Search NASA⌕ Search

SEARCH · Search NASA

Results for “WELDING, RESISTENCE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

140 records · Page 8

Joining Techniques for Novel Metal Polymer Hybrid Heat Exchangers

In the United States, over 50% of the unrecovered energy from industrial processes is in the form of low-grade heat (< 220°C). Materials and maintenance costs of common heat exchangers are typically too high to justify their usage. Polymers, though more affordable, are usually unsuitable for HX applications due to their low thermal conductivity (~0.2 W/mK). Here, we show that metal-polymer hybrids may be attractive from both performance and cost perspectives. The use of polymers further increases the resistance to corrosion by sulfuric and carbonic acids often present in flue gases. An ongoing work explores different configurations of layered polyimide-copper macroscale hybrids for heat exchanger applications using numerical simulations. This paper explores a manufacturing pathway for producing such layered hybrid tubes that involves directly rolling and bonding tapes made of polymer and copper foil into tubes. A critical problem in the fabrication process is the bonding of metal and polymers. We explore approaches involving adhesives (epoxy, acrylic and silicone) for metal/polymer interfaces and direct welding (ultrasonic) for metal/metal interfaces that can be integrated into the manufacturing process. We report characterizations of the thermomechanical properties of these joining processes. This work paves the way for realizing cost-effective manufacturing of heat exchangers for low grade waste heat recovery.

Kuntumalla, Gowtham↗

Water-Resistant Container Testing: A426-1000 Container Design

The purpose of this report is to detail the results of water ingress testing conducted on the A426-1000 container design and discuss these results against the water-resistant container requirements of TA55-AP- 522 and PA-RD-01009. The A426-1000 is a proposed commercially off the shelf inner container option for material storage inside of a glovebox and/or as an approved non-hermetically sealed inner of an approved packaging configuration inside of an approved outer container as listed in PA-RD-01022. The A426-1000 is shaped like a slip lid container, made of 316L stainless steel, and utilizes a smooth, threaded lid with a silicone O-ring for closure and containment. This container both lid and body is machined out of one billet piece of 316L stainless steel with no welds. See Figure 1 and Table 1 for a summary of the container specifications. For more details on the container design, see Section 1.4.

42 ENGINEERING↗

Water-Resistant Container Testing: 48 oz Bruntmor Container Design

The purpose of this report is to detail the results of water ingress testing conducted on the 48 oz Bruntmor container design and discuss these results against the water-resistant container requirements of TA55-AP 522 and PA-RD-01009. The 48 oz Bruntmor is a proposed commercially off the shelf inner container option for material storage inside of a glovebox and/or as an approved non-hermetically sealed inner of an approved packaging configuration inside of an approved outer container as listed in PA-RD-01022. The 48 oz Bruntmor is shaped like a slip lid container, made of 18-8 stainless steel, and utilizes a smooth, threaded lid with a silicone gasket for closure and containment. This container both lid and body is hot rolled out of 18-8 stainless steel with one seam weld on the body.

42 ENGINEERING↗

Design, Fabrication and Concept for the Surface Treatment of the SRF Cavity Prototype for the CLIC Damping Rings

The Compact Linear Collider (CLIC) Damping Rings (DRs) need to generate ultra-low emittance bunches to achieve high luminosity in CLIC. This requires many wiggler magnets with big energy loss which is compensated by the Radio Frequency (RF) system. The resulting strong beam loading transients lead to a challenging design for the RF system. A novel SRF cavity at 2 GHz with an ultra-low R/Q parameter of below 1 Ω is proposed to minimize the transient beam loading effects below acceptable level. The design and fabrication of the bulk Nb prototype based on turning from a single piece of Nb and EB welding is presented. Moreover, conceptual study of the system for cavity surface treatment to achieve the highest surface magnetic field which is the main goal of the prototype cold test is described as well. To enable excellent performance in this cavity, we plan to apply the 75/120C modified low temperature bake in combination with the cold electropolishing process. This surface treatment approach has been shown to consistently deliver high accelerating gradients and improved quality factors in TESLA-shaped 1.3 GHz SRF cavities. By adapting and implementing this process for the 2 GHz ultra-low R/Q design, we aim to maximize the achievable surface magnetic field while minimizing residual resistance and field emission. This treatment strategy will be critical for demonstrating that the cavity can meet the demanding performance requirements of the CLIC damping ring RF system under high beam loading conditions.

