Probing Electrolyte Solvents at Solid/Liquid Interface Using Gap-Mode Surface-Enhanced Raman Spectroscopy
Not Available
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
Abstract In pursuit of the highest possible energy density, researchers shift their focus to the ultimate anode material, lithium metal (Li 0 ), and high‐capacity cathode materials with high nickel content (Ni > 80%). The combination of these aggressive electrodes presents unprecedented challenges to the electrolyte. Here, we report a hybrid electrolyte consisting of a highly fluorinated ionic liquid and a weakly solvating fluorinated ether, whose hybridization structure enables the reversible operation of a battery chemistry based on Li 0 and LiNiO 2 (Ni = 100%), delivering nearly theoretical capacity of the latter (up to 249 mAh g −1 ) for >300 cycles with retention of 78.6% and in absence of unwanted morphological changes in both electrodes. Extensive characterization assisted by molecular dynamic simulation and density functional theory calculations reveals the function of the fluorinated ether to be far more profound than simple dilution and viscosity reduction. Instead, it induces drastic changes in Li + ‐solvation environment, the consequence of which engenders simultaneous stabilization of electrode/electrolyte and interfacing via formation of respective interfacial chemistries. This study further unlocks fundamental knowledge underneath the prevailing “diluent strategy” that is extensively applied by the electrolyte researchers and opens more design space for the next‐generation electrolytes and interphases for these coveted battery chemistries.
A high voltage LiNi0.5Mn0.3Co0.2O2/graphite cell with a fluorinated electrolyte formulation 1.0 m LiPF6 fluoroethylene carbonate/bis(2,2,2-trifluoroethyl) carbonate is reported and its electrochemical performance is evaluated at cell voltage of 4.6 V. Comparing with its nonfluorinated electrolyte counterpart, the reported fluorinated one shows much improved Coulombic efficiency and capacity retention when a higher cut-off voltage (4.6 V) is applied. Scanning electron microscopy/energy dispersive X-ray spectroscopy and X-ray photoelectron spectroscopy data clearly demonstrate the superior oxidative stability of the new electrolyte. The structural stability of the bulk cathode materials cycled with different electrolytes is extensively studied by X-ray absorption near edge structure and X-ray diffraction.
Ethylene carbonate (EC) is an important component in state-of-the-art electrolytes for lithium-ion batteries (LIBs). However, EC is highly susceptible to oxidation on the surface of high-nickel layered oxide cathodes, making it undesirable for next-generation high-energy-density LIBs. In this study, a simple, yet effective, EC-free electrolyte (20F1.5M-1TDI) is presented by adding 20 wt% fluoroethylene carbonate (FEC) and 1 wt% lithium 4,5-dicyano-2-(trifluoromethyl)imidazole (LiTDI) into 1.5 M LiPF 6 in an ethyl methyl carbonate (EMC) electrolyte. The 20F1.5M-1TDI electrolyte is found to efficiently passivate the graphite anode and stabilize high-nickel cathodes by a synergistic decomposition of FEC and LiTDI. The LiNi 0.9 Mn 0.05 Al 0.05 O 2 (NMA90)/graphite full cell with the 20F1.5M-1TDI electrolyte, therefore, exhibits an enhanced cycling stability and a suppressed voltage hysteresis growth compared to that with an EC-containing baseline electrolyte (1 M LiPF 6 in EC:EMC, 3:7 in weight, with 2 wt% vinyl carbonate). Advanced analytical tools, such as time-of-flight secondary ion mass spectrometry and X-ray photoelectron spectroscopy, are employed to understand the underlying working mechanism of the EC-free electrolyte. Furthermore, the present study clearly showcases the great potential of EC-free electrolytes as a straightforward, practical approach for LIBs with high-nickel cathodes.
