Search NASA⌕ Search

SEARCH · Search NASA

Results for “solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,567 records · Page 87

Single crystal growth of Ga[subscript 2](Se[subscript x]Te[subscript 1;#8722;x])[subscript 3] semiconductors and defect studies via positron annihilation spectroscopy

Small single crystals of Ga{sub 2}(Se{sub x}Te{sub 1-x}){sub 3} semiconductors, for x = 0.1, 0.2, 0.3, were obtained via modified Bridgman growth techniques. High resolution powder x-ray diffractometry confirms a zincblende cubic structure, with additional satellite peaks observed near the (111) Bragg line. This suggests the presence of ordered vacancy planes along the [111] direction that have been previously observed in Ga{sub 2}Te{sub 3}. Defect studies via positron annihilation spectroscopy show an average positron lifetime of {approx} 400 ps in bulk as-grown specimens. Such a large lifetime suggests that the positron annihilation sites in these materials are dominated by defects. Moreover, analyzing the electron momenta via coincidence Doppler broadening measurements suggests a strong presence of large open-volume defects, likely to be vacancy clusters or voids.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

An axial temperature profile curvature criterion for the engineering of convex crystal growth interfaces in Bridgman systems

A unifying idea is presented for the engineering of convex melt-solid interface shapes in Bridgman crystal growth systems. Previous approaches to interface control are discussed with particular attention paid to the idea of a “booster” heater. Proceeding from the idea that a booster heater promotes a converging heat flux geometry and from the energy conservation equation, we show that a convex interface shape will naturally result when the interface is located in regions of the furnace where the axial thermal profile exhibits negative curvature, i.e., where d 2 T/dz 2 < 0. This criterion is effective in explaining prior literature results on interface control and promising for the evaluation of new furnace designs. Here we posit that the negative curvature criterion may be applicable to the characterization of growth systems via temperature measurements in an empty furnace, providing insight about the potential for achieving a convex interface shape, without growing a crystal or conducting simulations.

36 MATERIALS SCIENCE↗

Sample environment effects on synchrotron-measured temperature profiles in an approximant of optical floating zone crystal growth

Even though the growth of crystals using optical floating zone furnaces has had an immense scientific impact, the implementation of this method remains more of an art than a science due to the difficulty of obtaining quantitative information about the sample thermal profile during crystal growth. Building on recent work demonstrating that in situ synchrotron studies can be used to map sample rod temperatures during heating, investigations were carried out to better understand how the sample environment affects the sample temperature profile. Through a combination of experimental studies and modeling efforts, it is shown that the environment in the furnace can strongly influence the sample temperature at the lamp focus, the steepness of the vertical temperature gradient, and the timescale required for sample heating and cooling - effects which can combine to produce a strong history-dependence to sample temperature profiles. It is demonstrated that the furnace effects can be effectively captured in thermal models, allowing both the steady-state and time-dependent behavior of the sample to be accurately reproduced with predictive models, and providing a launching point for improved furnace designs that can more readily deliver desired thermal profiles.

36 MATERIALS SCIENCE↗

An atomistic theory of nucleation: Self-organization via non-equilibrium work and fluctuations

For this work, insights from non-equilibrium statistical mechanics, highlighting the role of work and fluctuations at the microscale, are applied toward the development of a fundamental, rigorous and purely atomistic theory of nucleation. Nanoscale fluctuations in order, density and heat influence the local nucleation rate by orders of magnitude, necessitating their inclusion through a modern approach. Coarse-graining over the underlying Hamiltonian dynamics allows derivation of a microscale expression for the nucleation rate in terms of a classical path integral over far from equilibrium trajectories and their associated work. Second law violating states at the microscale, as found from the dynamics of small critical nucleation clusters, contribute exponentially to the observable macroscale nucleation rate.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

New anisotropic MnBi permanent magnets by field-annealing of compacted melt-spun alloys modified with Mg and Sb

