Search NASA⌕ Search

SEARCH · Search NASA

Results for “WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,549 records · Page 86

Method to seal reactive materials under vacuum

A method of sealing a low enriched uranium (LEU) foil in a vacuum is provided. The LEU foil is inserted into a stainless steel foil pouch. Sealing components are assembled with the stainless steel foil pouch with a vacuum pump connection extending through an opening in the pouch. Then an open end of the pouch is folded over and welded to form a vacuum tight bond. A vacuum pump is attached to the connection outside the pouch and the stainless steel foil pouch is evacuated. Then the stainless steel foil pouch is folded and welded to seal the LEU foil within a welded pouch portion. The remaining pouch portion including the vacuum sealing components is cut and separated from the welded pouch portion containing the LEU foil. The method uses on inexpensive readily available equipment, eliminating the need for electron beam welding equipment.

07 ISOTOPE AND RADIATION SOURCES↗

Three Sheet Al alloy assembly for automotive application

An update on joint characterization of three sheet friction stir lap welds (FSLW) in three aluminum alloys (7xxx, 5xxx, and 6xxx) for automotive assembly application is presented. Welding speed of 0.3-2.9m/min was used with pin length >5mm with the aim to reduce upturn hooking on the retreating side and avoid wormhole defect on the advancing side. Joints were also made in to enable T peel and U peel testing. Stitch welds were used to understand effects of weld length and ramp length on T peel performance. Hat sections were joined for 3-point bending and axial crush testing and tested with promising results. Several key issues that require further investigations are identified including flash management near the trim edge, weld quality with limited clamping, tool failures at speeds greater than 0.5m/min, and propensity of incipient melting for 7xxx stack-up.

Upadhyay, Piyush↗

RESIDUAL STRESSES IN 3013 CONTAINERS

The DOE Complex is packaging plutonium-bearing materials for storage and eventual disposition or disposal. The materials are handled according to the DOE-STD-3013 which outlines general requirements for stabilization, packaging and long-term storage. The storage vessels for the plutonium-bearing materials are termed 3013 containers. Stress corrosion cracking has been identified as a potential container degradation mode and this work determined that the residual stresses in the containers are sufficient to support such cracking. Sections of the 3013 outer, inner, and convenience containers, in both the as-fabricated condition and the closure welded condition, were evaluated per ASTM standard G-36. The standard requires exposure to a boiling magnesium chloride solution, which is an aggressive testing solution. Tests in a less aggressive 40% calcium chloride solution were also conducted. These tests were used to reveal the relative stress corrosion cracking susceptibility of the as fabricated 3013 containers. Significant cracking was observed in all containers in areas near welds and transitions in the container diameter. Stress corrosion cracks developed in both the lid and the body of gas tungsten arc welded and laser closure welded containers. The development of stress corrosion cracks in the as-fabricated and in the closure welded container samples demonstrates that the residual stresses in the 3013 containers are sufficient to support stress corrosion cracking if the environmental conditions inside the containers do not preclude the cracking process.

42 ENGINEERING↗

Effect of Exchanging Advancing and Retreating Side Materials on Mechanical Properties and Electrochemical Corrosion Resistance of Dissimilar 6013-T4 and 7003 Aluminum Alloys FSW Joints

Friction stir welding (FSW) was used to weld dissimilar joints between Al 6013-T4 and Al7003 alloys in this work. The effect of exchanging advancing (AS) and retreating (RS) side material on microstructure, mechanical behaviors and electrochemical corrosion resistance was discussed. Results showed that different joint cross sections were obtained when exchanging AS and RS materials. The material on the AS would be more deformed during the welding process. When the Al6013 placed on the AS, the plastic flow of weld is more sufficient. Whether on the AS or RS, the Al6013-T4 side is the weak region for both tensile specimens and hardness samples. The fracture position corresponds to the minimum hardness position. Also, more strengthening phase can be retained in the joint, and the joint of A6R7 has better corrosion resistance.

