Search NASA⌕ Search

SEARCH · Search NASA

Results for “Microstructures”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,531 records · Page 85

Effect of quenching rate on the microstructure and mechanical behavior of Ce75Al21Ga4 glassy alloy

Highlights: • Structural and microstructural changes with respect to quenching rate have been reported. • Ribbons synthesized at slow cooling rate shows higher hardness and yield strength. • Study is focused on the correlation between quenching rate and mechanical behavior. • Metallic glass synthesized at faster quenching rate contains the highest shear band density. - Abstract: The present study deals with the structural and microstructural changes with respect to the quenching rate and their correlation with mechanical behavior of melt-spun Ce{sub 75}Al{sub 21}Ga{sub 4} glassy alloys. The ribbons of the alloy have been synthesized at different quenching rates obtained through different wheel speeds (44, 36, 29, 22 and 15 m/s). The glass forming indicators and mechanical properties have been investigated at different quenching rates. The higher quenching rate obtained through high wheel speed (44, 36 and 29 m/s) has led to phase separation giving rise to nano-amorphous domains in a glassy matrix while the lower quenching rate obtained through lower wheel speed (22 and 15 m/s) produces nano-crystalline grains with size ranges from 25 ± 1 to 120 ± 1 nm. It has been found that the size of the nano-amorphous domains decreases with decrease in wheel speed. The mechanical behavior has been studied using micro-indentation technique. The indentation test indicates that with the same chemical composition, the ribbons synthesized at slow quenching rate exhibits higher hardness and yield strength than those synthesized at faster quenching rate. The ribbons synthesized at 44 m/s contains the large free volume and has the highest shear band density.

36 MATERIALS SCIENCE↗

TEM analysis of the deformation microstructure of polycrystalline cobalt plastically strained in tension

Highlights: • Deformation of cobalt was studied by TEM and AE. • Basal dislocation glide is the main deformation mechanism in first straining stage. • Twinning mechanism becomes predominant in the second stage. • Statistical analysis was performed in data set generated by electron diffraction. • Tensile {10 2-bar 1} twins are the most common twins in cobalt. - Abstract: The microstructure evolution of hexagonal close-packed cobalt at different stages of work hardening has been studied. The deformation microstructure of polycrystalline samples upon a tension test was investigated by Transmission Electron Microscopy (TEM). Corresponding straining mechanisms were also identified by acoustic emission measurements. It was shown that dislocation glide is the predominant deformation mechanism during the first stage of plastic deformation, while twinning becomes the prominent strain accommodation mechanism in the later stage. A detailed TEM study using electron diffraction allowed identifying different types of twins activated during tensile testing. Four single twinning modes were identified, from which two types correspond to tensile strain and two types to compressive strain (with respect to the c direction), double twins were also observed. A relative importance of various systems is estimated and it is shown that the vast majority of twins correspond to the {10 1-bar 2} twinning system.

36 MATERIALS SCIENCE↗

Effect of gadolinium addition on microstructural evolution and solidification characteristics of Al-15%Mg2Si in-situ composite

Highlights: • The Al{sub 3}Gd is the heterogeneous nucleation of primary Mg{sub 2}Si in Al-15%Mg{sub 2}Si composite. • Addition of Gd to Al-15%Mg{sub 2}Si resulted in the formation of Al{sub 2}Si{sub 2}Gd and AlSiGd intermetallic compounds. • Absorption of Gd atoms preferentially on {100} facets of Mg{sub 2}Si crystals changed its growth manners. • Primary Mg{sub 2}Si transformed from coarse-dendritic to perfect truncated octahedral shape after treating with 1.0 wt% Gd. • Gd addition increased the nucleation and growth temperatures of primary Mg{sub 2}Si. - Abstract: The current study investigated the effects of gadolinium (Gd) addition (0, 0.3, 0.5, 1.0, and 2.0 wt%) on microstructural development and solidification characteristics of hypereutectic Al-15%Mg{sub 2}Si in-situ composite. Microstructural examinations were carried out via optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), transmission electron microscopy (TEM), and electron backscattered diffraction (EBSD). The results showed that an addition of 1.0 wt% Gd, changed the morphology of primary Mg{sub 2}Si from coarse dendritic to fine truncated octahedral shape. Furthermore, the average size of primary Mg{sub 2}Si particles decreased from 40 μm to 20 μm and density increased from 495 to 1167 particles/mm{sup 2}. Besides that, cooling curve thermal analysis (CCTA) technique revealed that Gd addition increased nucleation and growth temperatures of primary Mg{sub 2}Si phase. It is proposed that modification and refinement mechanism of Gd addition are mainly attributed to formation of tiny Al{sub 3}Gd particles as the heterogeneous nucleation substrates for primary Mg{sub 2}Si, which results in a refined distribution of these particles and poisoning effect by adsorbing Gd atoms, preferentially on {100} facets of Mg{sub 2}Si crystals. Moreover, it is believed that formation of Gd intermetallic compounds is responsible for refinement of primary Mg{sub 2}Si particles.