Not Available
Ni-rich layered transition metal oxide (NMC, LiNi1-x-yMxCoyO2, 1 – x – y = 0.6) is promising for high-energy-density lithium-ion batteries, but its large-scale application is still hindered by several technical challenges, including secondary particle cracking, interfacial instability, and cell degassing during cycling. Here, we report a facile wet-chemical method to modify both the surface and the bulk of the LiNi0.76Mn0.14Co0.10O2 (NMC76) cathode with Al doping to effectively improve the structural/interfacial stability of the cathode, and hence its long-term cycling capability. With only 1 mol% Al doping, the Al-NMC76 electrode delivers a good capacity retention of 79.2% after 500 cycles at a high voltage limit of 4.5 V, which is far better than those of undoped NMC76 under the similar condition. The enhanced performance can be attributed to the Al doping in the NMC76, which not only strengthens the bulk structural stability through doping into the lattice, but also suppresses acidic attack from the electrolyte through altered surface structure of NMC76.
Through coupled experimental analysis and computational techniques, we uncover the origin of anodic stability for a range of nonaqueous zinc electrolytes. By examination of electrochemical, structural, and transport properties of nonaqueous zinc electrolytes with varying concentrations, it is demonstrated that the acetonitrile Zn(TFSI) 2 , acetonitrile Zn(CF 3 SO 3 ) 2 , and propylene carbonate Zn(TFSI) 2 electrolytes can not only support highly reversible Zn deposition behavior on a Zn metal anode (≥99% of Coulombic efficiency), but also provide high anodic stability (up to ~3.8 V). The predicted anodic stability from DFT calculations is well in accordance with experimental results, and elucidates that the solvents play an important role in anodic stability of most electrolytes. Molecular dynamics (MD) simulations were used to understand the solvation structure (e.g., ion solvation and ionic association) and its effect on dynamics and transport properties (e.g., diffusion coefficient and ionic conductivity) of the electrolytes. Lastly, the combination of these techniques provides unprecedented insight into the origin of the electrochemical, structural, and transport properties in nonaqueous zinc electrolytes
The electrolyte generally dictates the working temperature range of lithium ion batteries (LIBs), thus developing new class of electrolytes (primarily functional additives) in LIBs for wide temperature applications will be quite essential for further development of LIBs for electric vehicle market. In this study, we develop new functional electrolytes containing multiple additives to enable the LIBs to perform well in a wide temperature range from -40°C to 60°C. Importantly, those cells based on the above optimized electrolytes have been proven to behave significantly enhanced discharging performance at -40°C, the long-term cycling stability at 25°C (more than 85% of capacity retention after 1000 cycles at 1C/1C rates in 1 Ah pouch cells), as well as the obviously improved cycling stability at 60°C. These remarkable cell performances originate from the highly conductive, uniform and compact passivating films formed on both anode and cathode surfaces by the synergistic effects of the multiple additives. Our finding on the synergistic benefits originating from certain additive combination in the optimized electrolytes would favorably widen the working temperature range of future high-performance LIBs.
In our initial study on the high-voltage 5 V cobalt-free spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) cathode, we discovered a severe delamination issue in the laminates when cycled at a high upper cut-off voltage (UCV) of 4.95 V, especially when a large cell format was used. This delamination problem prompted us to investigate further by studying the transition metal (TM) dissolution mechanism of cobalt-free LNMO cathodes, and as a comparison, some cobalt-containing lithium nickel manganese cobalt oxides (NMC) cathodes, as the leachates from the soaking experiment might be the culprit for the delamination. Unlike other previous reports, we are interested in the intrinsic stability of the cathode in the presence of a baseline Gen2 electrolyte consisting of 1.2 M of LiPF 6 in ethylene carbonate/ethyl methyl carbonate (EC/EMC), similar to a storage condition. The electrode laminates (transition metal oxides, transition metal oxides, TMOs, coated on an Al current collector with a loading level of around 2.5 mAh/cm 2 ) or the TMO powders (pure commercial quality spinel LNMO, NMC, etc.) were stored in the baseline solution, and the transition metal dissolution was studied through nuclear magnetic resonance, such as 1 H NMR, 19 F NMR, scanning electron microscope (SEM), X-ray photoelectron spectroscopy (XPS) and inductively coupled plasma mass spectrometry (ICP-MS). Significant electrolyte decomposition was observed and could be the cause that leads to the TM dissolution of LNMO. To address this TM dissolution, additives were introduced into the baseline electrolyte, effectively alleviating the issue of TM dissolution. The results suggest that the observed delamination is caused by electrolyte decompositions that lead to etching, and additives such as lithium difluorooxalato borate and p-toluenesulfonyl isocyanate can alleviate this issue by forming a firm cathode electrolyte interface. This study provides a new perspective on cell degradation induced by electrode/electrolyte interactions under storage conditions.
