DISFRAC Version 2.0 Users Guide

DISFRAC is the implementation of a theoretical, multi-scale model for the prediction of fracture toughness in the ductile-to-brittle transition temperature (DBTT) region of ferritic steels. Empirically-derived models of the DBTT region cannot legitimately be extrapolated beyond the range of existing fracture toughness data. DISFRAC requires only tensile properties and microstructural information as input, and thus allows for a wider range of application than empirical, toughness data dependent models. DISFRAC is also a framework for investigating the roles of various microstructural and macroscopic effects on fracture behavior, including carbide particle sizes, grain sizes, strain rates, and material condition. DISFRAC s novel approach is to assess the interaction effects of macroscopic conditions (geometry, loading conditions) with variable microstructural features on cleavage crack initiation and propagation. The model addresses all stages of the fracture process, from microcrack initiation within a carbide particle, to propagation of that crack through grains and across grain boundaries, finally to catastrophic failure of the material. The DISFRAC procedure repeatedly performs a deterministic analysis of microcrack initiation and propagation within a macroscopic crack plastic zone to calculate a critical fracture toughness value for each microstructural geometry set. The current version of DISFRAC, version 2.0, is a research code for developing and testing models related to cleavage fracture and transition toughness. The various models and computations have evolved significantly over the course of development and are expected to continue to evolve as testing and data collection continue. This document serves as a guide to the usage and theoretical foundations of DISFRAC v2.0. Feedback is welcomed and encouraged.

Cochran, Kristine B.↗

Densification, Microstructural Evolution, Mechanical Properties and Oxidation Study of CrB{sub 2} + EuB{sub 6} Composite

This paper reports the results of investigation on densification, microstructural evolution, mechanical properties and oxidation study of CrB{sub 2} + EuB{sub 6} composite. CrB{sub 2} + EuB{sub 6} (10 and 20 wt.%) composites have been fabricated by hot pressing at a temperature of 1700 °C and 35 MPa pressure. The hardness and flexural strength were measured in the range of 21.25-24.48 GPa and 171-199 MPa, respectively. The fracture toughness increased from 3.3 to 4.01 MPa m{sup 1/2} by the addition of 20% EuB{sub 6}. Microstructural evolution revealed the uniform distribution of EuB{sub 6} and absence of any reaction product. Fracture surface analysis confirmed the presence of transgranular mode of fracture. Oxidation study at 1200 °C revealed that the developed composites have good oxidation resistance and followed the parabolic rate of oxidation.

36 MATERIALS SCIENCE↗

Microstructure and micro-texture evolution during large strain deformation of Inconel alloy IN718

The hot deformation behaviour of Inconel alloy IN718 was studied in the temperature range of 950–1100 °C and at strain rates of 0.01 and 1 s{sup −1} with a view to understand the microstructural evolution as a function of strain rate and temperature. For this purpose, a single hit, hot isothermal plane strain compression (PSC) technique was used. The flow curves obtained during PSC exhibited weak flow softening at higher temperatures. Electron backscattered diffraction analysis (EBSD) of the PSC tested samples at the location of maximum strain revealed dynamic recrystallisation occurring at higher temperatures. Based on detailed microstructure and microtexture analyses, it was concluded that single step, large strain deformation has a distinct advantage in the thermo-mechanical processing of Inconel alloy IN718. - Highlights: • Plane strain compression (PSC) on IN718 was conducted. • Evolution of microstructure during large strain deformation was studied. • Flow curves exhibited weak softening at higher temperatures and dipping of the flow curve at a strain rate of 1 s{sup −1}. • Optimization of microstructure and process parameter for hot rolling possible by plane strain compression testing • Dynamic recrystallisation occurs in specimens deformed at higher temperatures and lower strain rates.