36 MATERIALS SCIENCE↗

Fabrication, microstructure, and wear performance of WC-Fe composite/metal coating fabricated by resistance seam welding

Highlights: • WC-Fe/metal coating consisted of WC-Fe layer and metal interlayer was fabricated by resistance seam welding. • The microstructure, hardness and wear performance of coatings with different WC particles size were analyzed. • The wear mechanism of coatings showed huge difference following various sliding distance. - Abstract: WC-Fe composite/metal coatings consisting of a WC-Fe composite layer and a metal interlayer were successfully fabricated on an Al 6061 substrate by resistance seam welding. The microstructures and phase compositions of the WC-Fe composite/metal coatings with different WC particle sizes (nano, fine, and coarse) were investigated. The WC-Fe composite layer consisted of WC particles and a Fe-C-Si super hard alloy (SHA) component, whereas the metal interlayer was composed of SHA, FeAl{sub 3}, Fe{sub 2}Al{sub 5}, and Al 6061. The surface microhardness of the WC-Fe composite/metal coating increased with increasing WC particle size. The wear performance of the coatings tested with different sliding distances is discussed in detail. Coating-C (coarse) showed the best wear resistance. The wear rates of both coating-N (nano) and coating-C decreased as the sliding distance increased, while coating-F (fine) demonstrated the opposite behavior. The wear mechanisms of the coatings were drastically different owing to the significantly different WC particle behavior at various sliding distances.

36 MATERIALS SCIENCE↗

Microstructures and deformation mechanisms of Cr26Mn20Fe20Co20Ni14 alloys

Highlights: • The single-phase FCC alloy as the annealing temperature exceeding 1015 °C • The dual-phase structure as the annealing temperature lower than 1000 °C • The σ phases grow primarily at grain boundaries. • The single-phase alloy deforms via dislocations and twins. • In-situ tensile experiment reveals twinning at the crack tip. - Abstract: We investigated microstructures and tension properties of Cr{sub 26}Mn{sub 20}Fe{sub 20}Co{sub 20}Ni{sub 14} alloys that were produced by arc-melting and subsequent thermal-mechanical processing—hot-rolling → cold-rolling → annealing at different temperatures ranging from 500 °C to 1100 °C for 1 h → air cooling. Microstructure characterization shows the single-phase solid solution with face centered cubic structure as the annealing temperature exceeding 1015 °C while the dual-phase structure (Cr-rich σ phase and FCC solid solution) as the annealing temperature lower than 1000 °C. The σ phases grow primarily at grain boundaries and act as precipitation strengthening units to enhance strain hardening rate. The single-phase solid solution deforms plastically via dislocations and twins. Twin boundaries associated with deformation twinning impede dislocation motion, enhancing the strain hardening capacity. In-situ tensile experiment in transmission electron microscope further reveals that twinning occurs at the crack tip and facilitates the deflection of crack propagation towards twinning shear direction. This work implies that a strength-ductility combination can be realized by coupling precipitation strengthening and twinning-induced plasticity in multiple principle elements alloys.

36 MATERIALS SCIENCE↗

Hot-worked microstructure and hot workability of cold-work tool steels

Highlights: • Hot compression tests were conducted for D2 and an 8% Cr steel. • Processing maps were constructed for the evaluation of their hot workability. • They had similar hot workability concerning the flow instability. • The 8% Cr steel exhibited a larger resistance to dynamic recrystallization. - Abstract: The hot workability of two cold-work tool steels were evaluated and compared. A D2 and an advanced alloy based on 8% Cr steels (TDx) were deformed at high temperatures between 900 and 1100 °C with strain rates 0.001–10 s{sup − 1} via hot compression test. From the flow curves, processing maps were constructed based on the dynamic material model. The deformed microstructures were observed and compared in various scales with respect to the deformation conditions. Although the two alloys exhibited a large similarity in the flow instability consideration of the processing map, their behavior in microstructure evolution was different. While both alloys exhibited a tendency of strain localization in the conditions of instability, the efficiency of power dissipation in the processing maps showed an intricate correlation with the progress of dynamic recrystallization and carbide precipitation. TDx showed a distinctive behavior of carbide precipitation and a larger resistance to dynamic recrystallization, which implied a requirement on more delicate control of hot working conditions.

