At least 163 records · Page 9

Partial-Vacuum-Gasketed Electrochemical Corrosion Cell

An electrochemical cell for making corrosion measurements has been designed to prevent or reduce crevice corrosion, which is a common source of error in prior such cells. The present cell (see figure) includes an electrolyte reservoir with O-ring-edged opening at the bottom. In preparation for a test, the reservoir, while empty, is pressed down against a horizontal specimen surface to form an O-ring seal. A purge of air or other suitable gas is begun in the reservoir, and the pressure in the reservoir is regulated to maintain a partial vacuum. While maintaining the purge and partial vacuum, and without opening the interior of the reservoir to the atmosphere, the electrolyte is pumped into the reservoir. The reservoir is then slowly lifted a short distance off the specimen. The level of the partial vacuum is chosen such that the differential pressure is just sufficient to keep the electrolyte from flowing out of the reservoir through the small O-ring/specimen gap. Electrochemical measurements are then made. Because there is no gasket (and, hence, no crevice between the specimen and the gasket), crevice corrosion is unlikely to occur.

Bonifas, Andrew P.↗

Solution chemistry effects on the stress corrosion cracking behavior of alloy 2090 (Al-Li-Cu) and alloy 2024 (Al-Cu-Mg)

The SCC initiation behavior of alloys 2090 and 2024 is examined in various NaCl-based environments. The pre-exposure and bulk/local solution chemistry effects discovered by Holroyd et al. (1986) are investigated, with emphasis on the effect of bulk solution chemistries and atmospheric CO2 on the occluded cell environment and the role of the occluded environment in the crack initiation and early-stage propagation processes. It was found that constant immersion in NaCl does not promote SCC in alloy 2090 or alloy 2024. Upon removal from NaCl, SCC is quickly facilitated, but only in the presence of atmospheric CO2. The need for CO2 is attributed to an increase in carbonate concentrations, eventually allowing passivation of blunted fissures by precipitation of Li2CO3. It is inferred that any effects due to aging are small in magnitude, relative to the effects of subtle changes in the bulk/local solution chemistries.

Moran, James P.↗

Testing and Evaluation of Multifunctional Smart Coatings

A smart coating system, based on pH sensitive microcontainers (microparticles and microcapsules) has been developed. Various corrosion inhibitors have been encapsulated and incorporated into commercial and formulated coatings to test the functionality imparted on the coating by the incorporation of the inhibitor microcontainers. Coated carbon steel and aluminum alloy panels were tested using salt immersion, salt fog, and coastal atmospheric exposure conditions. This paper provides the details on coating sample preparation, evaluation methods, as well as test results of the inhibiting function of smart coatings.

Testing and Evaluation↗

SCC of Ti-6Al-4V foil by methanol - Effect of treatments with 2,4-pentanedione and its metal complexes.

The susceptibility of Ti-6Al-4V foil to stress corrosion cracking (SCC) by methanol can be decreased by treatment of the foil with 2,4-pentanedione prior to its immersion in the corroding media. It is assumed that such treatments remove from the protective film formed on the foil by exposure to the atmosphere, certain metal ions whose oxides are more readily penetrated by the ions, Na + and Cl- or Fe(3+) and Cl-, present in the corroding media.

Haney, E. G.↗

Comparison of Simultaneous PIV and Hydroxyl Tagging Velocimetry in Low Velocity Flows

Hydroxyl tagging velocimetry (HTV) is a molecular tagging velocimetry (MTV) technique that relies on the photo- dissociation of water vapor into OH radicals and their subsequent tracking using laser-induced fluorescence. At ambient temperature in air, the OH species lifetime is about 50 micro-s. The feasibility of using HTV for probing low- speed flows (a few m/s) is investigated by using an inert, heated gas as a means to increase the OH species lifetime. Unlike particle-based techniques, MTV does not suffer from tracer settling, which is particularly problematic at low speeds. Furthermore, the flow needs to be seeded with only a small mole fraction of water vapor, making it safer for both the user and facilities than other MTV techniques based on corrosive or toxic chemical tracers. HTV is demonstrated on a steam-seeded nitrogen jet at approximately 75 C in the laminar (Umean=3.31 m/s, Re=1,540), transitional (Umean=4.48 m/s, Re=2,039), and turbulent (Umean=6.91 m/s, Re=3,016) regimes at atmospheric pressure. The measured velocity profiles are compared with particle image velocimetry (PIV) measurements performed simultaneously with a second imager. Seeding for the PIV is achieved by introducing micron-sized water droplets into the flow with the steam; the same laser sheet is used for PIV and HTV to guarantee spatial and temporal overlap of the data. Optimizing each of these methods, however, requires conflicting operating conditions: higher temperatures benefit the HTV signals but reduce the available seed density for the PIV through evaporation. Nevertheless, data are found to agree within 10% for the instantaneous velocity profiles and within 5% for the mean profiles and demonstrate the feasibility of HTV for low-speed flows at moderate to high temperatures.

