Search NASA⌕ Search

SEARCH · Search NASA

Results for “BOROSILICATE GLASS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 163 records · Page 9

IMPROVED BAR IMPACT TESTS USING A PHOTONIC DOPPLER VELOCIMETER

Bar impact tests, using the techniques described elsewhere in this symposium, were used to measure compressive and tensile strengths of borosilicate glass, soda lime glass, and a glass ceramic. The glass ceramic was 25% crystalline spinel, furnished by Corning Inc. There are two measures of compressive strength: the peak stress that can be transmitted in unconfined compression, and the 'steady state' strength. For borosilicate glass and soda lime glass, these values were similar, being about 1.8 and 1.5 GPa, respectively. The glass ceramic (25% spinel) was almost 50% stronger. Tensile failure in the glass and glass ceramic takes places via surface flaws, and thus tensile strength is an extrinsic, as opposed to intrinsic property.

36 MATERIALS SCIENCE↗

AI/ML-assisted Design of Phosphate Glass and Ceramic Nuclear Waste Forms

Borosilicate glass is the widely accepted waste form for immobilization of high and medium level nuclear wastes. Advances in nuclear energies and new reactor designs require the development of new waste forms. For example, wastes from molten salt reactors and reprocessing of nuclear fuels lead to salt-based wastes that are difficult to be immobilized by conventional borosilicate glasses due to limited solubility and waste loading. In designing new waste forms, machine learning (ML) and artificial intelligence (AI) based approaches are much needed and can be beneficial in enabling a more efficient design in large parameter spaces as compared to traditional Edisonian trial-and-error approaches. Here, we report in this paper the rationale and latest progress of our ML/AI-based design of phosphate-based waste forms.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

SOLIDIFICATION OF THE HANFORD LAW WASTE STREAM PRODUCED AS A RESULT OF NEAR-TANK CONTINUOUS SLUDGE LEACHING AND SODIUM HYDROXIDE RECOVERY

The U.S. Department of Energy (DOE), Office of River Protection (ORP), is responsible for the remediation and stabilization of the Hanford Site tank farms, including 53 million gallons of highly radioactive mixed wasted waste contained in 177 underground tanks. The plan calls for all waste retrieved from the tanks to be transferred to the Waste Treatment Plant (WTP). The WTP will consist of three primary facilities including pretreatment facilities for Low Activity Waste (LAW) to remove aluminum, chromium and other solids and radioisotopes that are undesirable in the High Level Waste (HLW) stream. Removal of aluminum from HLW sludge can be accomplished through continuous sludge leaching of the aluminum from the HLW sludge as sodium aluminate; however, this process will introduce a significant amount of sodium hydroxide into the waste stream and consequently will increase the volume of waste to be dispositioned. A sodium recovery process is needed to remove the sodium hydroxide and recycle it back to the aluminum dissolution process. The resulting LAW waste stream has a high concentration of aluminum and sodium and will require alternative immobilization methods. Five waste forms were evaluated for immobilization of LAW at Hanford after the sodium recovery process. The waste forms considered for these two waste streams include low temperature processes (Saltstone/Cast stone and geopolymers), intermediate temperature processes (steam reforming and phosphate glasses) and high temperature processes (vitrification). These immobilization methods and the waste forms produced were evaluated for (1) compliance with the Performance Assessment (PA) requirements for disposal at the IDF, (2) waste form volume (waste loading), and (3) compatibility with the tank farms and systems. The iron phosphate glasses tested using the product consistency test had normalized release rates lower than the waste form requirements although the CCC glasses had higher release rates than the quenched glasses. However, the waste form failed to meet the vapor hydration test criteria listed in the WTP contract. In addition, the waste loading in the phosphate glasses were not as high as other candidate waste forms. Vitrification of HLW waste as borosilicate glass is a proven process; however the HLW and LAW streams at Hanford can vary significantly from waste currently being immobilized. The ccc glasses show lower release rates for B and Na than the quenched glasses and all glasses meet the acceptance criterion of < 4 g/L. Glass samples spiked with Re{sub 2}O{sub 7} also passed the PCT test. However, further vapor hydration testing must be performed since all the samples cracked and the test could not be performed. The waste loading of the iron phosphate and borosilicate glasses are approximately 20 and 25% respectively. The steam reforming process produced the predicted waste form for both the high and low aluminate waste streams. The predicted waste loadings for the monolithic samples is approximately 39%, which is higher than the glass waste forms; however, at the time of this report, no monolithic samples were made and therefore compliance with the PA cannot be determined. The waste loading in the geopolymer is approximately 40% but can vary with the sodium hydroxide content in the waste stream. Initial geopolymer mixes revealed compressive strengths that are greater than 500 psi for the low aluminate mixes and less than 500 psi for the high aluminate mixes. Further work testing needs to be performed to formulate a geopolymer waste form made using a high aluminate salt solution. A cementitious waste form has the advantage that the process is performed at ambient conditions and is a proven process currently in use for LAW disposal. The Saltstone/Cast Stone formulated using low and high aluminate salt solutions retained at least 97% of the Re that was added to the mix as a dopant. While this data is promising, additional leaching testing must be performed to show compliance with the PA. Compressive strength tests must also be performed on the Cast Stone monoliths to verify PA compliance. Based on testing performed for this report, the borosilicate glass and Cast Stone are the recommended waste forms for further testing. Both are proven technologies for radioactive waste disposal and the initial testing using simulated Hanford LAW waste shows compliance with the PA. Both are resistant to leaching and have greater than 25% waste loading.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Effects of Al:Si and (Al+Na):Si Ratios on the Properties of the International Simple Glass, Part II: Structure

