Characterization of Microstructure, Mechanical Properties and Formability of Cryorolled AA5083 Alloy Sheets

In this work, microstructure, mechanical properties and formability of cryorolled and annealed AA5083 alloy sheets have been characterized and a comparison has been made with cold rolled and annealed sheets. Five-millimeter-thick sheets of this alloy were cryorolled in multiple passes to a final thickness of 1 mm (80% reduction with a true strain of 1.6). Effect of annealing time and temperature on hardness has been studied, and it has been found that a short annealing at 275 °C for 15 min after cryorolling would yield a good combination of strength and ductility. Microstructural investigations showed that the cryorolled and short annealed samples possess bimodal grain structure which is responsible for better mechanical properties than cold rolled sheets. From the experimentally determined forming limit diagrams, the limit strains of cryorolled sheets have been found to be almost equal to conventional cold rolled and annealed sheets in all modes of deformation. No major differences have been found in strain distribution also. This work clearly demonstrates that cryorolling of AA5083 alloy sheets followed by a short annealing with bimodal grain structure can be used for sheet metal forming applications with higher strength and toughness than conventional sheets without any reduction in formability.

36 MATERIALS SCIENCE↗

Effect of Electropulsing-Assisted Ultrasonic Nanocrystalline Surface Modification on the Surface Mechanical Properties and Microstructure of Ti-6Al-4V Alloy

The effect of electropulsing-assisted ultrasonic nanocrystalline surface modification (EP-UNSM) on surface mechanical properties and microstructure of Ti-6Al-4V alloy is investigated. Compared to conventional ultrasonic nanocrystalline surface modification (UNSM), EP-UNSM can effectively facilitate surface roughness and morphology, leading to excellent surface roughness (reduced from Ra 0.918 to Ra 0.028 μm by UNSM and Ra 0.019 μm by EP-UNSM) and smoother morphology with less cracks and defects. Surface friction coefficients are enhanced, resulting in lower and smoother friction coefficients. In addition, the surface-strengthened layer and ultra-refined grains are significantly enhanced with more severe plastic deformation and a greater surface hardness (a maximum hardness value of 407 HV and an effective depth of 550 μm, in comparison with the maximum hardness value of 364 HV and effective depth of 300 μm obtained by conventional UNSM). Remarkable enhancement of surface mechanical properties can be attributed to the refined gradient microstructure and the enhanced severe plastic deformation layer induced by coupling the effects of UNSM and electropulsing. The accelerated dislocation mobility and atom diffusion caused by the thermal and athermal effects of electropulsing treatment may be the primary intrinsic reasons for these improvements.

36 MATERIALS SCIENCE↗

Characterization of Microstructure and Wear Resistance of PEO Coatings Containing Various Microparticles on Ti6Al4V Alloy

Titania-based composite coatings were prepared by plasma electrolytic oxidation (PEO) treatment of Ti6Al4V alloy in electrolyte with α-Al{sub 2}O{sub 3}, Cr{sub 2}O{sub 3} or h-BN microparticles in suspension. The microstructure, composition of PEO composite coatings were analyzed by SEM, EDS and XRD. The wear resistance of composite ceramic coatings was studied by ball-on-disk wear test at ambient temperature and 300 °C. The results showed that the addition of microparticles accelerated the growth rate of PEO coating and changed the microstructure and composition of PEO coating. PEO coating was porous and mainly composed of rutile-TiO{sub 2}, anatase-TiO{sub 2} and Al{sub 2}TiO{sub 5}. PEO/α-Al{sub 2}O{sub 3} (Cr{sub 2}O{sub 3} or h-BN) composite coating only had small micropores and appeared some α-Al{sub 2}O{sub 3} (Cr{sub 2}O{sub 3} or h-BN) phase. Besides, the addition of α-Al{sub 2}O{sub 3} (Cr{sub 2}O{sub 3} or h-BN) microparticles greatly improved the wear resistance of PEO coating. At ambient temperature, abrasive wear dominated the wear behavior of PEO coating, but abrasive wear and adhesive peel simultaneously happened at 300 °C. Whether at ambient temperature or 300 °C, PEO composite coating had better wear resistance than PEO coating. Besides, PEO/h-BN composite coating outperformed other composite coatings regardless of the temperature.

