Search NASA⌕ Search

SEARCH · Search NASA

Results for “polyurethane”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Degradation of Polyester Polyurethane by Aspergillus sp. Strain S45 Isolated from Soil

A polyurethane (PU)-degrading fungus designated as strain S45 was isolated from a solid waste-dumping site in Islamabad, Pakistan. Strain S45 was identified as Aspergillus sp. through microscopic, morphologic as well as 18S rRNA sequencing (99% similarity with Aspergillus fumigatus). The degradation ability of strain S45, was analyzed through measurement of weight loss and evolution of CO{sub 2} as a result of breakdown of PU film. The degradation was confirmed through scanning electron microscopy, fourier transform infrared (FTIR) spectroscopy and differential scanning calorimetry (DSC). Surface changes like pits, cracks and holes were observed in scanning electron micrographs upon degradation of PU film by strain S45. FTIR spectra were carefully examined, changes were observed in various peaks at different wavelength ranges that also correspond to degradation of PU film. Differential scanning calorimetric technique was used to measure the melting temperature of PU film pieces before and after incubation with strain S45. DSC curve indicated an increase in melting temperature of PU from 191 to 196 °C that might be due to increase in crystallinity of the exposed PU after degradation of amorphous soft segment. A gradual increase in specific activity of esterase was observed up to the maximum of 15th day of incubation with PU film in mineral salt medium. Enzyme activity was further confirmed by tween 20 agar plates, demonstrated by formation of calcium complex. It is concluded from the results that Aspergillus sp. strain S45 might be applied for the treatment of plastics-contaminated environments.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Vegetable Oil Based Polyurethane Containing 1,2,3-Triazolium Functional Groups as Antimicrobial Wound Dressing

Preparation of antimicrobial polyurethane wound dressing membranes from a mixture of castor oil and a novel soybean oil-based polyol containing 1,2,3-triazolium rings (QTSBO) was described in this research. QTSBO was prepared through N-alkylation of 1,2,3-triazole functional soybean oil (TSBO) with methyl iodide, and TSBO was synthesized from an azidated soybean oil and propargyl alcohol through click reaction. The excellent tensile strength of these dressings under dry state and minimum deterioration of this property at fully hydrated state guaranteed the mechanical protection of wounds during the entire period of the healing process. The measured quantities of equilibrium water absorption and water vapor transmission rate for the optimized dressings confirmed the applicability of the selected formulations for the preservation of proper moist environment over low exuding wounds. The cyto-compatibility of dressings was verified by the excellent ability of the dressings to support the growth and proliferation of dermal fibroblasts. Due to the presence of 1,2,3-triazolium rings the dressing showed efficient antimicrobial activity against different bacterial and fungal stains. Therefore, these dressing could promote wound healing by preserving moist and hygienic environment over the wound bed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Nanocomposites of Waterborne Polyurethane Reinforced with Cellulose Nanocrystals from Sisal Fibres

Cellulose nanocrystals (CNC) were isolated from sisal fibres and were incorporated in the form of an aqueous suspension to a waterborne polyurethane (WBPU) synthesized from components derived from natural sources using an aliphatic diisocyanate. Transparent nanocomposite films with different CNC contents were prepared using a casting method. The morphology, thermal behaviour and mechanical properties of the nanocomposite films were characterized. Homogeneous distribution of CNC in the WBPU, even at high CNC contents was observed, resulting in an increase of 100% in modulus for systems with 5 and 10 wt% of CNC, with high elongations around 650%.

36 MATERIALS SCIENCE↗

Polyurethane Foams Based on Biopolyols from Castor Oil and Glycerol

In this work, the synthesis of biopolyols derived from castor oil and different glycerols was performed by chemical glycerolysis with sodium hydroxide as catalyst at 225 °C. The biopolyol obtained from high purity glycerol led to predominantly MAG formation, whereas the biopolyol produced using crude glycerol, byproduct from biodiesel industry, resulted in higher DAG, TAG and FFA content due to the higher amount of water. Both biopolyols were employed for the synthesis of polyurethane (PU) foams by bulk polymerization using methylene diphenyl diisocyanate (MDI) at different NCO:OH ratios. The foams were evaluated by apparent density, insoluble fraction, Fourier transform infrared spectroscopy, scanning electron microscope and thermogravimetric analysis. The results showed that crude glycerol provided PU foams as much as commercial glycerol, however the characteristics may be different, mainly due to the presence of water in the reaction medium.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