A technique has been designed for manufacturing rare-earth-free MnBi-based magnets capable of filling the existing "gap" between the ferrite and rare-earth permanent magnets. Whereas the earlier approaches relied on sintering of fine and easily degrading single-crystal MnBi particles, the new method achieves refinement of the key α-MnBi phase through melt-spinning combined with appropriate alloying. Modification of the MnBi alloys with Mg and Sb generates a high-coercivity nanostructure of the metastable β' phase. A subsequent compaction at 150 °C produces fully dense materials while converting the β' phase into the stable α phase. Lastly, a short annealing at 265–300 °C in a magnetic field of 3 T increases the fraction of the α phase to 97–98% and aligns the c axes of the α crystallites. A maximum energy product (BH) max of 11.5 MGOe and an intrinsic coercivity Hc of 5.6 kOe have been obtained in a magnet with the nominal composition Mn 50 Bi 46.5 Mg 3 Sb 0.5 . Because the coercivity increases with temperature, the maximum energy product of this magnet is still as high as 8.9 MGOe at 175 °C. Increasing the Sb content to 1.5 at.% increases the H c to 9.3 kOe, but at the same time inhibits the development of the texture thus decreasing the (BH) max . The addition of Mg was found to increase the c lattice parameter of the α phase resulting in an unusually large ratio c/a ≈1.432.

36 MATERIALS SCIENCE↗

MnBi-based magnets prepared from melt-spun alloys: Effect of $α → β$ phase transformation during field annealing

The temperature of the annealing treatment applied to the MnBi alloys with the intention to stabilize the α -MnBi “low-temperature” phase – a promising material for the rare-earth-free permanent magnets – is usually kept below the range of the β -Mn 1.08 Bi “high-temperature” phase. This work is focused on the investigation of the effects of partial and complete α → β phase transformation in bulk magnetic-field-annealed magnets on their structure and magnetic properties. MnBi alloys modified with In, Mg and Sb were melt-spun, compacted to their full density and then heated in a magnetic field of 30 kOe to temperatures sufficiently high for the beginning of the α → β transformation. A heating of 15 °C/min was used which was immediately followed by cooling at the rate of 7.5 °C/min; the degree of the phase transformation was measured by in situ monitoring of changes in the sample magnetization. In all the studied alloys, the α → β transformation was found to improve the [0 0 1] fiber texture induced by the applied magnetic field, although it simultaneously decreased the coercivity. A partial transformation has resulted in a 11% increase of the maximum energy product for the Mn 50 Bi 49 Sb 0.5 In 0.5 magnet, to 8.3 MGOe, and a 3% increase for the Mn 50 Bi 46 Mg 3 Sb 0.5 In 0.5 magnet, to 12.8 MGOe. In the latter alloy, the α → β and reverse transformations were found to initially occur in well-defined pockets leading to clusters of large, highly textured α crystallites. In the Mn 50 Bi 48.5 Sb 1.5 magnet, only part of the α phase could be recovered after the transformation, which instead promoted the paramagnetic MnBi 0.9 Sb 0.1 phase.

36 MATERIALS SCIENCE↗

The role of ternary alloying elements in eutectoid transformation of U10Mo alloy part I. Microstructure evolution during arc melting and subsequent homogenization annealing in U9.8Mo0.2 X alloy ( X = Cr, Ni, Co)

This paper describes the microstructural evolution in an alloy of uranium with 10 wt.% molybdenum (U10Mo), with minor addition of a third alloying element, namely, Cr, Ni, or Co, at 0.2 wt.%. The microstructures of arc-melted buttons in the as-cast condition show significant Mo segregation. The segregation behavior of Cr, Ni, and Co was investigated through detailed scanning electron microscope imaging. A homogenization heat treatment at 900°C for 48 h results in uniform Mo distribution and associated grain growth in all of the four alloys that were fabricated. Further, formation of multiple phases was noted in U-9.8 wt.% Mo-0.2 wt.% Ni and U-9.8 wt.% Mo-0.2 wt.% Co alloys after the homogenization annealing step. The greatest grain-boundary-initiated eutectoid transformation as measured by % volume fraction was observed when the homogenized U-9.8 wt.% Mo-0.2 wt.% Ni alloy was aged at 500°C for 20 h. The least eutectoid transformation occurred in U10Mo.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Enhanced thermoelectric performance and novel nanopores in AgSbTe{sub 2} prepared by melt spinning

