Search NASA⌕ Search

SEARCH · Search NASA

Results for “DUCTILITY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,441 records · Page 80

Manufacturing of Ultra-Fine Particle Coal Fly Ash–A380 Aluminum Matrix Composites with Improved Mechanical Properties by Improved Ring Milling and Oscillating Microgrid Mixing

An experimental study is presented of ultra-fine coal fly ash (CFA) aluminum matrix composites produced by successive high-power ring milling of CFA, oscillating microgrid mixing of the CFA–aluminum melt, gravity casting and rapid cooling. Samples corresponding to different CFA concentrations and particle size distributions (1 μm average, or less) are produced and subjected to microstructural and mechanical characterization, including tensile, compressive, impact, hardness and wear testing. While the usual trade-off between increased strength and hardness and reduced ductility and toughness is observed, the obtained ultra-fine particle composites are confirmed to have overall improved mechanical properties compared to composites with larger size particles previously produced by ball milling.

36 MATERIALS SCIENCE↗

The Effect of Multistage Aging on Mechanical Properties and Microstructure of Forged 7050 Aluminum Alloys

A new four-stage aging treatment, which is composed of pre-aging, retrogression, natural aging (NA) and re-aging, is designed to increase the tensile properties and the fatigue life of forged 7050 aluminum alloy in this work. As compared to traditional T74 and RRA treatments, the four-stage aging-treated sample exhibits the highest tensile properties and ductility. The tensile strength and yield strength are 627 and 608 MPa, respectively, and the elongation is 11.3%. The results of TEM and DSC show that an increased G.P zones and fine η′ phase distributed in the matrix of the alloy are subjected by this new aging processing as compared with T74 and RRA treatments. The natural aging in four-stage aging treatment accelerates the diffusion of Mg vacancies, and promotes the precipitation of G.P zones in grain interior during re-aging stage. On the basis of dislocation shearing mechanism, more dense and fine G.P zones of four-stage aging temper result in the superior tensile strength as compared to T74 and RRA temper. In addition, a combination of shearable precipitates, fine GBPs and narrow PFZs is beneficial to the slip reversibility in the plastic zone at the crack tip, thereby reducing fatigue damage accumulation and increasing the fatigue life.

36 MATERIALS SCIENCE↗

A Comparative Study on Microstructure, Mechanical and Tribological Properties of A4, AE41, AS41 and AJ41 Magnesium Alloys

Microstructure, tensile and wear properties of as-cast A4 (Mg-4Al), AE41 (Mg-4Al-0.5Ce-0.5La), AS41 (Mg-4Al-1Si) and AJ41 (Mg-4Al-1Sr) alloys were investigated, and the results were compared with each other in this study. Microstructures were investigated by XRD, optical and scanning electron microscopes. Tensile tests were conducted at both room and elevated temperatures. Tribological properties were examined by pin-on-disk wear tests under different applied loads. Microstructure characterizations revealed that the volume fraction of second phases considerably increased by alloying additions of 1 wt.% Ce/La, Si and Sr. The microstructure of A4 alloy consisted of α-Mg grains and divorced β-Mg{sub 17}Al{sub 12} phases. After individual alloying additions of 1 wt.% Ce/La, Si and Sr, the secondary phases were primarily replaced by needle-shaped and massive blocky-shaped Al{sub 11}(Ce,La){sub 3} phases in AE41 alloy, Chinese-script-type Mg{sub 2}Si phases in AS41 alloy and divorced globular-like and massive blocky-shaped Al{sub 4}Sr and (Mg,Al){sub 17}Sr{sub 2} phases in AJ41 alloy. The tensile tests showed that at both room and elevated temperatures alloying additions of 1 wt.% Ce/La, Si and Sr resulted in an increase in the strength but a decrease in the ductility. Among the studied alloys, AS41 alloy exhibited the best strength. Wear test results showed that AE41 and AJ41 alloys similarly exhibited the best wear resistance owing to the presence of hard and dense intermetallics. Abrasion was the main wear mechanism under low applied loads while delamination, adhesion and oxidation mechanisms were majorly observed under high applied loads.