36 MATERIALS SCIENCE↗

Microstructural evolution of an aluminide coating on alloy 625 during wet air exposure at 900 °C and 1000 °C

The microstructural changes of the aluminized alloy 625 during cyclic oxidation in air + 6% H 2 O at 900 °C and 1000 °C were analyzed using optical metallography (OM), scanning electron microscopy (SEM) with energy and wave length dispersive X-ray analysis (EDX/WDX) as well as electron backscatter diffraction (EBSD). An in-house developed thermodynamic-kinetic procedure was employed to predict the microstructural evolution of aluminized alloy 625 during high temperature exposure by considering simultaneously occurring surface oxidation and interdiffusion processes. Because of the lack of mobility data for the relevant alloying elements in the σ-phase, assumptions for the mobilities were made based on the value of the mobilities in α-Cr. Despite these assumptions, the calculated results were found to be in good agreement with experimental observations. The complete depletion of β-NiAl in the coating observed during exposure at 1000 °C was correctly predicted by the model. The model was also able to infer dissolution of the precipitate phases α-Cr and σ in the interdiffusion zone during exposures at 900 °C and 1000 °C. The model was yet unable to predict the formation of the μ-phase in the alloy after 1000 h of exposure at 1000 °C. The developed modelling method offers the potential to predict microstructural changes of aluminized nickel base alloys thus reducing cost and time consuming experimental efforts.

36 MATERIALS SCIENCE↗

In situ {sup 1}H-TD-NMR: Quantification and microstructure development during the early hydration of alite and OPC

An in situ framework for {sup 1}H time-domain nuclear magnetic resonance analysis was developed and applied on alite and OPC hydration. Highly time-resolved quantitative data on the evolution of proton reservoirs during hydration was collected for up to 40 h. Reservoirs could be clearly assigned to mobile (mix water), intermediate (C-S-H) and rigid fractions (CH, ettringite). Comparison of determined fraction quantities with data from in situ XRD measurements and heat flow calorimetry show very good agreement. During alite hydration at 23 °C, a bulk water content of 4 H{sub 2}O in C{sub 1.7}SH{sub x} was confirmed. T2 relaxation times of the mobile fraction shifted towards shorter times from the start of the main reaction until the maximum of the heat flow. Microstructure evolution is nearly finished at that point in time. T2 relaxation times are severely shortened for iron-containing OPC, but are still evaluable.

36 MATERIALS SCIENCE↗

Fabrication and Analysis of Tri-layer YBa{sub 2}Cu{sub 3}O{sub 7−δ} Thick Films by Low-Fluorine MOD Method

Improving the thickness of superconducting layer in coated conductors is an effective way to enhance its critical current. In this work, tri-layer YBCO/YBCO/YDyBCO films were successfully deposited on buffered Hastelloy substrate using the multi-coating lowfluorine metal-organic decomposition (LF-MOD) method and the thickness of the films can be up to 2.4 μ m. The effects of high-temperature annealing time on microstructures and superconducting properties of the films were systematically studied. Energy dispersive X-ray spectroscopy (EDS) results reveal that there remains a large amount of F element in the upper layer of the film when the annealing time is too short. With increasing the annealing time, the fluoride-containing precursor converts to YBCO grains completely. But the coarsening of grains appeared, and the critical current density (J{sub c}) of the film dropped slightly when the annealing time is too long. The cross-sectional scanning electron microscope (SEM) image and EDS plane analysis were applied to investigate the microstructure and element distribution of the final triple-layer YBCO films, respectively. The critical current of the final YBCO superconducting film could reach 316 A (77 k, self-field) for 1.2-cm-wide tapes with the optimal annealing conditions.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Chemical, Structural, and Microstructural Changes in Metallic and Silicon-Based Coating Materials Exposed to Iodine Vapor