36 MATERIALS SCIENCE↗

Effect of Yttrium Addition on the Microstructure and Mechanical Properties of Cu-Rich Nano-phase Strengthened Ferritic Steel

Due to the brittle problem of Cu-rich nano-phase strengthened ferritic steel (CNSFS) after air aging, the effect of Y addition in CNSFS was systemically investigated in the present work. The microstructure, tensile fracture morphology and oxide layer of the steels were surveyed by optical microscope and scanning electron microscope. Transmission electron microscope with the combination of energy-dispersive x-ray spectroscopy and selected area electron diffraction was used to analyze the morphology, size, number density, chemical compositions and crystal structure for nano-crystalline precipitates. Microstructural examinations of the nano-crystalline precipitates show that Cu-rich precipitates and Y compounds in the range of 2-10 and 50-100 nm, respectively, form in the Y-containing steel; meanwhile, the average size of nano-crystalline precipitates in Y-containing steel is larger, but the number density is lower, and the ferritic grains are refined. Furthermore, the tensile strength and ductility of Y-containing steel after air aging are improved, whereas the tensile strength is enhanced and the ductility decreased after vacuum aging. The drag effect of Y makes the oxide layer thinner and be compacted. Tensile properties of CNSFS after air aging are improved due to the refined grains, antioxidation and purification by the addition of Y.

36 MATERIALS SCIENCE↗

Investigation of the Microstructural Changes and Hardness Variations of Sub-Zero Treated Cr-V Ledeburitic Tool Steel Due to the Tempering Treatment

The microstructure and tempering response of Cr-V ledeburitic steel Vanadis 6 subjected to sub-zero treatment at − 196 °C for 4 h have been examined with reference to the same steel after conventional heat treatment. The obtained experimental results infer that sub-zero treatment significantly reduces the retained austenite amount, makes an overall refinement of microstructure, and induces a significant increase in the number and population density of small globular carbides with a size 100-500 nm. At low tempering temperatures, the transient M{sub 3}C-carbides precipitated, whereas their number was enhanced by sub-zero treatment. The presence of chromium-based M{sub 7}C{sub 3} precipitates was evidenced after tempering at the temperature of normal secondary hardening; this phase was detected along with the M{sub 3}C. Tempering above 470 °C converts almost all the retained austenite in conventionally quenched specimens while the transformation of retained austenite is rather accelerated in sub-zero treated material. As a result of tempering, a decrease in the population density of small globular carbides was recorded; however, the number of these particles retained much higher in sub-zero treated steel. Elevated hardness of sub-zero treated steel can be referred to more completed martensitic transformation and enhanced number of small globular carbides; this state is retained up to a tempering temperature of around 500 °C in certain extent. Correspondingly, lower as-tempered hardness of sub-zero treated steel tempered above 500 °C is referred to much lower contribution of the transformation of retained austenite, and to an expectedly lower amount of precipitated alloy carbides.

36 MATERIALS SCIENCE↗

Deformational Features and Microstructure Evolution of Copper Fabricated by a Single Pass of the Elliptical Cross-Section Spiral Equal-Channel Extrusion (ECSEE) Process

The objectives of this work are to study the deformational feature, textures, microstructures, and dislocation configurations of ultrafine-grained copper processed by the process of elliptical cross-section spiral equal-channel extrusion (ECSEE). The deformation patterns of simple shear and pure shear in the ECSEE process were evaluated with the analytical method of geometric strain. The influence of the main technical parameters of ECSEE die on the effective strain distribution on the surface of ECSEE-fabricated samples was examined by the finite element simulation. The high friction factor could improve the effective strain accumulation of material deformation. Moreover, the pure copper sample fabricated by ECSEE ion shows a strong rotated cube shear texture. The refining mechanism of the dislocation deformation is dominant in copper processed by a single pass of ECSEE. The inhomogeneity of the micro-hardness distribution on the longitudinal section of the ECSEE-fabricated sample is consistent with the strain and microstructure distribution features.

