Search NASA⌕ Search

SEARCH · Search NASA

Results for “Adhesion Testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

Replacing Chlorinated-Solvent-Based Cleaners And Adhesives

Brief report describes tests conducted to assess feasibility of using selected chemicals as replacements for selected cleaners, primers, and adhesives containing chlorinated solvents. Cleaners, primers, and adhesives in question used in bonding insulating material in steel cases of solid-fuel rocket motors. Necessary to phase out use of chlorinated solvents because of concerns over toxicity and adverse effects on ozone layer in upper atmosphere.

Heaton, Harley↗

Fatigue life prediction of bonded primary joints

The validation of a proposed fatigue life prediction methodology was sought through the use of aluminum butt and scarf joint and graphite/epoxy butt joint specimens in a constant amplitude fatigue environment. The structural properties of the HYSOL 9313 adhesive system were obtained by mechanical test of molded heat adhesive specimens. Aluminum contoured double cantilever beam specimens were used to generate crack velocity versus stress intensity factor data. The specific objectives were: (1) to ascertain the feasibility of predicting fatigue failure of an adhesive in a primary bonded composite structure by incorporating linear elastic crack growth behavior; and (2) to ascertain if acoustic emission and/or compliance measurement techniques can be used to detect flaws.

Knauss, J. F.↗

Investigation of package sealing using organic adhesives

A systematic study was performed to evaluate the suitability of adhesives for sealing hybrid packages. Selected adhesives were screened on the basis of their ability to seal gold-plated Kovar butterfly-type packages that retain their seal integrity after individual exposures to increasingly severe temperature-humidity environments. Tests were also run using thermal shock, temperature cycling, mechanical shock and temperature aging. The four best adhesives were determined and further tested in a 60 C/98% RH environment and continuously monitored in regard to moisture content. Results are given, however, none of the tested adhesives passed all the tests.

Perkins, K. L.↗

A Study of the Effects of Relative Humidity on Small Particle Adhesion to Surfaces

Ambient dust ranging in size from less than one micron up to 140 microns was used as test particles. Relative humidities of 33% to 100% were used to condition test surfaces after loading with the test particles. A 20 psi nitrogen blowoff was used as the removal mechanism to test for particle adhesion. Particles were counted before and after blowoff to determine retention characteristics. Particle adhesion increased drastically as relative humidity increased above 50%. The greatest adhesion changes occurred within the first hour of conditioning time. Data are presented for total particle adhesion, for particles 10 microns and larger, and 50 microns and larger.

Whitfield, W. J.↗

Surface characterization and adhesion of oxygen plasma-modified LARC-TPI

LARC-TPI, an aromatic thermoplastic polyimide, was exposed to an oxygen plasma as a surface pretreatment for adhesive bonding. Chemical and physical changes which occurred in the polyimide surface as a result of the plasma treatment were investigated using X-ray photoelectron spectroscopy (XPS), infrared reflection-absorption spectroscopy (IR-RAS), contact-angle analysis, ellipsometry, and high resolution SEM. A 180-deg peel test with an acrylate-based pressure sensitive adhesive as a flexible adherent was utilized to study the interactions of the plasma-treated polyimide surface with other polymeric materials. The surface characterization and adhesion testing results showed that the oxygen plasma treatment, while creating a more hydrophilic, polar surface, also caused chain scission, resulting in the formation of a weak boundary layer which inhibited adhesion.

Chin, J. W.↗

The Adhesion Strength of Impact Ice Measured Using a Modified Lap Joint Test

Numerous methodologies have been utilized to measure the adhesion strength of impact ice, and the data reported in the literature varies significantly from test to test. In order to initiate an investigation to determine the cause of this disparity, a new test methodology has been developed and utilized in the Icing Research Tunnel at the NASA Glenn Research Center. Data was obtained while varying the temperature, test section velocity, and cloud droplet mean volumetric diameter. The first data set acquired using this new test method is presented. New trends demonstrate the effect of annealing ice samples, with temperature being a key variable. Observations during the test and analysis of the results suggest the presence of large residual stresses in the samples.

Work, Andrew H., Jr.↗

Evaluation of high temperature structural adhesives for extended service

The evaluation, selection, and demonstration of structural adhesive systems for supersonic cruise research applications, and establishment of environmental durability of selected systems for up to 20,000 hours is described. Ten candidate adhesives were initially evaluated. During screening and evaluation, these candidates were narrowed to three of the most promising for environmental durability testing. The three adhesives were LARC-13, PPQ, and NR056X. The LARC-13 was eliminated because of a lack of stability at 505 K. The NRO56X was removed from the market. The LARC-TPI was added after preliminary evaluation and an abbreviated screening test. Only PPQ and LARC-TPI remained as the reasonable candidates late into the durability testing. Large area bond panels were fabricated to demonstrate the processibility of the selected systems. Specifications were prepared to assure control over critical material and process parameters. Surface characterization concentrated primarily upon titanium surface treatments of 10 volt chronic acid anodize, 5 volt chromic acid anodize and PASA-JELL. Failure analysis was conducted on lap shear adhesive bond failures which occurred in PPQ and LARC-13 test specimens after 10,000 hours at 505 K.

