Improving the Pitting Corrosion Performance of Additively Manufactured 316L Steel Via Optimized Selective Laser Melting Processing Parameters
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
The evaluation of simple thermal model of selective laser melting (SLM) process shows that the temperature distribution in the sample is characterized by two dimensionless parameters: normalized enthalpy and the ratio of dwell time to the thermal diffusion time. Here we demonstrated that the melt depth data taken for different machines for different materials collapsed in one curve, making possible to rescale the optimal processing parameters between the different materials and machines. The melt pool depth, width and the length are the universal function of these two parameters. Within the operational range of parameters for SLM these functions can be interpolated by the simple algebraic expressions given the possibility to reduce the calculation of the melt pool characteristic to spreadsheet model.
FeSiB alloys have been fabricated by selective laser melting (SLM) using a laser scan rate of 0.1–1.5 m/s, laser power of 90 W, scan line spacing of 40 μ m, and layer thickness of 50 μ m. X-ray diffraction, scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy, atomic force microscopy, profilometer, microdurometer, and vibrating sample magnetometer have been used to investigate the structural, microstructural, roughness, microhardness, and magnetic property changes during the laser melting process. The produced samples exhibit a nanocomposite structure consisting of nanocrystalline α-Fe{sub 0.95}Si{sub 0.05} and Fe{sub 2}B phases embedded into an amorphous ε-FeSi-type matrix. The selective laser-melted samples show high density, low surface roughness, higher microhardness values (1654–2273 Hv), and soft magnetic properties (M{sub s} = 188.6–199 emu/g and H{sub c} = 43.8–73 Oe).
Selective laser melting (SLM) is one of the additive manufacturing (AM) process that utilizes laser for selectively melting and fusing of a thin layer of powder. This technique allows manufacturing a part directly from computer-aided design (CAD) models by dividing the part into a set of two-dimensional slices, which are built sequentially on top of another. Here, SLM technology enables manufacturing of complex geometries, such as parts with inner cooling channels which could be difficult or time consuming to make by conventional manufacturing processes.
Additive manufacturing is a transformative technology with the potential to manufacture designs which traditional subtractive machining methods cannot. Additive manufacturing offers fast builds at near final desired geometry; however, material properties and variability from part to part remain a challenge for certification and qualification of metallic components. AM induced metallic microstructures are spatially heterogeneous and highly process dependent. Engineering properties such as strength and toughness are significantly affected by microstructure morphologies resulting from the manufacturing process Linking process parameters to microstructures and ultimately to the dynamic response of AM materials is critical to certifying and qualifying AM built parts and components and improving the performance of AM materials. The AM fabrication process is characterized by building parts layer by layer using a selective laser melt process guided by a computer. A laser selectively scans and melts metal according to a designated geometry. As the laser scans, metal melts, fuses, and solidifies forming the final geometry in a layerwise fashion. As the laser heat source moves away, the metal cools and solidifies forming metallic microstructures. This work describes a microstructure modeling application implemented in the SPPARKS kinetic Monte Carlo computational framework for simulating the resulting microstructures. The application uses Bzier curves and surfaces to model the melt pool surface and spatial temperature profile induced by moving the laser heat source; it simulates the melting and fusing of metal at the laser hot spot and microstructure formation and evolution when the laser moves away. The geometry of the melt pool is quite flexible and we explore effects of variances in model parameters on simulated microstructures.
Selective laser melting is a powder-based, additive-manufacturing process where a threedimensional part is produced, layer by layer, by using a high-energy laser beam to fuse the metallic powder particles. A particular challenge in this process is the selection of appropriate process parameters that result in parts with desired properties. In this study, we describe an approach to selecting parameters for high density (>99%) parts using 316L stainless steel. Though there has been significant success in achieving near-full density for 316L parts, this work has been limited to laser powers <225W. We discuss how we can exploit prior knowledge, design of computational experiments using a simple model of laser melting, and single-track experiments to determine the process parameters for use at laser powers up to 400W. Our results show that, at higher power values, there is a large range of scan speeds over which the relative density remains >99%, with the density reducing rapidly at high speeds due to insufficient melting, and less rapidly at low speeds due to the effect of voids created as the process enters keyhole mode.
