Effect of MWCNT Content on the Structure and Properties of Spark Plasma-Sintered Iron-MWCNT Composites Synthesized by High-Energy Ball Milling

The effect of multiwall carbon nanotube (MWCNT) content on the physical and mechanical properties of Fe-MWCNT composites has been studied. High-energy ball milling (HEBM) is employed to produce the composite powder; following this, spark plasma sintering (SPS) process has been adopted for powder consolidation. The composite powder and the sintered products were subjected to structural characterization by XRD. Microstructural studies were carried out by optical, field-emission scanning and high-resolution transmission electron microscopy. While Fourier transform infrared spectroscopic study of composites was done to understand the bonding characteristics, Raman spectroscopy was employed to assess the structural damage of MWCNT after HEBM. The effects of processing on the behavior of C-C, C-O and Fe-O bonds are studied by x-ray photoelectron spectroscopy. Microhardness and compressive strength of composites are also determined. Finally, magnetic and electrical properties of the composites were characterized. It was observed that optimized ball milling conditions help to preserve the structural identity of MWCNT. Consolidation by SPS insured good interfacial bonding. The microhardness and compression strength are significantly improved in MWCNT-reinforced iron matrix composite. MWCNT has appreciably improved the electrical conductivity of the composites. Tethering of MWCNT by iron oxide has led to appreciable improvement in saturation magnetization till 3 wt.% MWCNT.

36 MATERIALS SCIENCE↗

The synthesis and hydration of ternesite, Ca5(SiO4)2SO4

The hydration and strength evolution of two multi-phase ternesite-based cements with 15 and 29 wt% ternesite are reported. The synthesis and hydration properties of single phase ternesite, nominally Ca{sub 5}(SiO{sub 4}){sub 2}SO{sub 4}, are also reported including both chemically-pure ternesite and preparations doped with sodium, potassium, phosphorous, magnesium, manganese, strontium, zinc and titanium oxides. Hydration of the samples at 25 °C was studied by calorimetry and quantitative X-ray diffraction. Unconfined compressive strength development was determined for up to 1 year. Single-phase chemically activated ternesite hydrated rapidly at 25 °C achieved compressive strengths of ≈30 and ≈65 MPa at 28 and 90 days respectively, with C-S-H and gypsum as hydration products. The multi-phase ternesite-based cements reached 7 day strengths of ≈30 MPa. It is concluded that ternesite reacts with water, exhibiting strength gain. The future of calcium sulfoaluminate and sulfosilicate cements is discussed and it is suggested that a considerable, and as yet unrealised scope exists for simultaneously optimising cementing properties while lowering production costs and reducing CO{sub 2} emissions.

36 MATERIALS SCIENCE↗

Pozzolanic reaction of fly ash modified by fluidized bed reactor-vapor deposition

This study aimed to introduce fluidized bed reactor-vapor deposition (FBR-VD) into the modification of fly ash (FA) using the activators of NaOH, Na{sub 2}SO{sub 4}, and NaCl. The compressive strength, non-evaporable water and the hydration degree fly ash (HDFA) were investigated. The scanning electron microscopy (SEM), and the X-ray powder diffraction (XRD) Rietveld analysis were also conducted. The results demonstrate that FBR-VD can benefit the compressive strength when the dosage rates of NaOH, Na{sub 2}SO{sub 4} and NaCl are 0.1%, 0.5%, and 0.5%, respectively. The non-evaporable water and HDFA also increased at certain activator dosage rates. A modification layer consisting of nanometer-scale crystals forms on the surface of the FA beads, with NaOH or Na{sub 2}SO{sub 4} applied. NaOH can react with FA and promote its pozzolanic activity. Na{sub 2}SO{sub 4} and NaCl can benefit the HDFA by remaining undissolved, to increase their concentration around FA. The enhanced HDFA is also proved by the consumption of Ca(OH){sub 2}.

