Search NASA⌕ Search

SEARCH · Search NASA

Results for “Waste Form”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,531 records · Page 85

Methods and apparatus for catalytic hydrothermal gasification of biomass

Continuous processing of wet biomass feedstock by catalytic hydrothermal gasification must address catalyst fouling and poisoning. One solution can involve heating the wet biomass with a heating unit to a temperature sufficient for organic constituents in the feedstock to decompose, for precipitates of inorganic wastes to form, for preheating the wet feedstock in preparation for subsequent separation of sulfur contaminants, or combinations thereof. Treatment further includes separating the precipitates out of the wet feedstock, removing sulfur contaminants, or both using a solids separation unit and a sulfur separation unit, respectively. Having removed much of the inorganic wastes and the sulfur that can cause poisoning and fouling, the wet biomass feedstock can be exposed to the heterogeneous catalyst for gasification.

09 BIOMASS FUELS↗

Methods for sulfate removal in liquid-phase catalytic hydrothermal gasification of biomass

Processing of wet biomass feedstock by liquid-phase catalytic hydrothermal gasification must address catalyst fouling and poisoning. One solution can involve heating the wet biomass with a heating unit to a pre-treatment temperature sufficient for organic constituents in the feedstock to decompose, for precipitates of inorganic wastes to form, for preheating the wet feedstock in preparation for subsequent removal of soluble sulfate contaminants, or combinations thereof. Processing further includes reacting the soluble sulfate contaminants with cations present in the feedstock material to yield a sulfate-containing precipitate and separating the inorganic precipitates and/or the sulfate-containing precipitates out of the wet feedstock. Having removed much of the inorganic wastes and the sulfate contaminants that can cause poisoning and fouling, the wet biomass feedstock can be exposed to the heterogenous catalyst for gasification.

09 BIOMASS FUELS↗

Methods for sulfate removal in liquid-phase catalytic hydrothermal gasification of biomass

Processing of wet biomass feedstock by liquid-phase catalytic hydrothermal gasification must address catalyst fouling and poisoning. One solution can involve heating the wet biomass with a heating unit to a pre-treatment temperature sufficient for organic constituents in the feedstock to decompose, for precipitates of inorganic wastes to form, for preheating the wet feedstock in preparation for subsequent removal of soluble sulfate contaminants, or combinations thereof. Processing further includes reacting the soluble sulfate contaminants with cations present in the feedstock material to yield a sulfate-containing precipitate and separating the inorganic precipitates and/or the sulfate-containing precipitates out of the wet feedstock. Having removed much of the inorganic wastes and the sulfate contaminants that can cause poisoning and fouling, the wet biomass feedstock can be exposed to the heterogeneous catalyst for gasification.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

