Search NASA⌕ Search

SEARCH · Search NASA

Results for “dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,585 records · Page 88

Atomic-scale identification of defects in alite

Crystallographic defects play a crucial role in cement hydration, with initial dissolution being dominated by the formation of etch pits that rely on the intersection of defects on surfaces. However, the defects present in cement particles have remained a mystery due to the lack of detailed direct observation at the atomic scale. In this study, we used scanning transmission electron microscopy to unravel the defects in alite particles at the single-atom level. Our observations identified different types of defects, including vacancies, doping, dislocations, rough surfaces, and grain boundaries. Atomic ordering in the alite crystal was further examined based on our single-atom recognition method. Our findings indicate that defects in cement particles may serve as reactive sites during the early hydration stage, facilitating the initial dissolution and providing nucleation sites for hydration products. Finally, this work provides insights into cement defect formation at the single-atom level and offers new opportunities in tuning the hydration process through defect engineering of cement particles.

36 MATERIALS SCIENCE↗

Cold-cap formation from a slurry feed during nuclear waste vitrification

The time-temperature history of waste slurry feed during melting strongly affects various kinetic processes, such as reaction or dissolution rates, and, consequently, the melting rate. To analyze the time-temperature history of the feed in a cold-cap during nuclear waste vitrification, this work focuses on understanding how the main coldcap body forms, how the aqueous feed slurry interacts with the cold-cap, and estimating the cold-cap heat conductivity. To simulate the conditions during cold-cap formation, samples were prepared by rapid water evaporation from slurry feed. After water evaporated from the sample, a fresh slurry with tracer was poured onto the dry sample. X-ray fluorescence was then used to investigate the degree of penetration and/or mixing between the incoming slurry and the original sample. We show that the slurry does not interact or mix with the previously dry cold-cap crust, but that water-soluble components concentrate at the bottom of the boiling pools, where most of the water evaporates. Further, using the rate of water evaporation, the heat conductivity of the cold-cap was calculated from the measured temperature profile. The resulting conductivity is significantly higher than the values obtained in previous studies. We discuss the implications of the results for the cold-cap formation in the melter and for the development of the cold-cap mathematical model.

Hujova, Miroslava↗

The Controversial Role of Inter-diffusion in Glass Alteration

Current kinetic models for nuclear waste glasses (e.g. GM2001, GRAAL) are based on a set of mechanisms that have been generally agreed upon within the international waste glass community. These mechanisms are: hydration of the glass, ion exchange reactions (the two processes are referred as inter-diffusion), hydrolysis of the silicate network, and condensation/precipitation of partly or completely hydrolyzed species that produces a porous and amorphous layer and crystalline phases on surface of the altered glass. Recently, a new idea with origins in the mineral dissolution community has been proposed that excludes inter-diffusion process as a potential rate-limiting mechanism. To understand how the so-called interfacial dissolution/precipitation model can change the current understanding of glass behavior, a key experiment used to account for this model was replicated to further revisit the interpretation. This experiment was performed at 50°C, with SON68 glass, in static mode, deionized water and S/V ratio of 10 m-1 for 6 months. It turn out that glass alters in an intermediate kinetic regime between the forward and the residual rate. According to previous and new solid characterizations, it is concluded that neither a simple inter-diffusion model nor the interfacial dissolution precipitation model can account for the observed elemental profiles within the alteration layer. More generally, far and close-to-saturation conditions must be distinguished and literature provides evidences that inter-diffusion takes place in slightly acidic conditions and far from saturation. However, closer to saturation, when a sufficiently dense layer is formed, a new approach is proposed requiring a full description of chemical reactions taking place within the alteration layer and involving water molecules as it is thought that water accessibility to the pristine glass is the rate-limiting process.