36 MATERIALS SCIENCE↗

Mechanical Properties of High-Temperature Fiber-Reinforced Thermoset Composites with Plain Weave and Unidirectional Carbon Fiber Fillers

Fiber-reinforced thermoset composites are a class of materials that address the arising needs from the aerospace and hypersonic industries for high specific strength, temperature-resistant structural materials. Among the high-temperature resistant thermoset categories, phenolic triazine (PT) cyanate esters stand out thanks to their inherent high degradation temperature, glass transition temperature, and mechanical strength. Despite the outstanding properties of these thermosets, the performance of carbon fiber composites using PT cyanate esters as matrices has not been thoroughly characterized. This work evaluated PT and carbon fiber composites’ compressive properties and failure mechanisms with different fiber arrangements. A PT resin with both plain weave (PW) and non-crimped unidirectional (UD) carbon fiber mats was analyzed in this research. Highly loaded thermoset composites were obtained using process temperatures not exceeding 260 °C, and the composites proved to retain compressive strength at temperatures beyond 300 °C. Compressive testing revealed that PT composites retained compressive strength values of 50.4% of room temperature for UD composites and 61.4% for PW composites. Post-compressive failure observations of the gage section revealed that the mechanisms for failure evolved with temperature from brittle, delamination-dominant failure to shear-like failure promoted by the plastic failure of the matrix. This study demonstrated that PT composites are a good candidate for structural applications in harsh environments.

Hall, Samuel Ernesto↗

Effect of electrical field on TSA failure of cement-based materials

The impact of electrical field on the sulfate attack of cement-based materials at low temperatures was studied to rapidly detect Thaumasite Sulfate Attack (TSA) in the laboratory and in future engineering. Sulfate attack of cement paste with 30 wt% replacement of CaCO{sub 3} powder soaked in Na{sub 2}SO{sub 4} solution, MgSO{sub 4} solution, or CaSO{sub 4} solution was measured under the condition of 5 ± 2 °C when an electrical field was applied. Appearance changes and compressive strength of the samples were tested to evaluate the corrosion degree. Scanning Electron Microscopy (SEM), X-ray Diffraction (XRD), Fourier Transform Infrared Spectroscopy (FTIR) and Raman Spectroscopic measurements were applied to study the microstructure of the corrosion product. The test results indicate that sample damage was obvious, compression strength declined rapidly, and ettringite and/or thaumasite were found in the corrosion product after applying the electrical field for 90 days. A muddy product with TSA characteristics was formed, and thaumasite composition was found in the corrosion product after applying the electrical field for 120 days when MgSO{sub 4} solution was used as the corrosion medium. It is confirmed that an electrical field can accelerate TSA failure in cement-based materials.

36 MATERIALS SCIENCE↗

Comparative study on the characteristics of fly ash and bottom ash geopolymers

This research was conducted to compare geopolymers made from fly ash and ground bottom ash. Sodium hydroxide (NaOH) and sodium silicate (Na{sub 2}SiO{sub 3}) solutions were used as activators. A mass ratio of 1.5 Na{sub 2}SiO{sub 3}/NaOH and three concentrations of NaOH (5, 10, and 15 M) were used; the geopolymers were cured at 65 deg. C for 48 h. A Fourier transform infrared spectrometer (FT-IR), differential scanning calorimeter (DSC), and scanning electron microscope (SEM) were used on the geopolymer pastes. Geopolymer mortars were also prepared in order to investigate compressive strength. The results show that both fly ash and bottom ash can be utilized as source materials for the production of geopolymers. The properties of the geopolymers are dependent on source materials and the NaOH concentration. Fly ash is more reactive and produces a higher degree of geopolymerization in comparison with bottom ash. The moderate NaOH concentration of 10 M is found to be suitable and gives fly ash and bottom ash geopolymer mortars with compressive strengths of 35 and 18 MPa.