EFFECTS OF QUARTZ PARTICLE SIZE AND SUCROSE ADDITION ON MELTING BEHAVIOR OF A MELTER FEED FOR HIGH-LEVEL GLASS

The behavior of melter feed (a mixture of nuclear waste and glass-forming additives) during waste-glass processing has a significant impact on the rate of the vitrification process. We studied the effects of silica particle size and sucrose addition on the volumetric expansion (foaming) of a high-alumina feed and the rate of dissolution of silica particles in feed samples heated at 5 C/min up to 1200 C. The initial size of quartz particles in feed ranged from 5 to 195 {micro}m. The fraction of the sucrose added ranged from 0 to 0.20 g per g glass. Extensive foaming occurred only in feeds with 5-{micro}m quartz particles; particles {ge}150 {micro}m formed clusters. Particles of 5 {micro}m completely dissolved by 900 C whereas particles {ge}150 {micro}m did not fully dissolve even when the temperature reached 1200 C. Sucrose addition had virtually zero impact on both foaming and the dissolution of silica particles. Over 100 sites in the United States are currently tasked with the storage of nuclear waste. The largest is the Hanford Site located in southeastern Washington State with 177 subterranean tanks containing over fifty-million gallons of nuclear waste from plutonium production from 1944 through 1987. This waste will be vitrified at the Hanford Tank Waste Treatment and Immobilization Plant. In the vitrification process, feed is charged into a melter and converted into glass to be ultimately stored in a permanent repository. The duration of waste-site cleanups by the vitrification process depends on the rate of melting, i.e., on the rate of the feed-to-glass conversion. Foaming associated with the melting process and the rate of dissolution of quartz particles (silica being the major glass-forming additive) are assumed to be important factors that influence the rate of melting. Previous studies on foaming of high-alumina feed demonstrated that varying the makeup of a melter feed has a significant impact on foaming. The volume of feeds that contained 5-{micro}m quartz particles substantially increased because of foaming. The extent of foaming decreased as the particle size of quartz increased. Moreover, samples containing quartz particles 195 {micro}m formed agglomerates at temperatures above 900 C that only slowly dissolved in the melt. This study continues previous work on the feed-melting process, specifically on the effects of the size of silica particles on the formation of nuclear-waste glasses to determine a suitable range of silica particle sizes that causes neither excessive foaming nor undesirable agglomeration. Apart from varying the silica-particle size, carbon was added in the form of sucrose. Sucrose has been used to accelerate the rate of melting. In this study, we have observed its impact on feed foaming and quartz dissolution.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Decreased PCDD/F formation when co-firing a waste fuel and biomass in a CFB boiler by addition of sulphates or municipal sewage sludge

Highlights: • Two strategies to reduce PCDD/F formation when co-firing solid recovered fuel (SRF) and biomass. • They were co-combustion with municipal sewage sludge (MSS) and addition of ammonium sulphate. • PCDD/Fs were significantly reduced for a biomass rich in chlorine when adding ammonium sulphate. • MSS had a suppressing effect on PCDD/F formation during co-combustion with SRF. • A link is presented between gaseous alkali chlorides, chlorine in deposits and PCDD/F formation. - Abstract: Polychlorinated dibenzo-p-dioxins (PCDDs) and polychlorinated dibenzofurans (PCDFs) are formed during waste incineration and in waste-to-energy boilers. Incomplete combustion, too short residence times at low combustion temperatures (<700 °C), incineration of electronic waste and plastic waste containing chlorine are all factors influencing the formation of PCDD/Fs in boilers. The impact of chlorine and catalysing metals (such as copper and iron) in the fuel on PCDD/F formation was studied in a 12 MW{sub th} circulating fluidised bed (CFB) boiler. The PCDD/F concentrations in the raw gas after the convection pass of the boiler and in the fly ashes were compared. The fuel types were a so-called clean biomass with low content of chlorine, biomass with enhanced content of chlorine from supply of PVC, and solid recovered fuel (SRF) which is a waste fuel containing higher concentrations of both chlorine, and catalysing metals. The PCDD/F formation increased for the biomass with enhanced chlorine content and it was significantly reduced in the raw gas as well as in the fly ashes by injection of ammonium sulphate. A link, the alkali chloride track, is demonstrated between the level of alkali chlorides in the gas phase, the chlorine content in the deposits in the convection pass and finally the PCDD/F formation. The formation of PCDD/Fs was also significantly reduced during co-combustion of SRF with municipal sewage sludge (MSS) compared to when SRF was fired without MSS as additional fuel.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Treatment of Problematic Reactive Metal Wastes Using the GeoMelt{sup R} In-Container Vitrification (ICV{sup TM}) Process - 20326