High-alumina containing high-level waste (HLW) will be vitrified at the Waste Treatment Plant at the Hanford Site. The resulting glasses, high in alumina, will have distinct composition-structure-property (C-S-P) relationships compared to previously studied HLW glasses. These C-S-P relationships determine the processability and product durability of glasses and therefore must be understood. The main purpose of this study is to understand the detailed structural changes caused by Al:Si and (Al+Na):Si substitutions in a simplified nuclear waste model glass (ISG, International Simple Glass) by combining experimental structural characterizations and molecular dynamics (MD) simulations. The structures of these two series of glasses were characterized by neutron total scattering and 27Al, 23Na, 29Si, and 11B solid-state nuclear magnetic resonance (NMR) spectroscopy. Additionally, MD simulations were used to generate atomistic structural models of the borosilicate glasses and simulation results were validated by the experimental structural data. Short-range (e.g., bond distance, coordination number, etc.) and medium-range (e.g., oxygen speciation, network connectivity, polyhedral linkages) structural features of the borosilicate glasses were systematically investigated as a function of the degree of substitution. The results show that bond distance and coordination number of the cation-oxygen pairs are relatively insensitive to Al:Si and (Al+Na):Si substitutions with the exception of the B-O pair. Additionally, the Al:Si substitution results in an increase of tri-bridging oxygen species, while (Al+Na):Si substitution creates non-bridging oxygen species. Charge compensator preferences were found for Si-[NBO] (Na+), [3]B-[NBO] (Na+), [4]B (mostly Ca2+), [4]Al (nearly equally split Na+ and Ca2+), and [6]Zr (mostly Ca2+). The network former-BO-network former linkages preferences were also tabulated; Si-O-Al and Al-O-Al were preferred at the expense of lower Si-O-[3]B and [3]B-O-[3]B linkages. These results provide insights on the structural origins of property changes such as glass transition temperature caused by the substitutions, providing a basis for future improvements of theoretical and computer simulation models.