High Removal Capacity of Arsenic from Drinking Water Using Modified Magnetic Polyurethane Foam Nanocomposites

In this study, a novel polyurethane foam (PU) nanocomposite adsorbent based on silane-modified magnetic iron-oxide nanoparticles (Fe{sub 3}O{sub 4}@APTES) is synthesized via a low cost and simple in situ polymerization method for the removal of arsenic ions from aqueous solutions. The chemical structure and surface morphology of the prepared nanoparticles and adsorbent were characterized using Fourier transform infrared spectroscopy, attenuated total reflection, scanning electron microscopy, transmission electron microscopy, and energy-dispersive X-ray spectroscopy. Inductively coupled plasma mass spectrometry was used to measure the arsenic concentration of the treated solutions. Sorption isotherms models were applied to determine the adsorption mechanism and modeling parameters. The removal capacity of the modified PU foam was at its highest during a contact time of four hours which resulted in a removal capacity of 95%. Kinetic studies were conducted to determine the adsorption capacity and the uptake rate of arsenic. A Pseudo-order model was found to be the best fit model for adsorption. The prepared adsorbent can be separated from the solution by using an external magnet field.

36 MATERIALS SCIENCE↗

Fabrication and Testing of Soy-Based Polyurethane Foam for Insulation and Structural Applications

This study is focused on the fabrication and evaluation of polyurethane (PU) foam fabricated using soy-based polyol that can potentially replace conventional petroleum-based PU foam for thermal applications. Rigid soy-based PU foam samples investigated in this study were produced by copolymerization of diisocyanate with soy-based polyol in presence of Xiameter X0193 surfactant, dibutyltin dilaurate (DBTL) as a catalyst, and water as a blowing agent. Different formulations with varying amounts of blowing agent and catalyst were investigated to optimize the mechanical and thermal properties of soy-based PU foam when compared to commercial petroleum-based foam as a control sample. The prepared samples were tested for density, compressive strength, thermal conductivity, tensile strength, dimensional stability, and thermal stability using the ASTM standards. The cellular structure of the fabricated foam samples was investigated using scanning electron microscopy. It was observed that an increase in density leads to a decrease in insulation. Overall, soy-based foams exhibited similar thermal conductivity as compared to petroleum-based foams.

36 MATERIALS SCIENCE↗

Investigation of Thermoplastic Polyurethanes Synthesized via Two Different Prepolymers

The man aim of this work was to investigate the effect of the molecular weight of polyols, mixture of prepolymers, and [NCO]/[OH] molar ratio used during the prepolymer chain extending step on the chemical structure, thermomechanical and mechanical properties, and thermal stability of thermoplastic poly(ether-urethane)s In this work thermoplastic poly(ether-urethane)s were synthesized by using polyols with a various molecular weight, 4,4′-diphenylmethane diisocyanate and bio-based glycol. Materials were obtained by a two-step method. The tests were carried out for polyurethanes obtained from a mixture of prepolymers and for reference samples. In the case of materials obtained with using mixture of prepolymers, the ratio of both prepolymers was determined on 50/50 weight percent. Soft segments of materials prepared with using mixture consist of two different polyols. The chemical structure was analyzed using FTIR spectroscopy. The Gaussian deconvolution technique was used to study the hydrogen bonding as well as to decompose carbonyl region of three peaks in various TPUs. The thermal degradation behavior was investigated by using thermogravimetric analysis at heating rates of 10 °C/min. It was confirmed that the mixture of prepolymers has an effect of the degree of phase separation, thermal stability and selected properties of synthesized thermoplastic poly(ether-urethane)s.