Decommissioning of sodium-cooled reactors and fast reactor technologies has generated a number of reactive metal waste configurations that are problematic to treat and typically lack cost effective treatment methods and disposition options. As a result, Veolia Nuclear Solutions, under contract with Idaho National Laboratory (owned by the U.S. Department of Energy and managed and operated by Battelle Energy Alliance, LLC) demonstrated its GeoMelt{sup R} In-Container Vitrification (ICV){sup TM} technology to safely convert sodium metal to a non-reactive vitrified oxide form. The demonstration project, supported by glass formulation and crucible testing, consisted of a series of ICV{sup TM} melts that processed elemental sodium into stable non-reactive glass. INL is currently implementing GeoMelt{sup R} technology as a means to safely and reliably convert radioactive reactive metal residues that contaminate sodium cooled reactor components into waste forms that comply with existing disposition pathways. Reactive metal wastes require treatment in order to remove the Resource Conservation and Recovery Act (RCRA) reactivity and ignitability characteristics to comply with land disposal restrictions. GeoMelt{sup R}, which is an alternative to other potential treatment approaches, provides a robust approach that chemically converts the reactive metals to an inert oxide while also immobilizing radionuclides in a vitrified waste form with durability equal to or better than vitrified nuclear fuel reprocessing wastes (very robust and inert waste forms). Most other treatment approaches generate hydrogen gas which is problematic. In 2016, Veolia Nuclear Solutions first demonstrated the effectiveness of the GeoMelt{sup R} ICV{sup TM} process in deactivating reactive sodium metal. Crucible, bench-scale, and engineering-scale demonstrations were conducted on several surrogate waste configurations with various ratios of sodium metal and glass formers. Each ratio and configuration demonstrated complete deactivation of the surrogate sodium metal. Follow-on work in 2017 demonstrated the deactivation of reactive sodium by GeoMelt{sup R} ICV{sup TM} at a higher waste loading relative to previously demonstrated work performed in 2016; the higher waste loading optimized glass chemistry while enhancing the economical full-scale treatment of reactive metals. Additionally, follow-on demonstration testing in 2018 and 2019 focused on more complex shapes and other reactive-metals (mocked up Experimental Breeder Reactor II [EBR-II] subassembly, sodium filled heat exchanger, and a can containing sodium potassium alloy) which were all performed at engineering scale. Veolia Nuclear Solutions designed, installed, and commissioned in September 2018, at Perma-Fix Northwest in Richland Washington, a 10-metric ton full-scale GeoMelt unit (GeoMelt{sup R} Richland) for the treatment of reactive metal wastes. As of September 2019, over 900 55-gallon drums containing a total of around 3,500 lb of sodium with low levels of radioactivity have been treated at GeoMelt{sup R} Richland, with resulting glass monoliths disposed at the Nevada National Security Site (NNSS). A full-scale radiological demonstration melt on an actual EBR-II subassembly has also been performed using the full-scale melter in 2019. The GeoMelt{sup R} technology is a proven radioactive waste treatment technology capable of immobilizing radioactive wastes, including bulk rubble such as drums and other steel vessels usually without pretreatment. Utilizing the GeoMelt{sup R} technology to treat reactive metals eliminates pretreatment steps resulting from having to separate the reactive metal from steel containers or jackets as GeoMelt{sup R} can easily operate at temperatures sufficient to melt the steel and expose the reactive metal for treatment. Eliminating handling steps of reactive metals is a significant safety advantage since reactive metals are pyrophoric. The results generated as a part of the 2018-2019 demonstration program are presented in the paper. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Treatment of Problematic Reactive Metal Wastes Using the GeoMelt{sup R} In-Container Vitrification (ICV{sup TM}) Process - 18639

