Search NASA⌕ Search

SEARCH · Search NASA

Results for “module degradation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Onymous early‐life performance degradation analysis of recent photovoltaic module technologies

Abstract The cost of photovoltaic (PV) modules has declined by 85% since 2010. To achieve this reduction, manufacturers altered module designs and bill of materials; changes that could affect module durability and reliability. To determine if these changes have affected module durability, we measured the performance degradation of 834 fielded PV modules representing 13 module types from 7 manufacturers in 3 climates over 5 years. Degradation rates ( Rd ) are highly nonlinear over time, and seasonal variations are present in some module types. Mean and median degradation rate values of −0.62%/year and −0.58%/year, respectively, are consistent with rates measured for older modules. Of the 23 systems studied, 6 have degradation rates that will exceed the warranty limits in the future, whereas 13 systems demonstrate the potential of achieving lifetimes beyond 30 years, assuming Rd trends have stabilized.

14 SOLAR ENERGY↗

Quantifying Optical Loss of High-Voltage Degradation Modes in PV Modules Using Spectral Analysis [Slides]

The direct current bias for photovoltaic (PV) modules interconnected in series-strings may include both high voltage negative ("HV-") and positive ("HV+") polarity with respect to the electrical ground. Multiple degradation modes, resulting in quantifiable optical loss, were found to occur during HV-/HV+ sequential stress, including: corrosion of the external glass surface, encapsulant delamination (at its interfaces with the glass and the PV cell), internal haze formation (resulting from a chemical interaction between the glass and the encapsulant), corrosion and migration of the gridlines, and corrosion of the silicon nitride (SixNy) antireflective coating on the cell. The effects of these separate modes were examined using monolithic (e.g., glass or PV cell) and laminated-coupon (glass/encapsulant/glass or glass/encapsulant/cell/encapsulant/backsheet) specimens. Characterizations during and after unbiased accelerated testing at 85 degrees C/85% relative humidity included: spectrophotometry, optical microscopy, electron microscopy, and ellipsometry. For some module components (i.e., the glass and the SixNy coating), the optical performance was determined through iterative analysis of empirical measurements. Concentrating on just their spectral effect, a novel model was then developed to estimate the transfer of light to the PV cell and the return of light from the PV module with simultaneous degradation mechanisms, which was compared to a mini-module previously subjected to HV-/HV+ stress. The model suggests one-third of the current loss observed for the mini-module can be attributed to the optical degradation of the packaging materials. The dominant degradation modes include encapsulant delamination and corrosion of the SixNy coating. Recommendations are given so that the optical model may be improved relative to accelerated testing and validated relative to field aging.

14 SOLAR ENERGY↗

Quantifying optical loss of high-voltage degradation modes in photovoltaic modules using spectral analysis

The direct current bias for photovoltaic (PV) modules interconnected in series-strings may include both high voltage negative (“HV-”) and positive (“HV+”) polarity with respect to the electrical ground. Multiple degradation modes, resulting in quantifiable optical loss, were found to occur during HV-/HV+ sequential stress, including corrosion of the external glass surface, encapsulant delamination (at its interfaces with the glass and the PV cell), internal haze formation (resulting from a chemical interaction between the glass and the encapsulant), corrosion and migration of the gridlines, and corrosion of the silicon nitride (Si x N y ) antireflective coating on the cell. The effects of these separate modes were examined using monolithic (e.g., glass or PV cell) and laminated-coupon (glass/encapsulant/glass or glass/encapsulant/cell/encapsulant/backsheet) specimens. Characterizations during and after unbiased accelerated testing at 85°C/85% relative humidity included spectrophotometry, optical microscopy, electron microscopy, and ellipsometry. For some module components (i.e., the glass and the Si x N y coating), the optical performance was determined through iterative analysis of empirical measurements. Concentrating on just their spectral effect, a novel model was then developed to estimate the transfer of light to the PV cell and the return of light from the PV module with simultaneous degradation mechanisms, which was compared with a mini-module previously subjected to HV-/HV+ stress. Here the model suggests that one third of the current loss observed for the mini-module can be attributed to the optical degradation of the packaging materials. The dominant degradation modes include encapsulant delamination and corrosion of the Si x N y coating. Recommendations are given so that the optical model may be improved relative to accelerated testing and validated relative to field aging.

