Search NASA⌕ Search

SEARCH · Search NASA

Results for “TOUGH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Test-Free Fracture Toughness

Computational simulation results can give the prediction of damage growth and progression and fracture toughness of composite structures. The experimental data from literature provide environmental effects on the fracture behavior of metallic or fiber composite structures. However, the traditional experimental methods to analyze the influence of the imposed conditions are expensive and time consuming. This research used the CODSTRAN code to model the temperature effects, scaling effects and the loading effects of fiberbraided composite specimens with and without fiber-optic sensors on the damage initiation and energy release rates. The load-displacement relationship and fracture toughness assessment approach is compared with the test results from literature and it is verified that the computational simulation, with the use of established material modeling and finite element modules, adequately tracks the changes of fracture toughness and subsequent fracture propagation for any fiberbraided composite structure due to the change of fiber orientations, presence of large diameter optical fibers, and any loading conditions.

Minnetyan, Levon↗

Strength, Fracture Toughness, and Slow Crack Growth of Zirconia/alumina Composites at Elevated Temperature

Various electrolyte materials for solid oxide fuel cells were fabricated by hot pressing 10 mol% yttria-stabilized zirconia (10-YSZ) reinforced with two different forms of alumina particulates and platelets each containing 0 to 30 mol% alumina. Flexure strength and fracture toughness of platelet composites were determined as a function of alumina content at 1000 C in air and compared with those of particulate composites determined previously. In general, elevated-temperature strength and fracture toughness of both composite systems increased with increasing alumina content. For a given alumina content, flexure strength of particulate composites was greater than that of platelet composites at higher alumina contents (greater than or equal to 20 mol%), whereas, fracture toughness was greater in platelet composites than in particulate composites, regardless of alumina content. The results of slow crack growth (SCG) testing, determined at 1000 C via dynamic fatigue testing for three different composites including 0 mol% (10-YSZ matrix), 30 mol % particulate and 30 mol% platelet composites, showed that susceptibility to SCG was greatest with SCG parameter n = 6 to 8 for both 0 and 30 mol% particulate composites and was least with n = 33 for the 30 mol% platelet composite.

Choi, Sung R.↗

Test-Free Fracture Toughness

Computational simulation results can give the prediction of damage growth and progression and fracture toughness of composite structures. The experimental data from literature provide environmental effects on the fracture behavior of metallic or fiber composite structures. However, the traditional experimental methods to analyze the influence of the imposed conditions are expensive and time consuming. This research used the CODSTRAN code to model the temperature effects, scaling effects and the loading effects of fiber/braided composite specimens with and without fiber-optic sensors on the damage initiation and energy release rates. The load-displacement relationship and fracture toughness assessment approach is compared with the test results from literature and it is verified that the computational simulation, with the use of established material modeling and finite element modules, adequately tracks the changes of fracture toughness and subsequent fracture propagation for any fiber/braided composite structure due to the change of fiber orientations, presence of large diameter optical fibers, and any loading conditions.

Minnetyan, Levon↗

Strength, Fracture Toughness, Fatigue, and Standardization Issues of Free-standing Thermal Barrier Coatings

Strength, fracture toughness and fatigue behavior of free-standing thick thermal barrier coatings of plasma-sprayed ZrO2-8wt % Y2O3 were determined at ambient and elevated temperatures in an attempt to establish a database for design. Strength, in conjunction with deformation (stress-strain behavior), was evaluated in tension (uniaxial and trans-thickness), compression, and uniaxial and biaxial flexure; fracture toughness was determined in various load conditions including mode I, mode II, and mixed modes I and II; fatigue or slow crack growth behavior was estimated in cyclic tension and dynamic flexure loading. Effect of sintering was quantified through approaches using strength, fracture toughness, and modulus (constitutive relations) measurements. Standardization issues on test methodology also was presented with a special regard to material's unique constitutive relations.