Gin, Stephane↗

Comparative geochemistry of flowback chemistry from the Utica/Point Pleasant and Marcellus formations

Flowback/Produced fluid samples were collected from several wells from two Utica/Point Pleasant (UPP) sites (UPPW and UPPS) in Ohio, and one Marcellus (Marcellus Shale Energy and Environment Laboratory (MSEEL)) site in West Virginia over a period of approximately two years. Although these formations have different ages, depositional environments, diagenetic histories, and geochemical and mineralogical compositions (i.e. the UPP is significantly more carbonate rich than the Marcellus which is more siliceous), analysis of trends in fluid species over time shows that, overall, the TDS and major solubilized elements (Na, Ca, Cl) in the UPP and Marcellus brines are remarkably similar. Total dissolved solutes (TDS) in these brines ranged from approximately 40 to 250 g/L salt, and in general, concentrations increased with time elapsed since natural gas well completion and stimulation. The behavior of Na, Br, and Cl suggests that the produced water signatures from these formations are largely derived from the native formational brines which display evidence of originating from evaporated seawater. There is a strong correlation between Cl and Br, indicating that both species behave conservatively, and the similarity among each of these brines suggests no appreciable contribution of salt from halite dissolution because Br is excluded from the halite structure. Cl/Br ratios in the brines range from ~80 to 120 (mg/L/mg/L). Other elements, such as K, which readily reacts between fluids and ion exchange sites on clays, generally exhibit conservative behavior for an individual site, but show significant variations among each of the different well pads. The concentrations of Sr and Ba vary dramatically among well sites, and increase with respect to Cl- over time, suggesting increasing solubilization, presumably from desorption from clay minerals or dissolution of carbonates or sulfates from the source formation(s). The UPPW well site has very low Ba due to high-sulfate input fluid, which resulted in precipitation of barite/celestite in the brines. In contrast the UPPS well site had elevated Sr (~ 3500 mg/L), presumably due to the use of Sr-rich recycled brine used in hydraulic fracturing. The Marcellus site had the highest Ba concentrations (up to 10 g/L) and highest Ba/Sr ratios in the fluids, due to the high concentration of barium in the Marcellus target (~ 1000 ppm, as compared to ~200 ppm in the UPP). These observations suggest that solutes in the FP fluids are derived from native brines, water-rock interactions that have occurred over geologic time scales, as well as some contribution from contemporaneous reactions in the subsurface. The results also show that the composition of the injected fluid can influence flowback fluid chemistry and possibly production efficiency.

58 GEOSCIENCES↗

Recent developments in catalyst-related PEM fuel cell durability

Cost and durability remain the two major barriers to the widespread commercialization of polymer electrolyte membrane fuel cell (PEMFC)-based power systems, especially for the most impactful but challenging fuel cell electric vehicle (FCEV) application. Commercial FCEVs are now on the road; however, their PEMFC systems do not meet the cost targets established by the U.S. Department of Energy, primarily due to the high platinum loading needed on the cathode to achieve the requisite performance and lifetime. Furthermore, while the activities of a number of commercial Pt-based alloy cathode catalysts exceed the beginning-of-life (BOL) targets, these activities, and the overall cathode performance, degrade via a variety of mechanisms described herein. Degradation is mitigated in current FCEVs by utilizing a cathode catalyst with a lower BOL activity (e.g., much lower transition metal alloy content and larger BOL nanoparticle size), necessitating higher catalyst loadings, and through the utilization of system controls that avoid conditions known to exacerbate degradation processes, such as limiting the fuel cell stack voltage range. The design and development of active and robust materials and eliminating the need for vehicle mitigation strategies would greatly simplify the operating system, allowing for greater transient operation, avoiding large hybridization, and curtailing of fuel cell power. Although system mitigation strategies have provided the near-term pathway for FCEV commercialization, material-specific solutions are required to further reduce costs and improve operability and efficiency. Future material developments should focus on stabilization of the electrode structure and minimization of the catalyst particle susceptibility to dissolution caused by oxide formation and reduction over PEMFC cathode-relevant operating potentials plus minimization of support corrosion. Ex situ accelerated stress tests have provided insight into the processes responsible for material and performance degradation and will continue to provide useful information on the relative stability of materials and benchmarks for robust and stable materials-based solutions not requiring system mitigation strategies to achieve adequate lifetime.

