Search NASA⌕ Search

SEARCH · Search NASA

Results for “nafion”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Advances in solid polymer electrolyte fuel cell technology with low-platinum-loading electrodes

The Gemini Space program demonstrated the first major application of fuel cell systems. Solid polymer electrolyte fuel cells were used as auxiliary power sources in the spacecraft. There has been considerable progress in this technology since then, particularly with the substitution of Nafion for the polystyrene sulfonate membrane as the electrolyte. Until recently the performance was good only with high platinum loading (4 mg/sq cm) electrodes. Methods are presented to advance the technology by (1) use of low platinum loading (0.35 mg/sq cm) electrodes; (2) optimization of anode/membrane/cathode interfaces by hot pressing; (3) pressurization of reactant gases, which is most important when air is used as cathodic reactant; and (4) adequate humidification of reactant gases to overcome the water management problem. The high performance of the fuel cell with the low loading of platinum appears to be due to the extension of the three dimensional reaction zone by introduction of a proton conductor, Nafion. This was confirmed by cyclic voltammetry.

Srinivasan, Supramaniam↗

Near-ambient solid polymer fuel cell

Fuel cells are extremely attractive for extraterrestrial and terrestrial applications because of their high energy conversion efficiency without noise or environmental pollution. Among the various fuel cell systems the advanced polymer electrolyte membrane fuel cells based on sulfonated fluoropolymers (e.g., Nafion) are particularly attractive because they are fairly rugged, solid state, quite conductive, of good chemical and thermal stability and show good oxygen reduction kinetics due to the low specific adsorption of the electrolyte on the platinum catalyst. The objective of this program is to develop a solid polymer fuel cell which can efficiently operate at near ambient temperatures without ancillary components for humidification and/or pressurization of the fuel or oxidant gases. During the Phase 1 effort we fabricated novel integral electrode-membrane structures where the dispersed platinum catalyst is precipitated within the Nafion ionomer. This resulted in electrode-membrane units without interfacial barriers permitting unhindered water diffusion from cathode to anode. The integral electrode-membrane structures were tested as fuel cells operating on H2 and O2 or air at 1 to 2 atm and 10 to 50 C without gas humidification. We demonstrated that cells with completely dry membranes could be self started at room temperature and subsequently operated on dry gas for extended time. Typical room temperature low pressure operation with unoptimized electrodes yielded 100 mA/cm(exp 2) at 0.5V and maximum currents over 300 mA/cm(exp 2) with low platinum loadings. Our results clearly demonstrate that operation of proton exchange membrane fuel cells at ambient conditions is feasible. Optimization of the electrode-membrane structure is necessary to assess the full performance potential but we expect significant gains in weight and volume power density for the system. The reduced complexity will make fuel cells also attractive for smaller and portable power supplies and as replacement for batteries.

Holleck, G. L.↗

Performance and optimization of a combustion interface for isotope ratio monitoring gas chromatography/mass spectrometry

Conditions and systems for on-line combustion of effluents from capillary gas chromatographic columns and for removal of water vapor from product streams were tested. Organic carbon in gas chromatographic peaks 15 s wide and containing up to 30 nanomoles of carbon was quantitatively converted to CO2 by tubular combustion reactors, 200 x 0.5 mm, packed with CuO or NiO. No auxiliary source of O2 was required because oxygen was supplied by metal oxides. Spontaneous degradation of CuO limited the life of CuO reactors at T > 850 degrees C. Since NiO does not spontaneously degrade, its use might be favored, but Ni-bound carbon phases form and lead to inaccurate isotopic results at T < 1050 degrees C if gas-phase O2 is not added. For all compounds tested except CH4, equivalent isotopic results are provided by CuO at 850 degrees C, NiO + O2 (gas-phase mole fraction, 10(-3)) at 1050 degrees C and NiO at 1150 degrees C. The combustion interface did not contribute additional analytical uncertainty, thus observed standard deviations of 13C/12C ratios were within a factor of 2 of shot-noise limits. For combustion and isotopic analyses of CH4, in which quantitative combustion required T approximately 950 degrees C, NiO-based systems are preferred, and precision is approximately 2 times lower than that observed for other analytes. Water must be removed from the gas stream transmitted to the mass spectrometer or else protonation of CO2 will lead to inaccuracy in isotopic analyses. Although thresholds for this effect vary between mass spectrometers, differential permeation of H2O through Nafion tubing was effective in both cases tested, but the required length of the Nafion membrane was 4 times greater for the more sensitive mass spectrometer.

