Colossal dielectric constant and relaxation behaviors in Pr:SrTiO{sub 3} ceramics
Sr{sub 1-x}Pr{sub x}TiO{sub 3} ceramics (0.00{<=}x{<=}0.03) were prepared by a traditional solid-state reaction method. Two relaxation processes (marked as A and B) of the Sr{sub 0.09}Pr{sub 0.01}TiO{sub 3} ceramics were investigated by analyzing the E{sub a} values obtained from the Arrhenius law. Colossal dielectric constant (CDC) was first obtained in Sr{sub 0.09}Pr{sub 0.01}TiO{sub 3} ceramics, whose permittivity was up to 3000 (1 kHz, room temperature), greater than that of pure SrTiO{sub 3} ceramics and samples with more Pr addition (x=0.02 and 0.03). This CDC behavior was related to the internal barrier layer capacitance mechanism.