36 MATERIALS SCIENCE↗

Microstructure development and texture evolution of aluminum multi-port extrusion tube during the porthole die extrusion

Aluminum multi-port extrusion tube is processed by the porthole die extrusion and the internal tube walls are welded through the solid state metallurgical bonding. In order to observe the development of grains and their orientations under severe plastic deformation and solid state welding, the extrusion butt together with the die is quenched immediately after extrusion to preserve the grain structure in the processing. The forming histories of selected material points are obtained by analyzing the optical microscopy graph. The evolution of the microstructure along the forming path is characterized by electro backscattered diffraction. It is found that geometrical dynamic recrystallization happens in the process. Grains are elongated, scattered at the transition zone and shear intensive zone, and then pinched off when they are pushed out from the die orifice. The shear-type orientations are predominant at the surface layer on the longitudinal section of the tube web and have penetrated into the intermediate layer. The rolling-type orientations are formed at the central layer. Texture gradient through the thickness of the tube web is observed. And cube orientated grains are found at the seam weld region. - Highlights: •Microstructure of extrusion butt is preserved after the micro scale porthole die extrusion. •Grain morphology history along forming path is investigated. •Texture evolutions on three material flows are present. •Texture gradient exists on the longitudinal section of the internal wall of profile. •Rolling-type and cube textures are found at the solid state welding region.

36 MATERIALS SCIENCE↗

The correlation between acoustic and magnetic properties in the long working metal boiler drum with the parameters of the electron microscope

The present paper presents comparative analysis of measurement results of acoustic and magnetic properties in long working metal of boiler drums and the results obtained by methods of electronic microscopy. The structure of the metal sample from the fracture zone to the base metal (metal working sample long) and the center of the base metal before welding (weld metal sample) was investigated by electron microscopy. Studies performed by spectral acoustic, magnetic noise and electron microscopic methods were conducted on the same plots and the same samples of long working and weld metal of high-pressure boiler drums. The analysis of research results showed high sensitivity of spectral-acoustic and magnetic-noise methods to definition changes of microstructure parameters. Practical application of spectral-acoustic and magnetic noise NDT method is possible for the detection of irregularities and changes in structural and phase state of the long working and weld metal of boiler drums, made of a special molybdenum steel (such as 20M). The above technique can be used to evaluate the structure and physical-mechanical properties of the long working metal of boiler drums in the energy sector.

36 MATERIALS SCIENCE↗

Physical and mechanical metallurgy of high purity Nb for accelerator cavities

In the past decade, high Q values have been achieved in high purity Nb superconducting radio frequency (SRF) cavities. Fundamental understanding of the physical metallurgy of Nb that enables these achievements is beginning to reveal what challenges remain to establish reproducible and cost-effective production of high performance SRF cavities. Recent studies of dislocation substructure development and effects of recrystallization arising from welding and heat treatments and their correlations with cavity performance are considered. With better fundamental understanding of the effects of dislocation substructure evolution and recrystallization on electron and phonon conduction, as well as the interior and surface states, it will be possible to design optimal processing paths for cost-effective performance using approaches such as hydroforming, which minimizes or eliminates welds in a cavity.

43 PARTICLE ACCELERATORS↗

Optimizing diffusion bonding parameters to maximize the strength of AA6061 aluminum and AZ61A magnesium alloy joints

The main difficulty when joining magnesium (Mg) and aluminum (Al) alloys by fusion welding process lies in the existence of oxide films and formation of brittle intermetallic in the weld region. However, solid-state welding processes such as friction welding and diffusion bonding are suitable processes to join these two materials. The diffusion bonding process parameters such as bonding temperature, bonding pressure, holding time, and surface roughness of the bond specimen play a major role to determine the joint strength. In this investigation, an attempt was made to develop empirical relationships to predict the lap shear strength and bonding strength of diffusion bonded dissimilar joints of AZ61A magnesium and AA6061 aluminum alloys, incorporating the above-mentioned parameters. Response surface methodology (RSM) was applied to optimize the diffusion bonding process parameters to attain the maximum shear strength and bonding strength of the joint. From this investigation, it is found that the bonds fabricated with the bonding temperature of 420.43°C, bonding pressure of 7.70 MPa, holding time of 27.15 min, and surface roughness of 0.10 μm exhibited maximum shear strength and bonding strength of 51.24 and 72.10 MPa, respectively.