NASA Discipline Exobiology↗

New High-Temperature Membranes Developed for Proton Exchange Membrane Fuel Cells

Fuel cells are receiving a considerable amount of attention for potential use in a variety of areas, including the automotive industry, commercial power generation, and personal electronics. Research at the NASA Glenn Research Center has focused on the development of fuel cells for use in aerospace power systems for aircraft, unmanned air vehicles, and space transportation systems. These applications require fuel cells with higher power densities and better durability than what is required for nonaerospace uses. In addition, membrane cost is a concern for any fuel cell application. The most widely used membrane materials for proton exchange membrane (PEM) fuel cells are based on sulfonated perfluorinated polyethers, typically Nafion 117, Flemion, or Aciplex. However, these polymers are costly and do not function well at temperatures above 80 C. At higher temperatures, conventional membrane materials dry out and lose their ability to conduct protons, essential for the operation of the fuel cell. Increasing the operating temperature of PEM fuel cells from 80 to 120 C would significantly increase their power densities and enhance their durability by reducing the susceptibility of the electrode catalysts to carbon monoxide poisoning. Glenn's Polymers Branch has focused on developing new, low-cost membranes that can operate at these higher temperatures. A new series of organically modified siloxane (ORMOSIL) polymers were synthesized for use as membrane materials in a high-temperature PEM fuel cell. These polymers have an organic portion that can allow protons to transport through the polymer film and a cross-linked silica network that gives the polymers dimensional stability. These flexible xerogel polymer films are thermally stable, with decomposition onset as high as 380 C. Two types of proton-conducting ORMOSIL films have been produced: (1) NASA-A, which can coordinate many highly acid inorganic salts that facilitate proton conduction and (2) NASA-B, which has been produced and which incorporates strongly acidic (proton donating) functional groups into the polymer backbone. Both of these polymer films have demonstrated significantly higher proton conductivity than Nafion at elevated temperatures and low relative humidities. An added advantage is that these polymers are very inexpensive to produce because their starting materials are commodity chemicals that are commercially available in large volumes.

Kinder, James D.↗

Design, Development, and Testing of a Water Vapor Exchanger for Spacecraft Life Support Systems

Thermal and environmental control systems for future exploration spacecraft must meet challenging requirements for efficient operation and conservation of resources. Maximizing the use of regenerative systems and conserving water are critical considerations. This paper describes the design, development, and testing of an innovative water vapor exchanger (WVX) that can minimize the amount of water absorbed in, and vented from, regenerative CO2 removal systems. Key design requirements for the WVX are high air flow capacity (suitable for a crew of six), very high water recovery, and very low pressure losses. We developed fabrication and assembly methods that enable high-efficiency mass transfer in a uniform and stable array of Nafion tubes. We also developed analysis and design methods to compute mass transfer and pressure losses. We built and tested subscale units sized for flow rates of 2 and 5 cu ft/min (3.4–8.5 cu m/hr). Durability testing demonstrated that a stable core geometry was sustained over many humid/dry cycles. Pressure losses were very low (less than 0.5 in. H2O (125 Pa) total) and met requirements at prototypical flow rates. We measured water recovery efficiency across a range of flow rates and humidity levels that simulate the range of possible cabin conditions. We measured water recovery efficiencies in the range of 80 to 90%, with the best efficiency at lower flow rates and higher cabin humidity levels. We compared performance of the WVX with similar units built using an unstructured Nafion tube bundle. The WVX achieves higher water recovery efficiency with nearly an order of magnitude lower pressure drop than unstructured tube bundles. These results show that the WVX provides uniform flow through flow channels for both the humid and dry streams and can meet requirements for service on future exploration spacecraft. The WVX technology will be best suited for long-duration exploration vehicles that require regenerative CO2 removal systems while needing to conserve water.

