Search NASA⌕ Search

SEARCH · Search NASA

Results for “SiC Ceramic Fiber”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Spacecraft ceramic protective shield

A low areal density protective shield apparatus, and method for making same, for protecting spacecraft structures from impact with hypervelocity objects, including a bumper member comprising a bumper ceramic layer, a bumper shock attenuator layer, and a bumper confining layer. The bumper ceramic layer can be SiC or B.sub.4 C; the bumper shock attenuator layer can be zirconia felt; and the bumper confining layer can be aluminum. A base armor member can be spaced from the bumper member and a ceramic fiber-based curtain can be positioned between the bumper and base armor members.

Larriva, Rene F.↗

NASP launches new materials

Consideration is given to materials classes being developed for the National Aerospace Plane (NASP), which include titanium alloys and composites, carbon/carbon composites, ceramic-matrix composites, and copper-matrix composites. The forward areas on the skin of the fuselage, and on parts of the tail and wings, will be covered with panels of carbon/carbon or ceramic-matrix composites to protect against temperatures up to 1650 C. Timetal-21S, an advanced high-temperature version of a conventional alloy, combines heat resistance with excellent oxidation and corrosion resistance. Reinforced with SCS-6 SiC fibers, 21S withstands exposure to simulated NASP cycles that include temperature and load excursions representative of orbital and cruise missions. C/C panels a few millimeters thick would be mechanically attached to the underlying Timetal 21S structure over parts of the fuselage, providing protection up to 1650 C. Graphite/epoxy composites are the baseline materials for the hydrogen 'slush' fuel tank.

Ronald, Terence M. F.↗

High Temperature Tensile Properties and Fatigue Behavior of a Melt-Infiltrated SiC/SiC Composite

High temperature fatigue behavior of a woven, SiC/SiC ceramic matrix composite (CMC) was investigated in air at two temperatures. The reinforcement for the CMC consisted of 5HS Sylramic(Trademark) fabric with a [0deg/90deg]4s lay-up. The SiC matrix material was infiltrated into the fiber-preform with a slurry-cast, melt-infiltration process. Tensile and fatigue test specimens were machined from the CMC plates. Initially tensile tests were conducted to obtain the average values of tensile properties at 1038 and 1204 C. Subsequently, low-cycle fatigue (LCF) tests with zero and two-hour hold-times at the maximum stress were conducted at the same two temperatures. Fatigue life data generated in the LCF tests were used to determine the geometric mean fatigue lives. In this paper, the tensile behavior and the fatigue durability of the CMC determined under different loading conditions are documented. In addition, reductions observed in the cyclic lives of the composite due to the two hour hold-time at maximum tensile stress are discussed.

Kalluri, Sreeramesh↗

Improving Thermomechanical Properties of SiC/SiC Composites

Today, a major thrust toward improving the thermomechanical properties of engine components lies in the development of fiber-reinforced silicon carbide matrix composite materials, including SiC-fiber/SiC-matrix composites. These materials are lighter in weight and capable of withstanding higher temperatures, relative to state-of-the-art metallic alloys and oxide-matrix composites for which maximum use temperatures are in the vicinity of 1,100 C. In addition, the toughness or damage tolerance of the SiC-matrix composites is significantly greater than that of unreinforced silicon-based monolithic ceramics. For successful application in advanced engine systems, the SiC-matrix composites should be able to withstand component service stresses and temperatures for the desired component lifetimes. Inasmuch as the high-temperature structural lives of ceramic materials are typically limited by creep-induced growth of flaws, a key property required of such composite materials is high resistance to creep under conditions of use. Also, the thermal conductivity of the materials should be as high as possible so as to minimize component thermal gradients and thermal stresses. A state-of-the-art SiC-matrix composite is typically fabricated in a three-step process: (1) fabrication of a component-shaped architectural preform reinforced by thermally stable high-performance fibers, (2) chemical-vapor infiltration (CVI) of a fiber-coating material such as boron nitride (BN) into the preform, and (3) infiltration of an SiC-based matrix into the remaining porosity in the preform. Generally, the matrices of the highest-performing composites are fabricated by initial use of a CVI SiC matrix component that is typically more thermally stable and denser than matrix components formed by processes other than CVI. As such, the initial SiC matrix component made by CVI provides better environmental protection to the coated fibers embedded within it. Also, the denser CVI SiC imparts to the composite better resistance to propagation of cracks, enhanced thermal conductivity, and higher creep resistance.

DiCarlo, James A.↗

Importance of Measuring SiC Fiber Diameter Prior to Conducting Fiber Stress Rupture / Creep Tests?