Bafia, Daniel P. [Fermilab]↗

Fabrication and Testing of Solid-Solution Strengthened Corrosion Resistant Alloys For Service in Molten Fluoride Environments

The demand for higher system thermal efficiencies requires the operation of power generation cycles and heat conversion systems at progressively higher temperatures. As the system operating temperature increases, existing materials may not provide adequate mechanical properties or environmental compatibility or both. There is an increasing commercial interest in the development and deployment of liquid-fueled Molten Salt Reactors (MSRs). Hastelloy®N, the highest performing candidate MSR structural alloy, is not capable of operations at temperatures above 700°C, thus limiting the performance of these systems. Using an Integrated Computational Materials Engineering (ICME)-approach and small laboratory scale heats, ORNL developed a class of patented alloys covered by U.S. Patent 9, 435, 011 B2, “Creep-resistant, Cobalt-free alloys for high temperature, liquid-salt heat exchanger systems,” similar to Hastelloy®N in that they are primarily solid solution strengthened. In contrast to precipitation strengthened alloys, the microstructure of solid solution alloys and hence the high temperature mechanical properties are stable for extended periods of time allowing long reactor operating life. The new alloys have shown to possess good resistance to liquid fluorides at temperatures up to 850°C and have significantly improved creep properties when compared to Hastelloy®N. The purpose of the CRADA project was for ORNL to collaborate with Haynes International- a materials producer, MetalTek International- a foundry, and Kairos Power – an advanced reactor developer – to scale-up selected alloys, evaluate their properties, and identify one solid solution strengthened alloy that can meet the property requirements for the reactor being developed by Kairos Power and other similar liquid fluoride-salt cooled reactors. As part of the project, eight alloys were down-selected and fabricated in larger industrial scale heats by Haynes International. Resistance to molten salt was evaluated in flowing FLiNaK and FLiBe by Kairos Power using their Rotating Cage Loop (RCL) system. Accounting for iron deposition during these tests, the new alloys displayed very low net mass change showing excellent corrosion performance in molten salt. Creep properties evaluated at ORNL were found to be better than that of Hastelloy®N and 316 stainless steel. Long-term stabilities of the alloys evaluated by Haynes International showed that these alloys have excellent thermal stability in the temperature range 704.4-815.6°C, with the change in strength and ductility being less than 10-15% after a 4000-hour exposure at 815.6°C. Autogenously Gas Tungsten Arc Welding (GTAW) welded samples showed less than 10% change in yield strength / ultimate tensile strength / total elongation compared to the basemetal, indicating that the alloys have excellent weldability. Three parts were successfully investment-cast using one alloy with very little voiding showing feasibility of fabricating parts using the casting process. This project enabled extensive interaction between the material producer Haynes International, casting supplier MetalTek, and reactor developer Kairos Power. This facilitated testing of materials and components produced using the newly developed alloys by the end-user. This allowed the generation of critical dataset required for down-selection of a few promising alloys for further development. This data is also currently being shared with other reactor designers for them to evaluate the suitability of this alloy for their reactor design. The availability of this alloy will ultimately enable the design and development and deployment of MSRs with increased temperature of operation and thus, improved efficiencies.

99 GENERAL AND MISCELLANEOUS↗

Fabrication and Testing of Solid-Solution Strengthened Corrosion Resistant Alloys For Service in Molten Fluoride Environments