36 MATERIALS SCIENCE↗

Effects of Environmental Conditions on the Mechanical and Degradation Behavior of Polyurethane Foam Subjected to Various Deformation Histories

Since its development, polyurethane foam (PUF) has been widely used as an insulator, including in the marine industry. Liquefied natural gas (LNG) carriers have the highest market share in the LNG-related shipbuilding industry. PUF is used as an insulator in membrane-type cargo containment systems (CCSs) as one of the most important components of LNG carriers. Because PUF is subjected to constant load and deformation when used in insulation for LNG CCSs and is exposed to the cryogenics of the seawater environment for extended times, it is essential to evaluate the mechanical behavior of PUF in such environments. In this study, to investigate the effects of applying an initial strain and of immersion in various media on the mechanical properties of PUF, compression tests were carried out at ambient and cryogenic temperature using a universal testing machine. The mechanical behavior of PUF after deformation recovery upon subjection to various initial strain levels was estimated experimentally. In addition, the microstructure of the PUF specimen prior to testing was analyzed to investigate the effects of the initial strain level and immersion in different media on the mechanical behavior of PUF.

36 MATERIALS SCIENCE↗

Scalable fabrication of a tough and recyclable spore-bearing biocomposite thermoplastic polyurethane

Thermoplastic polyurethanes (TPUs) are a class of versatile thermoplastic elastomers, but most of their products lack a proper recycling strategy or have no end-of-life solutions. To pursue a sustainable end-of-life solution for TPU-based products, self-disintegrating biocomposite TPUs have recently been developed by embedding spores of TPU-degrading bacteria into TPUs via melt extrusion. Herein, we improve upon spore-bearing biocomposites and demonstrate industrially relevant manufacturing conditions for fabricating biocomposite TPUs. To minimize the coloration of biocomposite TPUs, spore production was modified. The innate brown color of the resulting materials was diminished by reducing FeSO 4 in sporulation media, generating white spores without compromising spore productivity, viability, morphology or heat-shock tolerance. Biocomposite TPUs containing white spores displayed a 45 % increase in toughness compared to TPUs without spores, while retaining ∼ 90 % spore viability post processing. Furthermore, biocomposite TPU fabrication was demonstrated using a scalable continuous extruder followed by injection molding. Biocomposite TPUs generated by these industry-relevant processes exhibited comparable toughness improvement and spore viability to biocomposite TPU prepared using a lab scale microcompounder, while enhancing productivity by 30-fold. Finally, spore addition significantly improved the recyclability of biocomposite TPUs, enabling 80 % toughness retention after 5 rounds of iterative melt processing. Additionally, no negative effect on the lifespan of the generated TPUs was observed over 1 year of storage. Overall, this study confirms that spore-bearing biocomposite TPUs are promising for practical applications, offering an accessible method to enhance toughness and sustainability of commercial TPUs through the incorporation of spore-based living fillers.

36 MATERIALS SCIENCE↗

Preparation and characterization of aminated co-solvent enhanced lignocellulosic fractionation lignin as a renewable building block for the synthesis of non-isocyanate polyurethanes

Lignin is a major bioresource from 2nd generation biorefinery process streams and from pulp and paper production that is still severely underutilized nowadays. Its natural polymeric and aromatic structures make it suitable as a potential building block for biopolymer production. Due to the growing environmental and health concerns over conventional polyurethane (PU) manufacturing processes that utilize toxic isocyanates, there is a great interest to develop a non-isocyanate PU (NIPU) route. Herein, we demonstrate a novel strategy that uses highly pure lignin isolated from co-solvent enhanced lignocellulosic fractionation (CELF) pretreatment of poplar wood to produce biobased NIPUs. In this strategy, hardwood poplar is firstly fractionated via a CELF pretreatment to produce a clean lignin stream that is rich in phenolics. The CELF lignin was then aminated by a Mannich reaction, and the aminated CELF lignin was finally reacted with bicyclic carbonates to yield an advanced NIPU. In this work, the structure, mechanical, and thermal properties of these novel NIPUs were elucidated by FTIR, NMR, tensile test, dynamic mechanical analysis (DMA), and thermogravimetric analysis (TGA). The mechanical properties of these lignin based NIPUs could be tuned from highly rigid to elastic polymers by simply modifying the lignin constituents of the polymer. The thermal stabilities of NIPUs were improved because of the addition of aminated lignin, and NIPU containing 55 and 23 wt% lignin showed the highest tensile strength (~1.2 MPa) and elongation at break (~140%), respectively. The results obtained in this study demonstrate that the reaction of cyclic carbonate with aminated lignin represents an interesting pathway for the synthesizing of lignin based NIPU with a relative high lignin content.