36 MATERIALS SCIENCE↗

Continuation of Studies on Development of ODS Heat Exchanger Tubing

The Department of Energy (DOE), National Energy Technology Center (NETL), has initiated a strategic plan for the development of advanced technologies needed to design and build fossil fuel plants with very high efficiency and environmental performance. These plants, referred to as 'Vision 21' and FutureGen programs by DOE, will produce electricity, chemicals, fuels, or a combination of these products, and possibly secondary products such as steam/heat for industrial use. MA956 is a prime candidate material being considered for a high temperature heat exchanger in the 'Vision 21' and FutureGen programs. This material is an oxide dispersion strengthened (ODS) alloy; however, there are some gaps in the data required to commit to the use of these alloys in a full-size plant. To fill the technology gaps for commercial production and use of the material for 'Advanced Power Generation Systems' this project has performed development activity to significant increase in circumferential strength of MA956 as compared to currently available material, investigated bonding technologies for bonding tube-to-tube joints through joining development, and performed tensile, creep and fire-side corrosion tests to validate the use and fabrication processes of MA956 to heat exchanger tubing applications. Development activities within this projected has demonstrated increased circumferential strength of MA956 tubes through flow form processing. Of the six fabrication technologies for bonding tube-to-tube joints, inertia friction welding (IFW) and flash butt welding (FBW) were identified as processes for joining MA956 tubes. Tensile, creep, and fire-side corrosion test data were generated for both base metal and weld joints. The data can be used for design of future systems employing MA956. Based upon the positive development activities, two test probes were designed and fabricated for field exposure testing at 1204 C ({approx}2200 F) flue gas. The probes contained tube portions with FBW and IFW welded MA956. Field testing of the probes and remaining heat exchanger design activity will be performed by Oak Ridge National Laboratory under DOE Contract DE-AC05-00OR22725.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Robotic Solutions for Remote Access and Retrieval of High-Level Radioactive Waste - 19544

This paper describes the ongoing development of robotic solutions for accessing and retrieving high-level radioactive waste from underground storage bins as part of the Calcine Retrieval Project at the INL Site. The waste is in the form of a solid powder, referred to as calcine, stored in a set of stainless steel bins within an underground concrete vault. Due to the radiation field produced by the calcine, all operations must be performed remotely. The Calcine Retrieval Project is currently carrying out proof-of-concept testing of methods for the various stages of calcine retrieval. The bins were designed with no means for access, so retrieval operations will require welding access riser pipes to the bins, followed by cutting through the bin walls from within the risers. These tasks are complicated by the fact that four of the risers must be placed off center on a domed surface, resulting in a weld joint that is curved and tilted relative to the riser axis. The Access Riser Connection robot is being developed to perform these operations using interchangeable welding and plasma cutting attachments. The majority of the calcine will be removed using a vacuum system and pneumatically transferred to storage. This system is not described in this paper. However, the bins contain several internal features that are expected to retain calcine, most notably circumferential stiffening rings on the walls and radial ribs on the floors. One of the solutions being developed for the task of retrieving this residual calcine is a vacuum crawler, a wheeled robot using vacuum to adhere to the interior walls of the bins. The vacuum crawler would use a separate vacuum system to remove residual calcine or would use compressed air to move calcine to a location from which it can be retrieved more easily. While comparable welding and wall-climbing robots have been developed before, this particular application has several constraints that are not satisfied by existing systems. For this reason, both the access riser welder and the vacuum crawler, although still under development, may be of interest to other projects faced with similar constraints. (author)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Experimental Investigation of Material Flows Within FSWs Using 3D Tomography