36 MATERIALS SCIENCE↗

Effects of Synchronous Rolling on Microstructure, Hardness, and Wear Resistance of Laser Multilayer Cladding

A synchronous rolling method was proposed to assist laser multilayer cladding, and the effects of this method on microstructure, microhardness, and wear resistance were studied. Results show that the microstructure and mechanical properties of the traditional cladding layer exhibit periodic inhomogeneity. Synchronous rolling breaks the columnar dendrite crystals to improve the uniformity of the organization, and the residual plastic energy promotes the precipitation of strengthening phases, as CrB, M{sub 7}C{sub 3}, etc. The hardness and wear resistance of the extruded cladding layer increase significantly because of the grain refinement, formation of dislocations, and dispersion strengthening. These positive significances of synchronous rolling provide a new direction for laser cladding technology.

36 MATERIALS SCIENCE↗

Mechanical Properties and Microstructure of High-Strength Steel Controlled by Hot Stamping Process

A novel design and manufacturing method, dubbed “precast,” of the cooling system and tools for a hot forming process was proposed in this paper. The integrated structures of the punch and blank holder were determined by analyzing the bending and reverse-bending deformation of the forming parts. The desired crashworthiness performance of an automotive front bumper constructed with this process was obtained by a tailored phase transformation, which generated martensite-bainite in the middle and full martensite transformation in the corner areas. Varying cooling effects in the formed parts caused the highest temperature to be located in the bottom and the lowest on the end of the formed parts. Moreover, the microstructural distributions demonstrated that the bottom possessed a relatively lower content of martensite, while, conversely, the end possessed a higher content. This was precisely the most desired phase distributions for the hot formed parts. For the six-process cycle stamping, the temperatures reached a stable status after an initial rapid increase in the first three process cycles. The microstructural results verified the feasibility of the hot forming tools under multiprocess cycles.

36 MATERIALS SCIENCE↗

Effects of TiB{sub 2} Particle and Short Fiber Sizes on the Microstructure and Properties of TiB{sub 2}-Reinforced Composite Coatings

In this study, particle and short fiber-reinforced titanium matrix composite coatings are prepared via laser in situ technique using (0.5 and 50 μm) TiB{sub 2} and Ti powder as cladding materials. The microstructure and properties of the composite coatings are studied, and the changing mechanism of the microstructure is discussed. The results reveal that particle agglomeration is prone to appear with using fine TiB{sub 2} particles. Decomposition of the particles preferentially occurs with using coarse TiB{sub 2} particles. The cracks and pores on the surface of the coating are formed at a lower laser energy density. With the increase in the laser energy density, cracking on the surface of the coating diminishes, but the coating exhibits depression behavior. The depression extent of the coating using fine TiB{sub 2} particle as the reinforcement is much less than that of the coating using coarse TiB{sub 2} particle. Moreover, the size of the aggregate and the tendency of cracking can be reduced with the increase in Ti addition. Meanwhile, short TiB fiber bundles are formed by the diffusion mechanism of rod aggregate, and randomly oriented TiB short fibers are formed mainly by the dissolution–precipitation mechanism of fine TiB{sub 2} particles. Moreover, the growth of short TiB fibers can be in an alternating manner between B27 and Bf structures. The micro-hardness and wear resistance of the coatings are evidently higher than that of the titanium alloy substrate. The wear resistance of the large size TiB{sub 2} coating is higher than that of the small size TiB{sub 2} coating under the condition of low load.

36 MATERIALS SCIENCE↗

Microstructure and Strain Rate-Dependent Tensile Deformation Behavior of Fiber Laser-Welded Butt Joints of Dual-Phase Steels

The microstructure and tensile deformation behavior of the fiber laser-welded similar and dissimilar dual-phase (DP) steel joints over a wide range of strain rates from 10{sup −3} to 10{sup 3} s{sup −1} were investigated for the further applications on the lightweight design of vehicles. The high strain rate dynamic tensile deformation process and full-field strain distribution of the base metals and welded joints were examined using the digital image correlation method and high-speed photography. The strain rate effects on the stress–strain responses, tensile properties, deformation, and fracture behavior of the investigated materials were analyzed. The yield stress (YS) and ultimate tensile strength (UTS) of the dissimilar DP780/DP980 welded joints were lying in-between those of the DP780 and DP980 base metals, and all materials exhibited positive strain rate dependence on the YS and UTS. Owing to the microstructure heterogeneity, the welded joints showed relatively lower ductility in terms of total elongation (TE) than those of the corresponding base metals. The strain localization started before the maximum load was reached, and the strain localization occurred earlier during the whole deformation process with increasing strain rate. As for the dissimilar welded joint, the strain localization tended to occur in the vicinity of the lowest hardness value across the welded joint, which was in the subcritical HAZ at the DP780 side. As the strain rate increased, the typical ductile failure characteristic of the investigated materials did not change.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded Dual-Phase Brass