The demand for higher system thermal efficiencies requires the operation of power generation cycles and heat conversion systems at progressively higher temperatures. As the system operating temperature increases, existing materials may not provide adequate mechanical properties or environmental compatibility or both. There is an increasing commercial interest in the development and deployment of liquid-fueled Molten Salt Reactors (MSRs). Hastelloy®N, the highest performing candidate MSR structural alloy, is not capable of operations at temperatures above 700°C, thus limiting the performance of these systems. Using an Integrated Computational Materials Engineering (ICME)-approach and small laboratory scale heats, ORNL developed a class of patented alloys covered by U.S. Patent 9,435,011 B2, “Creep-resistant, Cobalt-free alloys for high temperature, liquid-salt heat exchanger systems,” similar to Hastelloy®N in that they are primarily solid solution strengthened. In contrast to precipitation strengthened alloys, the microstructure of solid solution alloys and hence the high temperature mechanical properties are stable for extended periods of time allowing long reactor operating life. The new alloys have shown to possess good resistance to liquid fluorides at temperatures up to 850°C and have significantly improved creep properties when compared to Hastelloy®N. The purpose of the CRADA project was for ORNL to collaborate with Haynes International- a materials producer, MetalTek International- a foundry, and Kairos Power – an advanced reactor developer – to scale-up selected alloys, evaluate their properties, and identify one solid solution strengthened alloy that can meet the property requirements for the reactor being developed by Kairos Power and other similar liquid fluoride-salt cooled reactors. As part of the project, eight alloys were down-selected and fabricated in larger industrial scale heats by Haynes International. Resistance to molten salt was evaluated in flowing FLiNaK and FLiBe by Kairos Power using their Rotating Cage Loop (RCL) system. Accounting for iron deposition during these tests, the new alloys displayed very low net mass change showing excellent corrosion performance in molten salt. Creep properties evaluated at ORNL were found to be better than that of Hastelloy®N and 316 stainless steel. Long-term stabilities of the alloys evaluated by Haynes International showed that these alloys have excellent thermal stability in the temperature range 704.4-815.6°C, with the change in strength and ductility being less than 10-15% after a 4000-hour exposure at 815.6°C. Autogenously Gas Tungsten Arc Welding (GTAW) welded samples showed less than 10% change in yield strength / ultimate tensile strength / total elongation compared to the basemetal, indicating that the alloys have excellent weldability. Three parts were successfully investment-cast using one alloy with very little voiding showing feasibility of fabricating parts using the casting process. This project enabled extensive interaction between the material producer Haynes International, casting supplier MetalTek, and reactor developer Kairos Power. This facilitated testing of materials and components produced using the newly developed alloys by the end-user. This allowed the generation of critical dataset required for down-selection of a few promising alloys for further development. This data is also currently being shared with other reactor designers for them to evaluate the suitability of this alloy for their reactor design. The availability of this alloy will ultimately enable the design and development and deployment of MSRs with increased temperature of operation and thus, improved efficiencies.

36 MATERIALS SCIENCE↗

Tritium Aging Effects on Fracture Toughness of Stainless Steel Weldments

The long-term embrittlement effects of tritium and decay helium on the structural properties of stainless steels have been studied for years at Savannah River to provide required data for establishing safe operating conditions and lifetimes of pressure vessels used to contain tritium gas. In this study, the fracture toughness properties of the longest-aged tritium-precharged stainless-steel base metals and weldments tested at Savannah River were measured and compared to earlier results. The fracture toughness values were the lowest recorded here for tritium-exposed stainless steel. As-forged and as-welded specimens were thermally precharging with tritium gas at 34.5 MPa and 623 K, then aged for up to 17 years to buildin decay helium prior to testing. ASTM J-Integral fracture mechanics analyses, transmission electron microscopy (TEM), and small angle neutron scattering (SANS) examinations were conducted to characterize the effects of tritium and its radioactive decay product, helium-3. Results show that the fracture toughness values were reduced to less than 2-4% of the as-forged values for specimens with more than 1300 appm helium from tritium decay. The trend of decreasing fracture toughness values with increasing helium content was consistent with earlier observations, and the data show that Type 304L stainless steel is more resistant to tritium-induced cracking than Type 21-6-9 stainless at similar decay helium levels. The fracture toughness properties of long-aged weldments were also affected, but the reductions were not as severe over time because weldments did not retain as much tritium as did the base metals. TEM observations were used to characterize the effects of decay helium bubbles on the deformation substructures, but nanometer-sized helium bubbles were not easily resolved because of high dislocation densities within the forged microstructures. SANS results are presented that suggest the technique can provide information on decay helium bubble size, spacing, and distribution in these steels.

36 MATERIALS SCIENCE↗

Modeling-Based Design and Optimization of a Gradient Composite Transition Joint

An innovative additively manufactured gradient composite transition joint (AM-GCTJ) has been designed to join dissimilar metals, to address the pressing issue of premature failure observed in conventional dissimilar metal welds (DMWs) when subjected to increased cyclic operating conditions of fossil fuel power plants. The transition design, guided by computational modeling, developed a gradient composite material distribution, facilitating a smooth transition in material volume fraction and physical properties between different alloys. This innovative design seeks to alleviate structural challenges arising from distinct material properties, including high thermal stress and potential cracking issues resulting from the thermal expansion mismatch typically observed in conventional DMWs. In this study, we investigated the creep properties of transition joints comprising Grade 91 steel and 304 stainless steel through a combination of simulations and creep testing experiments. The implementation of a gradient composite design in the plate transition joint resulted in a significant enhancement of creep resistance when compared to the baseline conventional DMW. For instance, the creep rupture life of the transition joint was improved by > 400% in a wide range of temperature and stress testing conditions. Meanwhile, the failure location shifted to the base material of Grade 91 steel. Such enhancement can be primarily attributed to the strong mechanical constraint facilitated by the gradient composite design, which effectively reduced the stresses on the less creep-resistant alloy in the transition zone. Beyond examining plate joints, it is crucial to assess the deformation response of tubular transition joints under pressure loading and transient temperature conditions to substantiate and demonstrate the effectiveness of the design. The simulation results affirm that the tubular transition joint demonstrates superior resistance compared to its counterpart DMW when subjected to multiaxial stresses in tubular structures. In addition, optimization of the transition joint’s geometry dimensions has been conducted to diminish the accumulated deformation and enhance the service life. Lastly, the scalability and potential of the innovative transition joints for large-diameter pipe applications are addressed.