36 MATERIALS SCIENCE↗

In Situ X-Ray Diffraction Analysis of Face-Centered Cubic Metals Deformed at Room and Cryogenic Temperatures

The present study concerns the cryogenic processing of metals with simultaneous analysis of x-ray diffraction in a synchrotron ring. The mechanical properties improvement related to cryogenic processing of metals is attributed to the partial suppression of dynamic recovery. Thus, commercially pure metals with different stacking fault energies (silver, copper and aluminum) were deformed by uniaxial tensile tests and characterized by in situ x-ray diffraction, at room (293 K) and cryogenic (77 K) temperatures. The cryogenic processing allows a simultaneous improvement in ductility and strength for silver and copper and an improvement in strength for aluminum. This difference in mechanical properties was investigated by means of variations in crystallite size, microstrain and also the amount and size of dimples on the fracture surface. The microstructural refinement at cryogenic temperatures shows a tendency related to the stacking fault energies.

36 MATERIALS SCIENCE↗

On the Effect of Quenching on Postweld Heat Treatment of Friction-Stir-Welded Aluminum 7075 Alloy

This work focuses on the effect of postweld heat treatment (PWHT) on the mechanical properties and microstructural evolution of aluminum 7075 alloy processed via friction stir welding (FSW). FSW is known to be capable of grain refinement in the nugget zone (NZ). Two different quench media (water and air) were employed for PWHT. Regardless of the quench media, the PWHT led to the occurrence of grain growth in the NZ of the FSWed aluminum 7075 alloy. Abnormal grain growth occurred in the water quenched specimen. It is shown that ductility and strength of FSWed aluminum 7075 alloy are strongly dependent on the quenching rate. Changes in the mechanical properties and microstructure reveal that only at lower cooling rate this alloy is prone to the formation of precipitate-free zones (PFZs) in the vicinity of grain boundaries. Eventually, the PFZs deteriorate mechanical properties of this alloy.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on Microstructure and Mechanical Properties of Extruded Mg-4Zn-1.5Al-2Sn Alloy

The microstructure and mechanical properties of extruded Mg-4Zn-1.5Al-2Sn (ZAT422) alloy under different heat treatments were investigated by optical microscopy, scanning electron microscopy, x-ray diffraction, transmission electron microscopy, micro-hardness tests, and tensile tests. The results show that the as-extruded and heat-treated ZAT422 alloys mainly consisted of α-Mg and Mg{sub 2}Sn, and no ternary phase was detected. After aging, the amount of secondary phase precipitates increased significantly and the mechanical properties were improved. Among all the heat treatments, T5 heat treatment at 150 °C for 25 h resulted in the best combination of strength and ductility for ZAT422 alloy. The ultimate tensile strength, yield strength, and elongation (ε{sub f}) were found to be 290, 182 MPa, and 20%, respectively. Based on microstructural characterization, the variations in mechanical properties of the alloy subjected to heat treatment were analyzed in detail.

36 MATERIALS SCIENCE↗

Mechanical Behavior of Titanium-Based Layered Structures Fabricated Using Blended Elemental Powder Metallurgy

Mechanical behavior of bilayered structures composed of the layer of Ti-6Al-4 V (wt.%) (Ti-64) alloy and metal matrix composite (MMC) on the base of this alloy reinforced with 5 and 10% (vol.) of either TiB or TiC particles has been studied. Structures were fabricated using blended elemental powder metallurgy and studied by tensile and three-point flexural tests. Mechanical tests were performed on uniform single-layer samples of the alloy as well as individual MMCs. In addition, bilayered structures were also tested in three-point flexural experiment. Posttest fractographic inspections were made using the SEM. The deformation energy was measured based on engineering stress–strain curves obtained on tensile test. The results were compared with the data previously reported on Ti-64 alloy fabricated using cast and wrought technique. The presence of TiB and TiC reinforcement particles in the alloy causes substantial drop in strength and ductility of MMCs as compared to uniform sintered Ti-64 alloy, since those particles provide additional sites for the cracks and pores nucleation and promote the embrittlement of material. However, when MMC layers are used in bilayered structures with Ti-64 alloy layers, the three-point flexural test demonstrates significant increase in flexure stress compared to uniform Ti-64 alloy and uniform structures of MMCs. The suitability of studied structures for antiballistic impact application is discussed.