25 ENERGY STORAGE↗

Application of a temporal multiscale method for efficient simulation of degradation in PEM Water Electrolysis under dynamic operating conditions

Hydrogen is emerging as a vital energy carrier, driven by the need to reduce carbon emissions. Proton Electrolyte Membrane Water Electrolysis (PEMWE) enables hydrogen production under fluctuating renewable power conditions but requires improved understanding and stability of the anode catalyst layer under dynamic operating conditions, especially with low noble metal loadings. Long-term degradation experiments are both time-consuming and costly; therefore, a systematic, model-aided approach is essential. In the present work, a temporal multiscale method is applied to reduce the computational effort of simulating long-term degradation processes in PEMWE, with an exemplary focus on catalyst dissolution. A mechanistic model incorporating the oxygen evolution reaction, catalyst dissolution, and hydrogen permeation from the cathode to the anode was hypothesized and implemented. In this way, the local periodicity of transport and reaction processes in dynamic PEMWE operation, which influence the gradual degradation of the catalyst layer, is captured. The temporal multiscale method significantly reduces the computational effort of simulation, decreasing processing time from hours to mere minutes. This efficiency gain is attributed to the limited evolution of Slow-Scale variables during each period of time P of the Fast-Scale variables. Consequently, simulation is required only until local periodicity is achieved within each Slow-Scale time step. Hence, the fully resolved dynamic problem is decoupled into these two scales, employing a heterogeneous multiscale technique. The developed approach effectively accelerates parameter estimation and predictive simulations, supporting systematic modeling of PEMWE degradation under dynamic conditions.

08 HYDROGEN↗

Cryo-based Structural Characterization and Growth Model of Salt Film on Metal

Metal salt films play a critical role in high rate dissolution processes such as within an active pit. However, structural and compositional characterization of salt films is challenging owing to the dynamic nature of the dissolving interface. Here, the salt film formed on SS304 one-dimensional artificial pit surface was directly characterized using flash freezing and cryo-based focused ion beam/scanning electron microscopy. The salt film exhibits a porous structure. Ni is co-located with Fe in the salt film, indicating the formation of co-precipitated salt containing Fe2+ and Ni2+. Additionally, a salt film growth model is presented based on ion transport.

Salt film, Pitting corrosion, Cryogenic, Cryo-FIB/↗

Environmental degradation of electroplated nickel and copper coated SS316H in molten FLiNaK salt

Corrosion of nickel and copper electroplated coatings on SS316H in molten FLiNaK salt was studied. 500- and 1000-hour static corrosion tests were performed in molten FLiNaK at 700 degrees Celsius. Characterization of the coatings following corrosion indicated that they did not degrade in the molten salt during the corrosion experiment and fully protected the underlying SS316H from chromium dissolution. Interdiffusion between the copper coating and SS316H was extremely limited, interdiffusion between the nickel coating and SS316H. Diffusion modelling revealed that the nickel coatings still significantly reduced chromium dissolution over 60 years despite the interdiffusion.

36 MATERIALS SCIENCE↗

Corrosion characteristics of Mo and TZM alloy for plasma facing components in molten lithium at 623 K

Here, in this study, the corrosion behaviours of molybdenum (Mo) and a Mo-based alloy (TZM) were investigated using a static immersion corrosion technique. Weight loss, surface microstructure, and corrosion depth of Mo and the TZM alloy were correlated with elements. The compatibility of Mo and the TZM alloy in static liquid Li was suitable. Mo demonstrated uniform corrosion with a homogenous dissolution of free C and Mo, and TZM alloy exhibited a nonuniform corrosion behaviour with a preferential grain boundary attack caused by the selective dissolution of free C, Ti, and Zr. When the surface oxidation layer of the samples was consumed, free C from Mo and TZM diffused into molten Li to form Li 2 C 2 and then was captured by Zr, Ti, and Mo to form thermodynamically stable carbides, which resulted in the enrichment of the C layer near the sample surfaces. In addition, Ti and Zr acted as N-trappers in liquid Li; the formation of Zr and Ti nitrides resulted in the enrichment of N, Ti, and Zr elements on the surface and led to TZM corrosion increase. Thus, Zr and Ti depletion, pitting, and grain boundary corrosion were problematic for TZM under long-term exposure to liquid Li. Reducing the content of free C and nonmetallic N and increasing the amount of Ti and Zr carbides on the surface of and inside the raw TZM alloy helped improve the corrosion resistance of TZM in liquid Li.