Zhang, Wei↗

Electro-Thermo-Mechanical (ETM) Study on Submarine Dynamic Power Cables (SDPC) for Offshore Wind Transmission

Understanding the failure mechanisms of submarine dynamic power cables (SDPC) is critical for innovative design to meet the 2035 cost reduction target of U.S. DOE Floating Offshore Wind Shot. This is important because the current design suffers a significant failure rate in the field. This project conducted a systematic electro-thermo-mechanical (ETM) experimental study on the power cores extracted from a 15kV power cable with three cores of copper conductor, ethylene propylene rubber (EPR) insulation, and continuously corrugated welded aluminum armor (CCWA). An ETM testing system was developed by integrating a high voltage (HV) amplifier, two ceramic heaters, and a rod-plate transverse compression setup into a mechanical testing machine. Increasing temperature from room temperature (RT, 22 degree C) to 90 degree C resulted in the 67% decrease in the failure mechanical load as defined by the dielectric breakdown. Under creep mechanical loading, the dielectric breakdown time was decreased by 70% for a given mechanical load when the specimen temperature increased from RT to 90oC. The failure strain in both monotonic and creep mechanical loading modes was related to the maximum mechanical load applied. Although the dielectric breakdown occurred in the ETM test, the post-test measurement revealed an impressive recovery of electric resistance. The failure analysis on cross section of tested specimens indicated a sizable gap across insulation layer near the area between copper conductor and loading rod, which apparently resulted from online dielectric failure and offline elastic recovery of components including conductor and insulation layer.

17 WIND ENERGY↗

Operando neutron diffraction reveals mechanisms for controlled strain evolution in 3D printing

Abstract Residual stresses affect the performance and reliability of most manufactured goods and are prevalent in casting, welding, and additive manufacturing (AM, 3D printing). Residual stresses are associated with plastic strain gradients accrued due to transient thermal stress. Complex thermal conditions in AM produce similarly complex residual stress patterns. However, measuring real-time effects of processing on stress evolution is not possible with conventional techniques. Here we use operando neutron diffraction to characterize transient phase transformations and lattice strain evolution during AM of a low-temperature transformation steel. Combining diffraction, infrared and simulation data reveals that elastic and plastic strain distributions are controlled by motion of the face-centered cubic and body-centered cubic phase boundary. Our results provide a new pathway to design residual stress states and property distributions within additively manufactured components. These findings will enable control of residual stress distributions for advantages such as improved fatigue life or resistance to stress-corrosion cracking.

36 MATERIALS SCIENCE↗

Intrinsic thermal interfacial resistance measurement in bonded metal–polymer foils

Heat conduction through bonded metal–polymer interfaces often limits the overall heat transfer in electronic packaging, batteries, and heat recovery systems. To design the thermal circuit in such systems, it is essential to measure the thermal interfacial resistance (TIR) across ~1 µm to 100 µm junctions. Previously reported TIR of metal–polymer junctions utilize ASTM E1530-based two-block systems that measure the TIR by applying pressure across the interface through external heating and cooling blocks. Here, we report a novel modification of the ASTM-E1530 technique that employs integrated heaters and sensors to provide an intrinsic TIR measurement of an adhesively bonded metal–polymer junction. We design the measurement technique using finite element simulations to either passively suppress or actively compensate the lateral heat diffusion through the polymer, which can minimize the systematic error to ≲5%. Through proof-of-concept experiments, we report the TIR of metal–polymer interfaces made from DuPont’s Pyralux double-side copper-clad laminates, commonly used in flexible printed circuit boards. Our TIR measurement errors are <10%. We highlight additional sources of errors due to non-idealities in the experiment and discuss possible ways to overcome them. Our measurement technique is also applicable to interfaces that are electrically insulating such as adhesively joined metal–metal junctions and sputter-coated or welded metal–polymer junctions. Altogether, the technique is capable of measuring TIR ≳10 –5 m 2 KW –1 in bonded metal–polymer foils and can be tailored for in situ measurements in flexible electronics, circuit packaging, and other hybrid metal–polymer systems.