The elasto-plastic material behavior, material strength and failure modes of metals fabricated by additive manufacturing technologies are significantly determined by the underlying process-specific microstructure evolution. In this work a novel physics-based and data-supported phenomenological microstructure model for Ti-6Al-4V is proposed that is suitable for the part-scale simulation of laser powder bed fusion processes. The model predicts spatially homogenized phase fractions of the most relevant microstructural species, namely the stable β-phase, the stable α s -phase as well as the metastable Martensite α m -phase, in a physically consistent manner. In particular, the modeled microstructure evolution, in form of diffusion-based and non-diffusional transformations, is a pure consequence of energy and mobility competitions among the different species, without the need for heuristic transformation criteria as often applied in existing models. The mathematically consistent formulation of the evolution equations in rate form renders the model suitable for the practically relevant scenario of temperature- or time-dependent diffusion coefficients, arbitrary temperature profiles, and multiple coexisting phases. Due to its physically motivated foundation, the proposed model requires only a minimal number of free parameters, which are determined in an inverse identification process considering a broad experimental data basis in form of time-temperature transformation diagrams. Subsequently, the predictive ability of the model is demonstrated by means of continuous cooling transformation diagrams, showing that experimentally observed characteristics such as critical cooling rates emerge naturally from the proposed microstructure model, instead of being enforced as heuristic transformation criteria. Eventually, the proposed model is exploited to predict the microstructure evolution for a realistic selective laser melting application scenario and for the cooling/quenching process of a Ti-6Al-4V cube of practically relevant size. Numerical results confirm experimental observations that Martensite is the dominating microstructure species in regimes of high cooling rates, e.g., due to highly localized heat sources or in near-surface domains, while a proper manipulation of the temperature field, e.g., by preheating the base-plate in selective laser melting, can suppress the formation of this metastable phase.
Innovative designs for turbines can be achieved by advances in nickel-based superalloys and manufacturing methods, including the adoption of additive manufacturing. In this regard, selective electron beam melting (SEBM) and selective laser melting (SLM) of nickel-based superalloys do provide distinct advantages. Furthermore, the direct energy deposition (DED) processes can be used for repair and reclamation of nickel alloy components. The current paper explores opportunities for innovation and qualification challenges with respect to deployment of AM as a disruptive manufacturing technology. Here in the first part of the paper, fundamental correlations of processing parameters to defect tendency and microstructure evolution will be explored using DED process. In the second part of the paper, opportunities for innovation in terms of site-specific control of microstructure during processing will be discussed. In the third part of the paper, challenges in qualification of AM parts for service will be discussed and potential methods to alleviate these issues through in situ process monitoring, and big data analytics are proposed.
High-cycle fatigue (HCF) tests were conducted on samples fabricated by two powder-bed additive manufacturing techniques. Samples were tested with as-produced surfaces and after various non-contact surface improvement treatments. Ti-6Al-4V samples were made using both electron beam melting (EBM) and selective laser melting (SLM), while Inconel 625 was fabricated using SLM. Ti-6Al-4V was treated with a commercial chemically accelerated vibratory polishing process, with target material removal of approximately 200 µm from each surface for EBM samples and 100 µm for SLM samples. This technique led to increases in both the number of cycles before failure at a given loading condition and endurance limit (at 10{sup 7} cycles) compared to samples with as-produced surfaces. The results are interpreted as the reduction in elastic stress concentration factor associated with surface defects where fatigue cracks initiate. SLM 625 was treated with both an abrasive polishing method and laser surface remelting. Both methods led to improvements in surface roughness, but these did not lead to improvements in fatigue properties of SLM 625. For abrasive polished samples, the combination of improved measured surface roughness without fatigue property enhancement suggests that surface material is removed, but the roots of surface defects, where fatigue cracks initiate, were left intact. For laser treatment, the remelted surface layer retained a rapidly solidified microstructure that did not increase the number of cycles before crack initiation even though the surface was smoother compared to the surface prior to polishing.