Izenson, Michael G.↗

The effect of ion pairing on speciation and transport in ion exchange membranes at varying hydration levels: A four-state model

Understanding ion pairing in ion exchange membranes (IEMs) is essential for advancing IEM applications in energy and environmental technologies. Here, this study introduces a four-state molecular dynamics model to quantify speciation and transport within Nafion-117, specifically examining the role of ion pairing in monovalent and divalent counterions (NaCl, Na 2 SO 4 , and MgSO 4 ). By analyzing radial distribution functions (RDFs) and molecular snapshots, we distinguish ion pairing modes and classify counterions into four states: condensed counterion, condensed ion pair, free ion pair, and free counterion. A key finding is that while divalent counterions (e. g., Mg 2+ ) maintain stable speciation across hydration levels, monovalent counterions (e.g., Na + ) show notable speciation shifts with hydration. Both monovalent and divalent counterions are not diffusive when condensed onto the polymer (sorbed to membrane functional groups). In contrast, free counterions are diffusive across all hydration levels. To evaluate the overall diffusivity of counterions, four-state fractions and diffusivities are computed, each contributing to counterion transport. The condensed/free ion speciation for multivalent sulfate salts aligns with previous revisions to the Donnan-Manning framework that include ion pairing, thereby validating its relevance to established membrane theories. The four-state model's diffusivity results support several current ion exchange assumptions, including that the condensed counterions are immobile, while uncondensed counterions are mobile. The four-state model offers insights into contact ion pairing within IEMs, highlighting its potential even when undetected in aqueous solution experiments. This work advances the theoretical understanding of counterion speciation in IEMs while identifying model limitations that suggest avenues for refinement, such as distinguishing water-mediated ion pairs between fully hydrated ions.

Ion exchange membranes↗

Membrane-Induced Vanadium Crossover-Blocking Polybenzimidazole Copolymer with Exceptional Proton Selectivity

Broad deployment of redox flow batteries is hindered, in part, due to the lack of highly selective ion-exchange membranes with high proton conductivity. We report a post-functionalization strategy for polybenzimidazole copolymer (PBI-co) membranes by a reacting mixture of concentrated sulfuric and phosphoric acids that led to improved membrane selectivity while retaining high proton conductivity. Fourier-transform infrared spectroscopy confirmed successful sulfonation and protonation of benzimidazole functionalities. PBI-co exhibits a very high room-temperature proton conductivity of 0.138 S cm -1 , as measured by electrochemical impedance spectroscopy. PBI-co also demonstrates electromigration crossover mitigation under applied current densities up to 500 mA cm -2 , and voltage pulses up to 1.4 V, while also inhibiting diffusion-driven vanadium crossover for over 20 days. Single-cell vanadium flow battery testing on post-functionalized PBI-co further confirms state-of-the-art battery performance with an ~99.5% Coulombic efficiency at 100 mA cm -2 and an area-specific resistance of ~20 mO cm 2 lower than Nafion-212 membrane.

25 ENERGY STORAGE↗

Revealing the Crystalline Architecture of Semicrystalline Ion Exchange Membranes for the Design of Conductive and Durable Alkaline Anion Exchange Membranes

Alkaline anion exchange membrane (AAEM) fuel cells offer a cost-effective alternative to proton exchange membrane (PEM) fuel cells by eliminating the need for expensive precious metal catalysts. In both PEMs and AAEMs, semicrystalline polymers are a common choice, as the crystalline domains can act as mechanical reinforcements that limit swelling and promote mechanical durability in the material. However, spatially resolved characterization of crystalline organization in ion exchange membranes beyond ensemble-averaged X-ray scattering is underrepresented, likely in part due to ionization damage limitations in soft materials. Here, in this study, we resolve the nanometer-size crystallites in semicrystalline ion exchange membranes by applying cryogenic four-dimensional scanning transmission electron microscopy (cryo-4D-STEM) along with data-processing algorithms designed to optimize signals at a low dose to minimize radiation damage. We investigate the effects of synthesis components, including molecular weight and thermal treatment, on a model system of AAEMs in comparison to Nafion, the most commonly used and commercially successful PEM today. We find that excess water uptake in polymer membranes, a property directly associated with weak mechanical durability and with possible negative impacts on ion conductivity, can be reduced by over 30% by varying the polymer's crystalline morphology through changes in synthesis parameters such as molecular weight and thermal history. Our results indicate that this improvement is correlated with smaller crystalline domains with a more homogeneous distribution. More broadly, these results demonstrate how the crystalline architecture of polymer membranes can be tuned through their chemistry and thermal treatment in order to improve their conductivity and durability for commercial fuel cell performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Adsorption-Engineered Hydrocarbon Ionomers for Durable Proton-Exchange Membrane Fuel Cells