We report a melt-spinning spark-plasma-sintering synthesis process of the polycrystalline p-type material composed of AgSbTe{sub 2} coarse grains and evenly formed 5-10 nm pores that occur primarily on the surface of matrix grains. The formation mechanism of nanopores and their influences on the thermoelectric properties have been studied and correlated. Microstructure analysis shows that the as-prepared sample can be regarded as a nanocomposite of matrix and in situ generated nanopores evenly coated on matrix grains. For the single-phase component and the possible energy-filter effect caused by the nanopores, the electrical transport properties are improved. Moreover, the thermal conductivity is significantly reduced by strong phonon scattering effect resulted from the nanopores. The thermoelectric performance of the as prepared sample enhances greatly and a ZT of 1.65 at 570 K is achieved, increasing{approx}200% compared with the sample prepared by traditional melt and slow-cooling method. -- Graphical abstract: Representative nanostructure of AgSbTe{sub 2} sample (a) ribbons obtained after melt spinning (b) bulk AgSbTe{sub 2} material obtained after spark plasma sintering. Display Omitted

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Microstructural and mechanical characterization of various modified 7XXX series spray formed alloys

Microstructural analysis was conducted on the second phase constituent particles in various modified 7XXX series alloys produced by spray forming. High gas-to-metal ratios of 4.45, as opposed to low gas-to-metal ratios of 1.95, were found to produce a more refined grain structure with an evenly distributed second phase. To elucidate the influence of Zn, Cr, Cu and Zr additions on the microstructure, five different alloy compositions were chosen. The microstructure after extrusion and aging was studied using optical, scanning and transmission electron microscopy. The coarse constituent particles were found to be Al{sub 6}(MnFe) and Al{sub 7}Cu{sub 2}Fe. Two different types of dispersoids were identified; fine, of the L1{sub 2} type (Al{sub 3}Zr) and larger dispersoids of the Al{sub 18}Mg{sub 3}Cr{sub 2} compound referred to as the E-Phase. Room temperature mechanical properties of spray formed Al-Zn-Mg-Cu alloys were investigated in the T6 and T7 aged condition. Variations in structural particle concentration were found based on aging and composition type.

36 MATERIALS SCIENCE↗

Evolution of the microstructure and hardness of a rapidly solidified/melt-spun AZ91 alloy upon aging at different temperatures

The effect of aging at different temperatures on a rapidly solidified/melt-spun AZ91 alloy has been investigated in depth. The microstructures of as-spun and aged ribbons with a thickness of approximately 60 {mu}m were characterized using X-ray diffraction, transmission electron microscopy and laser optical microscopy; microhardness measurements were also conducted. It was found that the commercial AZ91 alloy undergoes a cellular/dendritic transition during melt-spinning at a speed of 34 m/s. A strengthening effect due to aging was observed: a maximum hardness of 110 HV/0.05 and an age-hardenability of 50% were obtained when the ribbon was aged at 200 deg. C for 20 min. The {beta}-Mg{sub 17}Al{sub 12} phase exhibits net and dispersion types of distribution during precipitation. The dispersion of precipitates in dendritic grains or cells is the main source of strengthening.

36 MATERIALS SCIENCE↗

Dendritic coarsening of {gamma}' phase in a directionally solidified superalloy during 24,000 h of exposure at 1173 K

Dendritic coarsening of {gamma}' was investigated in a directionally solidified Ni-base superalloy during exposure at 1173 K for 24,000 h. Chemical homogeneity along different directions and residual internal strain in the experimental superalloy were measured by electronic probe microanalysis (EPMA) and electron back-scattered diffraction (EBSD) technique. It was indicated that the gradient of element distribution was anisotropic and the inner strain between dendrite core and interdendritic regions was different even after 24,000 h of exposure at 1173 K, which influenced the kinetics for the dendrite coarsening of {gamma}' phase.