36 MATERIALS SCIENCE↗

A New Approach for Consolidation of Pure Magnesium Powder Using an Integrated Severe Plastic Deformation Route

In this paper, a new approach using a novel severe plastic deformation route is presented for consolidation and processing of a high-density and ultrafine-grained pure magnesium. Pure magnesium particles were successfully consolidated at 400 °C into a sufficiently dense bulk material using a new combined method including cyclic extrusion compression, equal channel angular pressing (ECAP) and conventional extrusion. The grain refinement, consolidation behavior and mechanical properties were deeply investigated. Results showed that the as-consolidated material had a fine grain structure with excellent tensile strength and ductility compared to as-cast and as-ECAPed specimens. Vickers microhardness increased from 38.75 to 52.58 during the process. Porosity also reduced considerably from 12.55 to 1.2% during the process which led to a dense bulk material. Results indicate that the introduced method is a promising and effective process for producing strong bulk materials from metal powders.

36 MATERIALS SCIENCE↗

Improved Mechanical Properties of Structural Steel via Developing Bimodal Grain Size Distribution and Intercritical Heat Treatment

Intercritical annealing and tempering heat treatment combined with cold rolling were applied for improvement of tensile properties and strain-hardening rate of structural steel. Coarse dual-phase (DP) microstructure was processed via intercritical heat treatment of the ferritic–pearlitic sheet, which resulted in the increase in tensile strength and disappearance of the yield point phenomenon. However, the tensile toughness was not effectively enhanced, which is indicative of unaltered strength–ductility trade-off. A bimodal-sized ferrite structure was obtained by cold rolling of the DP microstructure followed by subcritical annealing (tempering), where its characteristic features are high yield stress and relatively poor work-hardening response. Afterward, the intercritical annealing of the bimodal steel resulted in the development of fine DP steel with excellent work-hardening capacity and pronounced enhancement of tensile toughness. Conclusively, this work demonstrates the possibility of controlling the tensile properties and work-hardening behavior of conventional steels by simple heat treatment routes with the aid of cold rolling.

36 MATERIALS SCIENCE↗

Microstructural Development and Mechanical Properties of Friction Stir Welded Ferritic Stainless Steel AISI 409

This work investigates the effect of friction stir welding process parameters (rotation rate and traverse speed) on the microstructural evolution of friction stir welded (FSWed) ferritic stainless steel (FSS) AISI 409. Optical microscope, scanning electron microscope and electron backscattering diffraction are used to quantitatively assess the development in grain structure and texture. The microstructural development suggested that thermo-mechanical deformation occurs in the stir zone within the austenite/ferrite phase region, ultimately transforming upon cooling into bainitic/ferritic microstructure. The fraction and size of the bainitic/ferritic grains are found to vary through the thickness of the joints. High fractions of coarse ferritic grains are found near the top of the stir zone, and low fraction of fine ferritic grains is found near the bottom of the stir zone. This bainitic/ferritic grain structure resulted in an increase in the hardness of the stir zone by about 74% relative to the base material. The tensile strength of the FSWed FSS joints is almost at the same level of the base material with reduction in the ductility as a result of the increased hardness of the weld zone.