Reducing reliance on perfluoroalkyl substances (PFAS) in proton-exchange membrane fuel cells requires hydrocarbon ionomers that combine high performance with long-term durability, a persistent challenge in catalyst-layer design. Here, we identify oxidation-driven ionomer-catalyst interfacial degradation as a dominant failure pathway in hydrocarbon ionomer-bonded cathodes and introduce an adsorption-engineering strategy to overcome this limitation. The comparison of a commercial sulfonated poly(phenylene) (Pemion) with structurally engineered sulfonated poly(fluorene)s demonstrated that electrode durability is governed by the interplay between ionomer adsorption strength and resistance to oxidative degradation on carbon-supported Pt catalysts. A poly(fluorene) ionomer with mobile alkyl sulfonic acid groups forms resilient interfaces, delivering 1.28 A cm−2 at 0.65 V under fully humidified H2/air conditions (80°C and 150 kPaabs), comparable to Pemion. After 90,000 accelerated potential cycles, the poly(fluorene)-bonded cathode exhibits significantly improved durability, with only 29% performance loss compared to 58% for Pemion; further molecular refinement reduces the loss to 17%, approaching that of Nafion-bonded cathodes (14%). These findings establish adsorption-engineered ionomer design that decouples interfacial anchoring from oxidative degradation as a general strategy for achieving durable, high-performance PFAS-free PEM fuel cell electrodes.

08 HYDROGEN↗

Sulfonated Diels–Alder Poly(Phenylene)s in Membrane Electrode Assemblies for Fuel Cells

The transition to environmentally sustainable materials in fuel cells requires alternatives to persistent polyfluoroalkyl substances (PFAS) like Nafion. This study investigates the performance-limiting factors of membrane electrode assemblies (MEAs) utilizing sulfonated Diels–Alder poly(phenylene)s (sDAPPs) as PFAS-free polymer electrolytes. Among the configurations evaluated, the greatest performance loss occurred when sDAPP is used as the cathode binder, primarily due to phenyl group adsorption on catalyst surfaces, which reduces oxygen reduction reaction activity and impedes oxygen transport. Additional performance degradation arises from membrane-electrode interfacial incompatibility and insufficient ionomer hydrophobicity. By addressing ionomer adsorption and improving interfacial contact, an sDAPP-based cathode achieved a current density of 1.57 A cm −2 at 0.6 V under fully humidified H 2 /air conditions at 80 °C and 150 kPa abs . These results offer key insights for advancing high-performance, PFAS-free fuel cell technologies.

08 HYDROGEN↗

Influence of Linker Group on Bipolar Redox-Active Molecule Performance in Non-Aqueous Redox Flow Batteries

Redox flow batteries (RFBs) are an attractive choice for stationary energy storage of renewables such as solar and wind. Non-aqueous redox flow batteries (NARFBs) have garnered broad interest due to their high voltage operation compared to their aqueous counterparts. Further, the utilization of bipolar redox-active molecules (BRMs) is a practical way to alleviate crossover faced by asymmetric RFBs. In this work, ferrocene (Fc) and phthalimide (PI) are covalently linked with various tethering groups which vary in structure and length. The compiled results suggest that the length and steric shielding ability of the linker group can greatly influence the stability and overall performance of Fc-n-PI BRM-based NARFBs. Primary sources of capacity loss are found to be BRM degradation for straight chain spacers <6 carbons and membrane (Nafion) fouling. Fc-hexyl-PI provided the most stable battery cycling and coulombic efficiencies of >98 % over 100 cycles (~13 days). NARFB using Fc-hexyl-PI as an active material exhibited high working voltage (1.93 V) and maximum capacity (1.28 Ah L -1 ). Additionally, this work highlights rational strategies to improve cycling stability and optimize NARFB performance.