36 MATERIALS SCIENCE↗

Microstructural and compositional change of NaOH-activated high calcium fly ash by incorporating Na-aluminate and co-existence of geopolymeric gel and C-S-H(I)

This study explores the reaction products of alkali-activated Class C fly ash-based aluminosilicate samples by means of high-resolution synchrotron X-ray diffraction (HSXRD), scanning electron microscope (SEM), and compressive strength tests to investigate how the readily available aluminum affects the reaction. Class C fly ash-based aluminosilicate raw materials were prepared by incorporating Na-aluminate into the original fly ashes, then alkali-activated by 10 M NaOH solution. Incorporating Na-aluminate reduced the compressive strength of samples, with the reduction magnitude relatively constant regardless of length of curing period. The HSXRD provides evidence of the co-existence of C-S-H with geopolymeric gels and strongly suggests that the C-S-H formed in the current system is C-S-H(I). The back-scattered electron images suggest that the C-S-H(I) phase exists as small grains in a finely intermixed form with geopolymeric gels. Despite providing extra source of aluminum, adding Na-aluminate to the mixes did not decrease the Si/Al ratio of the geopolymeric gel.

36 MATERIALS SCIENCE↗

The composition and performance of alite-ye'elimite clinker produced at 1300 °C

Alite-ye'elimite clinker is a high cementing clinker prepared by introducing calcium sulfoaluminate, a non-silicate mineral, into the cement clinker. The mineral composition and mechanics of tricalcium silicate-rich sulfur aluminate prepared at 1300 °C are reported. The effects of copper slag and phosphorus slag on the phase composition, heat release and compressive strength were investigated. The phase composition was analysed by X-ray powder diffraction. The results show that the copper slag and phosphorus slag can lower the burn temperature of the clinker and promote the coexistence of C{sub 3}S and C{sub 4}A{sub 3} S-bar . The quality of clinker produced at 1300 °C is satisfactory. The compressive strength of mortar curing at 28 d is higher than that of P·II 52.5.

36 MATERIALS SCIENCE↗

MODEL 9975 LIFE EXTENSION PACKAGE 2 FINAL REPORT

Life extension package LE2 (9975-04162) was instrumented and subjected to an extreme temperature environment for 81 weeks. During this time, the maximum fiberboard temperature was {approx}240 - 250 degrees F, and was established by a combination of internal heat (19 watts) and external heat. This temperature matches the fiberboard continuous service rating, although such extremes are not expected for normal operation in KAMS. Several tests and parameters were used to characterize the package components. Results from these tests generally indicate agreement between this full-scale shipping package and small-scale laboratory tests on fiberboard and O-ring samples. These areas of agreement include the rate of fiberboard weight loss, change in fiberboard thermal conductivity, fiberboard compression strength, and O-ring compression set. In addition, this package provides an example of the extent to which moisture within the fiberboard can redistribute in the presence of a temperature gradient such as might be created by a 19 watt internal heat load. Moisture re distribution in this package was further exaggerated by a majority of the fiberboard being heated to above the boiling point of water. The majority of water within the fiberboard migrated to the bottom layers of fiberboard, where it contributed to accelerated degradation beyond that expected based solely on the temperature.

47 OTHER INSTRUMENTATION↗

Development of Cement Solidification Technique for Sodium Borate Waste Produced in PWR Plants - 16061

A cement solidification process for treating sodium borate waste produced in pressurized water reactor (PWR) plants was studied. It is known that the setting and hardening reaction of cement is retarded by the presence of boron compounds. This technique was developed to obtain high uniaxial compressive strength more than 10 MPa which can satisfy various countries disposal regulations. As examples of disposal regulations, France requires 8 MPa for homogeneous solidified products. The sodium/ boron (Na/B) ratio was controlled to about 1 by adding NaOH to simulated liquid waste for the purpose of improving the workablility and mechanical strength. To obtain high volume reduction, simulated liquid waste was dehydrated and powdered by using a wiped film evaporator. Ordinary portland cement (OPC) was used for the solidification. The viscosity of cement mixture was controlled by the water/cement ratio. The resulting viscosity became less than 25 dPa.s, and it was possible to continuously mix the mixture. Solidified cement with containing 73 kg/m{sup 3} of boron had a uniaxial compressive strength of more than 10 MPa. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Use of waste gypsum to replace natural gypsum as set retarders in portland cement