Andre, Matthieu A.↗

Volatile products in the corrosion of Cr, Mo, Ti and four superalloys exposed to O2 containing H2O and gaseous NaCl

Cooled target collection techniques were used to study the formation of volatile products when samples of Cr, Ti, IN-738, 713C, NASA-TRW VIA and B-1900 were exposed, at elevated temperatures, to oxidizing environments containing H2O(g) and NaCl(g). Samples were heated to 1050 C in one atmosphere of slowly flowing oxygen, saturated with water at 21 C, and containing about 50 ppm NaCl(g). Volatile products were detected for all materials except B-1900 and Ti. High pressure mass spectrometric sampling was used to directly identify volatile products emanating from samples of Cr and IN-738 subject to the above environments.

Fryburg, G. C.↗

Chemical bonding technology for terrestrial photovoltaic modules

Encapsulated photovoltaic modules must hold together for 20 years, reliably resisting delamination and separation of any of the component materials. Delamination of encapsulation materials from each other, or from solar cells and interconnects, can create voids for accumulation of water, promoting corrosive failure. Delamination of silicone elastomers from unprimed surfaces was a common occurrence with early modules, but the incidences of silicone delamination with later modules decreased when adhesion promoters recommended by silicone manufacturers were used. An investigation of silicone delamination from unprimed surfaces successfully identified the mechanism, which was related to atmospheric oxygen and moisture. This early finding indicated that reliance on physical bonding of encapsulation interfaces for long life in an outdoor environment would be risky. For long outdoor life, the material components of a module must therefore be held together by weather-stable adhesion promoters that desirably form strong, interfacial chemical bonds.

Coulter, D. R.↗

Corrosion on Mars: Effect of the Mars Environment on Spacecraft Materials

This report presents the results of a one-year project, funded by NASA’s Kennedy Space Center Innovation Fund in FY18, to conduct a theoretical study on the effect of the Mars environment on spacecraft materials. Corrosion resistance is one of the most important properties in selecting materials for landed spacecraft and structures that will support surface operations for the human exploration of Mars. Currently, the selection of materials is done by assuming that the corrosion behavior of a material on Mars will be the same as that on Earth. This is understandable since there is no data on the corrosion resistance of materials in the Mars environment. However, given that corrosion is defined as the degradation of a metal that results from its chemical interaction with the environment, it cannot be assumed that corrosion is going to be the same in both environments since they are significantly different. The goal of this research was to develop a systematic approach to understand corrosion of spacecraft materials on Mars by conducting a literature search of available data, relevant to corrosion in the Mars environment. This project was motivated by the suggestion, by a team of researchers, that some of the structural degradation observed on Curiosity's wheels may have been caused by corrosive interactions with the transient liquid brines, reported to be present on Mars, while the most significant damage was attributed to rock scratching. An extensive literature search, on data relevant to corrosion on Mars, confirmed the need to investigate the interaction between materials, used for spacecraft and structures designed to support long-term surface operations on Mars, and the Mars environment. Previous preliminary experiments, designed to look at the interaction between aerospace aluminum alloy (AA7075-T73) and the gases present in the Mars atmosphere, at 20 degC and a pressure of 700 Pa, showed that there is an interaction between the small amount of oxygen present in the Mars gas and the alloy, when there is a scratch that removes the protective aluminum oxide film. Further studies are needed to consider many other important components of the Mars environment that can affect this interaction such as: the presence of brines, the interaction between these brines and materials, the effect of radiation on these interactions, and the possible catalytic effects of the clays present in the Martian regolith. This theoretical study provides strong justification to conduct experimental work to investigate the interaction between spacecraft materials with simulated Martian environments to reduce Mars exploration costs.