25 ENERGY STORAGE↗

Bismuth Detection in Alkaline Electrolyte via Anodic Stripping Voltammetry for Battery Separator Evaluation

Abstract Anodic stripping voltammetry (ASV) has been widely used for the detection of several heavy metal ions in neutral and acidic solution, in many cases employing electrodes and/or solutions incorporating Bi. In this work we demonstrate that Bi(OH) 4 − ion concentration can be measured in highly alkaline 8.5 M KOH solution using ASV. The addition of Pb in similar concentrations to the Bi(OH) 4 − being measured is shown to improve both the sensitivity and precision of the method. When the Pb additive is employed, a formal limit of detection of 8.5 ppb is achieved, compared to 17.3 ppb when the Pb additive is not used. Due to the use of Bi additives in alkaline battery chemistries, it follows that separators which limit Bi(OH) 4 − diffusion into the bulk electrolyte and away from the electrodes are of interest. For this purpose, we utilize ASV to determine Bi(OH) 4 − diffusion rates through Celgard 3501, cellophane 350P00, and Nafion 211. Bi(OH) 4 − crossover rates, as determined by ASV, are shown to be repeatable and consistent with expectations from the known separator structure.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Elucidating the impact of the ionomer equivalent weight on a platinum group metal-free PEMFC cathode via oxygen limiting current

Leveraging the interactions between ionomer and catalyst can increase the performance of proton exchange membrane fuel cells. The impacts of the equivalent weight (EW) of perfluorosulfonic acid–based ionomers on the platinum group metal-free electrode structure and fuel cell performance have not been fully explored. Four membrane electrode assemblies (MEAs) were prepared by using a commercial Fe–N–C catalyst, two perfluorosulfonic acid ionomers with different EWs, that is, Aquivion 720 (A720) and Nafion 1100 (N1100), and two ionomer-to-catalyst (I/C) ratios. The four MEAs were characterized to understand the impact of the ionomer EW and content on the capacitance, proton conductivity, and mass transport on the cathode. The mass transport resistance was measured for the first time using a new oxygen reduction reaction limiting current method enabling to couple the effects of oxygen diffusion with liquid water generation. Low EW ionomer combined with a moderate I/C results in improved performance due to its enhanced proton conductivity. However, when used at high I/C, it can cause severe water flooding at high current density due to the enhanced liquid water uptake, especially at high relative humidity, resulting in lower catalyst utilization and higher mass transport resistance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrochemically Grown Ultrathin Platinum Nanosheet Electrodes with Ultralow Loadings for Energy-Saving and Industrial-Level Hydrogen Evolution

Nanostructured catalyst-integrated electrodes with remarkably reduced catalyst loadings, high catalyst utilization and facile fabrication are urgently needed to enable cost-effective, green hydrogen production via proton exchange membrane electrolyzer cells (PEMECs). Herein, benefitting from a thin seeding layer, bottom-up grown ultrathin Pt nanosheets (Pt-NSs) were first deposited on thin Ti substrates for PEMECs via a fast, template- and surfactant-free electrochemical growth process at room temperature, showing highly uniform Pt surface coverage with ultralow loadings and vertically well-aligned nanosheet morphologies. Combined with an anode-only Nafion 117 catalyst-coated membrane (CCM), the Pt-NS electrode with an ultralow loading of 0.015 mg Pt cm -2 demonstrates superior cell performance to the commercial CCM (3.0 mg Pt cm -2 ), achieving 99.5% catalyst savings and more than 237-fold higher catalyst utilization. The remarkable performance with high catalyst utilization is mainly due to the vertically well-aligned ultrathin nanosheets with good surface coverage exposing abundant active sites for the electrochemical reaction. Overall, this study not only paves a new way for optimizing the catalyst uniformity and surface coverage with ultralow loadings but also provides new insights into nanostructured electrode design and facile fabrication for highly efficient and low-cost PEMECs and other energy storage/conversion devices.