36 MATERIALS SCIENCE↗

Investigation on microstructure characterization and property of rapidly solidified Mg-Zn-Ca-Ce-La alloys

Rapidly solidified (RS) Mg-Zn-Ca-Ce-La (wt.%) alloys have been produced via atomizing the alloy melt and subsequent splat-quenching on the water-cooled copper twin-rollers in the form of flakes. Microstructure characterization, phase compositions and thermal stability of the alloys have been systematically investigated. The results showed that with addition of RE (Ce and La) to the Mg-6Zn-5Ca alloy, the stable intermetallic compounds i.e. the Mg{sub x}Zn{sub y}RE{sub z} phase with a few Ca (about 3 at.%), shortened as the T Prime phase, were formed at the expense of the binary Mg-Zn and Ca{sub 2}Mg{sub 6}Zn{sub 3} phases, which was possibly beneficial to the enhanced thermal stability of the alloy. In the Mg-6Zn-5Ca-3Ce-0.5La alloy, the composition of the T Prime phase in the grain interior was different from that at the grain boundaries, in which the segregation of the La elements was found, and the atomic percentage ratio of Zn to Ce in the T Prime phase within the grains was close to 2. Moreover, the stable Mg{sub 2}Ca phases were detected around the T Prime phases at the grain boundaries in the alloy. - Research Highlights: Black-Right-Pointing-Pointer The phase constitution of RS Mg-6Zn-5Ca alloy can be improved by RE additions. Black-Right-Pointing-Pointer In the Mg-Zn-Ca-Ce-La alloys, the Mg{sub x}Zn{sub y}RE{sub z} phase with a few Ca (T Prime phase) is formed. Black-Right-Pointing-Pointer The formation of the T Prime phase leads to the loss of the Mg-Zn and Ca{sub 2}Mg{sub 6}Zn{sub 3} phases. Black-Right-Pointing-Pointer The composition of the T Prime phase differs from the grain interior to the grain boundary.

36 MATERIALS SCIENCE↗

Properties of the thermally stable Al{sub 95}Cr{sub 3.1}Fe{sub 1.1}Ti{sub 0.8} alloy prepared by cold-compression at ultra-high pressure and by hot-extrusion

An Al{sub 95}Cr{sub 3.1}Fe{sub 1.1}Ti{sub 0.8} (in at.%) alloy was made into rapidly solidified powder by melt atomization. The powder was compacted by two processes: 1) uni-axial cold compression at an ultra-high pressure of 6 GPa and 2) hot extrusion at 480 Degree-Sign C. The structures, mechanical properties and thermal stability of both materials were compared with the commercial AlSi{sub 12}Cu{sub 1}Mg{sub 1}Ni{sub 1} (in wt.%) casting alloy, which is generally considered to be thermally stable. It was found that cold compression at ultra-high pressure created a compact and porosity-free material, which was similar to the material that was prepared with the commonly used hot extrusion method. The Vickers hardness, compressive strength and compressive yield strength of the cold-compressed alloy were 161 HV, 680 MPa and 547 MPa, respectively, which were higher than the values obtained for the hot-extruded and casting alloys. The thermal stability of the hot-extruded Al{sub 95}Cr{sub 3.1}Fe{sub 1.1}Ti{sub 0.8} alloy was excellent because its mechanical properties did not change significantly, even after 100 h of annealing at 500 Degree-Sign C. The mechanical properties and thermal stability of the investigated materials were discussed in relation to their structures and diffusivities of the alloying elements. - Highlights: Black-Right-Pointing-Pointer The Al{sub 95}Cr{sub 3.1}Fe{sub 1.1}Ti{sub 0.8} alloy was prepared by compression at an ultra-high pressure of 6 GPa. Black-Right-Pointing-Pointer The resulting material was dense and porosity-free. Black-Right-Pointing-Pointer The material had high hardness of 161 HV and a compressive strength of 680 MPa. Black-Right-Pointing-Pointer The material had excellent thermal stability at 500 Degree-Sign C.