54 ENVIRONMENTAL SCIENCES↗

Corrosion-resistant polyurethane coatings from structure-homogenized biorefinery lignin through fractionation and oxypropylation

Using lignin for polyurethane (PU) synthesis is challenging because of its heterogeneous structure, i.e., broad molecule weight (MW) distribution and diverse hydroxyl (OH) functionality. This complexity influences the crosslinking reaction between lignin and isocyanate and affects the quality of PU products. Here, we propose a two-step strategy for lignin structure homogenization by lowering its MW and uniforming OH functionality (step 2). Step 1 involves a bioethanol fractionation process, yielding fractionated lignin with one order lower MW than the raw lignin while exhibiting better processability for the subsequent process. Step 2 is performed by an oxyalkylation process using fractionated lignin that converts phenolic and carboxylic OHs to aliphatic OHs. As a result, we obtained structure-homogenized lignin with good compatibility and crosslinking with hexamethylene diisocyanate for PU coating synthesis. Moreover, PU coatings prepared from structure-homogenized lignin display a defect-free microscopic structure and show better corrosion resistance than coatings fabricated from its raw lignin alternative. Overall, the structure homogenization process is a beneficial way of using lignin as biopolyol in PU synthesis toward the application-oriented design of corrosion-resistant lignin-based PU coatings.

36 MATERIALS SCIENCE↗

Effect of polymer-nanoparticle interactions on the glass transition dynamics and the conductivity mechanism in polyurethane titanium dioxide nanocomposites

We report on the glass transition dynamics and the conductivity properties of a nanodielectric system composed of pre-synthesized TiO{sub 2} nanoparticles embedded in thermoplastic polyurethane. Increase of TiO{sub 2} loading results in enhanced segmental mobility of the composites and less steep temperature dependence, i.e., lower fragility index. The decrease in the fragility index and glass transition temperature is discussed based on the FTIR results. We observe different behavior of conductivity for temperatures above and below the glass transition temperature. At high temperatures the composites exhibit conductivity values more than 2 orders of magnitude higher than those in the pristine matrix. At the same time, at sub-Tg temperatures composites are characterized by superior electrical insulation properties compared to pristine matrix material. Such drastic temperature dependence of the conductivity/insulating ability of the flexible and light-weight, low-Tg composite material can be utilized in various applications including sensing and temperature switching materials.

36 MATERIALS SCIENCE↗

Tailoring High Hardness and Rigidity in Biodegradable Thermoplastic Polyurethanes

In response to escalating environmental concerns, there is a pressing demand for materials capable of delivering both sustainability and robust mechanical properties, thereby substituting nonrenewable counterparts in various applications. This study presents a comprehensive investigation into the synthesis and characterization of biobased aliphatic thermoplastic polyurethanes (TPUs) that exhibit impressive mechanical properties, including tensile strength in the range of 48–41 MPa and flexural modulus up to 2.2 GPa. These biodegradable TPUs displayed high shore A and D hardness between 95 and 98 and 51–42, respectively, and thus can be categorized as “extra hard” plastics according to the durometer scale for PUs. Herein, we have prepared a series of four 100% biobased polyester polyols from biobased diacid and chain-extender as precursors with molecular weights varying from 500 to 1400 g/mol. The corresponding TPUs that were prepared by using an aliphatic diisocyanate were evaluated for their thermal stability, microphase separation, mechanical properties, and biodegradation. By leveraging renewable feedstocks, these TPUs offer a sustainable alternative to petroleum-derived materials, with their mechanical performance meeting conventional benchmarks. Furthermore, postcomposting analysis revealed significant surface degradation, affirming their biodegradability and environmental compatibility.

36 MATERIALS SCIENCE↗

ZnO Nanorod Thermoplastic Polyurethane Nanocomposites: Morphology and Shape Memory Performance