Choi, Sung R.↗

Refinements to the Mixed-Mode Bending Test for Delamination Toughness

The mixed-mode bending (MMB) test for delamination toughness was first introduced in 1988. This simple test is a combination of the standard Mode I (opening) test and a Mode II (sliding) test. This MMB test has become widely used in the United States and around the world for mixed-mode toughness measurements. Because of the widespread use of this test method, it is being considered for standardization by ASTM Committee D30. This paper discusses several improvements to the original test method. The improvements to the MMB test procedure include an improved method for calculating toughness from the measured test quantities, a more accurate way of setting the mixed-mode ratio to be tested, and the inclusion of a new alignment criterion for improved consistency in measured values.

Reeder, James R.↗

Slow Crack Growth and Fracture Toughness of Sapphire for the International Space Station Fluids and Combustion Facility

The fracture toughness, inert flexural strength, and slow crack growth parameters of the r- and a-planes of sapphire grown by the Heat Exchange Method were measured to qualify sapphire for structural use in the International Space Station. The fracture toughness in dry nitrogen, K(sub Ipb), was 2.31 +/- 0.12 MPa(square root of)m and 2.47 +/- 0.15 MPa(squre root of)m for the a- and r-planes, respectively. Fracture toughness measured in water via the operational procedure in ASTM C1421 was significantly lower, K(sub Ivb) = 1.95+/- 0.03 MPa(square root of)m, 1.94 +/- 0.07 and 1.77 +/- 0.13 MPa(square root of)m for the a- , m- and r-planes, respectively. The mean inert flexural strength in dry nitrogen was 1085 +/- 127 MPa for the r-plane and 1255 +/- 547 MPa for the a-plane. The power law slow crack growth exponent for testing in water was n = 21 +/- 4 for the r-plane and n (greater than or equal to) 31 for the a-plane. The power law slow crack growth coefficient was A = 2.81 x 10(exp -14) m/s x (MPa(squre root of)m)/n for the r-plane and A (approx. equals)2.06 x 10(exp -15) m/s x (MPa(square root of)m)/n for the a-plane. The r- and a-planes of sapphire are relatively susceptible to stress corrosion induced slow crack growth in water. However, failure occurs by competing modes of slow crack growth at long failure times and twinning for short failure time and inert environments. Slow crack growth testing needs to be performed at low failure stress levels and long failure times so that twinning does not affect the results. Some difficulty was encountered in measuring the slow crack growth parameters for the a-plane due to a short finish (i.e., insufficient material removal for elimination of the damage generated in the early grinding stages). A consistent preparation method that increases the Weibull modulus of sapphire test specimens and components is needed. This would impart higher component reliability, even if higher Weibull modulus is gained at the sacrifice of absolute strength of the component. The current specification frequently used for the preparation of sapphire test specimens and components (e.g., a "60/40" scratch-dig finish) is inadequate to avoid a short finish.

Salem, Jonathan A.↗

Effects of Cryogenic Temperature on Fracture Toughness of Core-Shell Rubber (CSR) Toughened Epoxy Nanocomposites

This study investigated the effects of core-shell rubber (CSR) nanoparticles on the mechanical properties and fracture toughness of an epoxy resin at ambient and liquid nitrogen (LN2) temperatures. Varying amounts of Kane Ace MX130 toughening agent were added to a commercially available EPON 862/Epikure W epoxy resin. Elastic modulus was calculated using quasi-static tensile data. Fracture toughness was evaluated by the resulting breaking energy measured in Charpy impact tests conducted on an instrumented drop tower. The size and distribution of the CSR nanoparticles were characterized using Transmission Electron Microscopy (TEM) and Small Angle X-ray Scattering (SAXS). Scanning Electron Microscopy (SEM) was used to study the fracture surface morphology. The addition of the CSR nanoparticles increased the breaking energy with negligible change in elastic modulus and ultimate tensile stress (UTS). At ambient temperature the breaking energy increased with increasing additions of the CSR nanoparticles, while at LN2 temperatures, it reached a maximum at 5 wt% CSR concentration. KEY WORDS: liquid nitrogen (LN2) properties, fracture toughness, core-shell rubber (CSR).