The desalination characteristics of capacitive deionization (CDI) are significantly impacted by the cell resistance. Here we apply electrochemical impedance spectroscopy (EIS) to analyze the resistive properties of a CDI device, which include EIS measurements on a complete assembled cell (in two wire mode) and EIS measurements with additional contacts to decouple electrode/electrolyte and contact impedances (four wire mode). These measurements shed light on the interface between current collector and electrode as well as the internal capacitive and resistive elements of the cell. With two-wire and four-wire EIS measurements, we find that the often observed high-frequency arc(s) in the impedance spectra can be due to contact effects and/or an internal ionic-transfer resistance that is locally in parallel with macropore wall capacitance. In some cases, the two associated arcs in the Nyquist plot are overlapping and present simultaneously, making their identification in the EIS spectra difficult unless both two-wire and four-wire measurements are made. Despite causing a large high-frequency arc in the Nyquist plot, we find that the apparent internal ionic-transfer resistance is negligible compared to the resistances of the electrode, separator, and external electronic components. Here, an investigation of the contact impedance between the electrode and current collector reveals a parallel RC arc that can grow over time if an improper material is used (e.g., titanium). In our system, the electrode ionic resistance dominates the total Ohmic power dissipation, which has implications for scale-up of CDI systems and future improvements of cell design.
Abstract Solid‐state polymer electrolytes provide better flexibility and electrode contact than their ceramic counterparts, making them a worthwhile pursuit for all‐solid‐state lithium‐metal batteries. However, their large Li/solid state electrolyte interfacial resistance, small critical current density, and rapid lithium dendrite growth during cycling still limit their viability. Owing to these restrictions, all‐solid‐state cells with solid polymer electrolytes must be cycled above room‐temperature and with a small current density. These problems can be mitigated with an in situ formed artificial solid electrolyte interphase that rapidly conducts Li + ions. Herein, a Li 3 P layer formed in situ at the Li‐metal/solid polymer electrolyte interphase is reported that significantly reduces the electrode/electrolyte interfacial resistance. Additionally, this layer increases the wettability of the solid polymer by the metallic lithium anode, allowing for the critical current density of lithium symmetric cells to be doubled by homogenizing the current density at the interface. All‐solid‐state Li/Li symmetric cells and Li/LiFePO 4 cells with the Li 3 P layer show improved cycling performance with a high current density.
Low initial Coulombic efficiency and severe capacity/voltage fading during cycling caused by serious irreversible oxygen release, especially in the initial cycle, and resultantly induced unstable electrode/electrolyte interfacial chemistry, largely prohibit the commercial application of high-capacity Li-rich layered oxide cathodes (LLOs). Here, in this work, a dual reductive gas interface cotreatment strategy is applied to regulate the lattice oxygen redox activity and reversibility with a multiple defective structure design including Li/O/TM (TM = transition metal) vacancies and the intrinsic TM doping as well as a full-surface protective layer, which can suppress the irreversible TM migration and then undesirable phase transformation, resisting the corrosion of electrolyte during cycling effectively. Importantly, the introduced reversible SO 3 2- /SO 4 2- redox couple that provides extra capacity compensation could alleviate the distortion of oxygen-central octahedral structure and structural collapse caused by immoderate oxygen oxidation. Thus, the lattice oxygen redox chemistry is optimized, with negligible oxygen loss during the initial cycle. And the designed AS-LLO cathode with greatly enhanced structure stability shows high-capacity retentions of 99.2% at 0.3C after 100 cycles and 82.4% even after 1000 cycles at 5C. This work provides a guideline for manipulating the oxygen redox chemistry to achieve long-lifespan Li-rich layered oxide cathodes for high-energy-density lithium batteries.