36 MATERIALS SCIENCE↗

Microstructural evolution during solution treatment of Co-Cr-Mo-C biocompatible alloys

Three different Co-Cr-Mo-C alloys conforming to ASTM F75 standard were poured in an industrial environment and subjected to a conventional solution treatment at 1225 Degree-Sign C for several time intervals. The microstructural changes and transformations were studied in each case in order to evaluate the way in which treatment time influences the secondary phase fraction and clarify the microstructural changes that could occur. To assess how treatment time affects microstructure, optical microscopy and image analyzer software, scanning electron microscopy and energy dispersion spectrometry analysis were employed. The main phases detected in the as-cast state were: {sigma}-phase, M{sub 6}C, and M{sub 23}C{sub 6} carbides. The latter presented two different morphologies, blocky type and lamellar type. Despite being considered the most detrimental feature to mechanical properties, {sigma}-phase and lamellar carbides dissolution took place in the early stages of solution treatment. M{sub 23}C{sub 6} carbides featured two different behaviors. In the alloy obtained by melting an appropriate quantity of alloyed commercial materials, a decrease in size, spheroidization and transformation into M{sub 6}C carbides were simultaneously observed. In the commercial ASTM F75 alloy, in turn, despite being the same phase, only a marked decrease in precipitates size was noticed. These different behaviors could be ascribed to the initial presence of other phases in the alloy obtained from alloyed materials, such as {sigma}-phase and 'pearlitic' carbides, or to the initial precipitate size which was much larger in the first than in the commercial ASTM F75 alloy studied. M{sub 6}C carbides dissolved directly in the matrix as they could not be detected in samples solution-treated for 15 min. - Highlights: Black-Right-Pointing-Pointer Three different Co-Cr-Mo alloys were poured under an industrial environment. Black-Right-Pointing-Pointer Transformation of existing phases followed during conventional solution treatment. Black-Right-Pointing-Pointer In as-cast/treated samples, phases were identified by color metallography, SEM and EDS. Black-Right-Pointing-Pointer M{sub 23}C{sub 6} {yields} M{sub 6}C transformation was corroborated by SEM and EDS analysis. Black-Right-Pointing-Pointer Carbide spheroidization was also detected prior a noticeably carbide size decreasing.

36 MATERIALS SCIENCE↗

Effect of cooling rate and Mg addition on the structural evaluation of rapidly solidified Al-20wt%Cu-12wt%Fe alloy

The present work examines the effect of Mg contents and cooling rate on the morphology and mechanical properties of Al{sub 20}Cu{sub 12}Fe quasicrystalline alloy. The microstructure of the alloys was analyzed by scanning electron microscopy and the phase composition was identified by X-ray diffractometry. The melting characteristics were studied by differential thermal analysis under an Ar atmosphere. The mechanical features of the melt-spun and conventionally solidified alloys were tested by tensile-strength test and Vickers micro-hardness test. It was found that the final microstructure of the Al{sub 20}Cu{sub 12}Fe samples mainly depends on the cooling rate and Mg contents, which suggests that different cooling rates and Mg contents produce different microstructures and properties. The average grain sizes of the melt spun samples were about 100–300 nm at 35 m/s. The nanosize, dispersed, different shaped quasicrystal particles possessed a remarkable effect to the mechanical characteristics of the rapidly solidified ribbons. The microhardness values of the melt spun samples were approximately 18% higher than those of the conventionally counterparts. - Highlights: •Quasicrystal-creating materials have high potential for applications. •Different shaped nanosize quasicrystal particles were observed. •The addition of Mg has an important impact on the mechanical properties. •H{sub V} values of the MS0, MS3 and MS5 samples at 35 m/s were 8.56, 8.66 and 8.80 GPa. •The volume fraction of IQC increases with increasing cooling rates.