Lu, Xiaonan↗

The formation of crystals in glasses containing rare earth oxides

Korean spent nuclear fuel will reach the capacity of the available temporary storage by 2016. Pyroprocessing and direct disposal seems to be an alternative way to manage and reuse spent nuclear fuel while avoiding the wet reprocessing technology. Pyroprocessing produces several wastes streams, including metals, salts, and rare earths, which must be converted into stabilized form. A suitable form for rare earth immobilization is borosilicate glass. The borosilicate glass form exhibits excellent durability, allows a high waste loading, and is easy to process. In this work, we combined the rare earths waste of composition (in wt%) 39.2Nd{sub 2}O{sub 3}–22.7CeO{sub 2}–11.7La{sub 2}O{sub 3}–10.9PrO{sub 2}–1.3Eu{sub 2}O{sub 3}–1.3Gd{sub 2}O{sub 3}–8.1Sm{sub 2}O{sub 3}–4.8Y{sub 2}O{sub 3} with a baseline glass of composition 60.2SiO{sub 2}–16.0B{sub 2}O{sub 3}–12.6Na{sub 2}O–3.8Al{sub 2}O{sub 3}–5.7CaO–1.7ZrO{sub 2}. Crystallization in waste glasses occurs as the waste loading increases. It may produce complicate glass processing and affect the product quality. To study crystal formation, we initially made glasses containing 5%, 10% and 15% of La{sub 2}O{sub 3} and then glasses with 5%, 10% and 15% of the complete rare earth mix. Samples were heat-treated for 24 hours at temperatures 800°C to 1150°C in 50°C increments. Quenched samples were analyzed using an optical microscope, scanning electron microscope with energy dispersive spectroscopy, and x-ray diffraction. Stillwellite (LaBSiO{sub 5}) and oxyapatite (Ca{sub 2}La{sub 8}Si{sub 6}O{sub 26}) were found in glasses containing La{sub 2}O{sub 3}, while oxyapatite (Ca{sub 2}La{sub 8}Si{sub 6}O{sub 26} and NaNd{sub 9}Si{sub 6}O{sub 26}) precipitated in glasses with additions of mixed rare earths. The liquidus temperature (T{sub L}) of the glasses containing 5%, 10% and 15% La{sub 2}O{sub 3} were 800°C, 959°C and 986°C, respectively; while T{sub L} was 825°C, 1059°C and 1267°C for glasses with 5%, 10% and 15% addition of mixed rare earth oxides. The component coefficients T{sub B2O3}, T{sub SiO2}, T{sub CaO}, and T{sub RE2O3} were also evaluated using a recently published study.

36 MATERIALS SCIENCE↗

Boron Coordination in Multicomponent Glasses: Analytical Models and Machine Learning With Uncertainty

Borosilicate glasses are extensively used in a variety of applications from kitchenware to nuclear waste immobilization due to the strong network formed by the Si-O-B bond that makes it resistant to chemical corrosion and gives it a low thermal expansion. Boron, however, exists in both trigonal BO3 and tetrahedral BO4 bonds in glass systems, which impacts the chemical durability and thermal resistance of the glass, amongst other properties. Boron coordination (N4), or the ratio of the amount of BO4 to BO3 within a glass, may aid in predicting these properties but is difficult to derive without experimental data due to the complexity of impacts from varied glass compositions and processing factors. For this reason, compositional models have been developed to predict boron coordination, but the models typically include a limited number of glass components. To help fill this gap in the models, in this work, a diverse multicomponent glass dataset of 809 glasses is compiled from a literature search, and then a number of analytical and machine learning (ML) models are trained on the dataset. Previously developed modified Bernstein and modified Du Stebbins analytical models were fitted to update parameters with the new dataset. Then, partially Bayesian neural networks, Gaussian process regressor, and heteroskedastic deterministic neural networks were evaluated. The ML models examined all have different strategies to overcome the potential for overfitting as a result of a limited training dataset, and return results that account for model uncertainty, which can be valuable for understanding model reliability. For the first time, cooling rate is introduced as an input parameter for ML models, showing consistent improvements in performance and solidifying the importance of including parameters outside of composition alone for N4 prediction. The machine learning models examined here show promise in accurate predictions of boron coordination in borosilicate glasses, all achieving R2 values of 0.91.

boron coordination↗

Microbial interactions with phosphorus containing glasses representative of vitrified radioactive waste

The presence of phosphorous in borosilicate glass (at 0.1 – 1.3 mol % P 2 O 5 ) and in iron-phosphate glass (at 53 mol % P 2 O 5 ) stimulated the growth and metabolic activity of anaerobic bacteria in model systems. Dissolution of these phosphorous containing glasses was either inhibited or accelerated by microbial metabolic activity, depending on the solution chemistry and the glass composition. The breakdown of organic carbon to volatile fatty acids increased glass dissolution. The interaction of microbially reduced Fe(II) with phosphorus-containing glass under anoxic conditions decreased dissolution rates, whereas the interaction of Fe(III) with phosphorous-containing glass under oxic conditions increased glass dissolution. Phosphorous addition to borosilicate glasses did not significantly affect the microbial species present, however, the diversity of the microbial community was enhanced on the surface of the iron phosphate glass. Results demonstrate the potential for microbes to influence the geochemistry of radioactive waste disposal environments with implication for wasteform durability.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Application of the immobilized low-activity waste glass corrosion model to the static dissolution of 24 statistically-designed alkali-borosilicate waste glasses

