The Stability of SiO{sub 2} Fe{sub 3}O{sub 4} Nanoparticles for Uranium Extraction in Acidic Media - 20189
This comprehensive study has shown that the proposed strategy of SiO{sub 2} coating of Fe{sub 3}O{sub 4} nanoparticles (NPs) for the use of uranium (U) extraction in acidic media was successful. The breakdown of Fe{sub 3}O{sub 4} in acidic media has proven to be a challenge when applying to a nuclear waste removal scenario, leading to the dissolution of Fe{sub 3}O{sub 4} and preventing uptake of U ions in the waste. To overcome this a SiO{sub 2} passivating layer was grafted to the Fe{sub 3}O{sub 4} NPs, to which an acid stability test was conducted between pH 3 and pH 4. It has been shown via Transmission Electron Microscopy (TEM) and zeta potential measurements that the uncoated Fe{sub 3}O{sub 4} NPs exhibit rapid coagulation when exposed to acidic conditions, moving from a stable zeta potential of -44 mV to an unstable zeta potential of +6 mV. SiO{sub 2} coated Fe{sub 3}O{sub 4} on the other hand can remain stable for several hours and continue to be stable beyond that. Throughout acid exposure the zeta potential of these NPs remained at ∼ -38 mV, showing great stability. As a functionality is needed on the surface of the NPs for separation and extraction, the phosphate complex used was also tested for its acid stability. It was determined that with a constant zeta potential of ∼ -20 mV, the phosphate functionality was able to remain stable in the acidic conditions simulating the environment of certain nuclear wastes. Overall SiO{sub 2} coated (PO)x-Fe{sub 3}O{sub 4} NPs show great promise for application in separation and removal of U in acid media. (authors)