36 MATERIALS SCIENCE↗

Assessment of phase constitution on the Al-rich region of rapidly solidified Al-Co-Fe-Cr alloys

The formation of quasicrystalline approximants in rapidly solidified Al-Co-Fe-Cr alloys was investigated. Alloys of atomic composition Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8}, Al{sub 77}Co{sub 11}Fe{sub 6}Cr{sub 6} and Al{sub 76}Co{sub 19}Fe{sub 4}Cr{sub 1} were produced using melt spinning and arc melting methods and their microstructural characterization was carried out by X-ray diffraction, scanning electron microscopy and transmission electron microscopy. Up to the present there is no consensus in the literature regarding the formation of quasicrystalline phase or quasicrystalline approximants in the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} alloy. This work presents, for the first time, a detailed structural characterization of selected alloys in the Al-Co-Fe-Cr system close to the atomic composition Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8}. The results indicated the samples to be composed, mostly, by two intermetallic phases, which are quaternary extensions of Al{sub 5}Co{sub 2} and Al{sub 13}Co{sub 4} and are quasicrystalline approximants. Although the Al{sub 5}Co{sub 2} phase has already been reported in the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} alloy, the presence of the monoclinic Al{sub 13}Co{sub 4} is now identified for the first time in the as cast state. In the binary Al-Co system a quasicrystalline phase is known to form in a rapidly solidified alloy with composition close to the monoclinic and orthorhombic Al{sub 13}Co{sub 4} phases. This binary quasicrystalline phase presents an average valence electron per atom (e/a) between 1.7 and 1.9; thus, in addition to the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} alloy, the compositions Al{sub 77}Co{sub 11}Fe{sub 6}Cr{sub 6} and Al{sub 76}Co{sub 19}Fe{sub 4}Cr{sub 1} were chosen to be within the region of formation of the quaternary extension of the Al{sub 13}Co{sub 4} phase and also within the (e/a) of 1.7 to 1.9. However, no quasicrystalline phase is present in any of the studied alloys. The Al-Co-Fe-Cr system, around the compositions studied, is composed of quaternary extensions of Al-Co intermetallic phases, which present solubility of Fe and Cr at Co atomic sites. - Highlights: •The Al rich region of the AlCoFeCr system is studied concerning phase formation on rapidly solidified alloys. •The alloys were composed mostly by quaternary extensions of Al-Co intermetallic phases. •Al{sub 5}Co{sub 2} and Al{sub 13}Co{sub 4} were the major phases observed in the alloys and are approximants of a quasicrystalline phase. •No quasicrystalline phase was observed in the Al{sub 71}Co{sub 13}Fe{sub 8}Cr{sub 8} composition.

36 MATERIALS SCIENCE↗

Nano-phase formation accompanying phase separation in undercooled CoCrCuFeNi-3 at.% Sn high entropy alloy

Highlights: • Undercooled multi-component CoCrCuFeNi-3 at.% Sn high-entropy alloy was studied. • Accompanying phase separation, the nano-precipitates were detected. • The effect of Sn on the microstructures and properties was clarified. • The microhardness increased markedly with the increase of undercooling. - Abstract: Highly undercooled multi-component CoCrCuFeNi-3 at.% Sn high-entropy alloy was studied by adopting molten glass purification combined with cycle superheating methods. Based on the critical undercooling ΔT{sup ⁎}, the characteristic of liquid-phase separation was researched at different undercoolings. Accompanying phase separation, two phases (CoCrFeNi-rich and CuNi-rich) and three kinds of nano-precipitates (CrCo-rich, CrSn-rich and Sn-rich nano-precipitates) were detected. The microhardness of undercooled CoCrCuFeNi-3 at.% Sn high-entropy alloys increased markedly with the increase of undercooling. The effect of Sn on the microstructure evolution and properties in the process of phase separation was clarified with the aid of nano-precipitates.

36 MATERIALS SCIENCE↗