Characterization of the bulk microstructure using neutron diffraction has been applied to investigate the phase fractions and textures of α- and β-phases in Ti-6Al-4V fabricated by additive manufacturing. The microstructure of a specimen cut from a fan structure, built by either electron beam melting (EBM) or selective laser melting, indicated that predominantly the build direction and not the fan angle determines the microstructure. In situ heating experiments of specimens from a rod built using EBM provided insight into the lattice strain, phase fraction, and texture evolution, providing a rich picture of the microstructure changes during heat treatment of additively manufactured Ti-6Al-4V. Finally, a remarkably low weight fraction of β-phase at lower temperatures, deviations from thermal expansion behavior attributed to vanadium repartitioning, as well as texture strengthening were observed.
Additive manufacturing (AM) allows for the fabrication of complex near net shape components, leading to new design opportunities and significant savings, for example by decreasing tooling and materials cost or by accelerating prototype development. New Ni-based alloy heat exchangers with thin-walled areas exposed to hot gases will, however, suffer from corrosion degradation, and the high temperature oxidation performance of AM alloys needs to be addressed. Alloy N06002 (Ni-22Cr-18Fe-9Mo) fabricated by electron beam melting (EBM) and selective laser melting (SLM) along with EBM-fabricated N07247 and modified N07247 were cyclic oxidation tested at 950°C in air and humid air for durations ranging from 100 h to 5000 h. Increased spallation rates were observed initially for the AM N06002 alloys in comparison with wrought N06002 alloy because of the AM alloy specific microstructures. After ~2000 h, the situation was reversed with significant spallation observed for the wrought HX alloy only. Low mass gains were observed for the EBM N07247 alloys at 950°C, but thick oxide scales were observed locally due to the presence of oxidized cracks. Massive oxidation of these cracks led to fast oxidation rates at 1100°C.
Multi-material processing in selective laser melting using a novel approach, by the separation of two different materials within a single dispensing coating system was investigated. 316L stainless steel and UNS C18400 Cu alloy multi-material samples were produced using selective laser melting and their interfacial characteristics were analyzed using focused ion beam, scanning electron microscopy, energy dispersive spectroscopy and electron back scattered diffraction techniques. A substantial amount of Fe and Cu element diffusion was observed at the bond interface suggesting good metallurgical bonding. Quantitative evidence of good bonding at the interface was also obtained from the tensile tests where the fracture was initiated at the copper region. Nevertheless, the tensile strength of steel/Cu SLM parts was evaluated to be 310 ± 18 MPa and the variation in microhardness values was found to be gradual along the bonding interface from the steel region (256 ± 7 HV{sub 0.1}) to the copper region (72 ± 3 HV{sub 0.1}). - Highlights: • Multi-material processing was successfully implemented and demonstrated in SLM. • Bi-metallic laminates of steel/Cu were successfully produced with the SLM process. • A substantial amount of Fe and Cu diffusion was observed at the bond interface. • Good metallurgical bonding was obtained at the interface of the steel/Cu laminates. • Highly refined microstructure was obtained due to rapid solidification in SLM.
Selective Laser Melting is utilized to build metallic parts directly from CAD-Data by solidification of thin powder layers through application of a fast scanning laser beam. In this study layerwise monitoring of the temperature distribution is used to gather information about the process stability and the resulting part quality. The heat distribution varies with different kinds of parameters including scan vector length, laser power, layer thickness and inter-part distance in the job layout which in turn influence the resulting part quality. By integration of an off-axis mounted uncooled thermal detector the solidification as well as the layer deposition are monitored and evaluated. Errors in the generation of new powder layers usually result in a locally varying layer thickness that may cause poor part quality. For effect quantification, the locally applied layer thickness is determined by evaluating the heat-up of the newly deposited powder. During the solidification process space and time-resolved data is used to characterize the zone of elevated temperatures and to derive locally varying heat dissipation properties. Potential quality indicators are evaluated and correlated to the resulting part quality: Thermal diffusivity is derived from a simplified heat dissipation model and evaluated for every pixel and cool-down phase of a layer. This allows the quantification of expected material homogeneity properties. Maximum temperature and time above certain temperatures are measured in order to detect hot spots or delamination issues that may cause a process breakdown. Furthermore, a method for quantification of sputter activity is presented. Since high sputter activity indicates unstable melt dynamics this can be used to identify parameter drifts, improper atmospheric conditions or material binding errors. The resulting surface structure after solidification complicates temperature determination on the one hand but enables the detection of potential surface defects on the other hand. These issues and proper key figures for thermographic monitoring of the Selective Laser Melting process are discussed in the paper. Even though microbolometric temperature measurement is limited to repetition rates in the Hz-regime and sub megapixel resolution, current results show the feasibility of process surveillance by thermography for a limited section of the building platform in a commercial system.