Wang, J.↗

Mode II Interlaminar Fracture Toughness and Fatigue Characterization of a Graphite Epoxy Composite Material

Mode II interlaminar fracture toughness and delamination onset and growth characterization data were generated for IM7/8552 graphite epoxy composite materials from two suppliers for use in fracture mechanics analyses. Both the fracture toughness testing and the fatigue testing were conducted using the End-notched Flexure (ENF) test. The ENF test for mode II fracture toughness is currently under review by ASTM as a potential standard test method. This current draft ASTM protocol was used as a guide to conduct the tests on the IM7/8552 material. This report summarizes the test approach, methods, procedures and results of this characterization effort.

O'Brien, T. Kevin↗

Inverse Method for Estimation of Composite Kink-Band Toughness from Open-Hole Compression Strength Data

Fiber-reinforced polymer matrix composite materials can fail by kink-band propagation mechanism when subjected to in-plane compressive loading. This mode of failure is especially prevalent in compressive loading of laminates with holes, cut-outs, or impact damage. Most of the successful models for predicting compressive strength of such laminates require “fracture” toughness associated with kink-band propagation under in-plane compression. However, this property is difficult to measure experimentally, limiting the use of such models in design practice. In this paper an inverse method is proposed to estimate the kink-band toughness of the laminate from its open-hole compression strength data, which is an easier property to measure experimentally. Furthermore, a scaling relationship is proposed to estimate kink-band toughness for other laminate configurations of the same material.

Luke Borkowski↗

Post-Irradiation Fracture Toughness Characterization of Generation II FeCrAl Alloys

FeCrAl alloys are promising candidate materials for the accident tolerant fuel (ATF) cladding application due to their exceptional resistance to oxidation in elevated temperature steam environments. Currently, limited fracture toughness data are available for the FeCrAl alloys, including the FeCrAl alloys newly developed at Oak Ridge National Laboratory (ORNL) under the U.S. Department of Energy’s Advanced Fuels Campaign (AFC) program. In this study, two Generation II candidate FeCrAl alloys, i.e., C06M (81.8Fe-10Cr-6Al-0.03Y-2Mo-0.2Si) and C36M (78.8Fe-13Cr-6Al-0.03Y-2Mo-0.2Si), were irradiated in the High Flux Isotope Reactor (HFIR) at ORNL to assess the fracture characteristics of these alloys after neutron irradiation. A total of six rabbit capsules were irradiated in HFIR at target temperatures of 200°C, 330°C, and 500°C up to target damage doses of 8 displacements per atom (dpa) and 16 dpa. Post-irradiation fracture toughness testing was performed following the Master Curve method in the ASTM E1921 standard. The main findings of this study are:1) Both the C06M and C36M alloys exhibited a similar response to irradiation concerning irradiation hardening and embrittlement.2) The irradiation temperature played different roles in terms of irradiation hardening and embrittlement for both C06M and C36M: after irradiation between 166°C and 204°C, both materials exhibited significant irradiation hardening and embrittlement; after irradiation between 315°C and 343°C, both materials showed small irradiation hardening without irradiation embrittlement. After irradiation between 501°C and 507°C, however, the irradiation softening without irradiation embrittlement was observed in both materials.3) Comparing the microhardness and Master Curve reference temperature T0q before and after neutron irradiation, we did not observe a linear correlation between the two parameters for both C06M and C36M steels. This should be mainly due to a flat response of the Master Curve reference temperature T0q to the irradiations at 166–204°C and 315–343°C ranges4) C06M showed a lower T0q, meaning better toughness, than C36M at the unirradiated condition, and such trend was kept even after neutron irradiation except for the 166–204°C irradiation after which both materials had similar T0q.5) In terms of hardening and embrittlement, the irradiation effect on both C06M and C36M appeared to saturate after an irradiation dose of 7 dpa.

Chen, Xiang↗

Effect of Specimen Thickness on Fracture Toughness and Plane Stress to Plane Strain Transition in Medium-Density Polyethylene

