Search NASA⌕ Search

SEARCH · Search NASA

Results for “Solid electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Effect of Salt Concentration on the Interfacial Solvation Structure and Early Stage of Solid–Electrolyte Interphase Formation in Ca(BH 4 ) 2 /THF for Ca Batteries

The Ca 2+ solvation structure at the electrolyte/electrode interface is of central importance to understand electroreduction stability and solid–electrolyte interphase (SEI) formation for the novel multivalent Ca battery systems. Here, using an exemplar electrolyte, the concentration-dependent solvation structure of Ca(BH 4 ) 2 -tetrahydrofuran on a gold model electrode has been investigated with various electrolyte concentrations via electrochemical quartz crystal microbalance with dissipation (EQCM-D) and X-ray photoelectron spectroscopy (XPS). For the first time, in situ EQCM-D results prove that the prevalent species adsorbed at the interface is CaBH 4 + across all concentrations. As the salt concentration increases, the number of BH 4 – anions associated with Ca 2+ increases, and much larger solvated complexes such as CaBH 4 + ·4THF or Ca(BH 4 ) 3 – ·4THF form at the interface at high concentrations prior to Ca plating. Different interfacial chemistries lead to the formation of SEIs with different components demonstrated by XPS. High electrolyte concentrations reduce the solvent decomposition and promote the formation of thick, uniform, and inorganic-rich (i.e., CaO) SEI layers, which contribute to improved Ca plating efficiency and current density in electrochemical measurements.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Operando investigations of the solid electrolyte interphase in the lithium mediated nitrogen reduction reaction

The lithium-mediated nitrogen reduction reaction (Li-NRR) represents a promising approach for electrochemical nitrogen activation, in which the solid electrolyte interphase (SEI) layer formed on the electrochemically plated lithium plays a key role. Herein, we used time-resolved, operando, grazing incidence wide-angle X-ray scattering (GI WAXS) to identify SEI species and reaction intermediates in the Li-NRR, comparing LiBF 4 and LiClO 4 as electrolyte salts. In this study, we demonstrated how the SEI composition influences the Li-NRR performance by regulating proton transport to the plated Li. When LiBF 4 is used as the electrolyte salt, the formation of LiF and lithium ethoxide (LiEtO) is observed. Reaction intermediates such as LiH and LiN x H y species were found and provide insight into reaction pathways towards undesired and desired products, respectively. Observed restructuring of the Cu (111) single crystal substrate also indicates interaction with plated Li that could possibly influence the Li-NRR performance. Together, these experiments give molecular insight into how to design Li-NRR systems and their SEI layers for optimal performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Evolution of solid electrolyte interphase and active material in the silicon wafer model system

Alloying anode materials for lithium-ion batteries, such as silicon (Si), are an important focus of materials research due to the demand for increased energy density for electric vehicles and stationary grid storage. However, progress towards next generation anode materials has been hindered by poor capacity retention due to the instability of the Si active material and the solid electrolyte interphase (SEI). Herein, the evolution of the active Si material and the SEI are simultaneously investigated from the perspective of chemical, structural, morphological, and electronic evolution in the Si wafer model system through its cycling life, using time-of-flight secondary ion mass spectrometry (TOF-SIMS), scanning transmission electron microscopy (STEM), atomic force microscopy (AFM), and scanning spreading resistance microscopy (SSRM). The results illustrate a dynamic evolution of the SEI and active Si material through cycling. Through an improved understanding of evolution of SEI and Si active material within the Si wafer model system, mitigation strategies may be designed to extend the lifetime of Si anodes.

25 ENERGY STORAGE↗

Role of Inorganic Surface Layer on Solid Electrolyte Interphase Evolution at Li-Metal Anodes

Lithium metal is an ideal anode for rechargeable lithium battery technology. However, the extreme reactivity of Li-metal with the electrolyte leads to solid electrolyte interphase (SEI) layer which often impedes the Li + transport across the interface. The challenge is to predict the chemical, structural and topographical heterogeneity of SEI layer arising from multitude of interfacial constituents. Traditionally the pathways and products of electrolyte decomposition processes were analyzed with the basic presumption of pristine Li-metal surface for simplicity. However, ubiquitous inorganic passivation layers on Li-metal can dampen the electronic charge transfer to the electrolyte and significantly alter the SEI layer evolution. In this study, we analyzed the effect of nanometric Li 2 O, LiOH and Li 2 CO 3 as surface passivation layer on the interfacial reactivity of Li-metal using ab initio molecular dynamics (AIMD) calculations and X-ray photoelectron spectroscopy (XPS) measurements. These nanometric layers impede the electronic charge transfer to the electrolyte and thereby provide some degree of passivation (compared to pristine lithium metal) to the redox based decomposition process. The Li 2 O, LiOH and Li 2 CO 3 layers admits varying level of electron transfer from Li-metal slab and subsequent storage of the electronic charges within their structure. Nevertheless, their ability for electron transfer to the electrolyte molecules and the extent of bis(trifluoromethanesulfonyl)imide (TFSI) anion decomposition is significantly smaller than that on the pristine Li-metal. The XPS experiments showed that Li 2 O as major surface component had greater LiF phase formation, whereas a dominant LiOH layer shows enhanced sulfur decomposition process. Furthermore, these observations were explained based on different electronic charge transfer ability of the passivating films derived from AIMD results.