Glass corrosion models that capture the complex mechanisms of the glass-water reaction enable the prediction of nuclear waste glass durability in disposal scenarios. Parameterization of such models is challenging because of the need to capture changes in corrosion behavior with time, reaction conditions, and glass composition. In this report we describe and employ the immobilized low activity waste (ILAW) glass corrosion model (IGCM) in geochemical simulations of static dissolution tests, at two temperatures (40 °C and 90 °C), for a matrix of 24 enhanced low activity waste (eLAW) glasses statistically designed to cover a processable composition space defined by 8 major glass components (Al 2 O 3 , B 2 O 3 , CaO, Na 2 O, SiO 2 , SnO 2 , ZrO 2 , and Others as defined in the text). The IGCM includes a first-order chemical affinity term and an ion-exchange term that represents the net exchange of Na+ ions in the pristine glass with protons in aqueous solution. Constant, time-dependent, and time- and pH-dependent functional forms of the ion-exchange term are evaluated to reproduce the change in corrosion behavior with time in saturated, static dissolution tests. The agreement with measured aqueous concentrations of the main glass components (B, Na, and Si) improved significantly upon addition of a time-dependent term, which therefore constitutes a simple representation of the glass-water reaction progress. Due to the limited changes in pH in the static dissolution tests, past a short initial period of rapid increase, addition of a pH dependent term did not appreciably improve the fits, indicating that comprehensive model parameterization requires more than one type of glass corrosion test to capture a wide range of solution chemistries. IGCM parameters were found to be dependent on glass composition, and the parameter sets generated in this work will enable the development of composition–parameter correlation models that offer the promise of predicting IGCM parameters, and thus glass corrosion behavior, solely based on glass composition.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Glass Ceramic Formulation Data Package

A glass ceramic waste form is being developed for treatment of secondary waste streams generated by aqueous reprocessing of commercial used nuclear fuel (Crum et al. 2012b). The waste stream contains a mixture of transition metals, alkali, alkaline earths, and lanthanides, several of which exceed the solubility limits of a single phase borosilicate glass (Crum et al. 2009; Caurant et al. 2007). A multi-phase glass ceramic waste form allows incorporation of insoluble components of the waste by designed crystallization into durable heat tolerant phases. The glass ceramic formulation and processing targets the formation of the following three stable crystalline phases: (1) powellite (XMoO 4 ) where X can be (Ca, Sr, Ba, and/or Ln), (2) oxyapatite Y x, Z (10-x) Si 6 O 26 where Y is alkaline earth, Z is Ln, and (3) lanthanide borosilicate (Ln 5 BSi 2 O 13 ). These three phases incorporate the waste components that are above the solubility limit of a single-phase borosilicate glass. The glass ceramic is designed to be a single phase melt, just like a borosilicate glass, and then crystallize upon slow cooling to form the targeted phases. The slow cooling schedule is based on the centerline cooling profile of a 2 foot diameter canister such as the Hanford High-Level Waste canister. Up to this point, crucible testing has been used for glass ceramic development, with cold crucible induction melter (CCIM) targeted as the ultimate processing technology for the waste form. Idaho National Laboratory (INL) will conduct a scaled CCIM test in FY2012 with a glass ceramic to demonstrate the processing behavior. This Data Package documents the laboratory studies of the glass ceramic composition to support the CCIM test. Pacific Northwest National Laboratory (PNNL) measured melt viscosity, electrical conductivity, and crystallization behavior upon cooling to identify a processing window (temperature range) for melter operation and cooling profiles necessary to crystallize the targeted phases in the waste form.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Synergy in Materials: Leveraging Phosphosilicate Waste Forms for Electrochemical Salt Waste

Here, waste forms containing glassy and crystalline phosphate and silicate phases were produced to immobilize salt waste simulants from pyroprocessing and characterized by using Raman spectroscopy, Mössbauer spectroscopy, X-ray diffraction, scanning electron microscopy, heat capacity, and chemical durability measurements. In this work, a phosphosilicate waste form is presented to leverage the benefits of both borosilicate glasses and iron phosphate glasses. To improve waste loading, prior to immobilization, salt simulants were successfully dechlorinated using ammonium dihydrogen phosphate, mixed with a borosilicate frit (5–30 wt %) and Fe 2 O 3 , and vitrified. Additions of 2.5–15 wt % borosilicate glass (NBS3) improved normalized release rates for Cs relative to iron-phosphates without NBS3, resulting in chemical durabilities similar to high-level waste borosilicate glass reference materials. The release rates of the alkalis (i.e., Li, Na, K, Cs) were the lowest with the addition of 5 wt % NBS3. Although Sr was not specifically targeted in this study, evidence exists that it preferentially partitioned with Si to form an amorphous droplet phase within the iron phosphate glass matrix.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding the influence of iron on crystallization kinetics of nepheline based glasses - 15472