36 MATERIALS SCIENCE↗

Microstructural characterization of laser micro-welded Nitinol wires

Highlights: • FIB technique was used in the preparation of TEM foils of laser micro-welded joint. • Phase content in various zones of laser micro-welded Nitinol wires was revealed. • Welding induces the R-phase formation in HAZ and intermetallics precipitation in FZ. - Abstract: Laser micro-welding has been considered one of the most promising joining methods of manufacturing Nitinol biomedical devices. However, there is still a lack of understanding about how laser micro-welding influences the microstructure. This work attempts to reveal the phase content within various microstructural zones of laser micro-welded crossed Nitinol wires by transmission electron microscopy (TEM) with the assistance of the focused ion beam (FIB) technique. The base metal is composed of a single austenite phase (B2). The fusion zone exhibits the coexistence of austenite matrix and several intermetallics (T{sub 2}Ni, TiNi{sub 3} and Ti{sub 3}Ni{sub 4}). The precipitation of R-phase was observed in HAZ with B2 matrix due to thermally induced stresses during welding.

36 MATERIALS SCIENCE↗

Effect of microstructure on exfoliation corrosion resistance in an Al-Zn-Mg alloy

Highlights: • A quantitative method was proposed to characterize EXCO resistance. • The EXCO product lead to strain in ND and elongation in RD on nearby grains. • Recrystallized grains are more susceptible to EXCO than fibrous grains. • High fraction of high-angle grain boundaries reduces EXCO resistance. • High coverage ratio of η phases on high-angle grain boundaries reduces EXCO resistance. - Abstract: In this work, the effect of microstructure on exfoliation corrosion (EXCO) resistance in an Al-Zn-Mg alloy were investigated using standard EXCO test, together with detailed microstructural examinations mainly by scanning electron microscopy (SEM) and high-angle annular detector dark-field scanning transmission electron microscopy (HAADF-STEM). An EXCO product model was built based on morphologies of EXCO product on longitudinal section and cross section for further measurement and analysis. A quantitative characterization of EXCO resistance by measuring average thickness of EXCO product was conducted, showing average results of 6.94 μm, 10.21 μm and 18.14 μm, which are corresponding to EXCO ratings of P, EA and EB under ASTM G34 standard, respectively. It was concluded that recrystallization, high fraction of high-angle grain boundaries (HAGBs) and high coverage ratio of η phases on HAGBs reduced EXCO resistance.

36 MATERIALS SCIENCE↗

Effects of friction stir processing and minor Sc addition on the microstructure, mechanical properties, and damping capacity of 7055 Al alloy

Highlights: • Good mechanical and damping properties were obtained in the 7055 after FSP and Sc addition. • The strengthening and damping mechanisms of FSP 7055(-Sc) were analyzed. • FSP and Sc addition were found to be strategy of preparing 7xxx alloys with well damping and mechanical properties. - Abstract: This study investigated the effects of friction stir processing (FSP) and addition of 0.25% (mass ratio) Sc on the microstructure, mechanical properties, and damping capacity of AA 7055 alloy. Microstructure analyses revealed that a low tool rotation rate of 300 rpm effectively inhibited the grain coarsening in the recrystallization of the alloy during FSP. Sc addition prevented the coarsening of grains and precipitated η phase and the annihilation of dislocations in the FSP AA 7055 alloy. After being subjected to FSP at 300 rpm, the AA 7055 alloy containing Sc exhibited good mechanical and damping properties, which were mainly attributed to the fine recrystallized grain structure, fine precipitated η phase, and large number of nano-sized Al{sub 3}(Sc, Zr) particles located at the grain boundaries and dislocations. This work provides an effective strategy for preparing commercial Al alloys with excellent damping capacity and mechanical properties.