The impact of dispersed alkylthiol-modified ZnO nanorods, as a function of rod aspect ratio and concentration, on the shape memory character of a thermoplastic polyurethane with low hard-segment density (LHS-TPU) is examined relative to the enhanced performance occurring for carbon nanofiber (CNF) dispersion. Solution blending resulted in uniform dispersion within the LHS-TPU of the ZnO nanorods at low volume (weight) fractions (<2.9% v/v (17.75% w/w)). Tensile modulus enhancements were modest though, comparable to values observed for spherical nanofillers. Shape memory characteristics, which in this LHS-TPU result when strain-induced crystallites retard the entropic recovery of the deformed chains, were unchanged for these low volume fraction ZnO nanocomposites. Higher ZnO loadings (12% v/v (50% w/w)) exhibited clustering of ZnO nanorods into a mesh-like structure. Here, tensile modulus and shape recovery characteristics were improved, although not as great as seen for comparable CNF addition. Wide angle X-ray diffraction and NMR revealed that the addition of ZnO nanorods did not impact the inherent strain induced crystallization of the LHS-TPU, which is in contrast to the impact of CNFs and emphasizes the impact of interactions at the polymer-nanoparticle interface. Overall, these findings reinforce the hypothesis that the shape memory properties of polymer nanocomposites are governed by the extent to which nanoparticle addition, via nanoparticle aspect ratio, hierarchical morphology, and interfacial interactions, impacts the molecular mechanism responsible for trapping elastic strain.

36 MATERIALS SCIENCE↗

Reinforcement Mechanism Of Polyurethane-Urea/Clay Nanocomposites Probed By Positron Annihilation Lifetime Spectroscopy And Dynamic Mechanical Analysis

A basis for quantitative analysis of the reinforcement mechanism of polyurethane-urea/clay nanocomposites using two characterization methods, positron annihilation life time spectroscopy (PALS) and dynamic mechanical analysis (DMA) is provided. DMA was used to measure the constrained volume fraction of amorphous soft segments induced by nanoclay and the storage modulus of the nanocomposites. The interfacial interactions in the nanocomposites were investigated by PALS. The modulus enhancement of the organoclay nanocomposites was found to have a good correlation with the volume fraction of the constrained region and the interfacial interactions.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Preparation and Structural Analysis of CdS Nanoparticle Embedded Polyurethane Nanocomposites

Polymer nanocomposite samples of different weight ratio of CdS were developed by solution embedding of nanoparticles in polyurethane. XRD and Scanning Electron Microscopy (SEM) were used to understand the structural properties of polymer nanocomposite samples. SEM micrograph demonstrates the dispersion of CdS nanoparticles in polymer matrix. It has been observed that crystallinity of PU decreases with increase in concentration of CdS nanoparticles. The XRD data show the characteristic peaks of nanoparticles (i.e.CdS) in nanocomposite samples, which confirm the nanostructure formation in polymer matrix.

36 MATERIALS SCIENCE↗

Charging process of polyurethane based composites under electronic irradiation: Effects of cellulose fiber content

The study deals with the charging effect of polyurethanes-based composites reinforced with cellulose fibers, under electronic beam irradiation in a scanning electron microscope. The results indicate that the leakage current and the trapped charge as well as the kinetics of charging process significantly change beyond a critical concentration of 10% cellulose fibers. These features are correlated with the cellulose concentration-dependence of the electrical properties, specifically resistivity and capacitance, of the composite.

36 MATERIALS SCIENCE↗

Thermal and mechanical properties of palm oil-based polyurethane acrylate/clay nanocomposites prepared by in-situ intercalative method and electron beam radiation

Palm oil based-polyurethane acrylate (POBUA)/clay nanocomposites were prepared via in-situ intercalative polymerization using epoxidized palm oil acrylate (EPOLA) and 4,4' methylene diphenyl diisocyante (MDI). Organically modified Montmorillonite (ODA-MMT) was incorporated in EPOLA (1, 3 and 5%wt), and then subjected to polycondensation reaction with MDI. Nanocomposites solid films were obtained successfully by electron beam radiation induced free radical polymerization (curing). FTIR results reveal that the prepolymer was obtained successfully, with nanoclay dispersed in the matrix. The intercalation of the clay in the polymer matrix was investigated by XRD and the interlayer spacing of clay was found to be increased up to 37 Å, while the structure morphology of the nanocomposites was investigated by TEM and SEM. The nanocomposites were found to be a mixture of exfoliated and intercalated morphologies. The thermal stability of the nanocomposites was significantly increased by incorporation of nanoclay into the polymer matrix. DSC results reveal that the Tg was shifted to higher values, gradually with increasing the amount of filler in the nanocomposites. Tensile strength and Young's modulus of the nanocomposites showed remarkable improvement compared to the neat POBUA.

36 MATERIALS SCIENCE↗