25 ENERGY STORAGE↗

Auger Electrons as Probes for Composite Micro- and Nano- structured Materials: Application to Solid Electrolyte Interphases in Graphite and Silicon-Graphite Electrodes

In this study, Auger electron spectroscopy (AES) combined with ion sputtering profilometry, Xray photoelectron spectroscopy (XPS), and scanning electron microscopy (SEM) have been used in a complementary fashion to examine chemical and microstructural changes in graphite (Gr) and silicon/graphite (Si/Gr) blends contained in the negative electrodes of lithium-ion cells. We demonstrate how AES can be used to characterize morphology of the solid-electrolyte interphase (SEI) deposits in such heterogeneous media, complementing well-established methods, such as XPS and SEM. In this way we demonstrate that the SEI does not consist of uniformly thick layers on the graphite and silicon; the thickness of the SEI layers in cycle-life aged electrodes follows an exponential distribution with a mean of ca. 13 nm for the graphite and ca. 20-25 nm for the silicon nanoparticles (with a crystalline core of 50-70 nm in diameter). Furthermore, a “sticky-sphere” model, in which Si nanoparticles are covered with a layer of polymer binder (that is replaced by the SEI during cycling) of variable thickness is introduced to account for the features observed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Deliberate modification of the solid electrolyte interphase (SEI) during lithiation of magnetite, Fe 3 O 4 : impact on electrochemistry

Here, magnetite is a conversion anode material displaying multi-electron transfer during lithiation and delithiation. The solid electrolyte interphase (SEI) on magnetite, Fe 3 O 4 , electrodes for lithium ion batteries was deliberately modified through the use of fluoroethylene carbonate (FEC) electrolyte additive, improving both capacity retention and rate capability. Analysis showed reduction of FEC at higher voltage compared to non-fluorinated solvents with formation of a modified lithium flouride containing electrode surface.

25 ENERGY STORAGE↗

Hydrophobic versus Hydrophilic Interfacial Coatings on Silicon Nanoparticles Teach Us How to Design the Solid Electrolyte Interphase in Silicon-Based Li-Ion Battery Anodes

Herein, we evaluate the effect of covalently attached molecular coating hydrophobicity on the surface of the silicon nanoparticle (Si NP) active anode material for Li-ion batteries. The experiments are a means to identify the interfacial properties that help minimize electrochemical side reactions during cycling. Preformed coatings on the Si NP surfaces prior to electrode fabrication mimic the ionically conducting and electronically insulating properties of the solid electrolyte interphase (SEI). Hydrophilic oligomers such as polyethylene oxide (PEO) and other related structures are commonly identified as Li+-conducting components of the SEI. Here, we study the effect of such hydrophilic PEO versus hydrophobic alkyl molecular coatings on Si NP anode electrochemical performance. We also study the effect of the PEO oligomer length and the resulting effective thickness of the interfacial coating on the electrochemical performance. We find that PEO oligomers electrochemically isolate Si NPs when the PEO coating thickness approaches the electron tunneling distance of ~2.5 nm. Surprisingly, the thickness of the PEO-based coatings has a negligible effect on their ability to minimize electrochemical side reactions as measured by Coulombic efficiency. These results reveal how the interfacial coating on silicon anode materials should differ from an operando-formed SEI layer and discuss design strategies for an ideal interfacial active material coating based on these results.

25 ENERGY STORAGE↗

An Inorganic-Rich Solid Electrolyte Interphase for Advanced Lithium-Metal Batteries in Carbonate Electrolytes

In carbonate electrolytes, the organic-inorganic solid electrolyte interphase (SEI) formed on the lithium (Li) metal anode surface is strongly bonded to Li and experiences the same volume change as Li, thus it undergoes continuous cracking/reformation during plating/stripping cycles. Here we report, an inorganic-rich SEI is designed on a Li metal surface to reduce its bonding energy with Li metal by dissolving 4 M concentrated LiNO 3 in dimethyl sulfoxide (DMSO) as an additive for a fluoroethylene carbonate (FEC) based electrolyte. Due to the aggregate structure of NO 3 - ions and its participation in the primary Li + solvation sheath, abundant Li 2 O, Li 3 N, and LiN x O y grains are formed in the resulting SEI, in addition to the uniform LiF distribution from the reduction of PF 6 - ions. The inorganic-rich SEI’s weak bonding (high interface energy) to Li can effectively promote Li diffusion along the SEI/Li interface and prevent Li dendrite penetration into the SEI. As a result, our designed carbonate electrolyte enables a Li anode to achieve a high Li plating/stripping CE of 99.55% (1 mA cm -2 , 1.0 mAh cm -2 ) and the electrolyte also enables a Li||LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NMC811) full cell (2.5 mAh cm -2 ) to retain 75%of its initial capacity after 200 cycles with an outstanding CE of 99.83%.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dissolution of the Solid Electrolyte Interphase and Its Effects on Lithium Metal Anode Cyclability