36 MATERIALS SCIENCE↗

Hot corrosion behavior of 304 & P91 graded composite transition joint under molten sulfate salts

A novel graded composite transition joint (GCTJ) between AISI 304 stainless steel and ASTM A335 P91 steel, has been demonstrated remarkablely superior creep performance compared to the conventional dissimilar metal weldment (DMW) under equivalent conditions. However, this advance is challenged by hot corrosion under salt deposition at elevated temperatures. Here, this study investigates the hot corrosion behavior of 304&P91 GCTJ exposed to sulfate salts at 700°C. Compared to the 304 steel, corrosion attacks initiate in the P91 triangle, where the dual-phase microstructure of ferrite and tempered martensite significantly influences pitting initiation. Anodic dissolution mainly occurs within the tempered martensite due to more vulnerable sites within the tempered martensite. With prolonged exposure, corrosion propagates across both phases, and the corrosion depth within the P91 triangle is related to the exposed surface area ratio between 304 and P91. Electrochemical analysis reveals the occurrence of galvanic corrosion between the 304 and P91, with a positive linear relationship between anodic dissolution current density (I a ) and the exposed surface area ratio between 304 and P91 in molten salts, further emphasizing the critical impact of this ratio on the corrosion severity in the P91 triangle. These findings underscore the importance of transition zone design optimization in mitigating localized corrosion.

Galvanic corrosion↗

Understanding the high-temperature behavior and corrosion resistance of Cr-Nb coated cladding for BWRs

While Cr-coated Accident Tolerant Fuel has proven successful in Pressurized Water Reactors, its dissolution in high dissolved oxygen Boiling Water Reactor environments represents a major technological barrier. Here, this study presents a comprehensive evaluation of novel Cr-Nb alloys as a coating breakthrough solution for Accident Tolerant Fuel cladding in Boiling Water Reactors. We systematically investigated Physical Vapor Deposited Cr-Nb coatings with 13% and 24 at% Nb content on commercial Zr-based cladding through rigorous testing under both normal and accident conditions. Our results demonstrate Cr-Nb coatings remained completely intact during extended Boiling Water Reactor autoclave testing, while pure Cr coatings failed catastrophically due to oxide dissolution. Under Loss-of-Coolant Accident conditions at 1100°C, Cr-Nb coatings maintained protective capability for 45 min. At 800°C, the alloy coatings matched pure Cr's excellent corrosion resistance. Despite microstructural changes during prolonged high-temperature exposure, no coating delamination occurred, ensuring continued protection of the underlying Zr substrate. These findings establish Cr-Nb coatings as a viable Accident Tolerant Fuel solution for Boiling Water Reactors.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Inorganic Carbon Turnover caused by Digestion of Carbonate Sands and Metabolic Activity of Holothurians

Recent measurements have shown that holothurians (sea cucumbers) play an important role in the cycling of CaCO3 in tropical coral reef systems through ingestion and processing of carbonate sediment. In this study inorganic additional aspects of carbon turnover were determined in laboratory incubations of Holothuria atra, H. leucospilota and Stichopus herrmanni from One Tree Reef, Great Barrier Reef. The pH values of the gut lumen ranged from 6.1 to 6.7 in animals with empty digestive tracts as opposed to 7.0 to 7.6 when digestive tracts were filled with sediment. Empty gut volume estimates for H. atra and S. herrmanni were 36 ± 4 mL and 151 ± 14 mL, respectively. Based on these measurements it is estimated that these species process 19 ± 2kg and 80 ± 7kg CaCO3 sand yr-1 per individual, respectively. The annual dissolution rates of H. atra and S. herrmanni of 6.5±1.9g and 9.6±1.4g, respectively, suggest that 0.05±0.02% and 0.1±0.02% of the CaCO3 processed through their gut annually is dissolved. During the incubations the CaCO3 dissolution was 0.07±0.01%, 0.04±0.01% and 0.21±0.05% of the fecal casts for H. atra, H. leucospilota and S. herrmanni, respectively. The CaCO3 saturation state for both aragonite and calcite minerals during laboratory incubations decreased markedly due to a greater increase in dissolved inorganic carbon (DIC) relative to total alkalinity (AT) as a result of respiration by the animals. Our results support the hypothesis that deposit feeders such as sea cucumbers play an important ecological role in the coral reef CaCO3 cycle.

activity↗

Pt Catalyst Degradation in Aqueous and Fuel Cell Environments studied via In-Operando Anomalous Small-Angle X-ray Scattering