Not Available
Most metal additive manufacturing approaches are based on powder-bed melting techniques such as laser selective melting or electron beam melting, which often yield uncontrolled microstructures with defects (e.g., pores or microcracks) and residual stresses. Here, we introduce a proof-of-concept prototype of a 3D metal freeform fabrication process by direct writing of metallic alloys in the semi-solid regime. This process is achieved through controlling the particular microstructure and the rheological behavior of semi-solid alloy slurries, which demonstrate a well suited viscosity and a shear thinning property to retain the shape upon printing. Furthermore, the ability to control the microstructure through this method yields a flexible manufacturing route to fabricating 3D metal parts with full density and complex geometries.
In this paper, we report an ultra-fast sintering phenomenon of alumina achieved by the scanning laser irradiation method. Using CO 2 laser irradiation, we found that micrometer-sized alumina powder (d 50 = 1.2 µm) can be sintered close to full density within a few tens of seconds. The microstructure of laser-sintered alumina was different from that of the furnace-sintered alumina. The relative density and grain size of the laser-sintered alumina gradually decreased from the center of the laser beam to the edge. Anisotropy of the grain size was measured along and perpendicular to the scanning direction. This anisotropy decreased as the scanning speed decreased from 0.1 mm/s to 0.01 mm/s. The sintering master curve of grain size versus relative density, which reflects the sintering mechanism, was found to be affected by the laser scanning speed. When the laser scanning speed was 0.1 mm/s, grain size suppression was found for the almost fully dense alumina. However, at lower scanning speed (e.g., 0.01 mm/s), there was significant grain growth in the regions where the relative density was greater than 90%. Furthermore, these results clearly indicate that alumina can be sintered, in the solid-state, to a high density in a short time using scanning laser and the microstructure is different from the furnace-sintered alumina.
We present that Selective Laser Melting (SLM) of metal powder bed layers, whereby 3D metal objects can be printed from a digital file with unprecedented design flexibility, is spurring manufacturing innovations in medical, automotive, aerospace and textile industries. Because SLM is based on raster-scanning a laser beam over each layer, the process is relatively slow compared to most traditional manufacturing methods (hours to days), thus limiting wider spread use. Here we demonstrate the use of a large area, photolithographic method for 3D metal printing, using an optically-addressable light valve (OALV) as the photomask, to print entire layers of metal powder at once. An optical sheet of multiplexed ~5 kW, 20 ms laser diode and ~1 MW, 7 ns Q-switched laser pulses are used to selectively melt each layer. Finally, the patterning of near infrared light is accomplished by imaging 470 nm light onto the transmissive OALV, which consists of polarization-selective nematic liquid crystal sandwiched between a photoconductor and transparent conductor for switching.
Additive manufacturing (AM) technology is capable of fast and low-cost prototyping from complex 3D digital models. To take advantage of this technology, a stainless steel (SS) plate with parallel flow field served as a combination of a cathode bipolar plate and a current distributor; it was fabricated using selective laser melting (SLM) techniques and investigated in a proton exchange membrane electrolyzer cell (PEMEC) in-situ for the first time. The experimental results show that the PEMEC with an AM SS cathode bipolar plate can achieve an excellent performance for hydrogen production for a voltage of 1.779 V and a current density of 2.0 A/cm 2 . The AM SS cathode bipolar plate was also characterized by SEM and EDS, and the results show a uniform elemental distribution across the plate with very limited oxidization. As a result, this research demonstrates that AM method could be a route to aid cost-effective and rapid development of PEMECs.