36 MATERIALS SCIENCE↗

The effect of Cerium addition on microstructure and mechanical properties of high pressure die cast Mg-5Sn alloy

Highlights: • The alloying additive has good grain refinement effect. • The addition of Ce to the Mg-5Sn alloy led to the formation of the new intermetallic phases CeMgSn and Ce{sub 5}Sn{sub 4}. • The hardness, yield and tensile strength of Mg-5Sn alloy were improved with addition of Ce. • The elongation of Mg-5Sn was increased up to 5wt.%Ce addition, and then decreased with addition of 7 wt.%Ce. • The yield and tensile strength of the Ce added alloy were higher than those of the base alloy at elevated temperatures. - Abstract: The effect of Cerium addition to Mg-5Sn alloy and its influence on the microstructure and mechanical properties of the alloy were investigated in this work. The microstructural investigations indicate that the alloying addition of Ce leads to effective grain refinement. Also, it was observed that adding Ce to the Mg-5Sn alloy results in the formation of new phases in the alloy such as Ce{sub 5}Sn{sub 4} and CeMgSn. These intermetallic phases were considered to be effective on the enhancement of the hardness of Mg-5Sn alloy. Furthermore, the tensile test results at room temperature and elevated temperatures revealed that the yield and tensile strength of the Ce added alloy were higher than those of the base alloy. The elongation was also improved up to 5 wt% Ce addition while higher amounts decreased the elongation both at room and elevated temperatures.

36 MATERIALS SCIENCE↗

Growth of faceted SiC nanostructures using vapor phase condensation: Microstructural analysis

Highlights: • Synthesis of nanocrystalline SiC using thermal plasma route. • XRD data indicates presence of both α- and β-SiC polytypes with β-SiC as the major content. • HRTEM and SAED analysis reveals polytypic arrangement with stacking faults SiC nanoparticles. • TEM micrograph reveals presence of faceted structures such as hexagonal, triangular, triangular pyramidal structure. - Abstract: The paper emphasizes the morphological and microstructural analysis of SiC nanostructures grown by thermal plasma assisted gas phase condensation process. High Resolution Transmission Electron Microscopic and Selected Area Electron Diffraction studies are used to analyze the growth directions and the polytypic arrangement with stacking faults in the as synthesized SiC nanoparticles. The results help in understanding the hierarchical poly-types related to the observed geometries and showed the presence of both α- and β-SiC polytypes. The microstructural study is supported by X-Ray diffraction and UV–Visible absorption spectroscopic studies.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Microstructure, texture and tensile behavior of pulsed electrodeposited Ni–Al composites produced using organic additive-free sulfamate bath loaded with Al nanoparticles

Highlights: • Foils of fine grained Ni with Al nanoparticles reinforcement are produced by pulsed electro-codeposition. • Ni–Al composite foils exhibit increased compressive residual stresses with increasing Al content. • Well-dispersed Al nanoparticles refine Ni matrix microstructure and induces significant texture changes. • Ultrafine grained Ni-Al composites exhibit improved hardness and tensile strength. - Abstract: Nickel and Ni–Al composites with varying Al nanoparticle content were produced by pulsed electrodeposition using an organic additive-free sulfamate bath. The as-deposited Ni–Al composites exhibited increased compressive residual stresses with increasing Al nanoparticles. Detailed microstructural investigation revealed that Al codeposition led to significant refinement of the columnar morphology and grain structure of Ni matrix along with a texture change from strong <001> to <011> fiber texture parallel to the growth direction. The as-deposited Ni with bimodal grain structure displayed good tensile strength and ductility. The microhardness and tensile strength of the Ni deposits were increased initially with Al content and then decreased at higher particle content. Particle induced grain refinement and texture changes could be related to change in the growth of upcoming Ni nuclei on to the surface of well-dispersed Al nanoparticles. Significant grain refinement and lesser internal stresses along with good particle distribution and relatively harder <011> fiber texture at lower particles concentration collectively contributed to the observed higher strengths in Ni–Al composites as compared to Ni deposits. There was substantial change in fracture morphology from spherical dimples to flat regions with increasing Al content due to agglomeration of nanoparticles at higher particle loading.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Relationship between laser energy input, microstructures and magnetic properties of selective laser melted Fe-6.9%wt Si soft magnets