Hanford site in Washington is home to 55 million US gallons of high level radioactive waste rich in sodium, alumina and iron. The strategy is to vitrify this waste in borosilicate glasses. Crystallization of nepheline/carnegeite (NaAlSiO{sub 4}) in glass melts during vitrification and canister cooling is a big challenge as it severely deteriorates the chemical durability of the glass. As the HLW borosilicate glasses are similar to basalt glass on a borate-free basis and as no borate phase crystallize on the liquidus, the crystallization chemistry of waste glasses can be described by the known phase relations of the geochemical basalt quaternary Na{sub 2}O-Al{sub 2}O{sub 3}-Fe{sub 2}O{sub 3}-SiO{sub 2} system. The objective of this study is to understand the influence of iron on the thermal stability and crystallization kinetics of model sodium- and alumina- rich simplified silicate glasses in the Na{sub 2}O-Al{sub 2}O{sub 3}-Fe{sub 2}O{sub 3}-SiO{sub 2} system designed in the primary crystallization field of nepheline. The results obtained from this study will form the baseline for understanding the nucleation and crystallization kinetics of multicomponent complex nuclear waste glasses in future. A series of glasses with compositions 25Na{sub 2}O-(25-z) Al{sub 2}O{sub 3}-zFe{sub 2}O{sub 3} -50SiO{sub 2} (mol.%) where z varies between 0 -5% has been prepared by melt-quench technique. Glasses have been labelled in reference to their Fe{sub 2}O{sub 3} content, i.e. Fe-z. We could not obtain amorphous glasses with Fe{sub 2}O{sub 3} > 5 mol.% . Glass batches comprising oxides and carbonates were melted at 1650 deg. C in Pt-Rh crucibles for 2 h. The melts were quenched in cold water to yield ∼90 g of glass. Thermal stability and crystallization kinetics of glasses was studied using differential thermal analysis (DTA). Thermal scans (30-1580 deg. C) were collected on glass particles (particle size: 0.5 mm-1 mm) at four different heating rates: 5, 10, 15 and 20 K min{sup -1} in air and inert (N{sub 2}) atmosphere. Non-isothermal crystallization kinetics of the glasses was studied using the Augis-Bennett method and Ozawa method. In accordance with the crystallization data obtained from DTA, glasses were heated in the crystallization temperature range and air quenched. Glasses were also heated from 30 deg. C to 800, 900 and 1000 deg. C for 1 h, respectively, in air and inert (N{sub 2}) atmospheres, at heating rate of 10 K min{sup -1}. Resulting glass-ceramics were characterized for their crystalline phase evolution by X-ray diffraction (XRD) and scanning electron microscopy (SEM). Conversion of melt -to glass-ceramic during cooling DTA data was also collected for all the glasses during their conversion from melt -to -glass-ceramic during cooling at different cooling rates, in air and inert (N{sub 2}) atmosphere. In accordance with the DTA data, conversion of melt to glass-ceramic during cooling was studied by re-melting the glass frit in Pt-Rh crucibles at 1650 deg. C. The melt was allowed to cool at 10 K min{sup -1} and was air quenched at different temperatures (as per DTA data). The as obtained glass-ceramics were characterized by XRD and SEM Incorporation of Fe{sub 2}O{sub 3} in glasses decreases their crystallization temperature and increases their crystallization tendency. Parent glass (stoichiometric nepheline composition) is prone to surface crystallization. Incorporating 5 mol.% Fe{sub 2}O{sub 3} in these glasses transforms the crystallization kinetics from surface to volume nucleation. Crystallization kinetics of glass Fe-2.5 is affected by the environment (N{sub 2} vs. Air) while no significant impact of environment could be seen for glass Fe-5. Devitrification in all the glasses begins with the crystallization of carnegeite (NaAlSiO{sub 4}, orthorhombic) (∼1200 deg. C). Prolonged heat treatments leads to the crystallization of nepheline (NaAlSiO{sub 4}, hexagonal) (∼1200 deg. C) as a secondary phase. Fe{sub 2}O{sub 3} promotes the crystallization of nepheline over carnegeite via formation of magnetite as nucleation site. Iron incorporation pre-nucleates the glasses which upon heat treatment result in the formation of magnetite phase as nucleation sites, thus, shifting the mechanism of crystallization from surface to volume. Unlike carnegeite, the crystal structure of nepheline allows partial substitution of Fe{sup 3+}/Al{sup 3+}. This promotes the crystallization of nepheline over carnegeite in iron-containing glasses. Iron incorporation in nepheline-based sodium aluminosilicate glasses shifts crystallization mechanism from surface to bulk. Our results indicate that atmosphere does affect the crystallization kinetics of iron-containing aluminosilicate glasses but only when Fe{sub 2}O{sub 3} concentration is low. Since nepheline crystal structure can easily accommodate iron in comparison to carnegeite, iron seems to promote nepheline formation in these glasses at the expense of carnegeite through formation of Fe{sub 3}O{sub 4} phase as nucleation site. Future work will be focused on adding compositional complexity to these glasses and studying them further for their nucleation and crystallization behavior.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Multi-phase glass-ceramics as a waste form for combined fission products: alkalis, alkaline earths, lanthanides, and transition metals

