for damage nucleation. For $\langle$110$\rangle$ tensile loading, slip localization further enhances the activity of secondary slip, increases the density of geometrically necessary dislocations and leads to a distinct lattice rotation behavior compared to hydrogen-free specimens, as evidenced by electron backscatter diffraction (EBSD) maps. Finally, the results of this study provide a more comprehensive picture of the deformation aspect of hydrogen embrittlement in austenitic stainless steels.

36 MATERIALS SCIENCE↗

Methods of Measuring Residual Stresses in Additively Manufactured 316L Stainless Steel

The microstructure of AM 316L stainless steel Is different from steel manufactured using conventional methods e.g. casting and forging. Data on the effects of residual stresses in the structural integrity and importance of AM parts (fatigue behavior) must be quantified. Evaluate different methods and identify a viable process for determining residual stresses in 316L stainless steel. Next step is to conduct measurements of residual stresses of samples fabricated by different manufacturers.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Corrosion of 316L & 316H stainless steel in molten LiF-NaF-KF (FLiNaK)

The corrosion behavior of 316L and 316H stainless steels (low and high carbon, respectively) in molten LiF-NaF-KF (FLiNaK) salt at 700 °C for 500 h has been investigated. Tests were performed in 316L stainless steel, pyrolytic boron nitride, and glassy carbon capsule materials. The capsule material had a notable effect on the corrosion behavior of the two stainless steels. Further, the modes of corrosion for the two types of stainless steel in various capsule materials were classified into three categories, namely, uniform surface recession, selective grain boundary Cr dissolution, and the dissolution of Cr in the bulk grains. By most metrics, the 316H stainless steel exhibited slightly superior corrosion resistance, while by others the two stainless steels were comparable. These differences in corrosion behavior are attributed to the differences in grain size and the degree of sensitization.

36 MATERIALS SCIENCE↗

Synergistic Computational and Microstructural Design of Next- Generation High-Temperature Austenitic Stainless Steels

The purpose of this project was to: 1) study deformation twinning, its evolution, thermal stability, and the contribution on mechanical response of the new advanced stainless steels, especially at elevated temperatures; 2) study alumina-scale formation on the surface, as an alternative for conventional chromium oxide, that shows better oxidation resistance, through alloy design; and 3) design new generation of high temperature stainless steels that form alumina scale and have thermally stable nano-twins. The work involved few baseline alloys for investigating the twin formation under tensile loading, thermal stability of these twins, and the role of deformation twins on the mechanical response of the alloys. These baseline alloys included Hadfield Steel (Fe-13Mn-1C), 316, 316L and 316N stainless steels. Another baseline alloy was studied for alumina-scale formation investigations. Hadfield steel showed twinning but undesired second phases formed at higher temperatures. 316N stainless steel did not show signs of deformation twinning. Conventional 316 stainless steel demonstrated extensive deformation twinning at room temperature. Investigations on this alloy, both in single crystalline and polycrystalline forms, showed that deformation twins evolve in a hierarchical manner, consisting of micron–sized bundles of nano-twins. The width of nano-twins stays almost constant as the extent of strain increases, but the width and number of the bundles increase with increasing strain. A systematic thermomechanical cycling study showed that the twins were stable at temperatures as high as 900°C, after the dislocations are annealed out. Using such cycles, volume fraction of the thermally stable deformation twins were increased up to 40% in 316 stainless steel. Using computational thermodynamics and kinetics calculations, we designed two generations of advanced austenitic stainless steels. In the first generation, Alloy 1, which had been proposed as an alumina-forming austenitic stainless steel, is fully austenitic, but possesses carbides that were not dissolvable and could not be controlled. This alloy also did not show deformation twinning. Alloy 2 was designed based on alloy 1, but was not fully austenitic and had significant traces of uncontrollable precipitates as well. Alloy 3, also designed based on alloy 1, was mainly austenitic with evolution of a second phase along the grain boundaries, but also had precipitates that were not controllable. Based on the knowledge gained from the first generation of the designed steels, two more steels, called PGAA1 and PGAA2, were proposed using genetic algorithms that, based on the modelling, were supposed to exhibit alumina-scale formation. PGAA1, however, did not demonstrate a fully austenitic structure. PGAA2 could achieve a mostly austenitic structure through thermo-mechanical processing, and was then used for oxidation tests. The oxidation tests of PGAA2, with and without nitrogen impurities, along with alloy 1, suggested that PGAA2 can form alumina-scale similar to alloy 1, but N impurity will prevent formation of such a scale, probably through formation of aluminum nitrides. For the above mentioned genetic algorithm framework of alloy design, separate models were developed for specific design criteria. For prediction of alumina formation in stainless steels, a model was constructed based off of two criteria – effective valence and third element effect. These criteria capture the thermodynamics and kinetics of alumina formation in steels. To test the efficacy and robustness of this model, they were tested against alloys in the literature which had been experimentally verified to exhibit alumina formation and the predictions were in excellent agreement with the experiments. Another meta-model for prediction of twinning in unknown steel compositions was developed by an informatics based machine learning/data mining approach. Stacking Fault Energy data was captured from the literature for a large number of steel compositions and then this data was used to build a classifier to predict deformation mechanisms. Here a training set-test set based analysis was performed to test performance. The above genetic algorithm based optimization framework for alloy design was exhibited to be a successful methodology for accelerated materials discovery in the context of alloy design.