Friction stir welding (FSW) is an ideal process to join brass to avoid the evaporation of zinc. In the present investigation, 6-mm-thick dual-phase brass plates were joined efficiently using FSW at various tool rotational speeds. The microstructures were studied using optical microscopy, electron backscattered diffraction and transmission electron microscopy. The optical micrographs revealed the evolution of various zones across the joint line. The microstructure of the heat-affected zone was similar to that of base metal. The weld zone exhibited finer grains due to dynamic recrystallization. The recrystallization was inhomogeneous and the inhomogeneity reduced with increased tool rotational speed. The dual phase was preserved in the weld zone due to the retention of zinc. The severe plastic deformation created a lot of dislocations in the weld zone. The weld zone was strengthened after welding. The role of tool rotational speed on the joint strength is further reported.

36 MATERIALS SCIENCE↗

Microstructural Characteristics and Mechanical Properties of an Electron Beam-Welded Ti/Cu/Ni Joint

Electron beam welding experiments of TA15 titanium alloy to GH600 nickel superalloy with and without a copper sheet interlayer were carried out. Surface appearance, microstructure and phase constitution of the joint were examined by optical microscopy, scanning electron microscopy and x-ray diffraction analysis. Mechanical properties of Ti/Ni and Ti/Cu/Ni joint were evaluated based on tensile strength and microhardness tests. The results showed that cracking occurred in Ti/Ni electron beam weldment for the formation of brittle Ni-Ti intermetallics, while a crack-free electron beam-welded Ti/Ni joint can be obtained by using a copper sheet as filler metal. The addition of copper into the weld affected the welding metallurgical process of the electron beam-welded Ti/Ni joint significantly and was helpful for restraining the formation of Ti-Ni intermetallics in Ti/Ni joint. The microstructure of the weld was mainly characterized by a copper-based solid solution and Ti-Cu interfacial intermetallic compounds. Ti-Ni intermetallic compounds were almost entirely suppressed. The hardness of the weld zone was significantly lower than that of Ti/Ni joint, and the tensile strength of the joint can be up to 282 MPa.

36 MATERIALS SCIENCE↗

Effects of Multiple Rejuvenation Cycles on Mechanical Properties and Microstructure of IN-738 Superalloy

The scope of this work is to show the effects of multiple applications of a rejuvenation treatment studied for IN-738 on both the microstructure and the mechanical properties of the creep-damaged superalloy and to check the recovery obtained after one and two rejuvenation cycles through creep and tensile tests, whose results will be compared with the performance of the virgin material. This work will show that this rejuvenation treatment is able to recover the microstructure of creep-damaged specimens after one and two applications and that the mechanical properties of the rejuvenated alloy are very similar to the virgin material even after two rejuvenation cycles.

36 MATERIALS SCIENCE↗

Densification, Microstructural Evolution, Mechanical Properties and Oxidation Study of CrB{sub 2} + EuB{sub 6} Composite

This paper reports the results of investigation on densification, microstructural evolution, mechanical properties and oxidation study of CrB{sub 2} + EuB{sub 6} composite. CrB{sub 2} + EuB{sub 6} (10 and 20 wt.%) composites have been fabricated by hot pressing at a temperature of 1700 °C and 35 MPa pressure. The hardness and flexural strength were measured in the range of 21.25-24.48 GPa and 171-199 MPa, respectively. The fracture toughness increased from 3.3 to 4.01 MPa m{sup 1/2} by the addition of 20% EuB{sub 6}. Microstructural evolution revealed the uniform distribution of EuB{sub 6} and absence of any reaction product. Fracture surface analysis confirmed the presence of transgranular mode of fracture. Oxidation study at 1200 °C revealed that the developed composites have good oxidation resistance and followed the parabolic rate of oxidation.