Hill, S. G.↗

The effects of inherent flaws on the time and rate dependent failure of adhesively bonded joints

Inherent flaws, as well as the effects of rate and time, are shown by tests on viscoelastic adhesive-bonded single lap joints to be as critical in joint failure as environmental and stress concentration effects, with random inherent flaws and loading rate changes resulting in an up to 40% reduction in joint strength. It is also found that the asymptotic creep stress, below which no delayed failure may occur, may under creep loading be as much as 45% less than maximum adhesive strength. Attention is given to test results for the case of titanium-LARC-3 adhesive single-lap specimens.

Sancaktar, E.↗

Effect Of Molecular Weight On Adhesive Properties Of The Phenylethynyl-Terminated Polyimide LARC(sup TM)-PETI-5

Future civilian aircraft will require the use of advanced adhesive systems with high temperature capabilities. One such material has been developed at the NASA Langley Research Center, a phenylethynyl-terminated polyimide given the designation LARC(sup TM)-PETI-5. Recent work has shown the advantages of similar phenylethynyl-terminated polyimides as films, moldings, adhesives, and composite matrix resins. Phenylethynyl-terminated oligomers provide greater processing windows than materials which incorporate simple ethynyl endcaps. Since these low molecular weight, low melt viscosity oligomers thermally cure without the evolution of volatile by-products, they provide an excellent means of producing polymers with high glass transition temperatures, excellent solvent resistance, and high mechanical properties. Three different versions of LARC(sup TM)-PETI-5 with theoretical number average molecular weights (M(sub n)s) of 250, 5000, and 10000 g/mol were synthesized in this work. Differential Scanning Calorimetry (DSC) measurements were performed on the dry powder form of these materials to establish cure conditions which result in high glass transition temperatures (T(sub g)s). Lap shear specimens were prepared from adhesive tape made from each material and with the thermal cure conditions determined from the DSC data. The tensile shear data established processing conditions which provided the best adhesive strengths. Further testing was performed to establish the properties of LARC(sup TM)-PETI-5 as an adhesive material and to determine its solvent resistance.

Cano, Roberto J.↗

Polymer adhesives for hybrid circuits

Report discusses number of tests used in comparing polymer adhesives with metal bonding processes and includes charts and photographs to illustrate test results. Findings suggest reduced quality control costs when epoxies are used in fabrication of microcircuits.

Caruso, S. V.↗

Residual Silicone Detection

Both photoelectron emission and ellipsometry proved successful in detecting silicone contamination on unpainted and epoxy painted metal surfaces such as those of the external tank and the solid rocket booster. Great success was achieved using photoelectron emission (PEE). Panels were deliberately contaminated to controlled levels and then mapped with PEE to reveal the areas and levels that were contaminated. The panels were then tested with regard to adhesive properties. Tapes were bonded over the contaminated and uncontaminated regions and the peel force was measured, or the contaminated panels were bonded (with CPR 483 foam) to uncontaminated panels and made into lap shear specimens. Other panels were bonded and made into wedge specimens for hydrothermal stress endurance tests. Strong adhesion resulted if the PEE signal fell within an acceptance window, but was poor outside the acceptance window. A prototype instrument is being prepared which can automatically be scanned over the external liquid hydrogen tank and identify those regions that are contaminated and will cause bond degradation.

Smith, T.↗

A fundamental approach to the sticking of insect residues to aircraft wings

A proposed testing scheme is described for obtaining data on the effects of surface roughness and surface energy on insect adhesion. The road test apparatus is discussed as well as surface preparation techniques. Uncoated and polymer coated metal substrates were analyzed by SEM/ESCA/IRS before and following collision with insects. Critical surface tensions of unexposed Nyebar and poly sulfone coatings were 10 and 33 dynes/cm, respectively, as determined from contact angles. A total of 95% of insect residues collected belong to order Diptera. Significantly less insect debris was detected on the coated plates as compared to the uncoated plates. Minimal contamination at the 5 nm level of both coated and uncoated plates occurs even after hours of exposure to road conditions as determined by ESCA analysis. The presence of nitrogen detected by ESCA on exposed plates is unequivocal evidence for insect residues left on plates.