The evolution of Pt nanoparticle cathode electrocatalyst size distribution in a polymer electrolyte membrane fuel cell (PEMFC) was followed during accelerated stress tests using in-operando anomalous small-angle X-ray scattering (ASAXS). This evolution was compared to that observed in an aqueous electrolyte environment using stagnant electrolyte, flowing electrolyte, and flowing electrolyte at elevated temperature to reveal the different degradation trends in the PEMFC and aqueous environments and to determine the relevance of aqueous measurements to the stability of Pt nanoparticle catalyst in the fuel cell environment. The observed changes in the particle size distributions (PSDs) were analyzed to elucidate the extent and mechanisms of particle growth and corresponding mass and active surface area losses in the different environments. These losses indicate a Pt nanoparticle surface area loss mechanism controlled by Pt dissolution, the particle size dependence of Pt dissolution, the loss of dissolved Pt into the membrane and electrolyte, and, to a lesser extent, the re-deposition of dissolved Pt onto larger particles. Based on the geometric surface area loss, mass loss, and mean particle size increase trends, the aqueous environment best reflecting the fuel cell environment was found to be one in which the electrolyte is flowing rather than stagnant. Pt nanoparticle surface area loss resulting from potential cycling can be inhibited by reducing the number of particles smaller than a critical particle diameter (CPD), which was found to be similar to 3.5 to similar to 4 nm, with the CPD dependent on both the cycling protocol (square wave vs triangle wave) and the catalyst environment (fuel cell, aqueous stagnant, aqueous flowing electrolyte, or elevated temperature flowing electrolyte)

Anomalous small-angle X-ray scattering↗

Understanding the Origin of Irreversible Capacity loss in Non-Carbonized Carbonate - based Metal Organic Framework (MOF) Sulfur hosts for Lithium - Sulfur battery

Li-Sulfur (Li-S) batteries are emergent next-generation energy storage devices due to their very high specific energy density (~2567 Wh g -1 ) but are limited by polysulfide dissolution issues. In this paper, chemically synthesized sulfur containing non-carbonized metal organic framework (S-MOF) cathodes show initial specific capacities of 1476 mAh g -1 stabilizing at ~609 mAh g -1 with almost no fade for over 200 cycles. Post-cycled separators of the S – MOF cathodes display complete absence of polysulfides after cycle 1, 20 and 200, respectively. It was identified that the occurrence of carbonate species in the MOF structure resulted in the formation of C-S bonded species causing retention of polysulfide at the electrode surface ensuring long-term stability. However, this observed capacity drop during the first 10 cycles is attributed to the oxidation of some of the infiltrated sulfur by the MOF as determined by electrochemical and X-ray photoelectron spectroscopy (XPS) analyses. Nevertheless, the negligible fade rate (0.0014% cycle -1 ) and complete prevention of polysulfide dissolution renders these cathodes most promising candidates for Li-S batteries. Finally, understanding of this transformation behavior in sulfur-containing MOF is essential to engineer chemically-bonded host-structures capable of efficient polysulfide trapping, a key pathway to establishing novel platforms for achieving high power Li – S batteries.

25 ENERGY STORAGE↗

On the impact of temperatures up to 200°C in clay repositories with bentonite engineer barrier systems: A study with coupled thermal, hydrological, chemical, and mechanical modeling

One of the most important design variables for a geological nuclear waste repository is the temperature limit up to which the engineered barrier system (EBS) and the natural geologic environment can be exposed. Up to now, almost all design concepts that involve bentonite-backfilled emplacement tunnels have chosen a maximum allowable temperature of about 100°C. Such a choice is largely based on the consideration that in clay-based materials illitization and the associated mechanical changes in the bentonite (and perhaps the clay host rock) could affect the barrier attributes of the EBS. However, existing experimental and modeling studies on the occurrence of illitization and related performance impacts are not conclusive, in part because the relevant couplings between the thermal, hydrological, chemical, and mechanical (THMC) processes have not been fully represented in the models. This work presents a fully coupled THMC simulation of a nuclear waste repository in a clay formation with a bentonite-backfilled EBS for 1000 years. Two scenarios were simulated for comparison: a case in which the temperature in the bentonite near the waste canister can reach about 200°C and a case in which the temperature in the bentonite near the waste canister peaks at about 100°C. The model simulations demonstrate some degree of illitization in both the bentonite buffer and the surrounding clay formation. Other chemical alterations include the dissolution of K-feldspar and calcite, and precipitation of quartz, chlorite, and kaolinite. In general, illitization in the bentonite and the clay formation is enhanced at higher temperature. However, the quantity of illitization is affected by many chemical factors and therefore varies a great deal. The most important chemical factors are the concentration of K in the pore water as well as the abundance and dissolution rate of K-feldspar; less important ones are the concentration of sodium and the quartz precipitation rate. In our modeling scenarios, the calculated decrease in smectite volume fraction in bentonite ranges from 1 to 8% of the initial volume fraction of smectite in the 100°C scenario and 1–27% in the 200°C scenario. Chemical changes in the 200°C scenario could also lead to a reduction in swelling stress up to 15–18% whereas those in the 100°C scenario result in about 14–15% reduction in swelling stress for the base case scenario. Model results also show that the 200°C scenario results in a much higher total stress than the 100°C scenario, mostly due to thermal pressurization. While cautions should be taken regarding the model results due to some limitations in the models, the modeling work is illustrative in light of the relative importance of different processes occurring in EBS bentonite and clay formation at higher than 100°C conditions, and could be of greater use when site specific data are available.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Experimental evidence for chemo-mechanical coupling during carbon mineralization in ultramafic rocks