14 SOLAR ENERGY↗

Thermal Assessment and In-Situ Monitoring of Insulated Gate Bipolar Transistors in Power Electronic Modules: Preprint

Insulated gate bipolar transistor (IGBT) power modules are devices commonly used for switching of high voltages and currents. Usage and environmental conditions can cause these power modules to degrade over time, and this gradual process may eventually lead to catastrophic failure of the device. This degradation process may cause some early performance symptoms related to the state of health of the power module, making it possible to detect reliability degradation of the IGBT module. Testing can be used to accelerate this process, permitting a rapid determination of whether specific declines in device reliability can be characterized. In this study, thermal cycling was conducted on multiple power modules simultaneously in order to assess the effect of thermal cycling on the degradation of the power module. In-situ monitoring of temperature was performed from inside each power module using high temperature thermocouples. Device imaging and characterization was performed along with temperature data analysis, to assess failure modes and mechanisms within the power modules. While the experiment was aimed to assess the potential damage effects of thermal cycling on die attach, results indicated that wirebond degradation was the life limiting failure mechanism.

33 ADVANCED PROPULSION SYSTEMS↗

Transmission Electron Microscopy Study on Microstructure of Degraded CdTe Mini-Modules

In this paper, we employ transmission electron microscopy coupled with energy-dispersive X-ray spectrometry (EDS) to study the structure and chemistry of cadmium telluride (CdTe) thin-film solar cells with different extents of degradation. The studied regions originate from the same photovoltaic mini-module, which was subjected to one-sun light exposure at a temperature of 100 degrees C for 400 h to induce light and heat degradation. EDS maps reveal a discontinuous CdS layer and particles rich in O and S but Te-depleted within the CdTe absorber layer after the light and heat stress. These features could act as enhanced recombination centers, resulting in decreased photovoltaic conversion efficiency. Additionally, the most degraded CdTe sample shows a strong accumulation of Na precisely localized in the discontinuous part of the CdS layer. The local Na concentration is determined to be ~16 at.%. In addition, appreciable Na accumulation is observed at the soda-lime glass/transparent conductive oxide interface in both degraded CdTe solar cells. The microstructure of the baseline CdTe mini-module with no stress was also investigated to demonstrate that the structure difference was caused by the light- and heat-induced degradation, instead of module fabrication. These results highlight the need to control the distribution of Na in fielded CdTe modules to sustain long-term high-power output.

14 SOLAR ENERGY↗

Modeling Time to Failure in Potential-Induced Degradation of Silicon Solar Modules based on Quantitative Sodium Kinetics

We present a physics-based simulation environment for the prediction of potential-induced-degradation (PID) failure time in silicon solar modules. Our model is based on experimental sodium migration kinetics obtained from our recently developed trap-corrected bias-stress-temperature method and from secondary ion mass spectrometry measurements. Furthermore, we model sodium migration to stacking faults and subsequent formation of conductive pathways through the p-n junction, which causes a decrease of the shunt resistance and loss of efficiency.

42 ENGINEERING↗

Mechanisms of adhesion degradation at the photovoltiac module's cell metallization-encapsulant interface

Adhesion measurements and chemical characterization of the encapsulant/silver metallization interface of a photovoltaic (PV) module through temperature, humidity, and voltage bias exposures were conducted. Results demonstrate two independent degradation mechanisms: (a) with voltage bias, the ionic conduction of Na + ions through the encapsulant results in the formation of sodium silicate at the silver metallization surface, thereby weakening that interface and (b) with moisture ingress, dissociation of the silane bonding to silver in the silver oxide similarly weakens this interface resulting in significantly lower debond energies.

14 SOLAR ENERGY↗

Elucidating PID Degradation Mechanisms and In Situ Dark I–V Monitoring for Modeling Degradation Rate in CdTe Thin-Film Modules

A progression of potential-induced degradation (PID) mechanisms are observed in CdTe modules, including shunting/junction degradation and two different manifestations of series resistance depending on the stress level and water ingress. The dark I-V method for in-situ characterization of Pmax based on superposition was adapted for the thin-film modules undergoing PID in view of the degradation mechanisms observed. An exponential model based on module temperature and relative humidity was fit to the PID rate for multiple stress levels in chamber tests and validated by predicting the observed degradation of the module type in the field.