Decommissioning of sodium cooled reactors and fast reactor technologies have generated a number of reactive metal waste configurations that are problematic to treat and typically lack cost effective treatment methods and disposition options. As a result, Veolia Nuclear Solutions, under contract with Idaho National Laboratory (owned by the U.S. Department of Energy and managed and operated by Battelle Energy Alliance, LLC) demonstrated its GeoMelt{sup R} In-Container Vitrification (ICV){sup TM} technology to safely convert sodium metal to a non-reactive vitrified oxide form. The demonstration project, supported by glass formulation and crucible testing, consisted of a series of ICV{sup TM} melts that processed elemental sodium into stable non-reactive glass. Battelle Energy Alliance, LLC is evaluating the GeoMelt{sup R} technology as a means to safely and reliably convert radioactive reactive metal residues that contaminate components from sodium cooled reactors into waste forms that comply with existing disposition pathways. Reactive metal wastes at INL require treatment in order to remove the Resource Conservation and Recovery Act (RCRA) reactivity and ignitability characteristics in order to comply with land disposal restrictions. GeoMelt{sup R}, which is an alternative to other potential treatment approaches, provides a robust approach that chemically converts the reactive metals to an inert oxide while also immobilizing radionuclides in a vitrified waste form with durability equal to or better than vitrified nuclear fuel reprocessing wastes (very robust and inert waste forms). Most other treatment approaches generate hydrogen gas which is problematic. In 2016, Veolia Nuclear Solutions demonstrated the effectiveness of the GeoMelt{sup R} ICV{sup TM} process in deactivating reactive sodium metal. Crucible, bench-scale, and engineering-scale demonstrations were conducted on several surrogate waste configurations with various ratios of sodium metal and glassformers. Each ratio and configuration demonstrated complete deactivation of the surrogate sodium metal. Follow-on work in 2017 demonstrated the deactivation of reactive sodium by GeoMelt{sup R} ICV{sup TM} at a higher waste loading relative to previously demonstrated work performed in 2016. The higher waste loading optimized glass chemistry while enhancing the economical full-scale treatment of reactive metals. The GeoMelt{sup R} technology is a proven radioactive waste treatment technology capable of immobilizing radioactive wastes, including bulk rubble such as drums and other steel vessels usually without pretreatment. Utilizing the GeoMelt{sup R} technology to treat reactive metals eliminates pretreatment steps resulting from having to separate the reactive metal from steel containers or jackets as GeoMelt{sup R} can easily operate at temperatures sufficient to melt the steel and expose the reactive metal for treatment. Eliminating handling steps of reactive metals is a significant safety advantage since reactive metals are pyrophoric. The results of this two-year demonstration program and future planned activities are presented in the paper. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

ARRHENIUS MODEL FOR HIGH-TEMPERATURE GLASS VISCOSITY WITH A CONSTANT PRE-EXPONENTIAL FACTOR

A simplified form of the Arrhenius equation, ln η = A + B(x)/T, where η is the viscosity, T the temperature, x the composition vector, and A and B the Arrhenius coefficients, was fitted to glass-viscosity data for the processing temperature range (the range at which the viscosity is within 1 to 103 Pa.s) while setting A = constant and treating B(x) as a linear function of mass fractions of major components. Fitting the Arrhenius equation to over 550 viscosity data of commercial glasses and approximately 1000 viscosity data of glasses for nuclear-waste glasses resulted in the A values of -11.35 and -11.48, respectively. The R2 value ranged from 0.92 to 0.99 for commercial glasses and was 0.98 for waste glasses. The Arrhenius models estimate viscosities for melts of commercial glasses containing 42 to 84 mass% SiO2 within the temperature range of 1100 to 1550°C and viscosity range of 5 to 400 Pa.s and for waste glasses containing 32 to 60 mass% SiO2 within the temperature range of 850 to 1450°C and viscosity range of 0.4 to 250 Pa.s.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The effect of temperature on the speciation of U(VI) in sulfate solutions

Sulfate, one of the inorganic constituents that could be present in the nuclear waste repository, forms complexes with U(VI) and affects its migration in the environment. Results show that the complexation of U(VI) with sulfate is enhanced by the increase in temperature. The effect of temperature on the complexation and speciation of U(VI) in sulfate solutions is discussed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