It is known that storing carbon dioxide in the subsurface as carbonate minerals has the benefit of long-term stability and immobility. Ultramafic rock formations have been suggested as a potential reservoir for this type of storage due to the availability of cations to react with dissolved carbon dioxide and the fast reaction rates associated with minerals common in ultramafic formations; however, the rapid reactions have the potential to couple with the mechanical and hydraulic behavior of the rocks and little is known about the extent and mechanisms of this coupling. In this study, we argue that the dissolution of primary minerals and the precipitation of secondary minerals along pre-existing fractures in samples lead to reductions in both the apparent Young's modulus and shear strength of aggregates, accompanied by reduction in permeability. Hydrostatic and triaxial deformation experiments were run on dunite samples saturated with de-ionized water and carbon dioxide-rich solutions while stress, strain, permeability and pore fluid chemistry were monitored. Sample microstructures were examined after reaction and deformation using scanning electron microscopy (SEM). The results show that channelized dissolution and carbonate mineral precipitation in the samples saturated with carbon dioxide-rich solutions modify the structure of grain boundaries, leading to the observed reductions in stiffness, strength and permeability. A geochemical model was run to help interpret fluid chemical data, and we find that the apparent reaction rates in our experiments are faster than rates calculated from powder reactors, suggesting mechanically enhanced reaction rates. In conclusion, we find that chemo-mechanical coupling during carbon mineralization in dunites leads to substantial modification of mechanical and hydraulic behavior that needs to be accounted for in future modeling efforts of in situ carbon mineralization projects.

58 GEOSCIENCES↗

Near-infrared spectroscopic investigation of water in supercritical CO2 and the effect of CaCl2

Near-infrared (NIR) spectroscopy was applied to investigate the dissolution and chemical interaction of water dissolved into supercritical carbon dioxide (scCO2) and the influence of CaCl2 in the co-existing aqueous phase at fo empe e : 40 50 75 nd 100 C at 90 atm. Consistent with the trend of the vapor pressure of water, the solubility of pure water in scCO2 inc e ed f om 40 °C (0.32 mole%) o 100 °C (1.61 mole%). The presence of CaCl2 negatively affects the solubility of water in scCO2: at a given temperature and pressure the solubility of water decreased as the concentration of CaCl2 in the aqueous phase increased, following the trend of the activity of water. A 40 °C, the water concentration in scCO2 in contact with saturated CaCl2 aqueous solution was only 0.16 mole%, a drop of more than 50% as compared to pure water while that a 100 °C was 1.12 mole%, a drop of over 30% as compared to pure water, under otherwise the same conditions. Analysis of the spectral profiles suggested that water dissolved into scCO2 exists in the monomeric form under the evaluated temperature and pressure conditions, for both neat water and CaCl2 solutions. However, its rotational degrees of freedom decrease at lower temperatures due to higher fluid densities, leading to formation of weak H2O:CO2 Lewis acid-base complexes. Similarly, the nearly invariant spectral profiles of dissolved water in the presence and absence of saturated CaCl2 under the same experimental conditions was taken as evidence that CaCl2 dissolution in scCO2 was limited as the dissolved Ca2+/CaCl2 would likely be highly hydrated and would alter the overall spectra of waters in the scCO2 phase.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