Eiss, N. S., Jr.↗

Investigating the Adhesion Force of Lunar Regolith Particulates on Air Plasma Sprayed Alumina Coatings

Ceramic materials, often used to protect components due to their high strength, and wear resistance, have added benefits of being lightweight and providing multifunctional properties. They are, therefore, significant to provide durability and support during long-duration missions to the moon’s surface for rovers, landers, robotic systems, habitats, and many other components. Materials such as aluminum oxide with high mechanical strength and hardness can help to improve the durability of structures used in space exploration. Devices used for space exploration require the use of materials with the ability to withstand exposure to extreme environments. Lunar regolith is a constituent with the ability to adhere electrostatically and damage the components used to perform these missions due to adhesion of lunar dust projectiles that can cause delamination on surfaces, which may not be physically visible. The particulates of lunar dust are classified as corrosive material, leading to the degradation of structures. Aluminum oxide presents excellent resistance to different types of wear due to its high strength and hardness. Air plasma sprayed (APS) aluminum oxide coatings have demonstrated the potential to protect the surface to which they are applied. However, the parameters of roughness and porosity of the coatings need to be considered to establish if they can protect the components from extreme environments. Considering the electrostatic forces that the components are exposed to, the adhesion between the lunar regolith and the surface of the components needs to be investigated. In this work, the adhesion forces of lunar dust simulants with an average size of 30 𝜇m are investigated considering the roughness of the surface of the APS aluminum oxide. The centrifugal technique utilized here offers the advantage of establishing the adhesion force between particles with different shapes on smooth or rough surfaces. The simulants were deposited on the surface of APS aluminum oxide using an aerosolization technique to achieve a monolayer coating in three different locations across the specimen to determine the increments in adhesion force at the centrifuge. The roughness of the APS aluminum oxide was determined to be 2.257 𝜇m. The specimen was tested under an incremental centrifugal speed from 100 rpm to 3000 rpm for 20 seconds. Low magnification microscopy images were collected to cover a larger surface area of the test coating. The adhesion force was measured considering the distance from the centrifugal axis and the rotational speed. Due to the coating roughness, and the distance from the centrifugal axis, the results demonstrated a larger adhesion force in locations closer to the centrifugal axis. Smaller particles were entrapped within the roughness of the coating, and a stronger adhesion force was measured. In order to continue designing wear-resistant coating for structural protection in space missions, press-on experiments using a centrifuge will be performed. Future experiments will allow us to determine the design parameters for APS aluminum oxide coating to protect the structures from harsh space environments.

Perla Latorre-Suarez↗

Failure Criterion For Isotropic Time Dependent Materials Which Accounts for Multi-Axial Loading

The Space Shuttle's Reusable Solid Rocket Motor (RSRM) nozzle program has recently conducted testing to characterize the effects of multi-axial loading, temperature and time on the failure characteristics of TIGA321, EA913NA, EA946 (three filled epoxy adhesives). From the test data a "Multi-Axial, Temperature, and Time Dependent" or MATT failure criterion was developed. It is shown that this criterion simplifies, for constant load and constant load rate conditions, into a form that can be easily used for stress analysis. Failure for TIGA321 and EA913NA are characterized below their glass transition temperature. Failure for EA946 is characterized for conditions that pass through its glass transition. The MATT failure criterion is shown to be accurate for a wide range of conditions for these adhesives.

Richardson, D. E.↗

The oxidation behavior of Ni-Cr-Al-2ThO2 alloys at 1093 and 1204 C.

A pack diffusion process has been developed which permits the introduction of nearly 6 wt % Al into solid solution in the near surface region of TDNiCr (Ni-20 wt % Cr-2 vol % ThO2) and Ni-20Cr. Alumina scales, adherent under cyclic heating and cooling conditions, were produced on TDNiCr-5.86Al upon exposure to an environment of 1330 N/sq m (10 torr) or 101,000 N/sq m (760 torr) air at temperatures of 1093 and 1204 C. While the same oxidation kinetics were observed in isothermal tests for Ni-14.6Cr-5.86Al as were obtained for the TDNiCr-5.86Al, the dispersion-strengthened alloy exhibited superior oxide scale adhesion during cyclic testing. At 1204 C, continuous weight gains were observed under all test conditions for TDNiCr-5.86Al, in contrast to the weight loss with time which occurred several hours after exposure of TDNiCr to an oxidizing environment. TDNiCr with an initial aluminum surface concentration of 4.95 wt % has nearly comparable oxidation resistance to the TDNiCr-5.86Al alloy.

Seltzer, M. S.↗

Design, Fabrication and Test of Graphite/Polyimide Composite Joints and Attachments for Advanced Aerospace Vehicles

Standard and advanced bonded joint concepts were evaluated to develop a data base for the design and analysis of advanced composite joints for use at elevated temperatures (561K (550F)). Design concepts for specific joint applications and the fundamental parameters controlling the static strength characteristics of such joints were identified. Test results are presented for rail shear and sandwich beam compression tests and tension tests of moisture conditioned specimens and bonded on "T" sections. Coefficients of thermal expansion data are presented for A7F (LARC 13 Amide-imide modified) adhesion. Static discriminator test results for type 1 and type 2 bonded and bolted preliminary attachment concepts are presented and discussed.

Cushman, J. B.↗