GLYCOLIC ACID PHYSICAL PROPERTIES, IMPURITIES, AND RADIATION EFFECTS ASSESSMENT

The DWPF is pursuing alternative reductants/flowsheets to increase attainment to meet closure commitment dates. In fiscal year 2009, SRNL evaluated several options and recommended the further assessment of the nitric/formic/glycolic acid flowsheet. SRNL is currently performing testing with this flowsheet to support the DWPF down-select of alternate reductants. As part of the evaluation, SRNL was requested to determine the physical properties of formic and glycolic acid blends. Blends of formic acid in glycolic acid were prepared and their physical properties tested. Increasing amounts of glycolic acid led to increases in blend density, viscosity and surface tension as compared to the 90 wt% formic acid that is currently used at DWPF. These increases are small, however, and are not expected to present any difficulties in terms of processing. The effect of sulfur impurities in technical grade glycolic acid was studied for its impact on DWPF glass quality. While the glycolic acid specification allows for more sulfate than the current formic acid specification, the ultimate impact is expected to be on the order of 0.03 wt% sulfur in glass. Note that lower sulfur content glycolic acid could likely be procured at some increased cost if deemed necessary. A paper study on the effects of radiation on glycolic acid was performed. The analysis indicates that substitution of glycolic acid for formic acid would not increase the radiolytic production rate of H{sub 2} and cause an adverse effect in the SRAT or SME process. It has been cited that glycolic acid solutions that are depleted of O{sub 2} when subjected to large radiation doses produced considerable quantities of a non-diffusive polymeric material. Considering a constant air purge is maintained in the SRAT and the solution is continuously mixed, oxygen depletion seems unlikely, however, if this polymer is formed in the SRAT solution, the rheology of the solution may be affected and pumping of the solution may be hindered. A series of tests to determine whether the polymer will be formed is currently being outlined. The first phase will be a simple experiment where a simulated SRAT supernatant containing the 80:20 blend of glycolic - formic acid could be irradiated in the Co-60 gamma source at SRNL to a very large dose resembling the dose received by the radioactive SRAT solution after several weeks. The resulting solution could then be heated to simulate refluxing in the SRAT process. Finally a radioactive demonstration of the SRAT process should be performed in the SRNL Shielded Cells to confirm successful execution of the glycolic - formic acid flowsheet.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Sol-gel Synthesis and Characterization of Gels with Compositions Relevant to Hydrated Glass Alteration Layers

During the processes associated with glass corrosion, porous alteration gel layers typically form upon exposure to aqueous conditions for extended time periods. The impacts of the alteration gel layer on glass durability have not been agreed upon in the glass science community. In particular, the formation mechanisms of the alteration gel layers are still largely unknown and require further investigation. However, alteration gel layers often require months to years to develop and are often too thin to adequately characterize. Meanwhile, silicate sol-gels are relatively easy to synthesize in bulk with custom compositions relevant to alteration gel layers. If glass alteration gel layers and synthetic sol-gel silicate gels demonstrate physical and chemical properties that are sufficiently similar, synthetic silicate gels could be used as analogues for glass alteration gel layers in future studies. In this study, sol-gels were made with custom compositions at various pH values to evaluate the effect of pH on gel structure and morphology. Several other variables were examined as well, such as composition, drying, and aging. Sol-gels were created by sequential additions of organometallic precursors in a single container. Synthesis procedural steps are provided in further detail within the text. Sol-gels were analyzed with several techniques including Small Angle X-ray Scattering (SAXS), gas adsorption, and He pynchometry to determine the effects of the variables on physical properties. Results show that sol-gels prepared at pH 3 consistently contained fewer primary particles with diameters larger than 72 Å and fewer pores with diameters larger than 300 Å compared to sol-gels synthesized at pH 7 and 9. Composition was shown to have no discernable effect on primary particle and pore sizes at any pH.

Reiser, Joelle TG↗

Effects of Quartz Particle Size and Sucrose Addition on Melting Behavior of a Melter Feed for High-Level Waste Glass

The behavior of melter feed (a mixture of nuclear waste and glass-forming additives) during waste-glass processing has a significant impact on the rate of the vitrification process. We studied the effects of silica particle size and sucrose addition on the volumetric expansion (foaming) of a high-alumina feed and the rate of dissolution of silica particles in feed samples heated at 5°C/min up to 1200°C. The initial size of quartz particles in feed ranged from 5 to 195 µm. The fraction of the sucrose added ranged from 0 to 0.20 g per g glass. Extensive foaming occurred only in feeds with 5-μm quartz particles; particles >150 µm formed clusters. Particles of 5 µm completely dissolved by 900°C whereas particles >150 µm did not fully dissolve even when the temperature reached 1200°C. Sucrose addition had virtually zero impact on both foaming and the dissolution of silica particles.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Review: Waste-Pretreatment Technologies for Remediation of Legacy Defense Nuclear Wastes