14 SOLAR ENERGY↗

Analysis of the Long-Term Performance Degradation of Crystalline Silicon Photovoltaic Modules in Tropical Climates

For this study, the long-term performance degradation of five different types of commercial crystalline silicon (c-Si) photovoltaic (PV) modules (one sample for each type) in the tropics, or more specifically the tropical rainforest climate 'Af' by the Koppen climate classification (Singapore), is investigated over a period of seven years, based on outdoor I-V measurements at 10-s intervals. The degradation rates of these c-Si PV modules, based on the temperature-corrected performance ratio, range from -0.03 to -0.47%/year, which satisfy the products' performance warranty. Further analysis of the short-circuit current (I sc), open-circuit voltage, and fill factor for these modules shows that the performance degradation is mainly attributed to the l sc loss. Lastly, the possible causes of the module performance deterioration are also discussed.

14 SOLAR ENERGY↗

UV‐induced degradation of high‐efficiency silicon PV modules with different cell architectures

Abstract Degradation from ultraviolet (UV) radiation has become prevalent in the front of solar cells due to the introduction of UV‐transmitting encapsulants in photovoltaic (PV) module construction. Here, we examine UV‐induced degradation (UVID) in various commercial, unencapsulated crystalline silicon cell technologies, including bifacial silicon heterojunction (HJ), interdigitated back contact (IBC), passivated emitter and rear contact (PERC), and passivated emitter rear totally diffused (PERT) solar cells. We performed UV exposure tests using UVA‐340 fluorescent lamps at 1.24 W·m −2 (at 340 nm) and 45°C through 4.02 MJ·m −2 (2000 h). Our results showed that modern cell architectures are more vulnerable to UVID, leading to a significant power decrease (−3.6% on average; −11.8% maximum) compared with the conventional aluminum back surface field (Al‐BSF) cells (<−1% on average). The power degradation is largely caused by the decrease in short‐circuit current and open‐circuit voltage. A greater power decrease is observed in bifacial cells with rear‐side exposure compared with those with front‐side exposure, indicating that the rear side is more susceptible to UV damage. Secondary ion mass spectroscopy (SIMS) confirmed an increase in hydrogen concentration near the Si/passivation interface in HJ and IBC cells after UV exposure; the excess of hydrogen could result in hydrogen‐induced degradation and subsequently cause higher recombination losses. Additionally, surface oxidation and hot‐carrier damage were identified in PERT cells. Using a spectral‐based analysis, we obtained an acceleration factor of 5× between unpackaged cells (containing a silicon nitride antireflective coating on the front) in the UV test and an encapsulated module (with the front glass and encapsulant blocking 90% of the UV at 294 nm and 353 nm, respectively) in outdoor conditions. From the analytical calculations, we show that a UV‐blocking encapsulant can reduce UV transmission in the module by an additional factor of ~50.

14 SOLAR ENERGY↗

Multiscale Characterization of Photovoltaic Modules—Case Studies of Contact and Interconnect Degradation

The current popularity of photovoltaic (PV) systems is due in large part to their exceptional reliability and significantly lower cost than other energy sources. Studying cell and module degradation is key to promote further development in the state of the art. Fielded or accelerated aged modules exhibit different failure modes, of which metallization degradation (contacts and interconnections) is prevalent. In this work, we discuss how multiscale characterization methods can be applied to a variety of module technologies that have been field exposed and have undergone accelerated age testing. These methods include performing characterization on the module level, cell level, and finally the materials level. The observed performance losses from the module- and cell-level characterization can be correlated with materials properties to find out the root cause of degradation. We recommend an initial nondestructive characterization suite, including module- and cell-level current-voltage ( I--V ), Suns-V OC , photoluminescence and electroluminescence imaging, quantum efficiency, ultraviolet fluorescence imaging, and thermal infrared imaging. Samples are then extracted from particularly degraded regions of the module and prepared for materials characterization techniques, such as top-down and cross-sectional scanning electron microscopy, energy-dispersive X-ray spectroscopy, X-ray photoelectron spectroscopy, secondary ion mass spectrometry, Raman spectroscopy, and transmission electron microscopy, allowing a deeper look into the mechanism behind the metallization degradation. This article serves as an instructional review to introduce the different multiscale characterization methods and how they can be effectively applied to perform PV degradation studies. Furthermore, we also share some of our examples and discuss the strengths, limitations, and best practices for each of the characterization techniques.