Highlights: • Effect of laser energy input on magnetic properties of SLM Fe-6.9%wt.Si is described; • Magnetic properties can be described as function of as-built microstructure after stress-relief post-treatment; • Samples with density >99% and strong crystallographic texture along BD have the best magnetic properties; • At very high laser energy, a strong cube texture forms that deteriorates the magnetic properties. - Abstract: Selective Laser Melting (SLM), a powder-bed Additive Manufacturing technology, can be used in combination with high temperature post-annealing to produce high-silicon steel parts characterised by quasi-static magnetic properties comparable to those of commercial electrical steel. However, the role of the as-built microstructure on the magnetic properties is still unexplored. Therefore, in this study the effect of the energy input of the processing laser on the magnetic properties of the material is investigated. The magnetic properties are determined for 4 mm-high rings obtained using three laser energy input values that provide a good compromise in terms of porosity and crack formation. The best magnetic properties are obtained for the rings built using a value of energy input that produces a strong fibrous crystallographic texture, in which one of the crystallographic <001> axes is preferentially aligned along the build direction. Whether the magnetic properties change with sample direction as a result of the crystallographic texture will be the subject of future research.

36 MATERIALS SCIENCE↗

Effect of Bi on the microstructure and mechanical properties of Sn-Zn alloys processed by rolling

Highlights: • Sn-Zn-Bi is proposed for the first time as the cladding in linear explosive device. • Bi can significantly refine the microstructure of Sn-Zn. • Bi can enhance both strength and ductility of Sn-Zn processed by rolling. • The 5 wt% Bi in Sn-3Zn leads to finest and most homogenous grains after rolling. - Abstract: Sn-Zn based alloys including Sn-3Zn, Sn-3Zn-1Bi, and Sn-3Zn-5Bi were prepared by casting and rolling, in efforts to assess their feasibility for the application as cladding materials in detonating and explosive cords. It was found that Bi significantly refined the solidification microstructure, changing the configuration of Sn-Zn eutectic from well-aligned Zn-rich precipitates/needles to misaligned Zn-rich flakes. During deformation, second phases like Zn-rich precipitates and Bi particles, and Bi solutes were effective in grain refinement since second phase particles provided more sites for nucleation and more obstacles to growth of new recrystallized grains. Tensile results revealed that Bi addition enhanced both strength and ductility of the rolled Sn-Zn-Bi alloys. The Sn-3Zn-5Bi alloy possessed superior strength and ductility (UTS: 84.4 MPa; Yield strength: 68.3 MPa; Elongation: 75.2%) due to its finest and most homogeneous equiaxed grains. Based on decent mechanical properties, the Sn-Zn-Bi alloys could be well qualified for the application as cladding materials.

36 MATERIALS SCIENCE↗

Effects of Sn microalloying on cold rolling and recrystallization textures and microstructure of a ferritic stainless steel

Highlights: • Sn microalloying contributes to the enhancement in cold rolling texture intensity and the acceleration in cold rolling texture transformation. • Sn microalloying promotes the recrystallization process, and recrystallization occurs preferentially in steel with Sn compared with Sn-free steel. • Sn microalloying inhibits the growth of recrystallized grains, and the finer grains are obtained in steel with Sn. - Abstract: We investigated the effects of Sn microalloying on cold rolling and recrystallization textures and microstructure of a ferritic stainless steel. The as-received hot rolled sheets were cold rolled at 10%–90% reductions; the sheets cold rolled up to an 80% reduction were annealed at 740–880 °C for 5 min. For comparison, the cold rolling and recrystallization textures of the steel sheets with and without Sn were determined with the conventional X-ray diffraction method. The cold rolling and recrystallization metallographic microstructures were measured by scanning electron microscope and optical microscope, and the crystal orientation maps of the cold rolled and annealed samples were observed by electron backscattered diffraction. The micro-hardness was determined using a digital micro-hardness tester. Our results show that Sn microalloying in a medium chromium ferritic stainless steel plays multiple roles in the cold rolling and recrystallization processes. Sn micrcoalloying contributes to the enhancement in cold rolling texture intensity and the acceleration in cold rolling texture transformation. Sn microalloying is beneficial in promoting the recrystallization process. Recrystallization occurs preferentially in the ferritic stainless steel with Sn. Sn microalloying plays an important role in inhibiting the growth of recrystallized grains. The finer grains are obtained in ferritic stainless steel with Sn when annealing at high temperatures.