Sulfurized polyacrylonitrile (SPAN) represents one of the most promising directions for high-energy-density lithium (Li)-sulfur batteries. However, the practical application of Li||SPAN is currently limited by the insufficient chemical/electrochemical stability of electrode/electrolyte interphase (EEI). Here, a pinned EEI layer is designed for stabilizing a SPAN cathode by regulating the EEI formation mechanism in an advanced LiFSI/ether/fluorinated-ether electrolyte. Computational simulations and experimental investigations reveal that, benefiting from the nonsolvating nature, the fluorinated-ether can not only act as a protective shield to prevent the Li polysulfides dissolution but also, more importantly, endow a diffusion-controlled EEI formation process. It promotes the formation of a uniform, protective, and conductive EEI layer pinning into SPAN surface region, enabling the high loading Li||SPAN batteries with superior cycling stability, wide temperature performance, and high-rate capability. Finally, this design strategy opens an avenue for exploring advanced electrolytes for Li||SPAN batteries and guides the interface design for broad types of battery systems.
The main goal of this project is to develop a multi-scale modeling approach that connects micron-scale phase-field models and atomic-scale density functional theory (DFT)-based simulations via parameter- and relationship-passing in order to predict Li-metal dendrite morphology evolution, in both liquid and solid electrolytes. The key hypothesis of the DFT-informed phase-field multiscale modeling approach is that it can capture the electrochemical-mechanical driving forces and incorporate the roles of nano-meter-thin solid electrolyte interphase (SEI) in liquid electrolytes as well as of the microstructures of micro-meter-thick solid electrolytes (SEs) for all-solid-state batteries. In this project, we have formulated and implemented phase-field models to incorporate the electrochemical driving forces in liquid electrolytes and then incorporate mechanical driving forces to simulate dendrite growth in solid electrolytes with resolved microstructures. We have implemented two treatments for the SEI: an explicit model to include the microstructure of the SE or SEI in the phase field model and an implicit model to simulate the impact of nano-meter thick SEI in liquid electrolytes by varying the electrode/electrolyte interfacial properties. The key interfacial properties, including the electronic and ionic transport properties, the charge transfer reaction kinetics, and mechanical properties, were computed by DFT-based calculations. At the DFT-based model, one key advancement is to directly predict the charge transfer reaction kinetics at a complex Li/SEI/electrolyte interface by linking DFT with density functional tight binding (DFTB) calculations. As the main accomplishments, we have demonstrated two successful predictions in both solid electrolyte and liquid electrolyte based on this multiscale approach. The predicted intergranular Li dendrite growth in LLZO revealed the importance of trapped electrons at internal interfaces in the microstructure of LLZO. The predicted electroplating morphology of mossy Li and faceted Mg agreed well with experiments. The insights provided by the multiscale model and the model enabled electrolyte and SEI design will accelerate the development of Li-metal electrode for high energy density batteries, that meet DOE’s target on cell density (>350 Wh/kg) and cost below $100/kWhuse for EV applications.
Increasing the energy density of energy storage devices is currently the key target of many battery and supercapacitor research activities. For both types of devices, the electrochemical stability window (ESW) determines the effective energy density of the device. ESWs are defined by the effective oxidation and reduction potentials of the electrolyte, which are controlled by many various factors, including the HOMO/LUMO (highest/lowest unoccupied molecular orbital) energies of the electrolyte molecules, the nature of the electrode/electrolyte interphases, and other physicochemical properties. The concentration of the electrolyte would affect the HOMO/ LUMO levels thus also change the ESW. A higher concentration of salt induces specific arrangements among the anion, cation, and solvent molecules of an electrolyte, altering the bulk behavior of the electrolyte, resulting in drastic change in the electrode interfaces. These uniquely modified physicochemical properties extend the ESW in several different ways, including the enhancement in the kinetic stability of the electrodes, as well as the thermodynamic and Nernst shifts of the oxidation/reduction potentials of the electrolyte. For organic electrolytes, it is the reduced amount of free solvent molecules that plays the key role in such changes; whereas for aqueous electrolytes, it is the scarcity of free water molecules and the reduced water activity that control the key properties of the electrolyte. Here, we focus on elucidating the fundamental structural changes occurring within an electrolyte system with increasing salt concentrations. The underlying mechanisms which not only facilitates the extension of the ESW, but also enables higher rate capabilities and mitigates aluminum dissolution for batteries with organic electrolytes, are meticulously explained. Further, we thoroughly discuss the importance of high-voltage stability in aqueous battery systems by exploiting the changed properties observed with higher concentrations of salts. To finish, high-voltage supercapacitors enabled by superconcentrated electrolytes are also explored.