Calle, Luz M.↗

Analysis of Surveyor 3 television cable

A sample of cable described as four inches of TV cable, fabric wrapped, which had been exposed to the atmosphere for an unknown period of time, was subjected to extensive chemical analyses for the various components. The fabric was tested using attenuated total reflectance, chloroform extract, aqueous extraction, pyrolysis infrared, and reflectance spectroscopy. The wire insulation was tested using pyrolysis infrared, pyrolysis gas chromatography, differential thermal analysis, attenuated total reflectance subsurface, and tensile tests. Corrosion was also observed in parts of certain wires.

Gross, F. C.↗

Supercritical Water Oxidation (SCWO) for the treatment of spacecraft waste.

Supercritical water oxidation (SCWO) is a powerful waste treatment that has been considered as a substitute or complement to other potential spacecraft waste handling methods including jettisoning, compacted sealed storage, drying, and others. Combustible trash and garbage is mixed with water and then heated and pressurized above the critical point of water (705 °F and 218 atmospheres). The waste is nearly all oxidized to produce carbon dioxide, water and nitrogen. NOx is not formed. The combustion energy can be used to heat the input stream. SCWO is relatively complex, expensive, and hazardous compared to other methods. Oxidation of compounds containing chlorine and sulfur produces hydrochloric and sulfuric acid which can cause corrosion in the reactor. Neutralizing these acids produces salts which can precipitate and cause clogging. The major engineering challenges to implementing SCWO are chemical corrosion and fouling due to the deposition of salts. SCWO was first proposed for general waste treatment and for spacecraft in the 1980’s and extensive research has been carried out.

Harry W Jones↗

Evaluation of Stress Corrosion Cracking Susceptibility Using Fracture Mechanics Techniques, Part 1

Stress corrosion cracking (SSC) tests were performed on 13 aluminum alloys, 13 precipitation hardening stainless steels, and two titanium 6Al-4V alloy forgings to compare fracture mechanics techniques with the conventional smooth specimen procedures. Commercially fabricated plate and rolled or forged bars 2 to 2.5-in. thick were tested. Exposures were conducted outdoors in a seacoast atmosphere and in an inland industrial atmosphere to relate the accelerated tests with service type environments. With the fracture mechanics technique tests were made chiefly on bolt loaded fatigue precracked compact tension specimens of the type used for plane-strain fracture toughness tests. Additional tests of the aluminum alloy were performed on ring loaded compact tension specimens and on bolt loaded double cantilever beams. For the smooth specimen procedure 0.125-in. dia. tensile specimens were loaded axially in constant deformation type frames. For both aluminum and steel alloys comparative SCC growth rates obtained from tests of precracked specimens provide an additional useful characterization of the SCC behavior of an alloy.

Sprowls, D. O.↗

Potential Biofilm Control Strategies for Extended Spaceflight Missions

Biofilms, surface-adherent microbial communities, are associated with microbial fouling and corrosion in terrestrial water-distribution systems. Biofilms are also present in human spaceflight, particularly in the Water Recovery System (WRS) on the International Space Station (ISS). The WRS is comprised of the Urine Processor Assembly (UPA) and the Water Processor Assembly (WPA) which together recycles wastewater from human urine and recovered humidity from the ISS atmosphere. These wastewaters and various process streams are continually inoculated with microorganisms primarily arising from the space crew microbiome. Biofilm-related fouling has been encountered and addressed in spacecraft in low Earth orbit, including ISS and the Russian Mir Space Station. However, planned future missions beyond low Earth orbit to the Moon and Mars present additional challenges, as resupplying spare parts or support materials would be impractical and the mission timeline would be in the order of years in the case of a mission to Mars. In addition, future missions are expected to include a period of dormancy in which the WRS would be unused for an extended duration. The concepts developed in this review arose from a workshop including NASA personnel and representatives with biofilm expertise from a wide range of industrial and academic backgrounds. Here, we address current strategies that are employed on Earth for biofilm control, including antifouling coatings and biocides and mechanisms for mitigating biofilm growth and damage. These ideas are presented in the context of their applicability to spaceflight and identify proposed new topics of biofilm control that need to be addressed in order to facilitate future extended, crewed, spaceflight missions.