36 MATERIALS SCIENCE↗

The fatigue evaluation method for a structural stainless steel using the magnetic sensor composed of three pancake coils

May metallic structural materials, such as stainless steels, are currently used in our surroundings. If external force is repeatedly added for many years, it is thought that fatigue damage accumulates in stainless steels. When excessive fatigue damage accumulates in these metals, there is a possibility that they are destroyed by fatigue damage accumulation. Therefore, it is important to know the amount of the fatigue damage they have suffered in order to prevent them from being destroyed. We are developing the fatigue evaluation method for stainless steels with a magnetic sensor composed of three pancake type coils. In this research, the inspection object is ferritic stainless steels such as SUS430. The method of fatigue evaluation for ferritic stainless steels uses the three coil type sensor, and shows a good correlation between the number of stress cycles and the output signal of the sensor, even though the correlation between the output signal and an added stress is not completely accurate. This paper describes the evaluation method of fatigue damage in ferritic stainless steel using a magnetic sensor composed of three pancake-type coils.

36 MATERIALS SCIENCE↗

Identification of the mechanism that confers superhydrophobicity on 316L stainless steel

This study develops a rapid method to confer superhydrophobicity on 316L stainless steel surfaces with an amphiphilic reagent such as dodecanoic acid. The highest contact angle (approaching 173°) was obtained after forming hierarchical structures with a non-aqueous electrolyte by an electrolytic process. Our goal was to induce superhydrophobicity directly on 316L stainless steel substrates and to establish which molecules cause the effect. The superhydrophobic behaviour is analysed by contact angle measurements, scanning electron microscopy (SEM), IR spectroscopy and atomic force microscopy (AFM). The growth mechanism is analysed using FE-SEM, TOF-SIMS and XPS in order to determine the molecules involved in the reaction and the growth. The TOF-SIMS analysis revealed that the Ni{sup 2+} ions react with lauric acid to create an ester on the stainless steel surface. - Highlights: • This study develops a rapid and facile approach to impart superhydrophobicity properties to 316L stainless steel surfaces with an amphiphilic reagent such as dodecanoic acid. Surface character changes from superhydrophilicity to superhydrophobicity. • This process changes the surface character from superhydrophilicity to superhydrophobicity. • The process based on electrolysis of a nickel salt in lauric acid provides superhydrophobic behaviour in 316L stainless steel. • The growth mechanism is proposed as a mode island (Volmert- Weber mode). • TOF-SIMS and XPS provided the identification of the molecules involved in the surface modification reaction on AISI 316L inducing superhydrophobicity.