The chemical, structural and microstructural behavior of steels (304, 316 and A36), titanium-aluminum alloy (Ti-Al, (6Al-4V)), aluminum-magnesium alloy (Al-Mg, 6061), and coatings (Silcolloy and Dursan (SilcoTek Corporation)) were probed after exposure to iodine laminar flow. Exposures were carried out in a custom-built Iodine Vapor RIG (IVR) at 300 degrees C to an iodine laminar vapor flow of 1 mg min(exp. -1), carried by 145 mL-min(exp. -1) argon gas, for 5, 15 and 30 days. Samples were characterized before and after the experiment by gravimetric analysis, X-ray diffraction (XRD) and cross section electron microscopy analysis coupled with energy dispersive X-ray spectroscopy (EDS). All steels exposed for 30 days formed scales consisting mainly of metal (Cr, Fe, Ni) oxides showing different chemistry, microstructure and crystalline phases. Elemental iodine was only detected by EDS analysis in the scales of stainless steels 304 and 316. After 30 days, the Ti-Al exhibited no detectable scale, suggesting only a very thin film was formed. A scale consisting mainly of aluminum, iodine, and oxygen formed on the Al-Mg sample exposed to 30 days. Some pockets rich in magnesium, iodine and oxygen also formed in this Al-Mg alloy. Stainless steel 316, low carbon steel A36 and Ti-Al alloy coated with Silcolloy and stainless steel 304 coated with Dursan that were exposed for 30 days exhibited no oxidation. Stainless steel 304 coated with Silcolloy exposed for 30 days did not exhibit corrosion although the sample gained weight and the coating exhibited expansion. The weight gain per area performance of the materials exposed in iodine lamina flow containing oxygen at impurity level for 10, 15 and 30 days are reported from the lowest to the highest weight gain per area as follows: Steels: Less than 316 less than 304 less than A36; Ti-Al-Mg based alloys: Al-Mg less than Ti-Al: Considering the experimental uncertainties, no weight change was observed for Stainless steel 316, low carbon steel A36 and Ti-Al alloy coated with Silcolloy and stainless steel 304 coated with Dursan. The corrosion of the alloys is catalyzed by iodine in the presence of oxygen as impurity.

Costa, Gustavo C. C.↗

Dual microscopy to explore enhanced atmospheric ice nucleation on multi-component aerosols

Using an optical microscopy setup adapted to in-situ studies of ice formation at ambient pressure, we examined a specific multicomponent mineral, microcline, with the ultimate aim of gaining a more realistic understanding of ice nucleation in Earth’s atmosphere. We focused on a perthitic feldspar, microcline, to test the hypothesis that co-existence in some feldspars of K-rich and Na-rich phases are contributing to enhanced ice nucleation. On a sample deliberately chosen to contain lamella, a typical perthitic microstructure, and flat surface regions next to each other, we performed a series of ice formation experiments. We found microcline to promote ice formation, causing a large number of ice nucleation events at around - 27°C. The number of ice nuclei decreased from experimental run to experimental run, indicating surface aging upon repeated exposure to humidity. An analysis of 10 experimental runs of identical conditions did not reveal an obvious enhancement of ice formation at the lamellar microstructure. Instead, we find efficient nucleation at various surface sites that produce orientationally aligned ice crystallites with asymmetric shape. Based on this observation we propose that surface steps running along select directions produce microfacets of an orientation that is favorable to enhanced ice nucleation, similar to previously reported for K-rich feldspars.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Unraveling the implications of finite specimen size on the interpretation of dynamic experiments for polycrystalline aluminum through direct numerical simulations

Normal and Pressure-shear plate impact (NPI and PSPI) experiments are popular experimental techniques for studying the mean-field macroscopic behavior of polycrystalline metals under high-rate dynamic loading. However, since both configurations rely upon geometry for subjecting the specimen to high strain rates, these experiments often involve a limited specimen size. Moreover, because of the inherent heterogeneities present within polycrystalline metals, it is difficult to ascertain if the size of the specimen and/or regions where measurements are made are sufficiently large for making representative inferences about the mean-field macroscopic properties from single-point velocity measurements. In the present study, we quantify the expected measurement variability on observable point measurements in NPI and PSPI experiments by carrying out direct numerical simulations (DNS) of statistically representative polycrystalline microstructures subjected to dynamic compression and compression-shear loading. In particular, we consider the role of specific material heterogeneities (e.g. the grain-to-grain difference in size, crystallographic orientation) on dispersion in the normal and transverse particle velocity records and on local fluctuations in key state variables (e.g. velocity, accumulated plastic strain) by incorporating these effects directly into a representative synthetic microstructure geometry and crystalline description of pure polycrystalline aluminum. The form of the present study is a large parametric investigation, consisting of ten ensembles of one hundred simulations. Each of the thousand simulations reflects a randomly realized synthetic microstructure in one of five cases of decreasing average grain size for the two loading configurations. Our analysis of the DNS results demonstrates that for both of these experimental configurations, the grain size directly correlates with the coefficient of variation (CV) in simulated point measurements, showing a convergent decrease in CV to zero (i.e. particle velocity record approaches the mean-field value) with decreasing grain size. Remarkably, the magnitude of variations in the particle velocity record is shown to be largest where the deviatoric stresses are most significant. In the case of NPI, this occurs at the elastic and plastic wavefront, whereas, in the case of PSPI, the magnitude of fluctuations are approximately constant throughout the experimental window time. The reasoning for the scatter in particle velocity due to the heterogeneous microstructure is demonstrated to be dependent on the mechanisms for accommodating deformation and on the interaction of reflection waves generated at sites of heterogeneities occurring at the scale of grains. Lastly, we develop a power-law description for the magnitude of scattering versus characteristic length, which provides a statistical framework for assessing the required number of grains per characteristic specimen dimension for minimizing scatter within these two experimental configurations (NPI, PSPI).