A very significant amount of SiC fiber creep / stress rupture data has been generated and reported in the past by various researchers. Due to the difficulty of measuring fiber diameter and the amount of time required to make accurate measurements, researchers have quite often used an accepted average diameter value (which is fiber type-dependent) when determining the load that will be applied to a fiber to generate a specific stress during testing. Of course, this approach has less of an effect on data scatter when the individual fibers in a tow have very similar diameters (minimal fiber-to-fiber variation in diameter). NASA GRC has begun using a laser fiber diameter measurement system, and we are considering eventually characterizing each SiC fiber prior to testing in creep/stressed oxidation. The laser system will be described in this presentation, as well as examples of fiber diameter data obtained in the past at AFRL. We are currently discussing the merits of using an average diameter in testing/data analysis vs. using a measured or "known" diameter. Information about our current intermediate temperature SiC fiber stress rupture testing will also be provided.

ceramic matrix composites↗

Final Report

This cooperative agreement explored the novel polymerization of vinylsilane, alone and in combination with other alkenylsilanes, alkylsilanes, and/or crosslinking agents, using dimethyltitanocene as homogeneous catalyst. The reactions were found to be initiated photochemically under mild conditions, and no hydrogen gas was evolved when alkenylsilanes were polymerized. The polymers were found to have predominately a carbosilane-type backbone containing -SiH2-CH2-CH2-Si and -SiH2-CH(CH3)-Si type linkages. The mechanism of polymerization was found to be step-growth. Despite the relatively low molecular weight of the polymer (M(sub n) - 500 and M(sub W) - 1500), pyrolysis resulted in conversion to C-rich SiC ceramic in high char yields (-60%). Copolymerization with methylsilane resulted in higher chars and more crystalline polymer. Addition of crosslinking agents such as polybutadiene or methyltrivinylsilane increased the viscosity of the polymer produced and enabled application as coatings to fiber toes.

Source record↗

Mechanical Behavior of Notched SiC/SiC Composites

Gas turbine components such as combustor liners or turbine vanes are subject to regions of high stress-concentration, e.g., attachment to the frame or at cooling holes. Ceramic matrix composites (CMCs) are potential materials for high temperature applications in gas turbines. They offer some capability to relieve stress at regions of high stress-concentration via matrix damage accumulation. In this study notch sensitivity was examined for woven SiC fiber reinforced, melt-infiltrated SiC matrix composites with a BN interphase, utilizing either Hi-Nicalo(TM) fibers or the stiffer Sylramic fibers. The double-edge notched tensile test approach was used for a wide range of notch sizes and specimen widths. Both composite systems exhibited mild notch sensitivity similar to other CMC systems. Acoustic emission, detected during the tensile tests, indicated that matrix cracking occurred around notches at net-section stresses below the stress where matrix cracking first occurs in unnotched specimens. However, thermoelastic stress analysis did not show any measurable stress relief around notches after the specimens were preloaded.

Morscher, Gregory N.↗

Thermal response and ablation characteristics of light weight ceramic ablators

An account is given of the thermal performance and ablation characteristics of the NASA-Ames Lightweight Ceramic Ablators (LCAs) in supersonic, high-enthalpy convective environments, which use low density ceramic or carbon fiber matrices as substrates for main structural support, with organic resin fillers. LCA densities are in the 0.224-1.282 g/cu cm range. In-depth temperature data have been obtained to determine thermal penetration depths and conductivity. The addition of SiC and PPMA is noted to significantly improve the ablation performance of LCAs with silica substrates. Carbon-based LCAs are the most mass-efficient at high flux levels.

Tran, Huy K.↗

Factors Controlling Elevated Temperature Strength Degradation of Silicon Carbide Composites

For 5 years, the cooperative agreement NCC3-763 has focused on the development and understanding of Sic-based composites. Most of the work was performed in the area of SiC fiber-reinforced composites for UEET and NGLT and in collaboration with Goodrich Corporation under a partially reimbursable Space Act Agreement. A smaller amount of work was performed on C fiber-reinforced SiC matrix composites for NGLT. Major accomplishments during this agreement included: Improvements to the interphase used in melt-infiltrated (MI) SiC/SiC composites which increases the life under stressed-oxidation at intermediate temperatures referred to as "outside-debonding". This concept is currently in the patent process and received a Space Act Award. Mechanistic-based models of intermediate temperature degradation for MI SiC/SiC Quantification and relatively robust relationships for matrix crack evolution under stress in SiC/SiC composites which serve as the basis for stress-strain and elevated temperature life models The furthering of acoustic emission as a useful tool in composite damage evolution and the extension of the technique to other composite systems Development of hybrid C-SiC fiber-reinforced SiC matrix composites Numerous presentations at conferences, industry partners, and government centers and publications in recognized proceedings and journals. Other recognition of the author's accomplishments by NASA with a TGIR award (2004), NASA's Medal for Public Service (2004), and The American Ceramic Society s Richard M. Fulrath Award (2005). The following will briefly describe the work of the past five years in the three areas of interest: SiC/SiC composite development, mechanistic understanding and modeling of SiC/SiC composites, and environmental durability of C/SiC composites. More detail can be found in the publications cited at the end of this report.