36 MATERIALS SCIENCE↗

Stainless steel anodes for alkaline water electrolysis and methods of making

The corrosion resistance of stainless steel anodes for use in alkaline water electrolysis was increased by immersion of the stainless steel anode into a caustic solution prior to electrolysis. Also disclosed herein are electrolyzers employing the so-treated stainless steel anodes. The pre-treatment process provides a stainless steel anode that has a higher corrosion resistance than an untreated stainless steel anode of the same composition.

25 ENERGY STORAGE↗

Side-by-side evaluation of the outgassing rate and ultimate pressure achieved inside tubes made of low-carbon and stainless steel

The hydrogen outgassing rate of a vacuum chamber made of AISI 1020 low-carbon steel was found to be notably smaller than a similar chamber made of AISI 316L stainless steel following heat treatment at 150 °C. When the chambers were baked at 400 °C, the outgassing rate of the 1020 low-carbon steel chamber was approximately 2000 times smaller than that of the 316L stainless-steel chamber. After quantifying hydrogen outgassing rates, vacuum chambers made of 1020 low-carbon steel and 316L stainless steel were heated for a prescribed duration and then pumped with an ion pump and nonevaporable getter pump to reach “ultimate pressure.” The 1020 low-carbon steel chamber reached lower pressures than the 316L stainless-steel chamber. Monte Carlo simulation predictions using the measured hydrogen outgassing rates are in good agreement with the ultimate pressure measurements. Finally, our measurements indicate that low-carbon steel can provide pressures within the extreme high vacuum range (<7.5 × 10 -13 Torr) if care is taken to minimize the surface area contribution from stainless steel.

36 MATERIALS SCIENCE↗

Electroless Plated Nanodiamond Coating for Stainless Steel Passivation

Tritium gas sample bottles and manifold components require passivation surface treatments to minimize the interaction of the hydrogen isotopes with surface contamination on the stainless steel containment materials. This document summarizes the effort to evaluate electroless plated nanodiamond coatings as a passivation layer for stainless steel. In this work, we developed an electroless nanodiamond (ND)-copper (Cu) coating process to deposit ND on stainless steel parts with the diamond loadings of 0%, 25% and 50% v/v in a Cu matrix. The coated Conflat Flanged Vessel Assemblies (CFVAs) were evaluated on surface morphology, composition, ND distribution, residual hydrogen release, and surface reactivity with deuterium. For as-received Cu and ND-Cu coated CFVAs, hydrogen off-gassing is rapid, and the off-gas rates of H 2 was one to two orders of magnitude higher than that for both untreated and electropolished stainless steel CFVAs, and hydrogen and deuterium reacted to form HD as well. These results indicated that residual H 2 was entrapped in the Cu and ND-Cu coated CFVAs during the coating process, and moisture was adsorbed on the surface, and ND and/or Cu might facilitate catalytic isotope exchange reaction for HD formation. However, hydrocarbons (i.e., CH 3 ) did not form, and did not appear to be an issue for the Cu and ND-Cu coated CFVAs. After vacuum heating, residual H 2 and adsorbed H 2 O in the Cu and ND-Cu coated CFVAs were dramatically reduced. The H 2 off-gassing rate after the vacuum treatment of Cu and 50% ND-Cu coated CFVAs was on the level of 10 -14 l mbar/s cm 2 , while H 2 O off-gas rate was on the level of 10 -15 l mbar/s cm 2 , consistent with the untreated or electropolished stainless steel CFVA, but the HD formation remained. The Restek EP bottle was used as a reference for this work. The Restek Electro-Polished (EP) bottle and their SilTek coated bottles tested under a different research project exhibited very little hydrogen off-gassing and unmeasurable HD formation. ND and Cu were initially chosen to develop improved passivation technology, because Cu has a lower permeability of hydrogen, and diamond is more inert than other materials under a hydrogen atmosphere. However, our tests demonstrated that even after an 8-18 day vacuum extraction heat treatment, the electroless plated Cu and ND-Cu coated stainless steel CFVAs exhibited H 2 off-gassing rates that were just comparable to those for the untreated or electropolished stainless steel CFVA, and the HD formation was still observed. Thus, the Restek Electro-Polished (EP) bottle outperformed the electroless plated Cu and ND-Cu coated stainless steel CFVAs, and the electroless plated nanodiamond coating is not promising as a surface passivation technology. However, the ND-Cu coating may be beneficial to another application in which catalyzing the H 2 -D 2 exchange reaction is desired.