36 MATERIALS SCIENCE↗

Multiphase Microstructure in a Metastability-Assisted Medium Carbon Alloy Steel

A medium carbon alloy steel is processed by austenizing at 900 °C for 30 min, then rapid quenching into a patented quenching liquid and holding at 170 °C for 5 min, finally isothermally holding at 250 °C for different times. The morphology and mechanical properties are performed by using optical microscopy and scanning electron microscopy. A multiphase microstructure characterized by a mixture of lenticular prior martensite (PM), fine needle bainitic ferrite and filmy retained austenite (RA) is obtained. It is found that the PM formed firstly upon quenching can accelerate the subsequent bainitic transformation and promote refinement of multiphase colonies. The results show that an optimum mechanical property of a 4000.9 MPa bending strength and a 2030 MPa tensile strength is achieved at 250 °C for 120 min, which is attributed to the multiphase microstructural characteristics and a high product of the volume fraction of RA and the carbon content of austenite.

36 MATERIALS SCIENCE↗

Effect of Multiple Local Repairs on Microstructure and Mechanical Properties of T24 Steel Welded Joint

The effect of multiple local repairs on the microstructure and mechanical properties of the T24 steel welded joints was studied. T24 steel tubes were butt-welded by the GTAW method. Peripheral welded joints were made in four locations of the tube. In order to simulate the repair procedure, the welds were cut off from the root and the first local repair was performed. Other two local repairs were carried out in the same way. After each local repair, the microstructure and mechanical properties of the joints were evaluated. The results of the mechanical tests demonstrate that only two local repairs can be performed on the T24 steel peripheral welded joint. After the third local repair, impact energy of the welded joint was lower than required value, which is attributed to the coarser martensite and the coarser carbide precipitates formed in the heat-affected zone, compared with the weld metal.

36 MATERIALS SCIENCE↗

Effects of Controlled Cooling-Induced Ferrite–Pearlite Microstructure on the Cold Forgeability of XC45 Steel

The combination of hot/warm and cold forging with an intermediate controlled cooling process is a promising approach to saving costs in the manufacture of automobile parts. In this work, the effects of the ferrite–pearlite microstructure, which formed after controlled cooling, on the cold forgeability of a medium-carbon steel were investigated. Different specimens for both normal and notched tensile tests were directly heated to high temperature and then cooled down at different cooling rates, producing different ferrite volume fractions, ranging from 6.69 to 40.53%, in the ferrite–pearlite microstructure. The yield strength, ultimate tensile strength, elongation rate, percentage reduction of area, and fracture strain were measured by tensile testing. The yield strength, indicating deformation resistance, and fracture strain, indicating formability, were used to evaluate the cold forgeability. As the ferrite volume fraction increased, the cold forgeability of the dual-phase ferritic–pearlitic steel improved. A quantitatively relationship between the ferrite volume fraction and the evaluation indexes of cold forgeability for XC45 steel was obtained from the test data. To validate the mathematical relationship, different tensile specimens machined from real hot-forged workpieces were tested. There was good agreement between the predicted and measured values. Our predictions from the relationship for cold forgeability had an absolute error less than 5%, which is acceptable for industrial applications and will help to guide the design of combined forging processes.

36 MATERIALS SCIENCE↗

Microstructural Investigation of VPPA–GMAW Welded 7A52 Aluminum Alloys

In this study, the microstructural features of 7A52 heat-treatable aluminum alloys welded by variable polarity plasma arc (VPPA) combined with gas metal arc welding (GMAW) (VPPA–GMAW) were investigated and compared with those of 7A52 aluminum alloys welded by GMAW. The grain structures and modification of the precipitates were analyzed by optical microscopy and transmission electron microscopy. Complementary to modification of the precipitates, the precipitation evolution in the heat-affected zone and magnesium loss in the fusion zone were measured by differential scanning calorimetry and inductively coupled plasma spectroscopy. In VPPA–GMAW, the weld only needs one pass by depositing on one side of the 10-mm-thick aluminum alloy plates because of the large penetration capability of VPPA and good fluidity of the molten metal in the weld pool. Accordingly, the effect of excessive heat input on the microstructure can be minimized. The results show that the grain growth is not obvious and the magnesium loss is small in the fusion zone of VPPA–GMAW compared with that of GMAW under the condition of equal heat input to the workpiece. Small precipitates inside the grains remain homogeneously distributed, and a large volume fraction of the η′ phase exists. The VPPA–GMAW weld exhibits less tendency to soften; thus, VPPA–GMAW is appropriate for welding thick-plate aluminum alloys with a high production rate.