The present study is focused on clarifying the influence of waste gypsum (WG) in replacing natural gypsum (NG) in the production of ordinary Portland cement (OPC). WG taken from slip casting moulds in a ceramic factory was formed from the hydration of plaster of paris. Clinker and 3-5 wt% of WG was ground in a laboratory ball mill to produce cement waste gypsum (CMWG). The same procedure was repeated with NG to substitute WG to prepare cement natural gypsum (CMNG). The properties of NG and WG were investigated via X-ray Diffraction (XRD), X-ray fluorescence (XRF) and differential scanning calorimetry (DSC)/thermogravimetric (TG) to evaluate the properties of CMNG and CMWG. The mechanical properties of cement were tested in terms of setting time, flexural and compressive strength. The XRD result of NG revealed the presence of dihydrate while WG contained dihydrate and hemihydrate. The content of dihydrate and hemihydrates were obtained via DSC/TG, and the results showed that WG and NG contained 12.45% and 1.61% of hemihydrate, respectively. Furthermore, CMWG was found to set faster than CMNG, an average of 15.29% and 13.67% faster for the initial and final setting times, respectively. This was due to the presence of hemihydrate in WG. However, the values obtained for flexural and compressive strength were relatively the same for CMNG and CMWG. Therefore, this result provides evidence that WG can be used as an alternative material to NG in the production of OPC.

36 MATERIALS SCIENCE↗

Status of Graphite Oxidation Work

Data were developed to compare the extent of structural damage associated with high temperature exposure to an air leak. Two materials, NBG-18 graphite and unpurified PCEA graphite have been tested as of this report. The scope was limited to isothermal oxidation at a single temperature, 750°C. Ambient post-oxidation compression strength testing was performed for three levels of burn off (1%, 5%, and 10% mass loss) for two leak scenarios: 100% air and 10% air in helium. Temperature, gas flow, and dynamic mass loss oxidation conditions were monitored and recorded for each sample. The oxidation period was controlled with flow of inert gas during the thermal ramp and upon cool down with a constant 10 liter per minute flow maintained throughout furnace operation. Compressive strengths of parallel un-oxidized samples were tested to assess the relative mass loss effects. In addition to baseline samples matching the un-oxidized dimensions of the oxidized samples, two sets of mechanically reduced samples were prepared. One set was trimmed to achieve the desired mass loss by removing an effectively uniform depth from the geometric surface of the sample. The other set was cored to produce a full penetration axial hole down the center of each sample.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Utilisation of steel furnace slag coarse aggregate in a low calcium fly ash geopolymer concrete

This paper evaluates the performance of steel furnace slag (SFS) coarse aggregate in blended slag and low calcium fly ash geopolymer concrete (GPC). The geopolymer binder is composed of 90% of low calcium fly ash and 10% of ground granulated blast furnace slag (GGBFS). Mechanical and physical properties, shrinkage, and detailed microstructure analysis were carried out. The results showed that geopolymer concrete with SFS aggregate offered higher compressive strength, surface resistivity and pulse velocity than that of GPC with traditional aggregate. The shrinkage results showed no expansion or swelling due to delayed calcium oxide (CaO) hydration after 320 days. No traditional porous interfacial transition zone (ITZ) was detected using scanning electron microscopy, indicating a better bond between SFS aggregate and geopolymer matrix. Energy dispersive spectroscopy results further revealed calcium (Ca) diffusion at the vicinity of ITZ. Raman spectroscopy results showed no new crystalline phase formed due to Ca diffusion. X-ray fluorescence result showed Mg diffusion from SFS aggregate towards geopolymer matrix. The incorporation of Ca and Mg into the geopolymer structure and better bond between SFS aggregate and geopolymer matrix are the most likely reasons for the higher compressive strength observed in GPC with SFS aggregate.