This study investigates the effect of specimen thickness on fracture toughness and the transition from plane stress to plane strain conditions in Medium-Density Polyethylene (MDPE) using Single Edge Notched Bend (SENB) specimens. Three thickness groups (7.5 mm, 9.0 mm, and 12.1 mm) were tested following ASTM D5045 protocol. Conditional stress intensity factors (KQ) increased from 2.2 MPavm to 2.8 MPavm with increasing thickness, demonstrating significant size dependency. Confocal microscopy revealed a 34% reduction in maximum crack tip opening displacement (CTOD) from 0.478 mm to 0.314 mm as thickness increased, with plastic zone lateral extent decreasing by 32%. This quantitative evidence validates Irwin's theoretical prediction of plastic zone size transition from plane stress r_y˜ (1/2p) (K_I/s_y )^2 to plane strain conditions r_y˜ (1/6p) (K_I/s_y )^2.Scanning electron microscopy confirmed progressive suppression of shear lips and evolution from ductile tearing with extensive polymer chain drawing in thin specimens to localized crazing in thick specimens. Despite all specimens satisfying the ASTM D5045 criterion (B = 2.5(KQ/s_y )^2 ) ,residual shear lips persisted even in the thickest specimens, demonstrating that nominal size requirements alone are insufficient for achieving complete plane strain conditions in highly ductile polymers. The findings emphasize the necessity of integrated analytical and morphological assessment for valid fracture toughness characterization, with critical implications for life assessment and integrity prediction in thick-section polymer components such as natural gas distribution pipelines.

Medium-Density Polyethylene↗

Fracture toughness evaluation for thin-shell stainless steel weldment

Integrity of spent nuclear fuel (SNF) interim storage canisters are very important to the safety of the back-end nuclear fuel cycle. Stress corrosion cracking (SCC) potential of interim storage canister has been considered as a high priority. Because no post-weld heat treatment was required for forming these canisters, the high tensile residual stress existed within these canister welds. This can change the fracture resistance capacity significantly as well as increase SCC potential. Due to relative thin shell thickness of a canister weldment, the spiral notch torsion test (SNTT) method of small specimen approach was used to estimate the canister weldment fracture toughness. Most SNTT weldment samples fracture initiation sites are at heat-affected zone (HAZ) regions. The estimated fracture toughness $J_Q'$ for the baseline SS304 steel is at 283 kJ/m 2 . The estimated $J_Q'$ for the SS304/308 weld from HAZ and weld specimens are 126 kJ/m 2 and 148.9 kJ/m 2 , respectively.

36 MATERIALS SCIENCE↗

Simple, Tough, and Effective Porous Coating for Anti-Corrosion Application

This presentation discusses how a change in polymeric binder, the material used for assembling hydrophobic nanoparticles into a porous structure, led to better mechanical toughness and a simpler fabrication process based on 100% commercially available components. Most importantly, the optimized porous coating can reduce the corrosion rate by two orders of magnitude (0.003 mm/year) due to higher diffusion barrier based on a more resistant tortuous diffusion path. The combination of simplicity, toughness, effectiveness, and scalability greatly enhanced the prospect of commercializing this technology as an internal anti-corrosion coating for natural gas pipelines.

internal corrosion↗

Postweld Heat Treatment on Toughness of Electric- Resistance Welded X70 Steel

In this report the effect of postweld heat treatment (PWHT) on Charpy V-notch impact toughness of a highfrequency electric-resistance welded (HF-ERW) grade X70 pipeline steel is investigated. PWHT thermal cycles are simulated using the Gleeble on the as-welded specimens. Microstructure, along with crystallographic texture and microhardness, is characterized in specimens that are impact tested at –5°C (23°F), –30°C (–22°F), and –45°C (–49°F). The impact toughness values show a wide scatter band and decrease with the increasing peak temperature of the PWHT. For higher peak temperatures, the microstructure of the heat-affected zone (HAZ) gradually changed from equiaxed ferrite to bainitic ferrite. Furthermore, the prior austenite grain size (PAGS) increases with the increasing peak temperature. The density of high-angle grain boundaries decreases, and the fraction of cleavage planes {100} parallel to the impact fracture plane increases for higher peak temperatures of the PWHT

36 MATERIALS SCIENCE↗

Cryogenic Mixed Mode I – Mode II Fracture Toughness of Various Polymer Composite Materials

The present study investigates the mixed mode interlaminar fracture toughness of six polymer matrix composite materials at both room temperature and cryogenic liquid nitrogen temperature. The single leg bending test employed gives a mix of Mode I (opening) and Mode II (in-plane shearing) cracking. The tested thermoplastic-matrix composites were shown to have total mixed mode toughnesses 3.1–4.3 times higher than those of representative thermoset resin composites.