At >95% Coulombic efficiencies, most of the capacity loss for Li metal anodes (LMAs) is through the formation and growth of the solid electrolyte interphase (SEI). However, the mechanism through which this happens remains unclear. One property of the SEI that directly affects its formation and growth is the SEI’s solubility in the electrolyte. Here, in this work, we systematically quantify and compare the solubility of SEIs derived from ether-based electrolytes optimized for LMAs using in-operando electrochemical quartz crystal microbalance (EQCM). A correlation among solubility, passivity, and cyclability established in this work reveals that SEI dissolution is a major contributor to the differences in passivity and electrochemical performance among battery electrolytes. Together with our EQCM, X-ray photoelectron spectroscopy (XPS), and nuclear magnetic resonance (NMR) spectroscopy results, we show that solubility depends on not only the SEI’s composition but also the properties of the electrolyte. This provides a crucial piece of information that could help minimize capacity loss due to SEI formation and growth during battery cycling and aging.

25 ENERGY STORAGE↗

Role of conductive binder to direct solid–electrolyte interphase formation over silicon anodes

In this study, with the use of in situ neutron reflectometry (NR) we show how the addition of an electronically conductive polymeric binder, PEFM, mediates the solid–electrolyte interphase (SEI) formation and composition on an amorphous Si (a-Si) electrode as a function of the state-of-charge. Upon initial contact with the electrolyte a Li rich, 41 Å thick, layer forms on the surface of the anode below the polymer layer. At 0.8 V (vs. Li/Li + ), a distinct SEI layer forms from the incorporation of electrolyte decomposition products in the reaction layer that is organic in nature. In addition, solvent uptake in the PEFM layer occurs resulting in the layer swelling to ~200 Å. Upon further polarization to 0.4 and 0.15 V (vs. Li/Li + ) a thick layer (800 Å) on the surface of the Si is evident where a diffuse interface between the PEFM and SEI occurs resulting in a matrix between the two layers, as the binder has taken up a large amount of electrolyte. The two layers appear to be interchanging solvent molecules from the PEFM to the SEI to the Si surface preventing the lithiation of the a-Si. By 0.05 V (vs. Li/Li + ) a Li rich, 72 Å thick, SEI layer condenses on the surface of the anode, and a 121 Å intermixed layer on top of the SEI with LiF and Li–C–O species is present with the rest blended into the electrolyte.

36 MATERIALS SCIENCE↗

Stabilizing the Solid‐Electrolyte Interphase with Polyacrylamide for High‐Voltage Aqueous Lithium‐Ion Batteries

Abstract The introduction of “water‐in‐salt” electrolyte (WiSE) concept opens a new horizon to aqueous electrochemistry that is benefited from the formation of a solid‐electrolyte interphase (SEI). However, such SEI still faces multiple challenges, including dissolution, mechanical damaging, and incessant reforming, which result in poor cycling stability. Here, we report a polymeric additive, polyacrylamide (PAM) that effectively stabilizes the interphase in WiSE. With the addition of 5 molar % PAM to 21 mol kg −1 LiTFSI electrolyte, a LiMn 2 O 4 ∥L‐TiO 2 full cell exhibits enhanced cycling stability with 86 % capacity retention after 100 cycles at 1 C. The formation mechanism and evolution of PAM‐assisted SEI was investigated using operando small angle neutron scattering and density functional theory (DFT) calculations, which reveal that PAM minimizes the presence of free water molecules at the anode/electrolyte interface, accelerates the TFSI − anion decomposition, and densifies the SEI.