There exists significant prior work using tracers or pre-placed hardened markers within friction stir welding (FSWing) to experimentally explore material flow within the FSW process. Our experiments replaced markers with a thin sheet of copper foil placed between the 6061 aluminum lap and butt joints that were then welded. The absorption characteristics of x-rays for copper and aluminum are significantly different allowing for non-destructive evaluation (NDE) methods such as x-ray computed tomography (CT) to be used to demonstrate the material movement within the weldment on a much larger scale than previously shown. 3D CT reconstruction of the copper components of the weldment allows for a unique view into the final turbulent state of the welding process as process parameters are varied. The x-ray CT data of a section of the weld region was collected using a cone-beam x-ray imaging system developed at the INL. Six-hundred projections were collected over 360-degrees using a 160-kVp Bremsstrahlung x-ray generator (25-micrometer focal spot) and amorphoussilicon x-ray detector. The region of the object that was imaged was about 3cm tall and 1.5cm x 1cm in cross section, and was imaged at a magnification of about 3.6x. The data were reconstructed on a 0.5x0.5x0.5 mm3 voxel grid. After reconstruction, the aluminum and copper could be easily discriminated using a gray level threshold allowing visualization of the copper components. Fractal analysis of the tomographic reconstructed material topology is investigated as a means to quantify macro level material flow based on process parameters. The results of multi-pass FSWs show increased refinement of the copper trace material. Implications of these techniques for quantifying process flow are discussed.

36 MATERIALS SCIENCE↗

Study on Composition, Microstructure and Wear Behavior of Fe-B-C Wear-Resistant Surfacing Alloys

Fe-B-C alloy layers with various microstructures were welded on Q235 steel plates using welding powders/H08Mn2Si and welding wires composite surfacing technology. The relationship existing between the chemical composition, microstructure and wear resistance of the surfacing alloy layers was investigated by scanning electron microscopy, x-ray diffraction, electron backscatter diffraction and wear tests. The results demonstrated that the volume fractions and morphologies of the microstructures in the surfacing alloy layers could be controlled by adjusting the boron and carbon contents in the welding powders, which could further regulate the wear resistance of the surfacing alloy layers. The typical microstructures of the Fe-B-C surfacing alloy layers included dendritic Fe, rod-like Fe{sub 2}B, fishbone-like Fe{sub 2}B and daisy-like Fe{sub 3}(C, B). The wear resistance of the alloy layers with various morphologies differed. The wear resistance order of the different microstructures was: rod-like Fe{sub 2}B > fishbone-like Fe{sub 2}B > daisy-like Fe{sub 3}(C, B) > dendritic Fe. A large number of rod-like Fe{sub 2}B with high microhardness could be obtained at the boron content of 5.70 ~ 5.90 wt.% and the carbon content of 0.50 ~ 0.60wt.%. The highest wear resistance of the Fe-B-C alloy layers reached the value of 24.1 g{sup −1}, which demonstrates the main microscopic cutting wear mechanism of the Fe-B-C alloy layers.

36 MATERIALS SCIENCE↗

Laser Weldability of AlSi{sub 10}Mg Alloy Produced by Selective Laser Melting: Microstructure and Mechanical Behavior

Selective laser melting (SLM) allows 3D complex parts to be produced with integrated functionalities but does not permit to realize large dimension parts, as the building chamber volume of commercial SLM systems is limited. Therefore, the possibility of joining SLM-built parts by welding appears as extremely valuable. In this work, laser weldability of SLMed AlSi{sub 10}Mg parts has been investigated. The cooling rates induced by the welding process are lower than the ones of SLM; therefore, typical eutectic silicon network of SLM-built parts appears broken in both the melted zone and part of the heat-affected zone, as confirmed by calorimetric measurement. This microstructural evolution caused a local decrease of hardness from 132 HV to 73 HV and a reduction of ductility caused by porosity formation in the weld bead. Moreover, the thermal treatment, performed at 320°C, can limit the gap of tensile response among welded bead and base SLM material.