In this study, multi-phase silicate-based glass-ceramics were investigated as an alternate waste form for immobilizing non-fissionable products from used nuclear fuel. Currently, borosilicate glass is the waste form selected for immobilization of this waste stream, however, the low thermal stability and solubility of MoO{sub 3} in borosilicate glass translates into a maximum waste loading in the range of 15-20 mass%. Glass-ceramics provide the opportunity to target durable crystalline phases, e.g., powellite, oxyapatite, celsian, and pollucite, that will incorporate MoO{sub 3} as well as other waste components such as lanthanides, alkalis, and alkaline earths at levels 2X the solubility limits of a single-phase glass. In addition a glass-ceramic could provide higher thermal stability, depending upon the properties of the crystalline and amorphous phases. Glass-ceramics were successfully synthesized at waste loadings of 42, 45, and 50 mass% with the following glass additives: B{sub 2}O{sub 3}, Al{sub 2}O{sub 3}, CaO and SiO{sub 2} by slow cooling form from a glass melt. Glass-ceramics were characterized in terms of phase assemblage, morphology, and thermal stability. The targeted phases: powellite and oxyapatite were observed in all of the compositions along with a lanthanide borosilicate, and cerianite. Results of this initial investigation of glass-ceramics show promise as a potential waste form to replace single-phase borosilicate glass.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Summary of FY11 Sulfate Retention Studies for Defense Waste Processing Facility Glass