25 ENERGY STORAGE↗

Examining CO 2 as an Additive for Solid Electrolyte Interphase Formation on Silicon Anodes

In this study, we demonstrate that the addition of CO 2 to a standard 1.0 M LiPF 6 3:7 wt% ethylene carbonate:ethyl methyl carbonate electrolyte results in the formation of a thinner insoluble solid electrolyte interphase (SEI) that is dominated by the presence of LiF. In contrast, cells without CO 2 result in a thicker insoluble SEI layer containing more organic constituents. The CO 2 is incorporated in the dimethyl carbonate soluble part of the SEI composed primarily of polymeric poly(ethylene oxide) (PEO) on the surface of a thin inorganic layer. This combination of properties from CO 2 addition provides an improved cycling performance through the reduction of irreversible side reactions, leading to higher coulombic efficiency. The results indicate that CO 2 incorporates into the SEI and plays a role similar to additives like fluorinated ethylene carbonate and vinylene carbonate with respect to polymeric components.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Reduction Mechanism of Fluoroethylene Carbonate for Stable Solid–Electrolyte Interphase Film on Silicon Anode

Fluoroethylene Carbonate (FEC) is an effective electrolyte additive which can significantly improve the cyclability of Si and other anode materials. However, the fundamental mechanism on this improvement is still not well understood. Based on the results obtained from 6Li Nuclear Magnetic Resonance and X-ray Photoelectron Scanning study, we propose a molecular level mechanism on how FEC affects the formation of solid electrolyte interphase (SEI) film: 1) FEC is reduced through the opening of the five member ring leading to the formation of lithium poly (vinyl carbonate), LiF and some dimmers; 2) The high tensile strength of the FEC-derived lithium poly (vinyl carbonate) enhances the stability of the SEI film. This mechanism has been verified by the results of electrochemical tests.

Environmental Molecular Sciences Laboratory↗

Floatable Protective Layers: a Strategy to Minimize Solid Electrolyte Interphase Growth and Maximize the Lithium Utilization

Abstract Maximizing lithium (Li) utilization is crucial for enhancing the long‐term stability of Li‐based batteries. In anode‐free Li batteries (AFLBs), although the initial formation of solid electrolyte interphase (SEI) is beneficial on limiting further reaction between Li and electrolyte, large volume change of Li metal anode (LMA) during cycling often leads to continuous breakdown and re‐formation of SEI and formation of inactive Li, hindering its efficiency. In this study, a novel strategy is presented to protect Li metal by applying a floatable protection layer (FPL) on a copper substrate, enabling large Li particles to be primarily deposited below FPL, but SEI to be primarily formed above FPL. This approach effectively minimizes the direct contact between electrolyte and freshly deposited Li, therefore mitigating the continuous side reactions and early failure of AFLBs. As a result, Li consumption is minimized, and the overall stability of the battery is significantly enhanced. Further development of this approach can also be used to improve the performance of other Li‐based batteries for large‐scale applications.

Lim, Hyung‐Seok [Energy and Environment Directorat↗

Understanding Solid Electrolyte Interphase Nucleation and Growth on Lithium Metal Surfaces

Experiments and theory are needed to decode the exact structure and distribution of components of a passivation layer formed at the anode surface of Li metal batteries, known as the Solid Electrolyte Interphase (SEI). Due to the inherent dynamic behavior as well as the lithium reactivity, the SEI structure and its growth mechanisms are still unclear. This study uses molecular simulation and computational chemistry tools to investigate the initial nucleation and growth dynamics of LiOH and Li2O that provide us with thermodynamics and structural information about the nucleating clusters of each species. Following the most favorable pathways for the addition of each of the components to a given nascent SEI cluster reveals their preferential nucleation mechanisms and illustrates different degrees of crystallinity and electron density distribution that are useful to understand ionic transport through SEI blocks.

25 ENERGY STORAGE↗

Voltage-Dependent First-Principles Barriers to Li Transport within Li-Ion Battery Solid Electrolyte Interphases

Charging a Li-ion battery requires Li-ion transport between the cathode and the anode. This Li-ion transport is dependent on (among other factors) the electrostatic environment that the ion encounters within the solid electrolyte interphase (SEI), which separates the anode from the surrounding electrolyte. A previous first-principles work has illuminated the reaction barriers through likely atomistic SEI environments but has had difficulty accurately reflecting the larger electrostatic potential landscape that an ion encounters moving through the SEI. In this work, we apply the recently developed quantum continuum approximation (QCA) technique to provide an equilibrium electronic potentiostat for first-principles interface calculations. Using QCA, we calculate the potential barrier for Li-ion transport through LiF, Li 2 O, and Li 2 CO 3 SEIs along with LiF–LiF and LiF–Li 2 O grain boundaries, all paired with Li metal anodes. Here, we demonstrate that the SEI potential barrier is dependent on the electrochemical potentials of the anode in each system. Finally, we use these techniques to estimate the change in the diffusion barrier for a Li ion moving in a LiF SEI as a function of the anode potential. We find that properly accounting for interface and electronic voltage effects significantly lowers reaction barriers compared with previous literature results.

25 ENERGY STORAGE↗

Solvation Rule for Solid-Electrolyte Interphase Enabler in Lithium-Metal Batteries

Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium-metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium-metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. Here, we unambiguously demonstrated the solvation rule for the solid-electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥ 1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.

25 ENERGY STORAGE↗