36 MATERIALS SCIENCE↗

Enhanced joining strength in additive-manufactured polylactic-acid structures fused by embedded heated metallic meshes

Additively manufactured thermoplastic polymers, such as polylactic acid (PLA), hold significant promise for sustainable engineering structures, including wind turbine blades. Upscaling these structures beyond the limitations of 3D printer build volumes is a challenge; fusion joining presents a potential solution. This paper introduces a displacement-controlled resistance welding process for PLA, as an alternative to the typical force-controlled methods. Here, we investigated the bonding quality of resistance-welded and adhesive-bonded PLA beams through three-point bending and measured the surface deformations using digital image correlation. Different metal meshes (30%/0.11 mm Ni—Cu, 34%/0.07 mm Ni—Cu, and 36%/0.25 mm Co—Ni) served as heating elements. The process parameters were varied for the 34%/0.07 mm Ni—Cu mesh to identify an optimum set of parameters. Results showed that this optimized displacement-controlled welding achieved 94% of the original strength of monolithic samples. This indicates that the new welding process not only ensures high-quality bonding and fine surface finishing but also promotes sustainability, recyclability, and economic efficiency in various polymer and composite structural applications.

Additive manufacturing↗

Atom probe tomography characterization of neutron irradiated surveillance samples from the R. E. Ginna reactor pressure vessel

Surveillance samples of a low copper (nominally 0.05 wt.% Cu) forging and a higher copper (0.23 wt.% Cu) submerged arc weld from the R. E. Ginna reactor pressure vessel have been characterized by atom probe tomography (APT) after exposure to three levels of neutron irradiation, i.e., fluences of 1.7, 3.6 and 5.8 × 10 23 n.m –2 (E > 1 MeV), and inlet temperatures of ~289 °C (~552 °F). As no copper-enriched precipitates were observed in the low copper forging, and the measured copper content in the ferrite matrix was 0.04± <0.01 at.% Cu, after neutron irradiation to a fluence of 1.7 × 10 23 n.m –3 , this copper level was below the solubility limit. A number density of 2 × 10 22 m –3 of Ni–, Mn– Si-enriched precipitates with an equivalent radius of gyration of 1.7 ± 0.4 nm were detected in the sample. However, Cu-, Ni-, Mn-enriched precipitates were observed in specimens cut from different surveillance specimens from the same forging material in which the overall measured copper level was 0.08± <0.01 at.% (fluence of 3.6 × 10 23 n.m –3 ) and 0.09± <0.01 at.% Cu (fluence of 5.8 × 10 23 n.m –3 ). Therefore, these slightly higher copper contents were above the solubility limit of Cu under these irradiation conditions. A best fit of all the composition data indicated that the size and number density of the Cu-enriched precipitates increased slightly in both size and number density by additional exposure to neutron irradiation. High number densities of Cu-enriched precipitates were observed in the higher Cu submerged arc weld for all irradiated conditions. The size and number density of the precipitates in the welds were higher than in the same fluence forgings. Some Cu-enriched precipitates were found to have Ni-, Mn- Si-, and P-enriched regions on their surfaces suggesting a preferential nucleation site. Furthermore, atom maps revealed P, Ni, and Mn segregation to, and preferential precipitation of, Cu-enriched precipitates over the surface of a grain boundary in the low fluence weld.