36 MATERIALS SCIENCE↗

Evaluation of the microstructure and mechanical properties of WC particle reinforced aluminum matrix composites fabricated by friction stir processing

Highlights: • FSP was used for the preparation of aluminum matrix composites reinforced with WC particle. • WC particles were uniformly distributed in the composite. • WC particles refined the grains of aluminum matrix. • WC particles enhanced the hardness and tensile strength, but decreased the ductility. - Abstract: Tungsten carbide (WC) is an attractive reinforcing material for aluminum and its alloys. However, it is technically challenging to fabricate WC particle reinforced aluminum matrix composites (AMCs) with homogeneous distribution of WC particles by liquid state processing techniques because of large density gradient. The present work aim to produce WC particle reinforced aluminum matrix composites (AMCs) through friction stir processing (FSP) and analyze the effect of its volume fraction on the microstructural features and the mechanical behavior of the developed AMCs. Microstructural evaluation was conducted on the cross-sections of the samples by optical microscopy (OM), scanning electron microscopy (SEM) and electron backscattered diffraction (EBSD). Microhardness testing was conducted across the cross-sections of FSPed samples to obtain hardness profiles and tensile test was conducted on as-received Al and FSPed samples. The fabricated AMCs exhibited the homogeneous distribution of WC particle with no obvious particle clustering in the stir zone, irrespective of position and WC particle volume fraction. Excellent WC/Al interfacial bonding was obtained in all FSPed AMCs with obviously refined grains. The average size of WC particles after FSP was slightly reduced with the increased volume fraction. It was also found that increasing the volume fraction of WC particles favored the grain refinement, improved the hardness and strength, but decreased the ductility. This improvement in the hardness and strength was attributed to the grain refinement strengthening and homogeneous distribution of WC particles. The decreased ductility resulted from the introduction of more WC particles. Increasing the volume fraction of WC particles caused the nature of fracture to move towards brittle nature.

36 MATERIALS SCIENCE↗

Microstructure evolution and mechanical properties of the compressively deformed AgInCd alloy during annealing treatment

Highlights: • The microstructure of AgInCd alloy during annealing treatment is investigated. • Nanoscale deformation twins are formed in the deformed AgInCd alloy. • Deformation twins are transformed into stacking faults by detwinning mechanism. • Annealing twins show higher thermal stability than deformation twins. - Abstract: The microstructure evolution and mechanical properties of the compressively deformed AgInCd alloy during annealing treatment have been investigated in the present study. In the deformed AgInCd alloy, many deformation markings are formed and these deformation markings are mainly composed of nanoscale deformation twins. The AgInCd alloy exhibits a significant work hardening capability because of the formation of deformation twins. The recrystallization temperature of the deformed AgInCd alloy is between 300 °C and 350 °C. In the AgInCd alloy annealed at 300 °C, the deformation twins are eliminated and a large number of dark strips consisting of stacking faults are presented in the un-recrystallized regions, indicating that the deformation twins are transformed into stacking faults by the detwinning mechanism. The annealing twins show higher thermal stability than the deformation twins. The strength and microhardness of the deformed AgInCd alloy gradually decrease with the increase of annealing temperature.

36 MATERIALS SCIENCE↗

Interfacial microstructure evolution and weld formation during ultrasonic welding of Al alloy to Cu

Highlights: • Surface oxide layer was fractured and dispersed around the weld interface during ultrasonic welding of Al alloy to Cu. • Mechanical mixing around the weld interface was caused by compressive deformation with ultrasonic vibration. • Once micro-bonds were generated between Al and Cu, shear deformation occurred around the weld interface. • Enhanced Cu diffusion into Al in the severely deformed region significantly contributed to the weld formation. - Abstract: Dissimilar welds of Al alloy 1050 to Cu were prepared via ultrasonic spot welding in order to understand the formation of welds and interfacial microstructures. To observe oxide layer behavior at the weld interface, the anodized Al alloy 1050 was also welded to Cu. Mechanical mixing and material flow during ultrasonic welding broke and dispersed the oxide layers into the Al matrix. This material flow is attributed to compressive deformation that occurred due to ultrasonic vibrations. Direct bonding in the Al/Cu region increased with welding time. Once micro-bonds were generated between Al and Cu, the Al matrix in the vicinity of the weld interface was severely deformed in the direction of the ultrasonic vibrations. Consequently, a recrystallized microstructure with shear texture was formed in the Al matrix. Deformation heating and severe shear deformation formed Al{sub 2}Cu intermetallic compound layers at the weld interface. The growth rate of the Al{sub 2}Cu layer was much faster than had previously been estimated based upon the peak temperature and ultrasonic welding heating time. This is likely due to the increased rate of Cu diffusion into Al in the severely deformed region.

36 MATERIALS SCIENCE↗