Source record↗

Scatter in Carbon/Silicon Carbide (C/SiC) Composites Quantified

Carbon-fiber-reinforced silicon carbide matrix (C/SiC) composites processed by chemical vapor infiltration are candidate materials for aerospace thermal structures. Carbon fibers can retain properties at very high temperatures, but they are known to have poor oxidation resistance in adverse, high-temperature environments. Nevertheless, the combination of CVI-SiC matrix with higher stiffness and oxidation resistance, the interfacial coating, and additional surface-seal coating provides the necessary protection to the carbon fibers, and makes the material viable for high-temperature space applications operating under harsh environments. Furthermore, C/SiC composites, like other ceramic matrix composites (CMCs), exhibit graceful non-catastrophic failure because of various inherent energy dissipating mechanisms. The material exhibits nonlinearity in deformation even at very low stress levels. This is the result of the severe matrix microcracking present in the as processed composite because of large differences between the coefficients of thermal expansion of the fiber and the matrix. Utilization of these advanced composites in next generation space vehicles will require innovative structural configurations, updated materials, and refined analyses. Structural safety issues for these vehicles are in direct competition with performance and cost. One would have to quantify the uncertainties associated with the design using formal probabilistic methods. Specifically four fundamental aspects on which analyses are based-- (1) loading conditions, (2) material behavior, (3) geometrical configurations, and (4) structural connections between the composite components and baseline structure--are stochastic in nature. A direct way to formally account for uncertainties is to develop probabilistic structural analysis methods where all participating variables are described by appropriate probability density functions. The present work, however, focuses on analyzing the stochastic material behavior of these advanced composites using formal probabilistic analysis methods. Often, some of the desirable property characteristics that allow composites to offer advantages over conventional structural materials (like tailoring of composite properties) and the complexity are in fact responsible for their greater statistical variability and the requirements for more characterization tests. Composite properties are anisotropic as well, having different properties in different directions. This means that characterization of a property such as stiffness--which will vary greatly depending on the orientation of the fiber relative to the direction of the testing--must be repeated for several different directions and loading conditions. The fabrication process for composites also introduces statistical variations in properties and geometry. A composite part is produced in a number of steps, each of which introduces statistical variability. The matrix is usually produced from a combination of raw materials; and the fiber, which has its own set of properties, is often coated or surface treated, introducing yet another source of variability.

Murthy, Pappu L. N.↗

Ceramic Matrix Composite (CMC) Materials Characterization

Under the former NASA EPM Program, much initial progress was made in identifying constituent materials and processes for SiC/SiC ceramic composite hot-section components. This presentation discusses the performance benefits of these approaches and elaborates on further constituent and property improvements made under NASA UEET. These include specific treatments at NASA that significantly improve the creep and environmental resistance of the Sylramic(TM) SiC fiber as well as the thermal conductivity and creep resistance of the CVI Sic matrix. Also discussed are recent findings concerning the beneficial effects of certain 2D-fabric architectures and carbon between the BN interphase coating and Sic matrix.

Calomino, Anthony↗

Ceramic Matrix Composite (CMC) Materials Development

Under the former NASA EPM Program, much initial progress was made in identifying constituent materials and processes for SiC/SiC ceramic composite hot-section components. This presentation discusses the performance benefits of these approaches and elaborates on further constituent and property improvements made under NASA UEET. These include specific treatments at NASA that significantly improve the creep and environmental resistance of the Sylramic(TM) Sic fiber as well as the thermal conductivity and creep resistance of the CVI Sic matrix. Also discussed are recent findings concerning the beneficial effects of certain 2D-fabric architectures and carbon between the BN interphase coating and Sic matrix.

DiCarlo, James↗

Multiscale Modeling of Ceramic Matrix Composites

Results of multiscale modeling simulations of the nonlinear response of SiC/SiC ceramic matrix composites are reported, wherein the microstructure of the ceramic matrix is captured. This micro scale architecture, which contains free Si material as well as the SiC ceramic, is responsible for residual stresses that play an important role in the subsequent thermo-mechanical behavior of the SiC/SiC composite. Using the novel Multiscale Generalized Method of Cells recursive micromechanics theory, the microstructure of the matrix, as well as the microstructure of the composite (fiber and matrix) can be captured.

ceramic matrix composites↗

Facility for continuous CVD coating of ceramic fibers

An inductively heated CVD furnace of pilot-plant scale, whose hot zone is 150 mm in diameter x 300 mm in length, has been adapted for continuous coating of ceramic yarns. Coatings at very low pressures are possible in this facility due to the fact that the entire apparatus, including yarn feeding and collecting equipment, is under vacuum. SiC yarn has been coated with 0.1-0.2 microns of BN at yarn speeds of 60 cm/min; a 500-m spool; was coated in about 14 hrs. Coating capacity was tripled by adding pulleys to allow three yarn passes through the furnace.