36 MATERIALS SCIENCE↗

Probing rutile solid-phase crystallization of atomically mixed Mn-alloyed TiO 2 coatings through XANES analysis

Phase transformation via dopant introduction is an emerging strategy for tuning the electronic and catalytic properties of oxides. However, developing a general theory of ternary alloys and their microstructure evolution remains challenging due to the knowledge gaps in how point defects such as dopants lead to the formation of complex or metastable phases. We investigate the influence of Mn concentration and annealing temperature on the microstructure evolution of amorphous Mn-alloyed TiO 2 synthesized via Atomic Layer Deposition. In conclusion, our findings reveal a new crystallization pathway resulting in a direct amorphous TiO 2 to rutile transformation without an intermediate anatase phase and our multi-parameter thermal processing conditions show potential for AI-assisted data acquisition and analysis for studying complex oxide coatings.

36 MATERIALS SCIENCE↗

Structural and electrical properties of ternary Ru-AlN thin films prepared by plasma-enhanced atomic layer deposition

Highlights: Black-Right-Pointing-Pointer Ru-AlN thin films were grown by plasma-enhanced atomic layer deposition (PEALD). Black-Right-Pointing-Pointer Structural properties were systematically investigated by XRD, BF-STEM and EDX. Black-Right-Pointing-Pointer A drastic decrease in resistivity was due to the microstructural change of the films. -- Abstract: Ruthenium-aluminum-nitride (Ru-AlN) thin films were grown by plasma-enhanced atomic layer deposition (PEALD) at 300 Degree-Sign C. The Ru intermixing ratio of Ru-AlN thin films was controlled by the number of Ru unit cycles, while the number of AlN unit cycles was fixed to one cycle. The electrical resistivity of Ru-AlN thin film decreased with increasing the Ru intermixing ratio, but a drastic decrease in electrical resistivity was observed when the Ru intermixing ratio was around 0.58-0.78. Bright-field scanning transmission electron microscope (BF-STEM) and energy-dispersive X-ray spectroscopy (EDX) element mapping analysis revealed that the electrical resistivity of Ru-AlN thin film was strongly dependent on the microstructures as well as on the Ru intermixing ratio. Although the electrical resistivity of Ru-AlN thin films decreased with increasing the Ru intermixing ratio, a drastic decrease in electrical resistivity occurred where the electrical paths formed as a result of the coalescence of Ru nanocrystals.