08 HYDROGEN↗

Investigation of annealing temperature on microstructure and texture of Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel

Highlights: • Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel was investigated. • Shear bands provided recrystallization nucleation sites. • Annealing temperature can affect microstructure and texture. • r-bar increased to a maximum value (1.69) and then decreased to 1.42. - Abstract: The evolution of microstructure and texture of Fe-19Cr-2Mo-Nb-Ti ferritic stainless steel annealed at different temperatures was investigated using a combination of X-ray diffraction (XRD) and electron backscatter diffraction (EBSD). EBSD investigations confirm that the in-grain shear bands provide more recrystallization nucleation sites to γ-fiber recrystallization grains with high Taylor factor orientations during cold rolling requiring further annealing for a more homogenous equiaxied grain structure. As the annealing temperatures increase, the grains in center layer are oriented towards {110}∥ND, and the recrystallization grains at 1050 °C are dominated by the uniform and equiaxial γ-fiber grains favourable for the improvement of r-values, while the occurrence of {100} <011> texture detrimental to r-values indicates that an exorbitant annealing temperature can reduce the intensity of γ-fiber textures affecting the formability, accordingly, the average plastic strain ratio of ferritic stainless steel increases sharply up to a maximum value (1.69) and then decreases to a certain value (1.42).

36 MATERIALS SCIENCE↗

Degradation of impact toughness in cast stainless steels during long-term thermal aging

Cast austenitic stainless steels (CASSs) have been extensively used for the large components of nuclear reactor primary coolant systems. Since the cast steels inevitably contain degradable metastable phases and replacement of the large coolant system components is impractical, the thermal embrittlement of CASS components has been a serious concern in the extended-term operation of nuclear power plants. This study aimed to systematically measure and analyze the effect of long-term thermal aging on the Charpy impact toughness to provide a comprehensive understanding of thermal degradation behavior and a practical aging model to predict the degree of thermal degradation in the cast stainless steels. Additionally, the materials tested in the research include eight CASS alloys (two CF3s, one CF3M, three CF8s, and two CF8Ms) and two reference wrought materials (304L and 316L), in which the nominal δ-ferrite content ranges from ~2% to 33%. These stainless steels have been thermally aged at two light water reactor (LWR) temperatures (290 and 330 °C) and at two accelerated-aging temperatures (360 and 400 °C) for up to 30,000 h; these include both under-aged and over-aged conditions relative to the extended service lifetime (80 years). Charpy impact testing was performed for aged and non-aged specimens, and the impact (absorbed) energy parameters were correlated with a new aging parameter (A). Both the reduction of impact fracture toughness and the shift of ductile-brittle transition temperature were strongly dependent on the δ-ferrite content and degree of thermal aging. A linear relationship was found between the increasing rate of the index transition temperature T 41J and aging parameter A; base on which an empirical model was proposed for prediction of the transition temperature as a simple function of the aging parameter (A) and δ-ferrite content (F). Finally, the critical aging parameter for embrittlement (AC) was evaluated and compared with the existing δ-ferrite content criteria.

36 MATERIALS SCIENCE↗