Carbon fiber↗

Enhancing Composite Toughness Through Hierarchical Interphase Formation

High strength and ductility are highly desired in fiber-reinforced composites, yet achieving both simultaneously remains elusive. A hierarchical architecture is developed utilizing high aspect ratio chemically transformable thermoplastic nanofibers that form covalent bonding with the matrix to toughen the fiber-matrix interphase. The nanoscale fibers are electrospun on the micrometer-scale reinforcing carbon fiber, creating a physically intertwined, randomly oriented scaffold. Unlike conventional covalent bonding of matrix molecules with reinforcing fibers, here, the nanofiber scaffold is utilized - interacting non-covalently with core fiber but bridging covalently with polymer matrix - to create a high volume fraction of immobilized matrix or interphase around core reinforcing elements. This mechanism enables efficient fiber-matrix stress transfer and enhances composite toughness. Molecular dynamics simulation reveals enhancement of the fiber-matrix adhesion facilitated by nanofiber-aided hierarchical bonding with the matrix. The elastic modulus contours of interphase regions obtained from atomic force microscopy clearly indicate the formation of stiffer interphase. These nanoengineered composites exhibit a ≈60% and ≈100% improved in-plane shear strength and toughness, respectively. This approach opens a new avenue for manufacturing toughened high-performance composites.

36 MATERIALS SCIENCE↗

On the strength and fracture toughness of an additive manufactured CrCoNi medium-entropy alloy

An additively manufactured (nominally equiatomic) CrCoNi alloy was processed by laser powder bed fusion (LPBF). At ambient temperatures (298 K), this medium-entropy alloy displayed a yield strength, σ y of ~691 ± 9 MPa, and an ultimate tensile strength, σ u of ~926 ± 15.2 MPa; at cryogenic temperatures (77 K), yield and tensile strengths increased respectively to σ y ~ 944 ± 6 MPa and σ u ~ 1382 ± 11 MPa. These strength levels are 57 and 44% higher than that of the wrought alloy, due to strengthening from the solidification cellular structures intertwined with dislocations in the LPBF CrCoNi. The crack-initiation fracture toughness, K JIc was measured to be ~183.7 ± 28 MPa√m at 298 K; this value marginally decreased by ~4% to ~176 ± 11 MPa√m at 77 K. These K JIc values of the LPBF CrCoNi were 11% and 35% lower than the wrought CrCoNi alloy at 298 K and 77 K, respectively. Here, the resistance to crack growth of the LPBF CrCoNi from its hierarchical micro- and meso-structures was evaluated using nonlinear-elastic fracture mechanics by measuring R-curve behavior in the form of the J-integral as a function of crack extension. The specific features of the hierarchical microstructures at different length-scales provide a basis for the strengthening and toughening properties of this additively manufactured medium-entropy alloy. This correlation between the deformation and the hierarchical microstructures at different length-scales may provide future guidance for improving the fracture toughness properties of medium-entropy alloys.

36 MATERIALS SCIENCE↗

On the roles of welding residual stresses in determination of fracture toughness in austenitic stainless steel SUS 304 pipeline girth welds

Welding residual stresses especially the high tensile stresses are proved to have negative impacts on the fatigue and fracture behaviors of welded structures. In this study, a virtual fabrication of test specimens from welding process to specimen preparation was carried out by numerical simulation. An austenitic stainless steel multi-pass pipe welding was simulated by transient thermal–mechanical finite element analysis, the residual stresses were then mapped into the test specimen to evaluate fracture toughness. The findings in this study confirmed that, residual stress can be high in a sub-sized compact tensile specimen, which may accelerate or hinder the crack propagation during actual fatigue and fracture tests as reported in recent years. The influence of the cutting location and orientation of the specimen on fracture performance was investigated systematically to provide a fundamental understanding of welding residual stress and necessary insights into the specimen preparation procedure. Considering the limitation of measuring techniques and the complexity of the stress distribution, the developed numerical model can be a very useful tool to elucidate the stress evolution and quantify the effect of remaining welding stress on fracture toughness.

Fracture behavior↗