Luis Zea↗

Sulfur "Concrete" for Lunar Applications - Sublimation Concerns

Melting sulfur and mixing it with an aggregate to form "concrete" is commercially well established and constitutes a material that is particularly well-suited for use in corrosive environments. Discovery of the mineral troilite (FeS) on the moon poses the question of extracting the sulfur for use as a lunar construction material. This would be an attractive alternative to conventional concrete as it does not require water. However, the viability of sulfur concrete in a lunar environment, which is characterized by lack of an atmosphere and extreme temperatures, is not well understood. Here it is assumed that the lunar ore can be mined, refined, and the raw sulfur melded with appropriate lunar regolith to form, for example, bricks. This study evaluates pure sulfur and two sets of small sulfur concrete samples that have been prepared using JSC-1 lunar stimulant and SiO2 powder as aggregate additions. Each set was subjected to extended periods in a vacuum environment to evaluate sublimation issues. Results from these experiments are presented and discussed within the context of the lunar environment.

Grugel, Richard N.↗

Manufacture of high-density ceramic sinters

High density ceramic sinters are manufactured by coating premolded or presintered porous ceramics with a sealing material of high SiO2 porous glass or nitride glass and then sintering by hot isostatic pressing. The ceramics have excellent abrasion and corrosion resistances. Thus LC-10 (Si3N2 powder) and Y2O3-Al2O3 type sintering were mixed and molded to give a premolded porous ceramic (porosity 37%, relative bulk density 63%). The ceramic was dipped in a slurry containing high SiO2 porous glass and an alcohol solution of cellulose acetate and dried. The coated ceramic was treated in a nitrogen atmosphere and then sintered by hot isostatic pressing to give a dense ceramic sinter.

Hibata, Y.↗

Evaluation of Sulfur 'Concrete' for Use as a Construction Material on the Lunar Surface

Combining molten sulfur with any number of aggregate materials forms, when solid, a mixture having attributes similar, if not better, to conventional water-based concrete. As a result the use of sulfur "concrete" on Earth is well established, particularly in corrosive environments. Consequently, discovery of troilite (FeS) on the lunar surface prompted numerous scenarios about its reduction to elemental sulfur for use, in combination with lunar regolith, as a potential construction material; not requiring water, a precious resource, for its manufacture is an obvious advantage. However, little is known about the viability of sulfur concrete in an environment typified by extreme temperatures and essentially no atmosphere. The experimental work presented here evaluates the response of pure sulfur and sulfur concrete subjected to laboratory conditions that approach those expected on the lunar surface, the results suggesting a narrow window of application.

Grugel, R. N.↗

Mars Surface Environmental Issues

Planetary exploration by astronauts will require extended periods of habitation on a planet's surface, under the influence of environmental factors that are different from those of Earth and the spacecraft that delivered the crew to the planet. Human exploration of Mars, a possible near-term planetary objective, can be considered a challenging scenario. Mission scenarios currently under consideration call for surface habitation periods of from 1 to 18 months on even the earliest expeditions. Methods: Environmental issues associated with Mars exploration have been investigated by NASA and the National Space Biomedical Research Institute (NSBRI) as part of the Bioastronautics Critical Path Roadmap Project (see http ://criticalpath.jsc.nasa.gov). Results: Arrival on Mars will immediately expose the crew to gravity only 38% of that at Earth's surface in possibly the first prolonged exposure to gravity other than the 1G of Earth's surface and the zero G of weightless space flight, with yet unknown effects on crew physiology. The radiation at Mars' surface is not well documented, although the planet's bulk and even its thin atmosphere may moderate the influx of galactic cosmic radiation and energetic protons from solar flares. Secondary radiation from activated components of the soil must also be considered. Ultrafine and larger respirable and nonrespirable particles in Martian dust introduced into the habitat after surface excursions may induce pulmonary inflammation exacerbated by the additive reactive and oxidizing nature of the dust. Stringent decontamination cannot eliminate mechanical and corrosive effects of the dust on pressure suits and exposed machinery. The biohazard potential of putative indigenous Martian microorganisms may be assessed by comparison with analog environments on Earth. Even in their absence, human microorganisms, if not properly controlled, can be a threat to the crew's health. Conclusions: Mars' surface offers a substantial challenge to the health and safety of future human explorers.