36 MATERIALS SCIENCE↗

Influence of fabrication on microstructure and heat affected zone width in weldments of nuclear reactor pressure vessel steel

Advanced manufacturing routes such as electron beam welding and powder metallurgy with hot isostatic pressing are increasingly used across energy and aerospace industries, where the reliable prediction of weld behavior and heat affected zone (HAZ) evolution is critical. This study examines how fabrication routes and post-weld heat treatments influence phase distribution, crystallite size, microstrain, and dislocation density in nuclear reactor pressure vessel steels using synchrotron X-ray diffraction (SXRD). Retained austenite occurs only in samples that did not undergo austenitization, whereas an austenitizing heat treatment fully eliminates retained austenite and produces a more uniform microstructure across the weldment in terms of phase fraction, dislocation density, and microstrain. The Rosenthal solution underestimates the HAZ width for powder metallurgy samples. A newly proposed modified Rosenthal solution, reducing density by accounting for porosity, matches the SXRD-measured HAZ width with a 0.65% error. Structure–property correlations reveal that dislocation density correlates strongly with nanohardness in homogenous microstructures, while in heterogenous weldments nanohardness is further influenced by the presence of dissimilar phase boundaries. These findings provide new insight into the thermal and microstructural response of powder metallurgy fabricated steels and offer a framework for optimizing welding procedures and heat treatments in advanced manufacturing applications.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Additive manufacturing of Zr-based metallic glass structures on 304 stainless steel substrates via V/Ti/Zr intermediate layers

Welding of dissimilar metals is challenging, particularly between crystalline metals and metallic glasses (MGs). Here in this study, Zr 65.7 Cu 15.6 Ni 11.7 Al 3.7 Ti 3.3 (wt%) MG structures were built on 304 stainless steel (SS) substrates by laser-foil-printing (LFP) additive manufacturing technology in which MG foils were laser welded layer-by-layer onto the SS substrate with a transition route, i.e., SS → V → Ti → Zr → MG. The direct welding of MG on SS would lead to the formation of various brittle intermetallics and the consequent peeling off of the welded MG foils from the SS substrate, which could be resolved via the use of V/Ti/Zr intermediate layers. The chemical composition, formed phases, and micro-hardness were characterized in the dissimilar joints by energy dispersive spectroscopy, X-ray diffraction, and micro-indentation. Since the intermediate materials were highly compatible with the base metals or the adjacent intermediate metals, undesirable intermetallics were not detected in the dissimilar joint. The bonding tensile strength between the SS substrate and the MG part with intermediate layers was measured about 477 MPa.

36 MATERIALS SCIENCE↗

Enhanced Interfacial Bonding of Graft Copolymers

To understand how thermoplastic welding strength can be tuned through chemical modifications and macromolecular topology, we combined coarse-grained molecular dynamics (MD) simulations with experimental validation. Our simulations examined the diffusion dynamics of both linear and graft polymers across representative interfaces, revealing that diffusion-controlled interdigitation follows a power law, with the exponent decreasing from 0.34 to 0.11 as grafting density increases from 7.5 to 196% (with side chains grafted to both sides of a monomer unit). The addition of side chains enhances welding efficiency, as dense bottlebrush polymers with high grafting density reach maximum rupture strength faster than linear polymers. However, their saturated rupture strength is lower. This observation is subsequently corroborated by experimental lap-shear tests comparing linear polyethylene with octene grafted polyethylene elastomers. Our MD simulations show that unlike linear polymers, where backbone entanglements dominate, the grafted side chains introduce mechanisms in addition to entanglement dilution. The rapid interdigitation of side chains creates a dense mesh of entropic van der Waals contacts, which can also enhance the film welding. Furthermore, our MD simulations reveal a brittle rupture behavior in linear and comb-like (mildly grafted) polymers, while bottlebrush (densely grafted) polymers display elastomeric behavior with a pronounced stress plateau prior to fracture. Our simulations deconvolute the influence of polymer topology on deformation behavior. The rate of polymer deformation becomes lower than the applied strain rate prior to rupture, and the onset of this deviation is progressively delayed from linear to bottlebrush polymers. This trend highlights the critical role of molecular architecture in governing the mechanical response. In conclusion, these results provide deeper insight into the underlying welding mechanisms of topological polymers and present a potential approach for mitigating the interface anisotropy that is inherent in advanced manufacturing techniques such as fused filament fabrication.

graft copolymers↗