36 MATERIALS SCIENCE↗

Identify the influence of microstructure on mesoscale creep and fatigue damage

This report describes the development of a microstructural model that can quantify the uncertainty in the observed rupture life of Grade 91 steel. The model is microstructural, meaning it relates microstructural characteristics of the material to the resulting material response. As such, one of the uses of this model is to identify the key microstructural parameters controlling the development of damage in Grade 91 operating at elevated temperatures. The report describes two veins of work: improvements to the crystal plasticity model required to run the uncertainty quantification analysis and the results of that UQ analysis. For creep, the model identifies the grain boundary diffusivity as the critical parameter controlling the rupture life of the material. The report demonstrates that a reasonable microstructural distribution of grain boundary diffusivity can account for the observed macroscale variation in rupture life at fixed temperature and load.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Effect of moderate magnetic annealing on the microstructure, quasi-static and viscoelastic mechanical behavior of a structural epoxy

In this study the effect of moderate magnetic fields on the microstructure of a structural epoxy system was investigated. The changes in the microstructure have been quantitatively investigated using wide angle x-ray diffraction (WAXD) and pole figure analysis. The mechanical properties (modulus, hardness and strain rate sensitivity parameter) of the epoxy system annealed in the magnetic field were probed with the aid of instrumented nanoindentation and the results are compared to the reference epoxy sample. To further examine the creep response of the magnetically annealed and reference samples, short 45 min duration creep tests were carried out. An equivalent to the macro scale creep compliance was calculated using the aforementioned nano-creep data. Using the continuous complex compliance (CCC) analysis, the phase lag angle, tan (δ), between the displacement and applied force in an oscillatory nanoindentation test was measured for both neat and magnetically annealed systems through which the effect of low magnetic fields on the viscoelastic properties of the epoxy was invoked. The comparison of the creep strain rate sensitivity parameter , A/d(0), from short term(80 ), creep tests and the creep compliance J(t) from the long term(2700 s) creep tests with the tan(δ) suggests that former parameter is a more useful comparative creep parameter than the creep compliance. The results of this investigation reveal that under low magnetic fields both the quasi-static and viscoelastic mechanical properties of the epoxy have been improved.

36 MATERIALS SCIENCE↗

Microstructural impacts on ionic conductivity of oxide solid electrolytes from a combined atomistic-mesoscale approach

Abstract Although multiple oxide-based solid electrolyte materials with intrinsically high ionic conductivities have emerged, practical processing and synthesis routes introduce grain boundaries and other interfaces that can perturb primary conduction channels. To directly probe these effects, we demonstrate an efficient and general mesoscopic computational method capable of predicting effective ionic conductivity through a complex polycrystalline oxide-based solid electrolyte microstructure without relying on simplified equivalent circuit description. We parameterize the framework for Li 7- x La 3 Zr 2 O 12 (LLZO) garnet solid electrolyte by combining synthetic microstructures from phase-field simulations with diffusivities from molecular dynamics simulations of ordered and disordered systems. Systematically designed simulations reveal an interdependence between atomistic and mesoscopic microstructural impacts on the effective ionic conductivity of polycrystalline LLZO, quantified by newly defined metrics that characterize the complex ionic transport mechanism. Our results provide fundamental understanding of the physical origins of the reported variability in ionic conductivities based on an extensive analysis of literature data, while simultaneously outlining practical design guidance for achieving desired ionic transport properties based on conditions for which sensitivity to microstructural features is highest. Additional implications of our results are discussed, including a possible connection between ion conduction behavior and dendrite formation.

25 ENERGY STORAGE↗

Relationship between Material Properties and Local Formability of DP980 Steels

A noticeable degree of inconsistent forming behaviors has been observed for the 1st generation advanced high strength steels (AHSS) in production, and they appear to be associated with the inherent microstructural-level inhomogeneities for various AHSS. This indicates that the basic material property requirements and screening methods currently used for the mild steels and high strength low alloys (HSLA) are no longer sufficient for qualifying today’s AHSS. In order to establish more relevant material acceptance criteria for AHSS, the fundamental understandings on key mechanical properties and microstructural features influencing the local formability of AHSS need to be developed. For this purpose, in this study, DP980 was selected as model steels and eight different types of DP980 sheet steels were acquired from various steel suppliers. Various experiments were then performed on the eight different DP980 steels such as chemical composition analysis, static tensile test, hole expansion test, channel forming test. Scanning electron microscope (SEM) pictures of the DP980 steels were also obtained, and image processing tools were then adopted to those SEM pictures in order to quantify their various microstructural features. The results show that all DP980 steels show large discrepancy in their performance and that the tensile properties and hole expansion properties of these steels do not correlate with their local formability. According to the results up to date, it is not possible to correlate the microstructural features alone to the macroscopically measured deformation behaviors. In addition to image analysis, other experiments (i.e., nano-indentation test) are also planned to quantify the individual phase properties of the various DP steels.