36 MATERIALS SCIENCE↗

Mechanical and physical properties of inorganic polymer cement made of iron-rich laterite and lateritic clay: A comparative study

In this work, two different laterites (iron contents of 13.07 and 49.34 wt%, respectively, for lateritic clay, LAC, and iron-rich laterite, LAI) were selected and calcined at 600 °C. The obtained calcined laterites, namely LAI600 and LAC600, were separately mixed with an alkaline solution (silicate modulus of 1.35) or an acidic solution (phosphoric acid solution at pH ≤ 2) for the synthesis of inorganic polymer products. The fabricated products were cured at 20 °C (ambient) and 40 °C (oven). The obtained results showed that the compressive strength of each series of alkaline-based inorganic polymer binder increased with ageing time (7 and 28 days) for room temperature curing, while the reverse trend was noted for oven-cured specimens. The best mechanical performance was obtained when using a phosphoric acid solution, 38 and 52 ± 1 MPa; 62 and 65 ± 1 MPa at 28 days for LAC and LAI respectively. It appeared that a higher iron content within the laterite contributed to an increase in the compressive strength under acidic conditions (LAI (59 MPa) > LAC (48 MPa)) compared to the behavior obtained under alkaline conditions (LAI (6 MPa) < LAC (29 MPa)). Accordingly, the acidic products exhibited a dense structure (with lower porosity) and contained amorphous iron/aluminium phosphate phases such as berlinite (FePO{sub 4}), iron hydrogen phosphate hydrate (Fe{sub 3}H{sub 15}(PO{sub 4}){sub 8·}4H{sub 2}O), ferrowyllieite (AlFe{sub 2}Na{sub 2}(PO{sub 4}){sub 3}) and sodium iron phosphate (Na{sub 3}Fe{sub 2}(PO{sub 4}){sub 3}) arising from the alteration of iron minerals in an acidic medium, confirmed by Mössbauer spectroscopy and electron paramagnetic resonance spectroscopy.

36 MATERIALS SCIENCE↗

Influence of CaO/FeO ratio on the formation mechanism and properties of alkali-activated Fe-rich slags

Highlights: • Effect of the CaO/FeO molar ratio in alkali-activated Fe-rich slags is unraveled. • Low CaO/FeO molar ratios enhance the early kinetics and compressive strength. • Reaction extent and strength further increase with higher CaO/FeO ratio after 7 days. • Fe{sup 2+}-trioctahedral layers of the binder are hydroxylated and in a silicate phase. • The final strength is determined by the influence of Ca on the reaction products. In the search for CO{sub 2} mitigating cement technologies, alkali-activated Fe-rich slags present a possible alternative. The influence of the chemical composition of the synthetic Fe-silicate slag on the reaction mechanisms is assessed by varying the CaO/FeO molar ratio. The alkali-activated Fe-rich slags consist of trioctahedral layers that are shown to be hydroxylated and in contact with silicates, in a similar way to phyllosilicate minerals. The formation of this phyllosilicate-like structure is hindered during the first days for samples with high CaO/FeO ratios, because of the partial incorporation of Ca in the trioctahedral layers. At later ages, the samples with higher CaO/FeO ratios gain in reaction extent, to exceed the reaction extent of low CaO/FeO ratios at 28 days and beyond. The increase in compressive strength is even more pronounced than the effect on the reaction extent, which underlines the importance of Ca on the inherent strength of the binding phases.

36 MATERIALS SCIENCE↗

Multi-scale investigation on mechanical behavior and microstructural alteration of C-S-H in carbonated Alite paste

Carbonation treatment is a promising option to enhance recycled concrete aggregate (RCA) quality and eventually improve concrete performance. This study investigated the multi-scale mechanical properties of calcium silicate hydrates (C-S-H) in a mature alite paste subjected to accelerated carbonation treatment by testing macro compressive strength, microhardness and nanoindentation. The results show that, carbonation treatment resulted in a heterogeneous distribution of carbonation products in the alite sample. Reinforcement of C-S-H by the randomly precipitated calcite and vaterite crystals prevailed over the nano-structural and compositional alteration of C-S-H induced by carbonation, leading to an increase of nano-indentation modulus at the edge of the sample. Also, the microhardness at the edge zone was markedly higher than that at the core of the carbonated sample. The carbonated peripheral zone with improved nano-scale modulus and microhardness was likely serving as a “hard shell”, contributing to the improved macro compressive strength. The new insights into the multi-scale mechanical properties of carbonated C-S-H contribute to further understanding of the enhanced properties of RCA after carbonation treatment.