The U.S. Department of Energy (DOE) is responsible for retrieving, immobilizing, and disposing of radioactive waste that has been generated during the production of nuclear weapons in the United States. The vast bulk of this waste material is stored in underground tanks at the Savannah River Site in South Carolina and the Hanford Site in Washington State. The general strategy for treating the radioactive tank waste consists of first separating the waste into high-level and low-activity fractions. This initial partitioning of the waste is referred to as pretreatment. Following pretreatment, the high-level fraction will be immobilized in a glass form suitable for disposal in a geologic repository. The low-activity waste will be immobilized in a waste form suitable for disposal at the respective site. This paper provides a review of recent developments in the application of pretreatment technologies to the processing of the Hanford and Savannah River radioactive tank wastes. Included in the review are discussions of 1) solid/liquid separations methods, 2) cesium separation technologies, and 3) other separations critical to the success of the DOE tank waste remediation effort. Also included is a brief discussion of the different requirements and circumstances at the two DOE sites that have in some cases led to different choices in pretreatment technologies.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

SALTSTONE MATRIX CHARACTERIZATION AND STADIUM SIMULATION RESULTS

SIMCO Technologies, Inc. was contracted to evaluate the durability of the saltstone matrix material and to measure saltstone transport properties. This information will be used to: (1) Parameterize the STADIUM{reg_sign} service life code, (2) Predict the leach rate (degradation rate) for the saltstone matrix over 10,000 years using the STADIUM{reg_sign} concrete service life code, and (3) Validate the modeled results by conducting leaching (water immersion) tests. Saltstone durability for this evaluation is limited to changes in the matrix itself and does not include changes in the chemical speciation of the contaminants in the saltstone. This report summarized results obtained to date which include: characterization data for saltstone cured up to 365 days and characterization of saltstone cured for 137 days and immersed in water for 31 days. Chemicals for preparing simulated non-radioactive salt solution were obtained from chemical suppliers. The saltstone slurry was mixed according to directions provided by SRNL. However SIMCO Technologies Inc. personnel made a mistake in the premix proportions. The formulation SIMCO personnel used to prepare saltstone premix was not the reference mix proportions: 45 wt% slag, 45 wt% fly ash, and 10 wt% cement. SIMCO Technologies Inc. personnel used the following proportions: 21 wt% slag, 65 wt% fly ash, and 14 wt% cement. The mistake was acknowledged and new mixes have been prepared and are curing. The results presented in this report are assumed to be conservative since the excessive fly ash was used in the SIMCO saltstone. The SIMCO mixes are low in slag which is very reactive in the caustic salt solution. The impact is that the results presented in this report are expected to be conservative since the samples prepared were deficient in slag and contained excess fly ash. The hydraulic reactivity of slag is about four times that of fly ash so the amount of hydrated binder formed per unit volume in the SIMCO saltstone samples is less than that expected for saltstone containing the reference amount of slag (45 wt.% of the total cementitious mixture versus 21 wt.% used in the SIMCO samples). Consequently the SIMCO saltstone samples are expected to have lower strengths, and tortuosity and higher porosity, water diffusivity, and intrinsic permeability compared to the reference case MCU saltstone. MCU reference saltstone contains nonradioactive salt solution with a composition designed to simulate the product of the Modular Caustic Side Solvent Extraction (MCU) Unit [Harbour, 2009]. The SIMCO saltstone samples were cast in molds and cured for three days under plastic with a source of water to prevent drying. Details of the sample preparation process are presented in Attachment 2. The molds were then removed and the samples were cured at a constant temperature (76 F, 24 C) and 100 percent relative humidity for up to one year. Selected samples were periodically removed and characterized the evolution of the matrix as a function of age. In order to preserve the age dependent microstructure at the specified curing times it is necessary to stop hydration. This was accomplished by immersing the samples in isopropanol for 5 days to replace water with alcohol. The microstructure of the matrix material was also characterized as a function of aging. This information was used as a base line for comparison with leached microstructures. After curing for 137 days, specimens were cut into 20 mm disks and exposed to deionized water with a pH maintained at 10.5. Microstructure and calcium sulfur leaching results for samples leached for 31 days are presented in this report. Insufficient leached material was generated during the testing to date to obtain physical and mineralogical properties for leached saltstone. Longer term experiments are required because the matrix alteration rate due to immersion in deionized water is slow.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Preliminary IHLW Formulation Algorithm Description