14 SOLAR ENERGY↗

Comprehensive study of performance degradation of field‐mounted photovoltaic modules in India

Abstract The All India Survey of Photovoltaic Module Reliability 2014 is an enhanced version of the survey conducted in the previous year, with detailed characterization of PV modules including current‐voltage, infrared and electroluminescence imaging, visual inspection, insulation resistance test and interconnect breakage test. More than a thousand modules were inspected in the field and the main results of the survey are presented in this paper. The average P max degradation rate for the so‐called ‘good’ modules (Group X) is 1.33%/year which is higher than that commonly projected by manufacturers, and widely employed in financial calculations. Modules falling in the ‘not‐so‐good’ category (Group Y) show even higher degradation rates, and it is at least partly due to higher number of micro‐cracks in the modules, and increased degradation of the packaging materials like encapsulant, backsheet, etc. Modules in ‘Hot’ climates degrade faster than modules in the ‘Non‐Hot’ climates. Degradation in fill factor is the primary cause for performance degradation in the young modules (ages <5 years), whereas short‐circuit current degradation is the main contributor to power degradation in the older modules. Small installations (<100 kW p capacity) show higher degradation than large systems, which may be partly due to lack of proper due diligence by the owner at the time of procurement and installation.

Dubey, Rajiv↗

Sodium accumulation at potential-induced degradation shunted areas in polycrystalline silicon modules

Here, we investigated potential-induced degradation (PID) in silicon mini-modules that were subjected to accelerated stressing to induce PID conditions. Shunted areas on the cells were identified with photoluminescence and dark lock-in thermography (DLIT) imaging. The identical shunted areas were then analyzed via time-of-flight secondary-ion mass spectrometry (TOFSIMS) imaging, 3-D tomography, and high-resolution transmission electron microscopy. The TOF-SIMS imaging indicates a high concentration of sodium in the shunted areas, and 3-D tomography reveals that the sodium extends more than 2 um from the surface below shunted regions. Transmission electron microscopy investigation reveals that a stacking fault is present at an area identified as shunted by DLIT imaging. After the removal of surface sodium, tomography reveals persistent sodium present around the junction depth of 300 nm and a drastic difference in sodium content at the junction when comparing shunted and nonshunted regions.

14 SOLAR ENERGY↗

Characterization of Field-Exposed Photovoltaic Modules Featuring Signs of Contact Degradation

Here, this work investigates several photovoltaic (PV) modules that have shown signs of metal contact corrosion due to field exposure in a hot and humid climate. This includes two multicrystalline silicon aluminum back surface field systems with 10 and 14 years of exposure and one monocrystalline silicon passivated emitter and rear cell system with four years of exposure. A comprehensive, multiscale characterization process is used to evaluate these PV modules in great detail. Current–voltage (I−V), Suns-V OC measurements, electroluminescence imaging, infrared imaging, and ultraviolet fluorescence imaging were performed, and locations of interest were cored and analyzed using cross-sectional scanning electron microscopy (SEM). A rigorous, quantitative analysis procedure for the cross-sectional SEM images is proposed and implemented. Careful characterization does reveal that some of these PV modules do indeed exhibit the same classic signs of acetic-acid-based corrosion of the glass frit that is present at the silver/silicon interface, which have been observed previously in PV modules exposed to damp heat in an environmental chamber.