36 MATERIALS SCIENCE↗

Effect of bioglass 45S5 addition on properties, microstructure and cellular response of tetracalcium phosphate/monetite cements

Tetracalcium phosphate/nanomonetite (TTCPMH) cement composites with 7.5 and 15 wt% addition of melt-derived 45S5 bioactive glass were prepared by mechanical homogenization of powder components and 2% NaH{sub 2}PO{sub 4} solution was used as a hardening liquid. The properties of composites with the acidic (Ca/P ratio equal 1.5) or basic (Ca/P ratio equal 1.67) TTCPMH component were compared. Addition of glass component caused rapid rise in pH of composites up to 10. In microstructure of basic cement composite, the large bioglass particles weakly bounded to surrounding cement matrix were found contrary to a more compact microstructure of acidic cement composites with the high number of spherical silica particles. Both the significant refinement of hydroxyapatite particles and the change to needle-like morphology with rise in the content of bioglass were identified in hydroxyapatite coatings created during soaking of composites in phosphate buffered saline. In acidic cement mixtures, the increase of compressive strength with an amount of bioglass was found whereas the opposite tendency was revealed in the case of basic cement mixtures. The higher concentrations of ions were verified in solutions after immersion of acidic cement composites. The severe cytotoxicity of extracts and composite cement substrates containing 15 wt% of bioglass demonstrated adverse effects of both the ionic concentrations and unappropriate surface texture on proliferation of mesenchymal stem cells. The enhanced ALP activities of cells cultured on composite cements confirmed the positive effect of bioactive glass addition on differentiation of mesenchymal stem cells. - Highlights: • Novel B45S5 bioglass/tetracalcium phosphate/nanomonetite cement composites • Cement basicity negatively affected their microstructure. • Acid composite cements had higher compressive strengths than basic composites. • Fast differentiation of MSC to osteoblast line on composite with 7.5 wt% of bioglass • Severe cytotoxicity of 24 h extracts from composites with 15 wt% of bioglass.

36 MATERIALS SCIENCE↗

Failure strength predictions for closed-cell polyvinyl chloride foams

This paper describes an effort to model mechanical strength of closed-cell polyvinyl chloride foams under static loading. The study presented here is a continuation of an earlier study to model elastic stiffness of closed-cell polyvinyl chloride foams as effective transversely isotropic materials. An engineering approach is used in the study and governing equations are developed for predicting the strength of polyvinyl chloride foams. To account for foam microstructure and cell-shape anisotropy on foam strength, a unit cell representation of the polyvinyl chloride foam microstructure is used to derive equations to assess tensile and shear strengths of polyvinyl chloride foams. The differential stretching of polyvinyl chloride foam cell walls (in the rise direction and in the in-plane directions) on the strength of the foam-matrix polymer is also taken into account in modeling the mechanical strength of polyvinyl chloride closed-cell foams. The behavior of closed-cell polyvinyl chloride foams under compression is different from that under tension. In the paper, the equations for predicting compressive strength of closed-cell polyvinyl chloride foams are based on an approximate theory developed in an earlier study of compressive strength of unidirectional composites. The validity of the foam strength predictive equations, derived in the paper, is first demonstrated through comparison of the predictions with the results on Divinycell H (DIAB) foams obtained from a systematic in-house test program. A comparison is also carried out between the strength predictions and the test results published by two polyvinyl chloride foam manufacturers for different density polyvinyl chloride foams. Good agreements are found for all the different density foams studied.