Charles, John↗

Chemical Characterization and Reactivity of Fuel-Oxidizer Reaction Product

Fuel-oxidizer reaction product (FORP), the product of incomplete reaction of monomethylhydrazine and nitrogen tetroxide propellants prepared under laboratory conditions and from firings of Shuttle Reaction Control System thrusters, has been characterized by chemical and thermal analysis. The composition of FORP is variable but falls within a limited range of compositions that depend on three factors: the fuel-oxidizer ratio at the time of formation; whether the composition of the post-formation atmosphere is reducing or oxidizing; and the reaction or post-reaction temperature. A typical composition contains methylhydrazinium nitrate, ammonium nitrate, methylammonium nitrate, and trace amounts of hydrazinium nitrate and 1,1-dimethylhydrazinium nitrate. Thermal decomposition reactions of the FORP compositions used in this study were unremarkable. Neither the various compositions of FORP, the pure major components of FORP, nor mixtures of FORP with propellant system corrosion products showed any unusual thermal activity when decomposed under laboratory conditions. Off-limit thruster operations were simulated by rapid mixing of liquid monomethylhydrazine and liquid nitrogen tetroxide in a confined space. These tests demonstrated that monomethylhydrazine, methylhydrazinium nitrate, ammonium nitrate, or Inconel corrosion products can induce a mixture of monomethylhydrazine and nitrogen tetroxide to produce component-damaging energies. Damaging events required FORP or metal salts to be present at the initial mixing of monomethylhydrazine and nitrogen tetroxide.

David, Dennis D.↗

Chemical Characterization and Reactivity Testing of Fuel-Oxidizer Reaction Product (Test Report)

The product of incomplete reaction of monomethylhydrazine (MMH) and nitrogen tetroxide (NTO) propellants, or fuel-oxidizer reaction product (FORP), has been hypothesized as a contributory cause of an anomaly which occurred in the chamber pressure (PC) transducer tube on the Reaction Control Subsystem (RCS) aft thruster 467 on flight STS-51. A small hole was found in the titanium-alloy PC tube at the first bend below the pressure transducer. It was surmised that the hole may have been caused by heat and pressure resulting from ignition of FORP. The NASA Johnson Space Center (JSC) White Sands Test Facility (WSTF) was requested to define the chemical characteristics of FORP, characterize its reactivity, and simulate the events in a controlled environment which may have lead to the Pc-tube failure. Samples of FORP were obtained from the gas-phase reaction of MMH with NTO under laboratory conditions, the pulsed firings of RCS thrusters with modified PC tubes using varied oxidizer or fuel lead times, and the nominal RCS thruster firings at WSTF and Kaiser-Marquardt. Fourier transform infrared spectroscopy (FTIR), differential scanning calorimetry (DSC), accelerating rate calorimetry (ARC), ion chromatography (IC), inductively coupled plasma (ICP) spectrometry, thermogravimetric analysis (TGA) coupled to FTIR (TGA/FTIR), and mechanical impact testing were used to qualitatively and quantitatively characterize the chemical, thermal, and ignition properties of FORP. These studies showed that the composition of FORP is variable but falls within a limited range of compositions that depends on the fuel loxidizer ratio at the time of formation, composition of the post-formation atmosphere (reducing or oxidizing), and reaction or postreaction temperature. A typical composition contains methylhydrazinium nitrate (MMHN), ammonium nitrate (AN), methylammonium nitrate (MAN), and trace amounts of hydrazinium nitrate and 1,1-dimethylhydrazinium nitrate. The thermal decomposition reactions of FORP compositions used in this study were unremarkable, Neither the various compositions of FORP, the pure major components of FORP, nor mixtures of FORP with propellant-system corrosion products showed any unusual thermal activity when decomposed under laboratory conditions. Off-limit thruster operations were simulated by rapid mixing of liquid MMH and liquid NTO in a confined space. The test hardware was constructed with pressure- and temperature-measurement devices to determine if the expected fuel oxidizer reaction would result in increased energy release when FORP, FORP constituents, or propellant-system corrosion products were present. These tests demonstrated that FORP, MMHN, AN, or Inconel corrosion products can induce a mixture of MMH and NTO to produce component-damaging energies. The simulation-test program was not extensive enough to provide statistical probabilities for these events but did show that such events can occur. Damaging events required FORP or metal salts to be present at the initial mixing of MMH and NTO. Based on the results of these studies, it is suggested that removal or mitigation of a buildup of these materials may decrease the incidence of these high-energy, potentially damaging events.