47 OTHER INSTRUMENTATION↗

Nanostructured Alumina Forming Austenitic Alloy (NAFA) Production Using Mechanical Alloying and High-Temperature Consolidation

Alumina-forming austenitic (AFA) alloys are a promising class of nuclear materials because of their high-temperature oxidation/corrosion resistance and mechanical properties. Unfortunately, these alloys are limited in use for core material applications, and they are specifically limited for use as nuclear fuel cladding because of their high Ni-transmutation and helium generation rate in-service. Improving these alloys through a fine dispersion of oxide precipitates and thus increasing the effective irradiation sink strength of the alloy system may mitigate many of the degradation phenomena expected during alloy deployment. These phenomena include high-temperature helium embrittlement and cavity swelling for lead-cooled fast reactor applications. This work effort uses combination of conventional and advanced manufacturing approaches are being used to fabricate nanostructured AFA (NAFA) materials. As the first objective of this initiative, a conventional AFA was modified using mechanical alloying and extrusion to alter the precipitation characteristics to include a fine dispersion of nanoscale oxides intended to serve as traps for irradiation-induced point defects and transmuted He within the lattice. This analysis compared the efficacy of the conventional mechanical alloying and extrusion approach with the unalloyed AFA consolidated approach using hot isostatic pressing (HIP). It was found that, although the mechanical alloying approach is successful in producing a fine distribution of oxides within the first nanostructured AFA (NAFA-1), the distribution is heterogeneous because of the mild milling parameters used to prevent cold welding of powder to the spherical milling media. The additional dispersion of oxides, coupled with a higher volume fraction of other secondary phases in the NAFA-1, produces higher alloy strengths that range up to 600°C in comparison to the unalloyed HIP AFA, thus exceeding the operating temperature of lead-cooled fast reactors. However, the strength of the NAFA-1 is lower than that of the HIP AFA at 800°C, which is presumed to be a function of increased secondary phases from the nonoptimized AFA chemistry. Future work is planned on a newly procured NAFA-2 chemistry that is more suitable for advanced reactor applications exploring new manufacturing routes.

36 MATERIALS SCIENCE↗

Improving Economics of Generation 3 CSP System Components Through Fabrication and Application of High Temperature Nickel-Based Alloys

To improve the efficiency and lower the cost of Concentrating Solar Power (CSP) plants, new Generation 3 ‘Gen 3’ CSP concepts using novel salts, solids, or gas heattransfer media envisaged to integrated with a supercritical CO 2 (sCO 2 ) power block at temperatures >715ºC are being investigated. Regardless of the specific pathway, critical components including receivers, piping, and heat-exchangers (HXs) will require the use of heat-resistant nickel-based alloys. Furthermore, the use of age-hardenable alloys, such as INCONEL® alloy 740H® (alloy 740H) may be needed to reduce capital cost. The unique challenges presented by CSP plants to material manufacture, such as small diameter thin-walled tubing in receivers, large diameter thin wall piping, and thin sheet and tubes for HXs can add to the cost to produce such alloys when compared to traditional wrought and cast processing. The goal of this project was to facilitate a reduction of plant cost by developing alternate manufacturing routes and quantifying the performance and economic benefits for alloy 740H in comparison to other candidate nickel-based alloys through fabrication trials, high-temperature mechanical property studies, and interactions with technology developers and codes and standards.

14 SOLAR ENERGY↗

Simulation-driven design optimization of reaction injection molding (RIM) process for polydicyclopentadiene (pDCPD): Minimizing cycle time, defects, and warpage

Replacing metal components in trucks, trailers, and buses with lightweight polymer composites is challenging due to high temperatures and complex manufacturing. The Reaction Injection Molding (RIM) process using Dicyclopentadiene (DCPD) resin offers a solution by producing robust parts with excellent stiffness, impact strength, and resistance properties. Simulations are essential for optimizing this process, predicting defects, and improving quality. However, most commercial software is tailored for thermoplastics, requiring thermoset users to generate their own datasets. In this study, a material data card for DCPD was developed to perform RIM simulations. Design of Experiments (DOE) was used to identify key factors affecting filling, curing, and warpage, aiming to minimize cycle time and defects. The simulations explored varying injection gate parameters (size, location, number) and process conditions (mold/resin temperature, injection/curing pressure). Results showed that gate design significantly impacts filling behavior and defects. A single central gate provided balanced flow with fewer defects, while two corner gates led to more defects. Additionally, lower injection pressure increased filling time, while higher mold temperature accelerated curing but led to more warpage. In conclusion, this optimization framework aims to enhance DCPD part performance and promote sustainable manufacturing by reducing waste and energy consumption.

42 ENGINEERING↗