This report describes the results of studies related to the incorporation of sulfate in high level waste (HLW) borosilicate glass produced at the Savannah River Site (SRS) Defense Waste Processing Facility (DWPF). A group of simulated HLW glasses produced for earlier sulfate retention studies was selected for full chemical composition measurements to determine whether there is any clear link between composition and sulfate retention over the compositional region evaluated. In addition, the viscosity of several glasses was measured to support future efforts in modeling sulfate solubility as a function of predicted viscosity. The intent of these studies was to develop a better understanding of sulfate retention in borosilicate HLW glass to allow for higher loadings of sulfate containing waste. Based on the results of these and other studies, the ability to improve sulfate solubility in DWPF borosilicate glasses lies in reducing the connectivity of the glass network structure. This can be achieved, as an example, by increasing the concentration of alkali species in the glass. However, this must be balanced with other effects of reduced network connectivity, such as reduced viscosity, potentially lower chemical durability, and in the case of higher sodium and aluminum concentrations, the propensity for nepheline crystallization. Future DWPF processing is likely to target higher waste loadings and higher sludge sodium concentrations, meaning that alkali concentrations in the glass will already be relatively high. It is therefore unlikely that there will be the ability to target significantly higher total alkali concentrations in the glass solely to support increased sulfate solubility without the increased alkali concentration causing failure of other Product Composition Control System (PCCS) constraints, such as low viscosity and durability. No individual components were found to provide a significant improvement in sulfate retention (i.e., an increase of the magnitude necessary to have a dramatic impact on blending, washing, or waste loading strategies for DWPF) for the glasses studied here. In general, the concentrations of those species that significantly improve sulfate solubility in a borosilicate glass must be added in relatively large concentrations (e.g., 13 to 38 wt % or more of the frit) in order to have a substantial impact. For DWPF, these concentrations would constitute too large of a portion of the frit to be practical. Therefore, it is unlikely that specific additives may be introduced into the DWPF glass via the frit to significantly improve sulfate solubility. The results presented here continue to show that sulfate solubility or retention is a function of individual glass compositions, rather than a property of a broad glass composition region. It would therefore be inappropriate to set a single sulfate concentration limit for a range of DWPF glass compositions. Sulfate concentration limits should continue to be identified and implemented for each sludge batch. The current PCCS limit is 0.4 wt % SO 4 2- in glass, although frit development efforts have led to an increased limit of 0.6 wt % for recent sludge batches. Slightly higher limits (perhaps 0.7-0.8 wt %) may be possible for future sludge batches. An opportunity for allowing a higher sulfate concentration limit at DWPF may lay lie in improving the laboratory experiments used to set this limit. That is, there are several differences between the crucible-scale testing currently used to define a limit for DWPF operation and the actual conditions within the DWPF melter. In particular, no allowance is currently made for sulfur partitioning (volatility versus retention) during melter processing as the sulfate limit is set for a specific sludge batch. A better understanding of the partitioning of sulfur in a bubbled melter operating with a cold cap as well as the impacts of sulfur on the off-gas system may allow a higher sulfate concentration limit to be established for the melter feed. This approach would have to be taken carefully to ensure that a sulfur salt layer is not formed on top of the melt pool while allowing higher sulfur based feeds to be processed through DWPF.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Scoping Studies to Determine Impact of a Low-Alkali Phase Separated Frit on the Behavior of the Frit Slurry and Slurry Mix Evaporator Rheology

The frits used in the vitrification process at the Defense Waste Processing Facility (DWPF) are alkali borosilicate glasses, which are composed mainly of B 2 O 3 , alkali (Li 2 O and Na 2 O) and SiO 2 . As the total alkali concentration in a borosilicate glass is reduced, liquid-liquid immiscibility is exhibited by the glassforming melt, which is analogous to the behavior of oil and water. Upon cooling, the resulting glass matrix is said to be phase separated. The immiscible region is controlled by both composition and temperature. Viscosity of the melt is also a factor as it impacts the reaction rate (kinetics) of phase separation. The reaction rate (kinetics) leading to phase separation is slow for higher viscosity melts, and if such a melt is cooled rapidly (e.g., quenched in water), the resulting glass could be homogeneous, or the scale of the phase separated microstructure could be of no practical significance. Phase separated alkali borosilicate glasses tend to form a more durable silica-rich phase and a less durable alkali borate-rich phase. The overall durability of the phase separated glass depends on the morphology (physical arrangements) of each of these phases. For example, droplets of the alkali borate-rich phase may form within a silicate rich matrix, which would be a more durable glass than a glass with an interconnected alkali borate-rich phase.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Nepheline structural and chemical dependence on melt composition

Nepheline crystallizes upon slow-cooling in some melts concentrated in Na 2 O and Al 2 O 3 , which can result in a residual glass phase of low chemical durability. Nepheline can incorporate many components often found in high-level waste radioactive borosilicate glass, including glass network ions (e.g., Si, Al, Fe), alkali metals (e.g., Cs, K, Na, and possibly Li), alkaline-earth metals (e.g., Ba, Sr, Ca, Mg), and transition metals (e.g., Mn, and possibly Cr, Zn, Ni). When crystallized from melts of different compositions, nepheline chemistry varies as a function of starting glass composition. Five simulated high level nuclear waste borosilicate glasses shown to crystallize large fractions of nepheline on slow cooling, were selected for study. These melts constituted a range of Al 2 O 3 , B 2 O 3 , CaO, Na 2 O, K 2 O, Fe 2 O 3 , and SiO 2 compositions. Compositional analyses of nepheline crystals in glass by electron probe micro-analysis (EPMA) indicate that boron is unlikely to be present in any significant concentration, if at all, in nepheline. Here, several models are also presented for calculating the fraction of vacancies in the nepheline structure.

36 MATERIALS SCIENCE↗