36 MATERIALS SCIENCE↗

Effect of Solutionizing Time on Improving the Microstructure and Mechanical Properties of Aged AZ80 Mg Alloy

The effects of solutionizing soak time and aging on the microstructure and mechanical properties of cast AZ80 Mg alloy were investigated. Optical microscopy, scanning electron microscopy and x-ray diffraction revealed the dissolution of β-Mg{sub 17}Al{sub 12} phase in the solution-treated samples which was later detected in the aged condition. Solution treatments at 420 °C for 4-16 h with water quenching followed by aging at 200 °C for 10 h were carried out, causing discontinuous precipitates to be formed with different precipitate morphologies at the various soak times. The discontinuous precipitates were observed to transform from the interdendritic segregation to parallel lamellae with increasing soak time to 8-10 h. As the soak time increased to 16 h, parallel lamellae transformed into tree-like precipitate morphology. The results showed significant changes in the interlamellar spacing at different soak times, and such precipitate morphology could influence the microstructure and mechanical properties after the aging process. A good combination of strength and ductility was obtained when the cast AZ80 Mg alloy was solution-treated at 420 °C for 10 h and aged at 200 °C for 10 h. Compared to the as-cast condition, a significant increase in ultimate tensile strength (50%), yield strength (47%) and elongation (43%) were observed.

36 MATERIALS SCIENCE↗

Microstructure, Texture, and Mechanical Properties of Continuously Extruded and Rolled AZ31 Magnesium Alloy Sheets

It is difficult to fabricate magnesium alloy sheets at room temperature due to their hexagonal close-packed structure. In this paper, we proposed a new process that can be used to fabricate AZ31 magnesium alloy sheets with fine-grained microstructure and good mechanical properties. AZ31 magnesium alloy sheets with dimensions of 160 mm × 8 mm were obtained successfully by a continuous extrusion technique. The extruded sheets were then rolled by two different rolling routes, Route 1: the extruded sheet was heated at 350 °C and then rolled without heating of rolls and Route 2: the sheet was rolled without any previous heating by heating rolls at 280 °C. The microstructure and texture evolution as well as mechanical properties of the continuously extruded and rolled sheets were examined experimentally. The magnesium alloy sheets with relatively fine grains of 4.5-8.3 µm were obtained by continuous extrusion followed by rolling processes. The tensile strength of continuously extruded AZ31 Mg alloy sheets can be effectively increased by rolling using heating rolls (Route 2), while the ductility was enhanced by rolling heated sheets (Route 1). The mixed microstructure, consisting of refined DRX grains and deformed grains, contributes to enhancement in tensile strength of the sheet samples rolled by Route 2 due to grain-boundary strengthening and work hardening. Lower temperature and larger rolling reduction are two main factors for improving the tensile strength of AZ31magnesium alloy sheets.

36 MATERIALS SCIENCE↗

Predictive Reactor Pressure Vessel Steel Irradiation Embrittlement Models: Issues and Opportunities

Nuclear plant life extension to 80 years will require accurate predictions of neutron irradiation-induced increases in the ductile-brittle transition temperature ( T) of reactor pressure vessel (RPV) steels at high fluence conditions that are far outside the existing database. Remarkable progress in mechanistic understanding of irradiation embrittlement has led to physically motivated T correlation models that provide excellent statistical fi ts to the existing surveillance database. However, an important challenge is developing advanced embrittlement models for low fl ux-high fl uence conditions pertinent to extended life. These new models must also provide better treatment of key variables and variable combinations and account for possible delayed formation of late blooming phases in low copper steels. Other issues include uncertainties in the compositions of actual vessel steels, methods to predict T attenuation away from the reactor core, verifi cation of the master curve method to directly measure the fracture toughness with small specimens and predicting T for vessel annealing remediation and re-irradiation cycles.

36 MATERIALS SCIENCE↗

Metallic Glasses: Gaining Plasticity for Microsystems

Since the 1960s, metallic glasses (MGs) have attracted tremendous research interest in materials science and engineering, given their unique combination of mechanical properties. However, the industrial applications of MGs have been hindered due to their lack of ductility in bulk form at room temperature. In contrast, it was observed that MGs could exhibit excellent plasticity at the small size scale. In this article, we summarize the related experimental findings having been reported so far together with the possible origins of such a size effect in MGs. The enhanced plasticity of MGs in small volumes, together with their high mechanical strengths and remarkable thermoplastic formability, strongly implies that MGs are the promising materials for fabricating the next generation of micro- and nano-devices.