DP steel↗

A quantitative comparison of the fingerprint of twinned microstructures through surface and three-dimensional techniques

Assessing the fingerprint of a material’s microstructure is key for supporting materials design. With the emergence of a wide range of 3D characterization techniques, it is critical to understand the main differences in fingerprints reconstructed from 2D and 3D datasets. To this end, we introduce a graph-based microstructure reconstruction framework that enables structural comparisons of twin domain networks in high purity Ti using 3D and 2D electron backscatter diffraction. Insights into the structure of the twin networks are facilitated by combining statistical analysis of twin crystallography with visual and graphical analysis of the novel graph abstractions of the twins. We demonstrate that compared to 3D reconstructions, conventional 2D views of twinning miss key aspects of the microstructure including the high interconnectivity of domains into networks that span the full reconstruction volume. The reduced cross-grain and in-grain twin connectivity typically observed in 2D has notable implications on our understanding of how twinning mediates the plastic response of microstructures and how twin networks evolve. It is thus clear that 3D characterization is critical for accurately inferring both twin network morphologies as well as the key unit processes facilitating network formation.

36 MATERIALS SCIENCE↗

Atomic resolution strain analysis in highly textured FePt thin films

In this work, we present a detailed investigation of FePt-substrate interfaces and their influence towards the microstructural and magnetic configurations of the resulting metallic films. Discontinuous FePt films of roughly 15 nm thickness are deposited at 750 °C on MgO, MgAl{sub 2}O{sub 4}, SrTiO{sub 3}, and (La,Sr)(Al,Ta)O{sub 3} single-crystalline substrates. All of these films mainly show out-of-plane textured FePt islands; however, fractions of L1{sub 2} and in-plane oriented crystals are observed for the films on substrates with reduced lattice mismatch. Reduced easy axis coercivities and enhanced hard axis remanence values affirm this observation. Moreover, quantitative high-resolution transmission electron microscope analysis reveals that the reduced lattice mismatch results in a decreased density of dislocations, especially misfit dislocations, at the FePt-substrate interface. To further extend the research, carbon-doped FePt+32%C films are deposited on single-crystalline and sputtered MgO at 750 °C and 650 °C, respectively, to characterize the influence of a segregating media and reduced grain size. A comparison to the pure FePt sample reveals that the presence of seed layer grain boundaries leads to an increased fraction of in-plane oriented material, while the density of misfit dislocations solely depends on the degree of lattice mismatch.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Exploring the tempering behaviour of additively manufactured high-alloy tool steel using synchrotron X-ray and neutron techniques

Post-processing heat treatment provides a critical pathway toward the commercialisation of additively manufactured (AM) S390 high-speed steel, which is a representative high-alloy tool steel employed in precision manufacturing, offering up to 1.5 times longer tool life and over 20% higher cutting speeds compared to conventional grades. In this study, the phase evolution of AM S390 steel during heat treatment, with particular emphasis on carbide precipitation behaviour, was systematically investigated using a combination of synchrotron X-ray and neutron techniques. The metastable M2C carbides were found to dissolve during austenitisation, while the stable primary carbides MC and M6C experienced coarsening with an average size increase of about 60 nm after just 2 min of tempering. Moreover, the austenite lattice parameters reduced from 3.618 to 3.608 Å within the first 10 min of tempering, suggesting carbon depletion in the steel matrix was likely associated with the formation of secondary carbides. This interpretation was substantiated by small-angle scattering results, which revealed the presence of nanoscale precipitates with a volume fraction of 3.1% after 60 min of tempering. These microstructural evolutions collectively accounted for the observed peak hardness of 921 HV. Furthermore, a comparative analysis of synchrotron and neutron small-angle scattering data highlighted the complementary strengths of each technique, offering critical insight into their suitability for characterising nanoscale features in AM high-alloy steels.

Synchrotron X-ray diffraction↗