Moore, Arthur W.↗

Chemical Stability of the Fiber Coating/Matrix Interface in Silicon-Based Ceramic Matrix Composites

Carbon and boron nitride are used as fiber coatings in silicon-based composites. In order to assess the long-term stability of these materials, reactions of carbon/Si3N4 and BN/SiC were studied at high temperatures with Knudsen effusion, coupon tests, and microstructural examination. In the carbon/Si3N4 system, carbon reacted with Si3N4 to form gaseous N2 and SiC. The formation of SiC limited further reaction by physically separating the carbon and Si3N4. Consequently, the development of high p(N2) at the interface, predicted from thermochemical calculations, did not occur, thus limiting the potential deleterious effects of the reaction on the composite. Strong indications of a reaction between BN and SiC were shown by TEM and SIMS analysis of the BN/SiC interface. In long-term exposures, this reaction can lead to a depletion of a BN coating and/or an unfavorable change of the interfacial properties, limiting the beneficial effects of the coating.

Lee, Kang N.↗

Characterization of Ceramic Matrix Composite Vane Subelements Subjected to Rig Testing in a Gas Turbine Environment

Vane subelements were fabricated from a silicon carbide fiber-reinforced silicon carbide matrix (SiC/SiC) composite. A cross-sectional slice of an aircraft engine metal vane was the basis of the vane subelement geometry. To fabricate the small radius of the vane's trailing edge using stiff Sylramic SiC fibers, a unique SiC fiber architecture was developed. A test configuration for the vanes in a high pressure gas turbine environment was designed and fabricated. Testing was conducted using a pressure of 6 atm and combustion flow rate of 0.5 kg/sec, and consisted of fifty hours of steady state operation followed by 102 2-minute thermal cycles. A surface temperature of 1320 C was obtained for the EBC-coated SiC/SiC vane subelement. This paper will briefly discuss the vane fabrication, test configuration, and results of the vane testing. The emphasis of the paper is on characterization of the post-test condition of the vanes.

Verrilli, Michael↗

High Temperature Solid Particle Erosion in a Melt-Infiltrated SiC/SiC Ceramic Matrix Composite

Ceramic matrix composites (CMCs) are an enabling propulsion material system that offer weight benefits over current Ni-based superalloys, and have higher temperature capabilities that can reduce cooling requirements. Incorporating CMCs into the hot section of gas-turbine engines therefore leads to an increase in engine efficiency. While significant advancements have been made, challenges still remain for current and next-generation gas-turbines; particularly when operating in dust-laden or erosive environments. Solid particles entrained in the gas flow can impact engine hardware resulting in localized damage and material removal due to repeated, cumulative impacts. In this study, the erosion behavior of a melt-infiltrated (MI) silicon carbide fiber-reinforced silicon carbide (SiC/SiC) CMC is investigated at high temperature (1,200 °C) in a simulated combustion environment using 150 µm alumina particles as erodent. Particle impact velocities ranged from 100 to 200 m/s and the angle of impingement varied from 30° to 90°. Erosion testing was also performed on α-SiC to elucidate similarities and differences in the erosion response of the composite compared to that of a monolithic ceramic. Scanning electron microscopy (SEM) was used to study the post-erosion damage morphology and the governing mechanisms of material removal.

Ceramic matrix composites (CMCs), solid particle e↗

Thermal and mechanical behavior of metal matrix and ceramic matrix composites

The present conference discusses local stresses in metal-matrix composites (MMCs) subjected to thermal and mechanical loads, the computational simulation of high-temperature MMCs' cyclic behavior, an analysis of a ceramic-matrix composite (CMC) flexure specimen, and a plasticity analysis of fibrous composite laminates under thermomechanical loads. Also discussed are a comparison of methods for determining the fiber-matrix interface frictional stresses of CMCs, the monotonic and cyclic behavior of an SiC/calcium aluminosilicate CMC, the mechanical and thermal properties of an SiC particle-reinforced Al alloy MMC, the temperature-dependent tensile and shear response of a graphite-reinforced 6061 Al-alloy MMC, the fiber/matrix interface bonding strength of MMCs, and fatigue crack growth in an Al2O3 short fiber-reinforced Al-2Mg matrix MMC.

Kennedy, John M.↗