Abstract Protonic ceramic electrochemical cells (PCECs) offer promising paths for energy storage and conversion. Despite considerable achievements made, PCECs still face challenges such as physiochemical compatibility between componenets and suboptimal solid–solid contact at the interfaces between the electrolytes and electrodes. In this study, a novel approach is proposed that combines in situ electrochemical characterization of interfacial electrical sensor embedded PCECs and machine learning to quantify the contributions of different cell components to total degradation, as well as to predict the remaining useful life. The experimental results suggest that the overpotential induced by the oxygen electrode is 48% less than that of oxygen electrode/electrolyte interfacial contact for up to 1171 h. The data‐driven machine learning simulation predicts the RUL of up to 2132 h. The root cause of degradation is overpotential increase induced by oxygen electrode, which accounts for 82.9% of total cell degradation. The success of the failure diagnostic model is demonstrated by its consistency with degradation modes that do not manifest in electrolysis fade during early real operations. This synergistic approach provides valuable insights into practical failure diagnosis of PCECs and has the potential to revolutionize their development by enabling improved performance prediction and material selection for enhanced durability and efficiency.
Here, a new deposition mechanism is presented in this study to achieve highly reversible plating and stripping of magnesium (Mg) anodes for Mg-ion batteries. It is known that the reduction of electrolyte anions such as bi s (trifluoromethanesulfonyl) imide (TFSI - ) causes Mg surface passivation, resulting in poor electrochemical performance for Mg-ion batteries. We reveal that the addition of sodium cations (Na + ) in Mg-ion electrolytes can fundamentally alter the interfacial chemistry and structure at the Mg anode surface. The molecular dynamics simulation suggests that Na + cations contribute to a significant population in the interfacial double layer so that TFSI - anions are excluded from the immediate interface adjacent to the Mg anode. As a result, the TFSI - decomposition is largely suppressed so does the formation of passivation layers at the Mg surface. This mechanism is supported by our electrochemical, microscopic, and spectroscopic analyses. The resultant Mg deposition demonstrates smooth surface morphology and lowered overpotential compared to the pure Mg(TFSI) 2 electrolyte.
Our EFRC was founded with the vision of creating a broadly collaborative and synergistic program that would lead to major breakthroughs in the molecular-level understanding of the critical interfacial charge separation and charge transfer (CST) processes that underpin the function of candidate materials for organic photovoltaic (OPV) and electrical-energy-storage (EES) applications. Research in these energy contexts shares an imposing challenge: How can we understand charge separation and transfer mechanisms in the presence of immense materials complexity that spans multiple length scales? To address this challenge, our 50-member Center undertook a total of 28 coordinated research projects aimed at unraveling the CST mechanisms that occur at interfaces in these nanostructured materials. This rigorous multi-year study of CST interfaces has greatly illuminated our understanding of early-timescale processes (e.g., exciton generation and dissociation dynamics at OPV heterojunctions; control of Li+-ion charging kinetics by surface chemistry) occurring in the immediate vicinity of interfaces. Program outcomes included: training of 72 graduate student and postdoctoral energy researchers at 5 institutions and spanning 7 academic disciplines in science and engineering; publication of 94 peer-reviewed journal articles; and dissemination of research outcomes via 340 conference, poster and other presentations. Major scientific outcomes included: implementation of a hierarchical strategy for understanding the electronic communication mechanisms and ultimate fate of charge carriers in bulk heterojunction OPV materials; systematic investigation of ion-coupled electron transfer processes in model Li-ion battery electrode/electrolyte systems; and the development and implementation of 14 unique technologies and instrumentation capabilities to aid in probing sub-ensemble charge separation and transfer mechanisms.