14 SOLAR ENERGY↗

Degradation Analysis of Field-Exposed Photovoltaic Modules with Non-Fluoropolymer-Based Backsheets

The selection of polymeric materials utilized in photovoltaic (PV) modules has changed relatively little since the inception of the PV industry, with ethylene-vinyl acetate (EVA), polyethylene terephthalate (PET), and fluoropolymer-based laminates being the most widely adopted primary components of the encapsulant and backsheet materials. The backsheet must serve to electrically insulate the solar cells and protect them from the effects of weathering. Due to continued downward pressure on cost, other polymeric materials are being formulated to withstand outdoor exposure for use in backsheets to replace either the PET film, the fluoropoymer film, or both. Because of their relatively recent deployment, less is known about their reliability and if they are durable enough to fulfill the greater than or equal to 25 year warranties of current PV modules. This work presents a degradation analysis of field-exposed modules with polyamide- and polyester-based backsheets. Modules were exposed for up to five years in different geographic locations: USA (Maryland, Ohio), China, and Italy. Surface and cross-sectional analysis included visual inspection, colorimetry, glossimetry, and Fourier-transform infrared spectroscopy. Each module experienced different types of degradation depending on the exposure site, even for the same material and module brand. For instance, the polyamide-based backsheet experienced hairline cracking and greater yellowing and chemical changes in China (Changsu, humid subtropical climate), while in Italy (Rome, hot-summer Mediterranean climate) it underwent macroscopic cracking and greater losses in gloss. Spectroscopic studies have permitted identification of degradation products and changes in polymer structure over time. Comparisons are made to fielded modules with fluoropolymer-based backsheets, as well as backsheet materials in accelerated laboratory exposures. Implications for qualification testing and service life prediction of the non-fluoropolymer-based backsheets are discussed.

14 SOLAR ENERGY↗

Improving solar panel durability through novel panel designs and advanced manufacturing equipment

Work in the project was spread across 4 main themes:1) Improved Understanding of Why Cracks Form and Cause Degradation in Solar Cells: We developed a finite element model which correlated well with experimental determined deflection vs load profiles and which predicted stress profiles vs load level and temperature. These profiles helped to guide brace designs and showed the high stress levels seen in the silicon near the interconnect wire locations as the temperature is cooled below -30C, likely forming "invisible" microcracks. Experiments showed how for polymer backsheet modules, a brief exposure to such low temperatures made modules extremely sensitive to propagation of these microcracks at relatively low load levels, and how thicker and softer encapsulant helped to reduce this crack sensitivity. We showed for some modules that most cracks that are seen under loading had their origin at short, hard to see, V-cracks from soldering damage, and how the shunting from cells with high densities of cracks reduces energy delivery more than Pmax. 2) Improved Durability Testing Methods With Respect to Cracked Cells: We lobbied the PV community throughout the project that IEC 61215 was insufficient to probe the sensitivity of module Pmax degradation due to cracks in that in did not have a test leg that included a crack creation step (static loading) followed by a crack opening step (cyclic loading and/or thermal cycling). We published extensively on how pre- existing cracks opened up with cyclic loading. The new IEC TS 63209-1 ED1 test sequence now include our recommendations, and this should lead to improved module designs and reduced risk for investors. We also published recommendations for a new "Cold Climate Test" sequence to probe the sensitivity of modules to degradation from short microcracks formed when modules see temperatures below -30C followed by front side loading. We participated in several USTAG meetings related to cracked cells, EL testing, and mechanical load testing and provided input to the group to improve new standards under consideration. We also showed how the act of performing an EL test can affect the test results due to heating from the injected current. 3) New Module Designs and Related Manufacturing Methods & Equipment: We demonstrated reduced crack sensitivity on encapsulated cell coupons the benefits of building protective compressive stress into the cells by laminating them in a bent state and then allowing the coupon to flatten out after lamination. Our attempts to scale this to the module level with a more manufacturable sequence did not demonstrate the same positive effects, but we hope that others will follow up with other variations on this bent lamination or bent cooling concept to make more durable modules. 4) New Module Mounting Designs: We explored a range of bracing concepts which pressed on the backsheet to slightly bow the glass outward and place cells in a state of protective compressive stress and to reduce the deflection under front side loads. These successfully reduced cell cracking and crack opening, but high static loads permanently deformed cost-effective braces, after which they provided little benefit. We settled on an elegant & effective solution – the RailPad, where lightweight bracing elements are placed between the mounting rail(s) and the backsheet, and the existing strength of the rails is used to prevent module deflection under load. New construction and retrofit designs were made, and test sites were implemented in FL and MA. We applied for RailPad patent protection.

14 SOLAR ENERGY↗