36 MATERIALS SCIENCE↗

Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials

The feasibility of using 'grain-boundary engineering' techniques to reduce the susceptibility of a metallic material to intergranular embrittlement in the presence of hydrogen is examined. Using thermomechanical processing, the fraction of 'special' grain boundaries was increased from 46% to 75% (by length) in commercially pure nickel samples. In the presence of hydrogen concentrations between 1200 and 3400 appm, the high special fraction microstructure showed almost double the tensile ductility; also, the proportion of intergranular fracture was significantly lower and the J{sub c} fracture toughness values were some 20-30% higher in comparison with the low special fraction microstructure. We attribute the reduction in the severity of hydrogen-induced intergranular embrittlement to the higher fraction of special grain boundaries, where the degree of hydrogen segregation at these boundaries is reduced.

36 MATERIALS SCIENCE↗

An assessment of the contributing factors to the superior properties of a nanostructured steel using in situ high-energy x-ray diffraction.

In contrast to most nanostructured materials, outstanding mechanical property has been demonstrated in a nanostructured metastable austenitic steel, owing to the new characteristics of deformation-induced martensitic transformation. In this paper, by employing an in situ high-energy X-ray diffraction technique, we explore these characteristics by examining factors from the load partitioning, Lueders banding, to texture development. It was found that the martensitic transformation was mainly driven through Lueders band propagation. Marked load transfer takes place from austenite to martensite as Lueders band propagates, and continues into the homogeneous deformation regime. The texture development is mostly contributed by martensitic transformation, but dislocation-based plasticity also plays a role. The effective load partitioning along with the deformability of martensite promotes sample ductility.

36 MATERIALS SCIENCE↗

Mechanical properties and determination of slip systems of the B2 YZn intermetallic compound

Single crystal specimens of YZn (B2) were tested in tension at room temperature. Specimens with a [1 0 1] tensile axis orientation exhibited {r_brace}0 1 1{l_brace} <100> primary slip and an ultimate tensile strength of 365MPa at 3.7% elongation. Specimens with [0 0 1] and [1 1 1] tensile axis orientations showed no slip lines and fractured at a stress of 180MPa at 3.3% and 130MPa at 2.9% elongation, respectively. Transmission electron microscopy (TEM) examination of the Burger's vector of dislocations in tensile tested specimens revealed <1 0 0>-type dislocations. TEM analysis suggested that a secondary slip system, {l_brace}0 0 1{r_brace}<1 0 0>, may be active. Banded features with a {l_brace}0 2 1{r_brace} orientation were observed in deformed YZn; these may be slip traces produced by the cross-slip of <1 0 0> dislocations. Acting together, {l_brace}0 1 1{r_brace} <1 0 0> and {l_brace}0 0 1{r_brace} <1 0 0> slip provide only three independent slip systems, and no extra independent systems are provided by the cross-slip. This finding is consistent with the low ductility of YZn.

36 MATERIALS SCIENCE↗

Mechanical properties of nanoporous gold in tension

We report results of the tensile properties of nanoporous gold (NPG) as a function of the density and average ligament diameter. As-dealloyed tensile samples were thermally treated to coarsen the length scale of the NPG structure while increasing the sample density resulting from thickness reductions. The behaviors of samples with mean ligament diameters ranging from 30 to 750 nm and corresponding densities ranging from 0.30 to 0.57 that of bulk gold were examined. Digital image analysis was used to obtain ligament size histograms that were fit to the Weibull distribution. The Young's modulus was found to obey a power law, but with an exponent larger than that predicted by Gibson-Ashby scaling. The fracture behavior showed a brittle-ductile transition as a function of increasing ligament size. For samples characterized by a mean ligament diameter less than ~ 220 nm, the tensile behavior was linear elastic to sample fracture while samples with larger scale ligaments showed macroscopic yielding prior to fracture. These results are interpreted within the framework of extreme value statistics.

36 MATERIALS SCIENCE↗