42 ENGINEERING↗

Amorphous Iridium Oxide-Integrated Anode Electrodes with Ultrahigh Material Utilization for Hydrogen Production at Industrial Current Densities

Herein, ionomer-free amorphous iridium oxide (IrO x ) thin electrodes are first developed as highly active anodes for proton exchange membrane electrolyzer cells (PEMECs) via low-cost, environmentally friendly, and easily scalable electrodeposition at room temperature. Combined with a Nafion 117 membrane, the IrO x -integrated electrode with an ultralow loading of 0.075 mg cm –2 delivers a high cell efficiency of about 90%, achieving more than 96% catalyst savings and 42-fold higher catalyst utilization compared to commercial catalyst-coated membrane (2 mg cm –2 ). Additionally, the IrO x electrode demonstrates superior performance, higher catalyst utilization and significantly simplified fabrication with easy scalability compared with the most previously reported anodes. Notably, the remarkable performance could be mainly due to the amorphous phase property, sufficient Ir 3+ content, and rich surface hydroxide groups in catalysts. Overall, due to the high activity, high cell efficiency, an economical, greatly simplified and easily scalable fabrication process, and ultrahigh material utilization, the IrO x electrode shows great potential to be applied in industry and accelerates the commercialization of PEMECs and renewable energy evolution.

08 HYDROGEN↗

Evaluation of IrO 2 catalysts doped with Ti and Nb at industrially relevant electrolyzer conditions: A comprehensive study

A series of commercial Oxygen Evolution Reaction (OER) IrO 2 -based materials doped with acid-stable titanium and niobium species were comprehensively characterized by Brunauer-Emmett-Teller (BET), X-ray diffraction analysis (XRD), X-ray photoelectron spectroscopy (XPS), transmission electron microscopy (TEM) with energy dispersive spectroscopy (EDS), and X-ray Scattering. Electrocatalysts were integrated into Membrane Electrode Assembly (MEA) using a fabrication method developed under the US DOE H2NEW consortium. An electrolysis performance in a commercial setup as well as a laboratory screening system was performed at conditions relevant to industrial application. According to the comprehensive characterizations, the studied materials are closer to doped iridium oxides rather than core–shell structures. In an electrolysis cell, the IrO 2 /TiO x catalyst slightly outperforms the IrO 2 /NbO x based on the activity. It was demonstrated that the operation of electrolysis cells at elevated temperatures and the implementation of thinner Nafion-type membranes allows for substantially increased performance, which is consistent with the literature report. Finally, this work provides valuable baselines including characterization and performance for guiding future research in this direction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of water droplet growth dynamics on electrode current in fuel-cell catalyst layers

Fuel cells are a promising next-generation energy-conversion technology designed to replace internal combustion engines in transportation applications. However, much work remains to optimize them. Operation at high humidities causes liquid water droplet formation on Pt catalyst particles during oxygen reduction, potentially impeding reactant arrival to the reactive electrode. In this work, four different cases of water droplet growth in fuel-cell catalyst layers are considered: pinned or advancing droplets on a bare Pt surface, advancing droplets on a Nafion film, and water-layer growth in carbon nanopores. Transient drop growth is captured with a combination of mass, species mass, and momentum balances, and the subsequent limiting current is determined via oxygen diffusion and Tafel kinetics. Further, water droplets are found not to be mass-transfer limiting due to the relatively large liquid-gas area compared to the Pt nanoparticle. Mass-transfer-limited behavior is calculated in carbon nanopores.

25 ENERGY STORAGE↗

Experimental measurements of fuel and water crossover in an active DMFC

This work measured polarization curves as well as the high-frequency resistance of active direct methanol fuel cell (DMFC) operates at around 80 °C with active controls of temperature, methanol concentration, airflow rate, and relative humidity. The relative humidity of the air did not have noticeable impacts on the fuel cell unless the operating temperature was near the evaporation temperature of water (100 °C). The hydrophobic water management layer (WML) between the membrane electrode assembly (MEA) and cathode air channel increases the mass transfer resistance and improves the water retention in MEA. Adding a WML increased the peak power density, decreased the ohmic resistance, and improved the fuel efficiency of the fuel cell, especially when it operated near 100 °C. This study also quantitatively measured methanol and water crossover as well as the fuel efficiency at different operating currents. The fuel efficiency increased significantly with the increase of the current density. Using a hydrophobic fuel management layer (FML) between the anode fuel channel and MEA reduced the fuel and water crossover rates and increased the ohmic resistance due to the decrease of the water content of the Nafion membrane. The FML improved fuel efficiency by reducing the methanol crossover. The combination of the FML and WML enabled the steady operation of DMFC using highly concentrated methanol solutions (up to 75 wt%).

08 HYDROGEN↗