This report documents the initial algorithm that could be used by the Waste Treatment and Immobilization Plant (WTP) in batching high-level waste (HLW) and glass-forming chemicals (GFCs) in the HLW melter feed preparation vessel (MFPV) (HFP-VSL-00001 and -00005). Not all Hanford tank waste can be accommodated by the models developed for this report and significant expansion of the model boundaries could be achievable to reduce the WTP mission life and total canister production count. The immobilized HLW (IHLW) must meet a series of constraints to be acceptable for disposal in the Monitored Geologic Repository, which are contained in the Specification 1 of the Contract (DOE 2000), the Waste Acceptance Product Specifications (WAPS, DOE 1996), and the Waste Acceptance System Requirements Document (WASRD, DOE 2007). The IHLW Waste Form Compliance Plan (WCP, 24590-HLW-PL-RT-07-0001, Rev 3) specifies that the formulation algorithm will be developed and used to comply with the constraints associated with glass composition and properties. This report is not an engineering calculation, does not provide design input, and is not an engineering study. Algorithm inputs include the chemical analyses of the blended HLW in the HLW blend vessel (HBV) (HLP-VSL-00028, the volume and composition of the MFPV heel, the volume and composition of the MFPV after waste addition, the volume and composition of MFPV batch after GFC addition, the compositions of individual GFCs, and the mass of glass in each canister. In addition to these inputs, uncertainties in the HLW composition and processing parameters are included in the algorithm. Using the above inputs, the algorithm calculates the following outputs: 1) the volume of HLW to be transferred from the HBV to the MFPV, 2) the mass of each GFC for addition to the MFPV, 3) the composition of the glass that will be produced along with uncertainties, and 4) the predicted properties, with associated uncertainties, of the resulting IHLW. The algorithm uses the property-composition models to calculate properties with associated uncertainties and compares them with various constraints to ensure that a processable feed is formulated and a compliant IHLW is produced. The GFC additions are determined using an optimization approach to provide high confidence that the HLW glass will meet all product quality requirements and key processing constraints. For most HLW batches there are many possible glass compositions that meet all constraints. In these cases, the glass composition is optimized for a series of target component concentrations and target property values. The algorithm also incorporates process measurement and product quality uncertainties, based on the work of Piepel et al. (2005). Estimates of the various process and measurement uncertainties that affect glass compositions and predicted glass properties have been previously reported (Piepel et al. 2005, 2006) and the impacts of these estimated uncertainties on the IHLW composition envelope that meets product quality and processing-related properties with sufficient confidence were evaluated. The details of work performed to date to develop this initial GFC addition and batching algorithm are summarized in Sections 4 and 5. An example data set is used to illustrate the calculations of the algorithm summarized in Section 6. Finally, in Section 7, there is a statement of the required work to achieve a final operational IHLW formulation control algorithm. This report is not an engineering calculation, does not provide design input, and is not an engineering study.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Molten Flux Synthesis of Plutonium (IV) Silicates K 2 PuSi 2 O 7 and Rb 2 PuSi 6 O 15

Few plutonium containing silicates have been reported in the literature and only one other tetravalent plutonium silicate structure has been reported using the flux growth method. With the goal of understanding actinide incorporation into silicates, we describe herein two new plutonium (IV) silicates, Rb 2 PuSi 6 O 15 and K 2 PuSi 2 O 7 , synthesized using a mixed alkali chloride/alkali fluoride flux growth. Both structures crystallize in the C2/c space group with lattice parameters a=24.2980(10) Å, b=7.1466(3) Å, c=17.2025(8) Å and $\blacksquare$96.6560(10)° for Rb 2 PuSi 6 O 15 , and a=9.9478(2) Å, b=5.59820 (10) Å, c=13.1848(2) Å, and $\blacksquare$105.7400(10)° for K 2 PuSi 2 O 7 . Comparisons to the synthesis of other reported alkali actinide silicates (Ce, U, and Th) are made. Raman spectra and DFT calculations of formation enthalpies and vibrational modes provide confirmation of structure refinements and enhanced product characterization for comparison with other materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